Abstract

Evaluating the adhesion of micrometer or nanometer thick coatings is a challenging question which concerns many application fields. This is especially true for thin films deposited on a substrate of elastic modulus higher than that of the film, or for granular coatings, that do not allow the use of common adhesion tests. Usually, applied to characterize the wear resistance of bulk materials or thick coatings, the ultrasonic cavitation test is applied here to evaluate the adhesion strength of gold and copper thin films (~200 nm) that are evaporated on a silicon substrate. The test is shown to be sensitive enough to discriminate the influence of the surface chemistry on the adhesion strength of gold and copper films. Particularly, the role of (3-mercaptopropyl)triethoxysilane as an effective adhesion promotor is demonstrated. Furthermore, the role of surface roughness of the substrate is characterized and discussed in order to get further insights on the way this parameter interferes with the ultrasonic test and determines the adhesive strength of the coating. An estimate of the adhesive strength is given on the basis of the coating delamination kinetics.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Molecular Junctions and Nanostructures · Force Microscopy Techniques and Applications · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (66)

Show source-provided references
1. Mittal KL (1995) Adhesion measurement of films and coatings. VSP, Utrecht
2. Mohseni E, Zalnezhad E, Bushroa AR (2014) Comparative investigation on the adhesion of hydroxyapatite coating on Ti–6Al–4V implant: a review paper. Int J Adhes Adhes 48:238–257. doi: 10.1016/j.ijadhadh.2013.09.03010.1016/j.ijadhadh.2013.09.030 ↗
3. Vencl A, Arostegui S, Favaro G, Zivic F, Mrdak M, Mitrović S, Popovic V (2011) Evaluation of adhesion/cohesion bond strength of the thick plasma spray coatings by scratch testing on coatings cross-sections. Tribol Int 44:1281–1288. doi: 10.1016/j.triboint.2011.04.00210.1016/j.triboint.2011.04.002 ↗
4. Mittal KL (1995) Adhesion measurement of films & coatings: vol 2. VSP, Utrecht
5. Sinha SKK (2006) Scratching of materials and applications. Elsevier B.V, Amsterdam
6. Yaghoubi H, Taghavinia N, Alamdari EK, Volinsky AA (2010) Nanomechanical properties of TiO2 granular thin films. ACS Appl Mater Interfaces 2:2629–2636. doi: 10.1021/am100455q10.1021/am100455q ↗
7. Steller J (1999) International cavitation erosion test and quantitative assessment of material resistance to cavitation. Wear 233–235:51–64. doi: 10.1016/S0043-1648(99)00195-710.1016/S0043-1648(99)00195-7 ↗
8. NAG/DAGA (2009) International Conference on Acoustics, Rotterdam, 23–26 March 2009
9. Karimi A, Martin JL (1986) Cavitation erosion of materials. Int Met Rev 31:1–2610.1179/imr.1986.31.1.1 ↗
10. Chen Y, Huang L, Shih T (2003) Diagnosis of oxide films by cavitation micro-jet impact. Mater Trans 44:327–33510.2320/matertrans.44.327 ↗
11. Reisman GE, Brennen CE (1996) Pressure pulses generated by cloud cavitation. In: Fluids engineering division conference ASME, pp 319–328
12. Chahine GL (1984) Pressure generated by a bubble cloud collapse. Chem Eng Commun 28:355–36710.1080/00986448408940143 ↗
13. Kwok CT, Cheng FT, Man HC (1998) Laser surface modification of UNS S31603 stainless steel using NiCrSiB alloy for enhancing cavitation erosion resistance. Surf Coat Technol 107:31–40. doi: 10.1016/S0257-8972(98)00549-010.1016/S0257-8972(98)00549-0 ↗
14. Krella A, Czyżniewski A (2009) Cavitation resistance of Cr–N coatings deposited on austenitic stainless steel at various temperatures. Wear 266:800–809. doi: 10.1016/j.wear.2008.11.00210.1016/j.wear.2008.11.002 ↗
