Morphology of W fibers and kinetic undercooling in directionally solidified NiAl–W eutectic alloy
Source abstract
Abstract
The relationship between the cross-sectional shape of W fibers and kinetic undercooling in directionally solidified (DS) NiAl–W eutectic alloys was investigated. When the growth rate was less than 8 µm/s, the cross-sectional shape of W fibers was hexagonal (faceted); conversely, when the growth rate was more than 8 µm/s, their cross-sectional shape was elliptical (nonfaceted). Meanwhile, the NiAl matrix and W fibers in DS NiAl–W eutectic alloys presented a particular crystallographic orientation. The crystallographic orientation between NiAl matrix and W fibers was [ $$ \bar{1} $$ 11]NiAl//[200]W in the growth rate of 6 µm/s, and [ $$ \bar{1} $$ 11]NiAl//[ $$ \bar{1} $$ 11]W in the growth rate of 8 µm/s. A critical kinetic undercooling $$ \Delta Tk,Wc $$ can be used to predict the transition from the faceted to nonfaceted growth of W fibers in DS NiAl–W eutectic alloys. When the kinetic undercooling $$ \Delta Tk $$ of the W phase was less than $$ \Delta Tk,Wc $$ , the W fibers’ growth was faceted with a hexagonal shape, whereas when $$ \Delta Tk > \Delta Tk,Wc $$ , the W fibers exhibited nonfaceted growth with elliptical shape.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced materials and composites · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Noebe RD, Bowman RR, Nathal MV (1993) Review of the physical and mechanical properties of the B2 compound NiAl. Int Mater Rev 38:193–23210.1179/imr.1993.38.4.193 ↗
2. Miracle DB (1993) The physical and mechanical properties of NiAl. Acta Metall Mater 41:649–68410.1016/0956-7151(93)90001-9 ↗
3. Wang YL, Jones IP, Smallman RE (2006) The effects of iron on the creep properties of NiAl. Intermetallics 14:800–81010.1016/j.intermet.2005.12.008 ↗
4. Vaerst G, Löser W, Leonhardt M, Bächer I (1995) Elemental partitioning in directionally solidified NiAl single crystals. Intermetallics 3(4):303–30810.1016/0966-9795(95)97290-H ↗
5. Milenkovic S, Schneider A, Frommeyer G (2011) Constitutional and microstructural investigation of the pseudobinary NiAl–W system. Intermetallics 19(3):342–34910.1016/j.intermet.2010.10.019 ↗
6. Joslin SM, Chen XF, Oliver BF et al (1995) Fracture behavior of directionally solidified NiAl–Mo and NiAl–V eutectics. Mater Sci Eng, A 196(1–2):9–1810.1016/0921-5093(94)09683-X ↗
7. Milenkovic S, Hassel AW, Schneider A (2006) Effect of the growth conditions on the spatial features of Re nanowires produced by directional solidification. Nano Lett 6(4):794–79910.1021/nl0514238 ↗
8. Wang L, Shen J, Zhang Y et al (2017) Microstructure evolution and room temperature fracture toughness of as-cast and directionally solidified novel NiAl–Cr (Fe) alloy. Intermetallics 84:11–1910.1016/j.intermet.2016.12.021 ↗
9. Bei H, George EP (2005) Microstructures and mechanical properties of a directionally solidified NiAl–Mo eutectic alloy. Acta Mater 53(1):69–7710.1016/j.actamat.2004.09.003 ↗
10. Milenkovic S, Drensler S, Hassel AW (2011) A novel concept for the preparation of alloy nanowires. Phys Status Solidi 208(6):1259–126410.1002/pssa.201000968 ↗
11. Hassel AW, Milenkovic S, Smith AJ (2010) Large scale synthesis of single crystalline tungsten nanowires with extreme aspect ratios. Phys Status Solidi 207(4):858–86310.1002/pssa.200983319 ↗
12. Fenster C, Smith AJ, Abts A et al (2008) Single tungsten nanowires as pH sensitive electrodes. Electrochem Commun 10(8):1125–112810.1016/j.elecom.2008.05.008 ↗
13. Rodriguez BB, Smith AJ, Hassel AW (2008) Electrodeposition of gold on tungsten nanowires present in NiAl–W eutectics. J Electroanal Chem 618(1):11–1610.1016/j.jelechem.2008.02.021 ↗
14. Hassel AW, Smith AJ, Milenkovic S (2006) Nanostructures from directionally solidified NiAl–W eutectic alloys. Electrochim Acta 52(4):1799–180410.1016/j.electacta.2005.12.061 ↗
15. Hassel AW, Bello-Rodriguez B, Milenkovic S et al (2005) Electrochemical production of nanopore arrays in a nickel aluminium alloy. Electrochim Acta 50(15):3033–303910.1016/j.electacta.2004.12.046 ↗
16. Milenkovic S, Hassel AW (2009) Spatial features control of self-organised tungsten nanowire arrays. Phys Status Solidi A 206(3):455–46110.1002/pssa.200880471 ↗
17. Hassel AW, Bello-Rodriguez B, Smith AJ et al (2010) Preparation and specific properties of single crystalline metallic nanowires. Phys Status Solidi 247(10):2380–239210.1002/pssb.201046433 ↗
