Enzymatic degradation and radiopaque attenuation of iodinated poly(ester-urethane)s with inherent radiopacity
Source abstract
Abstract
Biodegradable radiopaque iodinated polyurethanes (I-PUs) based on poly(e-caprolactone) diol (PCL) as soft segment have been synthesized using 4,4′-isopropylidene-(2,6-diiodophenol) (IBPA) as chain extender. In order to elucidate the effect of iodinated chain extender on degradation properties of I-PUs, a control polyurethane with bisphenol A as chain extender was also synthesized. The enzymatic degradation study of these I-PUs was carried out using phosphate-buffered solution (pH 7.4) at 37 °C. The mass loss, surface morphology, iodine content, radiopacity, hydrophilicity and thermal properties of the samples during degradation were characterized with scanning electron microscopy (SEM), energy-dispersive X-ray detector (EDX), differential scanning calorimetry (DSC), X-ray diffraction (XRD) and static contact angle. Results of enzymatic degradation during 3 months indicated that the incorporation of iodinated chain extender greatly hindered the in vitro degradation of I-PUs compared with the control PU-C sample. The reason for the retarded degradation was attributed to the bulky iodine atoms on IBPA chain extender with steric hindrance, which decreased the surface hydrophilicity of I-PUs and slowed water/lipase diffusion rate. Moreover, the radiopacity of I-PUs does not sharply attenuate after long-time degradation, which is useful for interventional biomedical applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: biodegradable polymer synthesis and properties · Orthopaedic implants and arthroplasty · Polymer composites and self-healing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Werkmeister JA, Adhikari R, White JF, Tebb TA, Le TPT, Taing HC, Mayadunne TR, Gunatillake PA, Danon S, Ramshaw JAM (2010) Biodegradable and injectable cure-on-demand polyurethane scaffolds for regeneration of articular cartilage. Acta Biomater 6(9):3471–348110.1016/j.actbio.2010.02.040 ↗
2. Tang YW, Labow RS, Santerre JP (2001) Enzyme-induced biodegradation of polycarbonate polyurethanes: dependence on hard-segment concentration. J Biomed Mater Res 56:516–52810.1002/1097-4636(20010915)56:4<516::AID-JBM1123>3.0.CO;2-B ↗
3. Szycher M, Siciliano AA, Reed AM (1994) Polyurethane elastomers in medicine. In: Dumitriu S (ed) Polymeric Biomaterials. Marcel Dekker, New York, pp 233–244
4. Lelah MD, Cooper SL (1986) Polyurethanes in Medicine. CRC Press, Boca Raton
5. Aviv H, Bartling S, Kieslling F, Margel S (2009) Radiopaque iodinated copolymeric nanoparticles for X-ray imaging applications. Biomaterials 30(29):5610–561610.1016/j.biomaterials.2009.06.038 ↗
6. James NR, Jayakrishnan A (2007) On imparting radiopacity to a poly (urethane urea). Biomaterials 28(21):3182–318710.1016/j.biomaterials.2007.03.025 ↗
7. Ponsart S, Coudane J, Vert M (2000) A novel route to poly (ε-caprolactone)-based copolymers via anionic derivatization. Biomacromolecules 1(2):275–28110.1021/bm005521t ↗
8. Mawad D, Mouaziz H, Penciu A, Méhier H, Fenet B, Fessi H, Chevalier Y (2009) Elaboration of radiopaque iodinated nanoparticles for in situ control of local drug delivery. Biomaterials 30:5667–567410.1016/j.biomaterials.2009.06.027 ↗
9. Subrata M, Darren M (2012) Hydrolytic degradation of segmented polyurethane copolymers for biomedical applications. Polym Degrad Stab 97(8):1553–156110.1016/j.polymdegradstab.2012.04.008 ↗
10. Gunatillake P, Mayadunne R, Adhikari R (2006) Recent developments in biodegradable synthetic polymers. Biotech Annu Rev 12:301–34710.1016/S1387-2656(06)12009-8 ↗
11. Kavlock KD, Pechar TW, Hollinger JO, Guelcherand SA, Goldstein AS (2007) Synthesis and characterization of segmented poly(esterurethane urea) elastomers for bone tissue engineering. Acta Biomater 3(4):475–48410.1016/j.actbio.2007.02.001 ↗
12. Guan JJ, Sacks MS, Beckmanand EJ, Wagner WR (2002) Synthesis, characterization, and cytocompatibility of elastomeric, biodegradable poly(ester-urethane) ureas based on poly(caprolactone) and putrescine. J Biomed Mater Res A 61(3):493–50310.1002/jbm.10204 ↗
13. Pan J, Li G, Chen Z, Chen X, Zhu W, Xu K (2009) Alternative block polyurethanes based on poly(3-hydroxybutyrate- co-4-hydroxybutyrate) and poly(ethylene glycol). Biomaterials 30(16):2975–298410.1016/j.biomaterials.2009.02.005 ↗
14. Kausar A, Zulfiqar S, Yavuz CT, Ilyas Sarwar MI. Investigation on novel thermoplastic poly(urethane-thiourea- imide)s with enhanced chemical and heat resistance. Polym Degrad Stab 2011; 96(7): 1333–134110.1016/j.polymdegradstab.2011.03.017 ↗