15. Chang JT, Yeh CH, He JL, Chen KC (2003) Cavitation erosion and corrosion behavior of Ni–Al intermetallic coatings. Wear 255:162–169. doi: 10.1016/S0043-1648(03)00199-610.1016/S0043-1648(03)00199-6 ↗
16. Lin CJ, Chen KC, He JL (2006) The cavitation erosion behavior of electroless Ni–P–SiC composite coating. Wear 261:1390–1396. doi: 10.1016/j.wear.2006.03.05410.1016/j.wear.2006.03.054 ↗
17. Vallat M-F, Haidara H, Ziegler P, Rey D, Papirer Y, Schultz J (1996) Adhesive behavior of aluminum layers evaporated on polyester films. In:The proceedings of the 53rd international meeting of physical chemistry: Organic coatings, vol 354. pp 14–2210.1063/1.49489 ↗
18. Haidara H, Vallat M, Schultz J (1989) Mesure de l’adhésion de couches minces par vibrations ultrasoniques. Comptes rendus de l’Académie des Sciences 309:1653–1657
19. Pigerre J (2004) Flash test development using ultrasonics for fast qualification of the mechanical resistance of industrial organic coatings Part I: methodological approach. Prog Org Coat 50:132–137. doi: 10.1016/j.porgcoat.2004.01.00410.1016/j.porgcoat.2004.01.004 ↗
20. Pigerre J, Rodriguez P, Mehinto T, Mansot J, Roos C (2005) Development of an ultrasonics-based flash test used for fast qualification of the mechanical resistance of industrial organic coatings Part II: comparative results. Prog Org Coat 54:377–383. doi: 10.1016/j.porgcoat.2005.07.00910.1016/j.porgcoat.2005.07.009 ↗
21. Fernandez Rivas D, Verhaagen B, Seddon JRT, Zijlstra AG, Jiang L-M, Van der Sluis LWM, Versluis M, Lohse D, Gardeniers HJGE (2012) Localized removal of layers of metal, polymer, or biomaterial by ultrasound cavitation bubbles. Biomicrofluidics 6:34114. doi: 10.1063/1.474716610.1063/1.4747166 ↗
22. Suhir E, Lee YC, Wong CP (2007) Micro- and opto-electronic materials and structures: physics, mechanics, design, reliability, packaging: materials physics—materials mechanics, vol 1. Springer, Boston
23. Ronald AC, Paul EK, Kevin DL, Robert LC (2004) Selecting metal alloy electric contact materials for MEMS switches. J Micromech Microeng 14:1157–116410.1088/0960-1317/14/8/006 ↗
24. Holloway PH, Nelson CC (1976) In situ formation of diffusion barriers in thin film metallization systems. Thin Solid Films 35:13–1610.1016/0040-6090(76)90233-9 ↗
25. Ono H, Nakano T, Ohta T (1994) Diffusion barrier effects of transition metals for Cu/M/Si multilayers (M = Cr, Ti, Nb, Mo, Ta, W). Appl Phys Lett 64:1511–1513. doi: 10.1063/1.11187510.1063/1.111875 ↗
26. Miller D, Herrmann C, Maier H, George S, Stoldt C, Gall K (2005) Intrinsic stress development and microstructure evolution of Au/Cr/Si multilayer thin films subject to annealing. Scripta Mater 52:873–879. doi: 10.1016/j.scriptamat.2005.01.00410.1016/j.scriptamat.2005.01.004 ↗
27. Munitz A, Komem Y (1984) Electrical resistance and Auger electron spectroscopy characteristics of interdiffusion in Au/metal bilayer films. Thin Solid Films 112:139–14710.1016/0040-6090(84)90491-7 ↗
28. Holloway PH, Amos DE, Nelson GC (1976) Analysis of grain-boundary diffusion in thin films: chromium in gold. J Appl Phys 47:3769. doi: 10.1063/1.32325910.1063/1.323259 ↗
29. Love JC, Estroff L, Kriebel JK, Nuzzo RG, Whitesides GM (2005) Self-assembled monolayers of thiolates on metals as a form of nanotechnology. Chem Rev 105:1103–1169. doi: 10.1021/cr030078910.1021/cr0300789 ↗
30. Kim H, Boiadjiev V, Houston J, Zhu X, Kiely J (2001) Tribological properties of self-assembled monolayers on Au, SiOx and Si surfaces. Tribol Lett 10:97–10110.1023/A:1009014010006 ↗
31. Lee K-H, Huang K-M, Tseng W-L, Chiu T-C, Lin Y-W, Chang H-T (2007) Manipulation of the growth of gold and silver nanomaterials on glass by seeding approach. Langmuir 23:1435–1442. doi: 10.1021/la061880j10.1021/la061880j ↗
