A critical damage criterion for creeping solids
Source abstract
Abstract
Creep damage is the progressive reduction in the material’s ability to resist stress and is manifested as an increase in creep rate during tertiary creep eventually resulting in failure. Monkman–Grant relationship [1] that has contributed significantly to the development of creep fracture models [2], relates minimum creep rate em and rupture life tr as emtr = constant = CMG, for which, we provided a physical basis in terms of first order kinetics for creep [3–6]. In the present study, Monkman–Grant constant CMG is henceforth referred to as ‘Monkman–Grant Ductility (MGD)’ that is the contribution of secondary creep strain to strain to failure, ef (Fig. 1). Monkman–Grant relation does not describe evolution of damage and its coupling to the deformation rate. The two approaches that describe this coupling are ‘Continuum Creep Damage Mechanics (CDM)’ by Kachanov–Rabotnov [7, 8] and ‘Materials Properties Council (MPC)-Omega’ by Prager [9]. CDM treats damage as an internal state variable and an important outcome is the creep damage tolerance factor λ [10, 11] defined as ratio of ef to MGD (Fig. 1) i.e., λ = ef/(emtr) and is a constant. λ is suggested [10] to be a better measure of creep ductility as it assesses the susceptibility of a material to localized cracking at strain concentrations [12], and thus can be considered as a material performance characteristic. Ashby and Dyson [11] provided a physical basis to CDM approach and demonstrated that each damage micromechanism, when acting alone, results in a characteristic value of λ. According to MPC-Omega approach [9], creep rate e from its initial value e0 increases with strain e as e = e0 exp( pe), where p is reciprocal of MGD, i.e., p = 1/(emtr) for conditions showing negligible primary creep. The total damage coefficient p is the rate at which material’s ability to resist stress is degraded by strain and is a material performance characteristic that is related to creep damage tolerance, i.e., higher the p, lesser is the resistance to creep damage. In this paper, we identify that MGD is the critical strain at which true tertiary creep damage sets in and further introduces the concept of tMGD (Fig. 1) as the time at which MGD is reached along the creep curve and the total secondary creep ductility is exhausted. tMGD can be obtained as the time at which e − ep = MGD, ep is the limiting primary creep strain, and for negligible ep as shown in Fig. 1, tMGD is the time to reach MGD. Damage evolves along the creep curve and for any damage mechanism, we put forward that tMGD is the time at which damage attains a critical level, beyond which its accelerated growth leads to failure. For a typical case of cavitation mechanism, it is shown that time to reach critical cavity size tCCS matches well with tMGD. We propose a critical damage criterion based on CDM as well as MPC-Omega method in terms of a unique relationship between tMGD and tr that depends only on λ. Further, we demonstrate its universal applicability for a wide range of materials and discuss its implications to engineering creep design. In order to validate our proposition that tMGD is the time at which damage attains a critical level, we analyse the mechanistic data reported by Davis and Williams [13] on α-iron at various temperatures (815–978 K) and stress levels (17.24–68.95 MPa). They observed a two stage tertiary creep behaviour; in the first stage, tertiary creep strain-time followed a t4/3 law, whereas the second stage obeyed an exponential law. They concluded that the end of first stage corresponds to the time at which creep cavities attain a critical size and the second stage is the ‘true tertiary creep’. Accordingly, the time corresponding to the end of first stage is designated as time to attain critical cavity size tCCS. Creep curves that include secondary and tertiary creep regimes were generated using creep data as well as the tertiary creep strain–time relations given by Davis and Williams [13]. ef was obtained as the sum of ep, MGD and et (cf. Fig. 1), where et was calculated as et = A exp[β(tr − tot)] and the constant reported value [14] of ep was taken as 0.051. From the generated creep curves, λ (discussed later) and tMGD were determined; tMGD was obtained as the time at which e − ep = MGD. The plot of tCCS vs. tMGD in Fig. 2 demonstrates that tCCS matches well with tMGD and validates our proposition of tMGD as the time at which creep damage attains a critical level. We like to extend such a validation for other damage mechanisms, but it has not been possible due to the lack of mechanistic data. Further, when two coupled mechanisms operate as in the case of nickel base superalloys [12], we suggest that tMGD might correspond to the time at which cavitation intervenes the strain softening mechanism causing true tertiary creep damage. Based on CDM approach, recently we proposed [15] a new relationship between tMGD and tr in terms of λ, and a brief description is given here. According to CDM, the evolution of deformation and damage is expressed in terms of internal state damage variable ω and for uniaxial stressing [12, 16] e = e0 (σ/σ0)
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Fire effects on concrete materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. F. C. MONKMAN and N. J. GRANT, in Proceedings of American Society for Testing of Materials (ASTM), Philadelphia 56 (1956) 593.
