journal article·2007-12

Passivity breakdown of carbon steel in hot potassium carbonate solutions

S. J. Harjac, A. Atrens, C. J. Moss, V. Linton

Journal of Materials Science· Volume 42· Issue 24
Publisher page

Abstract

This research studied passivity breakdown of carbon steel in conditions typical of hot potassium carbonate (HPC) acid gas processing plants. The pitting potential, evaluated from polarisation curves, indicated resistance to pitting increased with increasing equivalent carbonate concentration. The pitting potential was much more positive than the free corrosion potential for uninhibited concentrated carbonate solutions with pH values of 8.5 to 9.5. Therefore pitting is not an issue in these solutions. However, the carbon steel was susceptible to pitting corrosion in the dilute 1.0% bicarbonate solution of pH 8.0 for chloride concentrations in excess of 0.5 wt%. The critical chloride concentration was considerably above the maximum concentration of 0.1 wt% recorded in a typical HPC plant. Consequently chlorides should not usually be of concern to plant integrity.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. American Petroleum Institute (1990) Avoiding Environmental Cracking in Amine Units, API Recommended Practice 945, 1st edn, Washington, DC
2. Harjac SJ, Atrens A, Moss CJ (2008) Eng Fail Anal, doi:10.1016/j.engfailanal.2007.05.00310.1016/j.engfailanal.2007.05.003 ↗
3. Scott B, Daniels JR, I-Meen Chao (1988) AICHE ammonia safety symposium 28, Minneapolis, p 123
4. Verduijn WD (1983) Plant/operations progress 2(3)10.1002/prsb.720020308 ↗
5. Purwonohadi P, Soeryanto J, Arun PT (1988) NGL Co, Society of Petroleum Engineers. Gas Technology Symposium, Dallas
6. Confidential Internal Santos Plant Vessel Inspection Reports (1985–2002)
7. Bienstock D, Field JH (1961) Corrosion 17(12):57410.5006/0010-9312-17.12.87 ↗
8. Harjac SJ, Atrens A, Moss CJ, Linton V (2007) J Mater Sci 42:776210.1007/s10853-007-1613-y ↗
9. Leeds JM (1986) Confidential Internal Santos Plant Correspondence
10. Jin S, Atrens A (1987) Appl Phys A 42:14910.1007/BF00616726 ↗
11. Jin S, Atrens A (1988) Appl Phys A 45:8310.1007/BF00618768 ↗
12. Jin S, Atrens A (1990) Appl Phys A 50:28710.1007/BF00324495 ↗
13. Lim AS, Atrens A (1992) Applied Physics A 54:50010.1007/BF00324328 ↗
14. Lim AS, Atrens A (1991) Applied Physics A 53:27310.1007/BF00324264 ↗
15. Evans UR (1971) Electrochimica Acta 16:182510.1016/0013-4686(71)85141-1 ↗
16. Uhlig H, Revie R (1985) Corrosion and corrosion control, 3rd edn. Wiley-Interscience
17. Nesic S, Nordsveen M, Stangeland A (2003) Corrosion 59:48910.5006/1.3277579 ↗
18. Mitrovic-Scepanovic V, MacDougall B, Graham MJ (1987) Corr Sci 3:23910.1016/0010-938X(87)90020-5 ↗
19. Streicher NA (1956) J Electrochem Soc 103:375110.1149/1.2430359 ↗
20. Milosev I et al (1992) J Electrochem Soc 139:240910.1149/1.2221241 ↗
21. Muralidara S, Saraswathy V, Thangavel K, Srinvasan S (2000) J Appl Electrochem 30:1255–125910.1023/A:1026570120698 ↗
22. Strehblow (2002) In: Marcus P (ed) Corrosion mechanisms in theory and practice, Chapt 8. Marcel Dekker Inc10.1201/9780203909188 ↗