15. Stefan O (2010) Dependence of fungal biodegradation of PEG/castor oil-based polyurethane elastomers on the hard-segment structure. Polym Degrad Stab 95(12):2396–240410.1016/j.polymdegradstab.2010.08.013 ↗
16. Bueno-Ferrer C, Hablot E, Garrigos MC, Bocchini S, Averous L, Jimenez A (2012) Relationship between morphology, properties and degradation parameters of novative biobased thermoplastic polyurethanes obtained from dimer fatty acids. Polym Degrad Stab 97(10):1964–196910.1016/j.polymdegradstab.2012.03.002 ↗
17. James NR, Philip J, Jayakrishnan A (2006) Polyurethanes with radiopaque properties. Biomaterials 27:160–16610.1016/j.biomaterials.2005.05.099 ↗
18. Kiran S, James NR, Joseph R, Jayakrishnan A (2009) Synthesis and characterization of iodinated polyurethane with inherent radiopacity. Biomaterials 30(29):5552–555910.1016/j.biomaterials.2009.06.049 ↗
19. Kiran S, James NR, Jayakrishnan A, Joseph R (2012) Polyurethane thermoplastic elastomers with inherent radiopacity for biomedical applications. J Biomed Mater Res A 100(12):3472–347910.1002/jbm.a.34295 ↗
20. Qu WQ, Xia WJ, Feng C, Tuo XL, Qiu T (2011) Synthesis and characterization of radiopaque poly(ether urethane) with iodine-containing diol as chain extender. J Polym Sci A 49(10):2191–219810.1002/pola.24649 ↗
21. Hu JL, Mondal S (2005) Structural characterization and mass transfer properties of segmented polyurethane: influence of block length of hydrophilic segments. Polym Int 54(5):764–77110.1002/pi.1753 ↗
22. Kiran S, Joseph R (2014) Synthesis and characterization of a noncytotoxic, X-ray opaque polyurethane containing iodinated hydroquinone bis(2-hydroxyethyl) ether as chain extender for biomedical applications. J Biomed Mater Res A 102(9):3207–3215.10.1002/jbm.a.34997 ↗
23. Sang L, Wei Z, Liu K, Wang X, Song K, Wang H, Qi M (2014) Biodegradable radiopaque iodinated poly(ester urethane)s containing poly(ε-caprolactone) blocks: Synthesis, characterization, and biocompatibility. J Biomed Mater Res A 102(4):1121–113010.1002/jbm.a.34777 ↗
24. Gu XZ, Wu J, Mather PT (2011) Polyhedral oligomeric silsesquioxane (POSS) suppresses enzymatic degradation of PCL-based polyurethanes. Biomacromolecules 12(8):3066–307710.1021/bm2006938 ↗
25. Tatai L, Moore TG, Adhikari R, Malherbe F, Jayasekara R, Griffiths I, Gunatillake PA (2007) Thermoplastic biodegradable polyurethanes: the effect of chain extender structure on properties and in vitro degradation. Biomaterials 28(36):5017–540710.1016/j.biomaterials.2007.08.035 ↗
26. Li S, Girard A, Garreau H, Vert M (2001) Enzymatic degradation of polylactide stereocopolymers with predominant D-lactyl contents. Polym Degrad Stab 71(1):61–6710.1016/S0141-3910(00)00152-X ↗
27. ASTM F640, Test methods for determining radiopacity for medical use. West Conshohocken, PA: ASTM Int.; 2007
28. Cortecchia E, Pacilli A, Pasquinelli G, Scandola M (2010) Biocompatible two-layer tantalum/titania-polymer hybrid coating. Biomacromolecules 11(9):2446–245310.1021/bm100619t ↗
29. Liu L, Li S, Garreau H, Vert M (2000) Selective enzymatic degradations of Poly(L-lactide) and poly(3-caprolactone) blend films. Biomacromolecules 1(3):350–35910.1021/bm000046k ↗
30. von Recum HA, Cleek RL, Eskin SG, Mikos AG (1995) Degradation of polydispersed poly(L-lactic acid) to modulate lactic acid release. Biomaterials 16(6):441–44710.1016/0142-9612(95)98816-W ↗
31. Luo YB, Wang XL, Wang YZ (2012) Effect of TiO2 nanoparticles on the long-term hydrolytic degradation behavior of PLA. Polym Degrad Stab 97(5):721–72810.1016/j.polymdegradstab.2012.02.011 ↗
32. Chang WL. Polyester-based polyurethane elastomers having excellent hydrolytic stability. In: Proceedings of the polyurethanes world congress’97, Amsterdam, Sept 29eOct. 1. Technomic Publ. Co. Inc.; 1997. pp. 705–710duhduh
33. Salazar MR, Thompson SL, Laintz KE, Pack RT (2002) Degradation of a poly(ester urethane) elastomer. I. Absorption and diffusion of water in estane@5703 and related polymers. J Polym Sci B 40(2):181–19110.1002/polb.10079 ↗
34. Gopferich A (1996) Mechanisms of polymer degradation and erosion. Biomaterials 17(2):103–11410.1016/0142-9612(96)85755-3 ↗
35. Aharoni SM (1998) Increased glass transition temperature in motionally constrained semicrystalline polymers. Polym Adv Techol 9(3):169–20110.1002/(SICI)1099-1581(199803)9:3<169::AID-PAT740>3.0.CO;2-Z ↗
36. Bei JZ, Li JM, Wang ZF, Le JC, Wang SG (1997) Polycaprolactone poly(ethylene-glycol) block copolymer. IV: biodegradation behaviour in vitro and in vivo. Polym Adv Techol 8(11):693–69610.1002/(SICI)1099-1581(199711)8:11<693::AID-PAT702>3.0.CO;2-B ↗
37. Huang YY, Qi M, Liu HZ, Zhao H, Yang DZ (2007) Degradation of porous poly (D, L-lactic-co-glycolic acid) films based on water diffusion. J Biomed Mater Res A 80(4):909–91510.1002/jbm.a.30980 ↗