Influence of a silicon-bearing film on the early stage oxidation of pure titanium
Source abstract
Abstract
Oxidation of pure titanium with and without silicon-bearing thin films was investigated using transmission electron microscopy, X-ray energy-dispersive spectroscopy, and nanoindentation to understand the initial stages of scale formation mechanisms. For pure titanium, results showed a two-layer oxide scale with dense outer and porous inner layers attributed to the simultaneous outward titanium and inward oxygen diffusion fluxes assessed through the use of a marker layer. Titanium specimens coated with Si before oxidation yielded a thinner oxide with an outer columnar scale and minimal porous inner oxide growth. These findings suggest that Si hinders oxygen transport to the oxide/metal interface, thus reducing overall oxide growth and oxygen ingress into the titanium metal substrate over short-term exposures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Lütjering G, Williams JC (2003) Titanium. Springer, New York10.1007/978-3-540-71398-2 ↗
2. Kofstad P, Anderson PB, Krudtaa OJ (1961) Oxidation of titanium in the temperature range 800–1200 °C. J Less Common Met 3:89–97. doi: 10.1016/0022-5088(61)90001-710.1016/0022-5088(61)90001-7 ↗
3. Stringer J (1960) The oxidation of titanium in oxygen at high temperatures. Acta Metall 8:758–766. doi: 10.1016/0001-6160(60)90170-X10.1016/0001-6160(60)90170-X ↗
4. Unnam J, Clark RK (1986) Oxidation of commercial purity titanium. Oxid Met 26:231–252. doi: 10.1007/Bf0065918610.1007/BF00659186 ↗
5. Bertrand G, Jarraya K, Chaix JM (1984) Morphology of oxide scales formed on titanium. Oxid Met 21:1–19. doi: 10.1007/Bf0065946410.1007/BF00659464 ↗
6. Lopes Gomes JE, Huntz AM (1980) Correlation between the oxidation mechanism of titanium under a pure oxygen atmosphere, morphology of the oxide scale, and diffusional phenomena. Oxid Met 14:249–261. doi: 10.1007/bf0060456710.1007/BF00604567 ↗
7. Oviedo C (1993) Oxidation-kinetics of pure titanium at low-pressures. J Phys Condens Matter 5:A153–A154. doi: 10.1088/0953-8984/5/33a/03710.1088/0953-8984/5/33A/037 ↗
8. Kofstad P (1967) High-temperature oxidation of titanium. J Less Common Met 12:449–464. doi: 10.1016/0022-5088(67)90017-310.1016/0022-5088(67)90017-3 ↗
9. Dai JJ, Zhu JY, Chen CZ, Weng F (2016) High temperature oxidation behavior and research status of modifications on improving high temperature oxidation resistance of titanium alloys and titanium aluminides: a review. J Alloys Compd 685:784–798. doi: 10.1016/j.jallcom.2016.06.21210.1016/j.jallcom.2016.06.212 ↗
10. Chaze AM, Coddet C (1987) Influence of silicon on the oxidation of titanium between 550 and 700 °C. Oxid Met 27:1–20. doi: 10.1007/Bf0065672610.1007/BF00656726 ↗
11. Rosa CJ (1982) Oxidation of Ti–1si and Ti–5si Alloys. Oxid Met 17:359–369. doi: 10.1007/Bf0074211710.1007/BF00742117 ↗
12. Vojtěch D, Bártová B, Kubatík T (2003) High temperature oxidation of titanium–silicon alloys. Mater Sci Eng A 361:50–57. doi: 10.1016/s0921-5093(03)00564-110.1016/S0921-5093(03)00564-1 ↗
13. Jiang ZL, Dai X, Middleton H (2011) Effect of silicon on corrosion resistance of Ti–Si alloys. Mater Sci Eng B Adv 176:79–86. doi: 10.1016/j.mseb.2010.09.00610.1016/j.mseb.2010.09.006 ↗
14. Li XY, Taniguchi S, Matsunaga Y, Nakagawa K, Fujita K (2003) Influence of siliconizing on the oxidation behavior of a γ-TiAl based alloy. Intermetallics 11:143–150. doi: 10.1016/s0966-9795(02)00193-010.1016/S0966-9795(02)00193-0 ↗
