Densification and phase formation in seeded, reactively sintered Sr0.53Ba0.47Nb2O6 ceramics
Source abstract
Abstract
Sr0.53Ba0.47Nb2O6 (SBN53) ceramics were reactively sintered from SrNb2O6 and BaNb2O6 powders. The formation temperature decreased from 1260°C for unseeded samples to 1130°C for the samples with 15.4 wt% seeds plus 0.85 mol% V2O5 at a heating rate of 4°C/min. For the V2O5-free samples, the activation energy was lowered from 554 ± 15 kJ/mol for unseeded samples to 241 ± 17 kJ/mol for the samples with 15.4 wt% seeds. In the V2O5-containing samples, densification and phase formation occurred simultaneously. In the V2O5-free samples, however, phase formation was completed before densification. In both cases, ceramics with ≥95% relative density were obtained. In all cases, SBN53 formed directly, rather than via a variety of intermediate SBN solid solutions. The microstructure evolution was also studied.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. M. N. Rahaman and L. C. DE jonghe, J. Amer. Ceram. Soc. 76 (1993) 1739.10.1111/j.1151-2916.1993.tb06642.x ↗
2. S. Yangyun and R. J. Brook, Sci. Sintering 17 (1985) 35.
3. W.-S. Hong, L. C. DE jonghe, X. Yang and M. N. Rahaman, J. Amer. Ceram. Soc. 78 (1995) 3217.10.1111/j.1151-2916.1995.tb07957.x ↗
4. W.-J. Lee and T.-T. Fang, ibid. 81 (1998) 1019.10.1111/j.1151-2916.1998.tb02440.x ↗
5. H.-Y. Lee and R. Freer, J. Appl. Phys. 81 (1997) 376.10.1063/1.364122 ↗
6. H.-Y. Lee and R. Freer, J. Mater. Sci. 33 (1998) 1703.10.1023/A:1004312128588 ↗
7. T.-T. Fang, N.-T. Wu and F.-S. Shiau, J. Mater. Sci. Lett. 13 (1994) 1746.10.1007/BF00776344 ↗
8. R. R. Neurgaonkar, W. K. Cory and J. R. Oliver, Ferroelectrics 51 (1983) 3.10.1080/00150198308009045 ↗
9. R. R. Neurgaonkar, J. R. Oliver and L. E. Cross, ibid. 56 (1984) 31.10.1080/00150198408012713 ↗
10. R. R. Neurgaonkar, W. W. Ho, W. K. Cory, W. F. Hall and L. E. Cross, ibid. 51 (1984) 185.10.1080/00150198408232554 ↗
11. S. Nishiwaki, J. Takahashi and K. Kodaira, J. Ceram. Soc. Japan, Int. Edition 103 (1995) 1233.10.2109/jcersj.103.1233 ↗
12. S. Nishiwaki, J. Takahashi and K. Kodaira, Jpn. J. Appl. Phys. 33 (1994) 5477.10.1143/JJAP.33.5477 ↗
13. S. Nishiwaki, J. Takahashi and K. Kodaira, J. Ceram. Soc. Japan, Int. Edition 104 (1996) 413.10.2109/jcersj.104.435 ↗
14. W.-J. Lee and T.-T. Fang, J. Amer. Ceram. Soc. 81 (1998) 193.10.1111/j.1151-2916.1998.tb02313.x ↗
15. R. R. Neurgaonkar, W. K. Cory, J. R. Oliver, E. J. Sharp, G. L. Wood and G. J. Salamo, Ferroelectrics 142 (1993) 167.10.1080/00150199308237896 ↗
16. K. C. Mouli, K. H. Rao, P. S. V. Subba rao and A. Bhanumathi, ibid. 67 (1986) 169.10.1080/00150198608245019 ↗
17. T. Kimura, S. Saiubol and K. Nagata, J. Ceram. Soc. Japan, Int. Edition 103 (1995) 132.10.2109/jcersj.103.132 ↗
18. P. F. StableinJr. and G. C. Kuczynski, Acta Metall. 11 (1963) 1327.10.1016/0001-6160(63)90027-0 ↗
19. G. C. Kuczynski, in “Sintering and Related Phenomena,” edited by G. C. Kuczynski, N. A. Hooton and C. F. Gibbon (Gordon and Breach, NY, 1967) p. 685.