32. Brito R, Rodríguez V, Figuero J, Cabrera C (2002) Adsorption of 3-mercaptopropyltrimethoxysilane and 3-aminopropyltrimethoxysilane at platinum electrodes. J Electroanal Chem 520:47–5210.1016/S0022-0728(01)00718-5 ↗
33. Ganesan PG, Kumar A, Ramanath G (2005) Surface oxide reduction and bilayer molecular assembly of a thiol-terminated organosilane on Cu. Appl Phys Lett 87:011905. doi: 10.1063/1.196841410.1063/1.1968414 ↗
34. Hu M, Noda S, Tsuji Y, Okubo T, Yamaguchi Y, Komiyama H (2002) Effect of interfacial interactions on the initial growth of Cu on clean SiO2 and 3-mercaptopropyltrimethoxysilane-modified SiO2 substrates. J Vac Sci Technol A 20:589–59610.1116/1.1458941 ↗
35. Tremont RJ, Blasini DR, Cabrera CR (2003) Controlled self-assembly of mercapto and silane terminated molecules at Cu surfaces. J Electroanal Chem 556:147–158. doi: 10.1016/S0022-0728(03)00340-110.1016/S0022-0728(03)00340-1 ↗
36. Kirchner C, George M, Stein B, Parak WJ, Gaub HE, Seitz M (2002) Corrosion protection and long-term chemical functionalization of gallium arsenide in an aqueous environment. Adv Funct Mater 12:266–27610.1002/1616-3028(20020418)12:4<266::AID-ADFM266>3.0.CO;2-U ↗
37. Goss CA, Charych DH, Majda M (1991) Application of (3-mercaptopropyl)trimethoxysilane as a molecular adhesive in the fabrication of vapor-deposited gold electrodes on glass substrates. Anal Chem 63:85–8810.1021/ac00001a018 ↗
38. Wasserman SR, Biebuyck H, Whitesides GM (1989) Monolayers of 11-trichlorosilylundecyl thioacetate: a system that promotes adhesion between silicon dioxide and evaporated gold. J Mater Res 4:886–89210.1557/JMR.1989.0886 ↗
39. Huang X, Huang H, Wu N, Hu R, Zhu T, Liu Z (2000) Investigation of structure and chemical states of self-assembled Au nanoscale particles by angle-resolved X-ray photoelectron spectroscopy. Surf Sci 459:183–190. doi: 10.1016/S0039-6028(00)00483-010.1016/S0039-6028(00)00483-0 ↗
40. Brust M, Bethell D, Kiely CJ, Schiffrin DJ (1998) Self-assembled gold nanoparticle thin films with nonmetallic optical and electronic properties. Langmuir 14:5425–5429. doi: 10.1021/la980557g10.1021/la980557g ↗
41. Snow AW, Ancona MG, Kruppa W, Jernigan GG, Foos EE, Park D (2002) Self-assembly of gold nanoclusters on micro- and nanoelectronic substrates. J Mater Chem 12:1222–1230. doi: 10.1039/b108859a10.1039/b108859a ↗
42. Childs WR, Nuzzo RG (2005) Large-area patterning of coinage-metal thin films using decal transfer lithography. Langmuir 21:195–202. doi: 10.1021/la047884a10.1021/la047884a ↗
43. Siegfried T, Ekinci Y, Martin OJF, Sigg H (2013) Engineering metal adhesion layers that do not deteriorate plasmon resonances. ACS Nano 7:2751–2757. doi: 10.1021/nn400200610.1021/nn4002006 ↗
44. Habteyes TG, Dhuey S, Wood E, Gargas D, Cabrini S, Schuck PJ, Alivisatos AP, Leone SR (2012) Plasmon damping and molecular linker as a nondamping alternative. ACS Nano 6:5702–570910.1021/nn301885u ↗
45. Gandhi DD, Ganesan PG, Chandrasekar V, Gan Z, Mhaisalkar SG, Li H, Ramanath G (2007) Molecular-nanolayer-induced suppression of in-plane Cu transport at Cu–silica interfaces. Appl Phys Lett 90:163507. doi: 10.1063/1.272266710.1063/1.2722667 ↗
46. Ben Ali M, Bessueille F, Chovelon JM, Abdelghani A, Jaffrezic-Renault N, Maaref M, Martelet C (2008) Use of ultra-thin organic silane films for the improvement of gold adhesion to the silicon dioxide wafers for (bio)sensor applications. Mater Sci Eng C 28:628–632. doi: 10.1016/j.msec.2007.10.04810.1016/j.msec.2007.10.048 ↗
47. Wortman JJ, Evans RA (1965) Young’s modulus, shear modulus, and poisson’s ratio in silicon and germanium. J Appl Phys 36:153. doi: 10.1063/1.171386310.1063/1.1713863 ↗