15. Xiong HP, Wei M, Xie YH, Cheng YY, Li XH (2005) Formation of silicide coatings on the surface of a TiAl-based alloy and improvement in oxidation resistance. Mat Sci Eng A Struct 391:10–18. doi: 10.1016/j.msea.2004.05.02610.1016/j.msea.2004.05.026 ↗
16. Taniguchi S, Kuwayama T, Zhu YC, Matsumoto Y, Shibata T (2000) Influence of silicon ion implantation and post-implantation annealing on the oxidation behaviour of TiAl under thermal cycle conditions. Mat Sci Eng A Struct 277:229–236. doi: 10.1016/S0921-5093(99)00542-010.1016/S0921-5093(99)00542-0 ↗
17. Dutta Majumdar J, Weisheit A, Mordike BL, Manna I (1999) Laser surface alloying of Ti with Si, Al and Si + Al for an improved oxidation resistance. Mater Sci Eng A 266:123–134. doi: 10.1016/s0921-5093(99)00045-310.1016/S0921-5093(99)00045-3 ↗
18. Roy TK, Balasubramaniam R, Ghosh A (1996) Determination of oxygen and nitrogen diffusivities in titanium aluminides by subscale microhardness profiling. Scr Mater 34:1425–1430. doi: 10.1016/1359-6462(96)00005-x10.1016/1359-6462(96)00005-X ↗
19. Oliver WC, Pharr GM (2011) Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology. J Mater Res 19:3–20. doi: 10.1557/jmr.2004.19.1.310.1557/jmr.2004.19.1.3 ↗
20. Okamoto H (2011) O–Ti (oxygen–titanium). J Ph Equilib Diffus 32:473–474. doi: 10.1007/s11669-011-9935-510.1007/s11669-011-9935-5 ↗
21. Salomonsen G, Norman N, Lonsjo O, Finstad TG (1990) Kinetics and mechanism of oxide formation on titanium, vanadium and chromium thin-films. J Less Common Met 158:251–265. doi: 10.1016/0022-5088(90)90060-W10.1016/0022-5088(90)90060-W ↗
22. Samimi P, Collins PC (2016) Oxidation behavior of binary Ti–xW (0 <= x <= 30, wt%) alloys at 650 degrees C as a function of W concentration. Corros Sci 111:531–540. doi: 10.1016/j.corsci.2016.05.03810.1016/j.corsci.2016.05.038 ↗
23. (2015) The interactive ellingham diagram. https://www.doitpoms.ac.uk/tlplib/ellingham_diagrams/interactive.php . Accessed 5 Apr 2017
24. Howard SM (2006) Ellingham diagrams. http://showard.sdsmt.edu/MET320/Handouts/EllinghamDiagrams/Binder_All_2009_12_06.pdf . Accessed 23 Mar 2017
25. Clevenger LA, Cabral C, Roy RA et al (1996) Formation of a crystalline metal-rich silicide in thin film titanium/silicon reactions. Thin Solid Films 289:220–226. doi: 10.1016/s0040-6090(96)08787-110.1016/S0040-6090(96)08787-1 ↗
26. Bentini GG, Nipoti R, Armigliato A, Berti M, Drigo AV, Cohen C (1985) Growth and structure of titanium silicide phases formed by thin Ti films on Si crystals. J Appl Phys 57:270–275. doi: 10.1063/1.33479910.1063/1.334799 ↗
27. Murarka SP, Fraser DB (1980) Thin film interaction between titanium and polycrystalline silicon. J Appl Phys 51:342–349. doi: 10.1063/1.32737810.1063/1.327378 ↗
28. Shalaeva EV, Borisov SV, Denisov OF, Kuznetsov MV (1999) Metastable phase diagram of Ti–Si–N(O) films (CSi < 30 at.%). Thin Solid Films 339:129–136. doi: 10.1016/s0040-6090(98)01259-010.1016/S0040-6090(98)01259-0 ↗
29. Akse JR, Whitehurst HB (1978) Diffusion of titanium in slightly reduced rutile. J Phys Chem Solids 39:457–465. doi: 10.1016/0022-3697(78)90022-710.1016/0022-3697(78)90022-7 ↗
30. Liu Z, Welsch G (1988) Literature survey on diffusivities of oxygen, aluminum, and vanadium in alpha titanium, beta titanium, and in rutile. Metall Trans A 19:1121–1125. doi: 10.1007/BF0262839610.1007/BF02628396 ↗
31. Chaze AM, Coddet C (1987) Influence of alloying elements on the dissolution of oxygen in the metallic phase during the oxidation of titanium alloys. J Mater Sci 22:1206–1214. doi: 10.1007/bf0123311010.1007/BF01233110 ↗
32. Young DJ (2016) High temperature oxidation and corrosion of metals, 2nd edn. Elsevier, Amsterdam