18. Garmong G, Rhodes CG, Spurlemg RA (1973) Crystallography and morphology of as-grown and coarsened Al–Al3Ni directionally solidified eutectic. Metall Trans 4(3):707–71410.1007/BF02643079 ↗
19. Khan S, Elliott R (1996) Quench modification of aluminium-silicon eutectic alloys. J Mater Sci 31(14):3731–3737. https://doi.org/10.1007/BF0035278710.1007/BF00352787 ↗
20. Gao K, Li SM, Fu HZ (2014) Microstructure evolution and orientation analysis of hypereutectic Al–Al2Cu alloy under directional solidification. Acta Metall Sin 50(8):962–970
21. Flood SC, Hunt JD (1981) Modification of Al-Si eutectic alloys with Na. Metal Sci 15(7):287–29410.1179/030634581790426813 ↗
22. Miller CE (1977) Faceting transition in melt-grown crystals. J Cryst Growth 42:357–36310.1016/0022-0248(77)90218-4 ↗
23. Jian ZY, Kuribayashi K, Jie WQ (2004) Critical undercoolings for the transition from the lateral to continuous growth in undercooled silicon and germanium. Acta Mater 52(11):3323–333310.1016/j.actamat.2004.03.027 ↗
24. Jackson KA (1958) Liquid metals and solidification, vol 174. American Society for Metals, Cleveland
25. Jackson KA, Hunt JD (1966) Lamellar and rod eutectic growth. Metall Soc AIME 236:1129–1142
26. Fan QN, Wang CY, Yu T et al (2015) A ternary Ni–Al–W EAM potential for Ni-based single crystal superalloys. Phys B 456:283–29210.1016/j.physb.2014.09.012 ↗
27. Stefanescu DM (2009) Science and engineering of casting solidification, 2nd edn. Springer, Berlin, p 176
28. Fu HZ, Guo JJ, Liu L, Lin JS (2008) Directional solidification and processing of advanced materials. Science Press, Beijing, pp 223–275
29. Villars P, Prince A, Okamoto H (1997) Handbook of ternary alloy phase diagrams, 2nd Printing. ASM International, USA, p 89
30. Ponomareva AV, Isaev EI, Vekilov YK et al (2012) Site preference and effect of alloying on elastic properties of ternary B2 NiAl–based alloys. Phys Rev B 85(14):14411710.1103/PhysRevB.85.144117 ↗
31. Bayles BJ, Ford JA, Salkind MJ (1967) The effect of elevated-temperature exposure on the microstructure and tensile strength of Al3Ni whisker-reinforced aluminum. AIME Trans 239:844–849
32. Gali A, Bei H, George EP (2010) Effects of boron on the microstructure and thermal stability of directionally solidified NiAl–Mo eutectic. Acta Mater 58(2):421–42810.1016/j.actamat.2009.09.020 ↗
33. Gali A, Bei H, George EP (2009) Thermal stability of Cr–Cr3Si eutectic microstructures. Acta Mater 57(13):3823–382910.1016/j.actamat.2009.04.041 ↗
34. Cline HE, Walter JL, Lifshin E et al (1971) Structures, faults, and the rod-plate transition in eutectics. Metall Trans 2(1):189–19410.1007/BF02662656 ↗
35. Ye DL, Hu JH (2002) Thermochemical data manual of practical mineral inorganic substance, 2nd edn. China Metallurgy Press, Beijing
36. Trivedi R, Laorchan V (1988) Crystallization from an amorphous matrix-I. Morphological studies. Acta Metall 36:1941–195010.1016/0001-6160(88)90296-9 ↗
37. Rao KN, Sekhar JA (1987) Solidification of the quasi crystalline phase in the Al–Cu–Li system. Scr Metall 21:805–81010.1016/0036-9748(87)90327-9 ↗
38. Cahn JW, Hillig WB, Sears GW (1964) The molecular mechanism of solidification. Acta Metall 12:1421–143910.1016/0001-6160(64)90130-0 ↗
39. Li JF, Zhou YH (2005) Influence of interface dynamics on eutectic growth process. Sci China, Ser E Eng Mater Sci 35(5):449–458
40. Zhou YH (1998) Solidification technology. China Machine Press, Beijing, pp 36–51
41. Liu RP, Volkmann T, Herlach DM (2001) Undercooling and solidification of Si by electromagnetic levitation. Acta Mater 49(3):439–44410.1016/S1359-6454(00)00330-X ↗
42. Li D, Eckler K, Herlach DM (1996) Undercooling, crystal growth and grain structure of levitation melted pure Ge and Ge–Sn alloys. Acta Mater 44(6):2437–244310.1016/1359-6454(95)00334-7 ↗
43. Rutter JW, Chalmers B (1953) A prismatic substructure formed during solidification of metals. Can J Phys 31(1):15–3910.1139/p53-003 ↗
44. Peteves SD, Abbaschina R (1991) Growth Kinetics of Solid-Liquid Ga Interfaces: Part I. Experimental. Metall Trans A 22A:1259–127010.1007/BF02660658 ↗
45. Yilmaz F, Elliott R (1984) Faceting in the Al–CuAl2 system. J Cryst Growth 66(2):465–46810.1016/0022-0248(84)90231-8 ↗
46. Cahn JW (1960) Theory of crystal growth and interface motion in crystalline materials. Acta Metall 8:554–56210.1016/0001-6160(60)90110-3 ↗