Liquid structure of Sn-Ag-xCu solders and its effect on the formation and growth of interfacial Cu6Sn5
Source abstract
Abstract
The liquid structure of Sn-3.5Ag and Sn-3.5Ag-0.7Cu (wt%) solders was first studied using high-temperature X-ray diffraction method. Only short-range order (SRO) was detected in the liquid Sn-3.5Ag melts. However, besides SRO, medium-range order (MRO) was also detected in the liquid Sn-3.5Ag-0.7Cu melts at 260 °C and 330 °C while not at 400 °C. The MRO structure was considered to be related to Cu6Sn5-type clusters which can stably exist below 330 °C. The parameters of the ordered SRO and MRO clusters were calculated. Then, Sn-3.5Ag-xCu (x = 0, 0.7 and 1.5) solders were reflowed on Cu substrate for different durations to investigate the effect of liquid structure on the formation and growth behavior of interfacial Cu6Sn5 intermetallic compound (IMC). The Cu6Sn5 layers were found to be thicker with higher initial Cu content in the solders. It is proposed that the Cu6Sn5-type MRO clusters provided potential nuclei for the formation of Cu6Sn5, which promoted the IMC growth rate. The difference in liquid structure of the solders was regarded as a key reason for the different IMC growth rate as well as IMC type at the soldering interfaces.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Metallurgical and Alloy Processes · 3D IC and TSV technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Wang FJ, Chen H, Huang Y, Liu LT, Zhang ZJ (2019) Recent progress on the development of Sn-Bi based low-temperature Pb-free solders. J Mater Sci Mater Electron 30:3222–324310.1007/s10854-019-00701-w ↗
2. Shao HK, Wu AP, Bao YD, Zhao Y, Zou GS, Liu L (2018) Microstructure evolution and mechanical properties of Cu/Sn/Ag TLP-bonded joint during thermal aging. Mater Charact 144:469–47810.1016/j.matchar.2018.07.041 ↗
3. Huang R, Ma HR, Shang SY, Kunwar A, Wang YP, Ma HT (2019) Size effect on interface reaction of Sn-xCu/Cu solder joints during multiple reflows. J Mater Sci Mater Electron 30:4359–436910.1007/s10854-019-00758-7 ↗
4. Kim JS, Jung SB, Yoon JW (2019) Optimal Ni(P) thickness and reliability evaluation of thin-Au/Pd(P)/Ni(P) surface-finish with Sn-3.0Ag-0.5Cu solder joints. J Alloy Compd 805:1013–102410.1016/j.jallcom.2019.07.184 ↗
5. Xiong MY, Zhang L (2019) Interface reaction and intermetallic compound growth behavior of Sn-Ag-Cu lead-free solder joints on different substrates in electronic packaging. J Mater Sci 54:1741–1768. https://doi.org/10.1007/s10853-018-2907-y10.1007/s10853-018-2907-y ↗
6. Gagliano RA, Ghosh G, Fine ME (2002) Nucleation kinetics of Cu6Sn5 by reaction of molten tin with a copper substrate. J Electron Mater 31:1195–120210.1007/s11664-002-0010-1 ↗
7. Pan CC, Yu CH, Lin KL (2008) The amorphous origin and the nucleation of intermetallic compounds formed at the interface during the soldering of Sn-3.0Ag-0.5Cu on a Cu substrate. Appl Phys Lett 93:06191210.1063/1.2973148 ↗
8. Wang CH, Lin CY (2019) Minor P doping to effectively suppress IMC growth in solder joints with electroplated Co(P) metallization. J Electron Mater 48:4552–456110.1007/s11664-019-07203-9 ↗
9. Lu T, Yi DQ, Wang HX, Tu XX, Wang B (2019) Microstructure, mechanical properties, and interfacial reaction with Cu substrate of Zr-modified SAC305 solder alloy. J Alloy Compd 781:633–64310.1016/j.jallcom.2018.12.098 ↗
10. Yu DQ, Wu CML, He DP, Zhao N, Wang L, Lai JKL (2005) Effects of Cu contents in Sn-Cu solder on the composition and morphology of intermetallic compounds at a solder/Ni interface. J Mater Res 20:2205–221210.1557/JMR.2005.0275 ↗
11. Xue XY, Bian XF, Geng HX, Qin XB (2003) Structural evolution of medium range and short-range order with temperature in Cu-25 wt.% Sn. Mater Sci Eng A 363:134–13910.1016/S0921-5093(03)00636-1 ↗
12. Krogh-Moe J (1956) A method for converting experimental x-ray intensities to an absolute scale. Acta Crystallogr 9:951–95310.1107/S0365110X56002655 ↗
13. Norman N (1957) The Fourier transform method for normalizing intensities. Acta Crystallogr 10:370–37310.1107/S0365110X57001085 ↗
14. Cromer DT, Mann JB (1967) Compton scattering factors for spherically symmetric free atoms. J Chem Phys 47:1892–189310.1063/1.1712213 ↗
15. Waseda Y (1980) The structure of non-crystalline materials. McGraw-Gill, New York
16. Ashcroft NW, Langreth DC (1967) Structure of binary liquid mix-tures. Phys Rev 156:685–69210.1103/PhysRev.156.685 ↗
17. Sadigh B, Dzugutov M, Elliot SR (1999) Vacancy ordering and medium-range structure in a simple liquid. Phys Rev B 59:1–410.1103/PhysRevB.59.1 ↗
18. Kaban I, Hoyer W, Il’inskii A, Slukhovskii O, Slyusarenko S (2003) Short-range order in liquid silver-tin alloys. J Non-Cryst Solids 331:254–26210.1016/j.jnoncrysol.2003.09.001 ↗
19. Vateva E, Savova E (1995) New medium-range order features in Ge-Sb-S glasses. J Non-Cryst Solids 192–193:145–14810.1016/0022-3093(95)00435-1 ↗
20. Sokolov AP, Kisliuk A, Soltwisch M, Quitmann D (1992) Medium-range order in glasses: comparison of Raman and diffraction measurements. Phys Rev Lett 69:1540–154310.1103/PhysRevLett.69.1540 ↗
21. Elliott SR (1991) Medium-range structural order in covalent amorphous solids. Nature 354:445–45210.1038/354445a0 ↗
22. Zhao Y, Bian XF, Qin XB, Qin JY, Hou XX (2007) Structural properties and evolution in the solidification process of Cu-Ag alloys. J Non-Cryst Solids 353:1177–118710.1016/j.jnoncrysol.2006.12.021 ↗
23. Schaefer M, Fournelle RA, Liang J (1998) Theory for intermetallic phase growth between Cu and liquid Sn-Pb solder based on grain boundary diffusion control. J Electron Mater 27:1167–117610.1007/s11664-998-0066-7 ↗
24. Gusak AM, Tu KN (2002) Kinetic theory of flux-driven ripening. Phys Rev B 66:11540310.1103/PhysRevB.66.115403 ↗
25. Huang ML, Loeher T, Ostmann A, Reichl H (2005) Role of Cu on dissolution kinetics of Cu metallization in molten Sn-based solders. Appl Phys Lett 86:18190810.1063/1.1925317 ↗