48. Martienssen W, Warlimont H (2005) Springer handbook of condensed matter and materials data. Springer, Heidelberg10.1007/3-540-30437-1 ↗
49. García-Atance Fatjó G, Torres Pérez A, Hadfield M (2011) Experimental study and analytical model of the cavitation ring region with small diameter ultrasonic horn. Ultrason Sonochem 18:73–79. doi: 10.1016/j.ultsonch.2009.12.00610.1016/j.ultsonch.2009.12.006 ↗
50. Qin CP, Zheng YG, Wei R (2010) Cavitation erosion behavior of nanocomposite Ti–Si–C–N and Ti/Ti–Si–C–N coatings deposited on 2Cr13 stainless steel using a plasma enhanced magnetron sputtering process. Surf Coat Technol 204:3530–3538. doi: 10.1016/j.surfcoat.2010.04.01210.1016/j.surfcoat.2010.04.012 ↗
51. Niebuhr D (2007) Cavitation erosion behavior of ceramics in aqueous solutions. Wear 263:295–300. doi: 10.1016/j.wear.2006.12.04010.1016/j.wear.2006.12.040 ↗
52. Fernandez Rivas D, Betjes J, Verhaagen B, Bouwhuis W, Bor TC, Lohse D, Gardeniers HJGE (2013) Erosion evolution in mono-crystalline silicon surfaces caused by acoustic cavitation bubbles. J Appl Phys 113:064902. doi: 10.1063/1.479158210.1063/1.4791582 ↗
53. Karunamurthy B, Hadfield M, Vieillard C, Morales G (2010) Cavitation erosion in silicon nitride: experimental investigations on the mechanism of material degradation. Tribol Int 43:2251–2257. doi: 10.1016/j.triboint.2010.06.01210.1016/j.triboint.2010.06.012 ↗
54. Majumder C, Briere TM, Mizuseki H, Kawazoe Y (2002) Structural investigation of thiophene thiol adsorption on Au nanoclusters: influence of back bonds. J Chem Phys 117:2819. doi: 10.1063/1.149140410.1063/1.1491404 ↗
55. Ulman A (1996) Formation and structure of self-assembled monolayers. Chem Rev 96:1533–155410.1021/cr9502357 ↗
56. Özer N, Tepehan F (1993) Structure and optical properties of electrochromic copper oxide films prepared by reactive and conventional evaporation techniques. Sol Energy Mater Sol Cells 30:13–2610.1016/0927-0248(93)90027-Z ↗
57. Chatain D, Chabert F, Ghetta V, Fouletier J (1993) New experimental setup for wettability characterization under monitored oxygen activity: I, role of oxidation state and defect concentration on oxide wettability by gold. J Am Ceram Soc 76:1568–157610.1111/j.1151-2916.1993.tb03941.x ↗
58. Pocius AV (2002) The mechanics of adhesion. Elsevier, Amsterdam
59. Mittal KL (2001) Adhesion aspects of thin films, vol 1. VSP, Utrecht
60. Han JT, Kim S, Karim A (2007) UVO-tunable superhydrophobic to superhydrophilic wetting transition on biomimetic nanostructured surfaces. Langmuir 23:2608–261410.1021/la0629072 ↗
61. Erck RA, Erdemir A, Fenske GR (1990) Effect of film adhesion on tribological properties of silver-coated alumina. Surf Coat Technol 43–44:577–58710.1016/0257-8972(90)90002-T ↗
62. Mittal KL (2001) Metallized plastics 7: fundamental and applied aspects. VSP, Utrecht
63. Jiang N, Liu S, Chen D (2008) Effect of roughness and wettability of silicon wafer in cavitation erosion. Chin Sci Bull 53:2879–288510.1007/s11434-008-0375-5 ↗
64. Lima MM, Godoy C, Modenesi PJ, Avelar-Batista JC, Davoson A, Matthews A (2004) Coating fracture toughness determined by Vickers indentation: an important parameter in cavitation erosion resistance of WC–Co thermally sprayed coat-ings. Surf Coat Technol 177:489–49610.1016/S0257-8972(03)00917-4 ↗
65. Launey ME, Ritchie RO (2009) On the fracture toughness of advanced materials. Adv Mater 21:2103–2110. doi: 10.1002/adma.20080332210.1002/adma.200803322 ↗
66. Singh J, Whitten JE (2008) Adsorption of 3-mercaptopropyltrimethoxysilane on silicon oxide surfaces and adsorbate interaction with thermally deposited gold. J Phys Chem C 112:19088–1909610.1021/jp807536z ↗