2. A. C. F. COCKS and M. F. ASHBY, Prog. Mater. Sci. 27 (1982) 189.10.1016/0079-6425(82)90001-9 ↗
3. C. PHANIRAJ, M. NANDAGOPAL, S. L. MANNAN and P. RODRIGUEZ, Acta Metall. Mater. 39 (1991) 1651.10.1016/0956-7151(91)90253-W ↗
4. C. PHANIRAJ, M. NANDAGOPAL, S. L. MANNAN, P. RODRIGUEZ and B. P. KASHYAP, Acta Mater. 44 (1996) 4059.10.1016/S1359-6454(96)00023-7 ↗
5. B. K. CHOUDHARY, C. PHANIRAJ, M. NANDAGOPAL and S. L. MANNAN, Key Eng. Mater. 171–174 (2000) 437.
6. Idem., ISIJ Inter. Suppl. 41 (2001) S73.10.2355/isijinternational.41.Suppl_S73 ↗
7. L. M. KACHANOV, Izv. Akad. Nauk. USSR, Otd Tekd Nauk. 8 (1958) 26.
8. Y. N. RABOTNOV, in “Creep Problems in Structural Members” (North Holland, Amsterdam, 1969).
9. M. PRAGER, J. Press. Vessel Technol., Trans. ASME 117 (1995) 95.10.1115/1.2842111 ↗
10. F. A. LECKIE and D. R. HAYHURST, Acta Metall. 25 (1977) 1059.10.1016/0001-6160(77)90135-3 ↗
11. M. F. ASHBY and B. F. DYSON, “Advances in Fracture Research”, edited by S. R. Valluri et al. (Pergamon Press, Oxford, 1984), Vol. 1, p. 3.
12. B. F. DYSON and T. B. GIBBONS, Acta Metall. 35 (1987) 2355.10.1016/0001-6160(87)90083-6 ↗
13. P. W. DAVIS and K. R. WILLIAMS, ibid. 17 (1969) 897.10.1016/0001-6160(69)90110-2 ↗
14. G. A. WEBSTER, A. P. D. COX and J. E. DORN, Metal Sci. J. 3 (1969) 221.10.1179/msc.1969.3.1.221 ↗
15. C. PHANIRAJ, B. K. CHOUDHARY, K. BHANU SANKARA RAO and BALDEV RAJ, Scripta Mater. 48 (2003) 1313.10.1016/S1359-6462(03)00021-6 ↗
16. F. A. LECKIE and D. R. HAYHURST, Proc. Roy. Soc. London Ser. A. 340A (1974) 323.10.1098/rspa.1974.0155 ↗
17. B. K. CHOUDHARY, S. SAROJA, K. BHANU SANKARA RAO and S. L. MANNAN, Metall. Mater. Trans. A 30 (1999) 2825.10.1007/s11661-999-0120-y ↗
18. J. B. CONWAY and P. N. FLAGELLA, in “Creep-Rupture Data for the Refractory Metals to High Temperatures” (Gordon and Breach, New York, 1971).
19. J. D. PARKER and B. WILSHIRE, Mater. Sci. Eng. 43 (1980) 271.10.1016/0025-5416(80)90113-5 ↗
20. R. R. HOUGH and R. ROLLS, Metal Sci. J. 5 (1971) 206.10.1179/030634571790439603 ↗
21. A. G. ROBERTSON, D. S. WILKINSON and C. H. CACERES, J. Amer. Ceram. Soc. 74 (1991) 915.10.1111/j.1151-2916.1991.tb04322.x ↗
22. T. TANAKA et al., in “Fracture Mechanics of Ceramics—Fracture Fundamentals, High Temperature Deformation, Damage, and Design”, edited by R. C. Bradt et al. (Plenum Press, New York, 1992), Vol. 10, p. 473.10.1007/978-1-4615-3348-1_31 ↗
23. J. D. FRENCH, S. M. WEIDERHORN and J. J. PETROVIC, in “High Temperature Silicides and Refractory Alloys”, Material Research Society Symposium, edited by C. L. Briant et al. (Materials Research Society, Pittsburgh, 1994), Vol. 322, p. 203.
24. ASME Boiler and Pressure Vessel Code, Section VIII, Division 1 and Section III, Division 1, Subsection NH (Class I Components in Elevated Temperatures Service), 2001.
25. D. A. WOODFORD, in “Materials Selection and Design”, ASM Handbook (ASM International, 1997), Vol. 20, p. 573.
26. R. VISWANATHAN, in “Damage Mechanisms and Life Assessment of High Temperature Components” (ASM, Metals Park, 1989).10.31399/asm.tb.dmlahtc.9781627083409 ↗