Carbon-micro or nano silicon carbide–boron carbide (C-micro or nanoSiC–B4C) composites were prepared by heating the mixtures of green coke and carbon black as carbon source, boron carbide and silicon at temperature of 1,400 °C. Green coke reacts with silicon to give micron sized silicon carbide while the reaction between silicon and carbon black gives nano silicon carbide in the resulting carbon–ceramic composites. The green coke was coated with a suitable coal tar pitch material and used to develop carbon-(micro or nano) silicon carbide–boron carbide composites in a separate lot. The composites were characterized for various properties including oxidation resistance. It was observed that both types of composites made from uncoated as well as pitch-coated green coke exhibited good oxidation resistance at 800–1,200 °C. The density and bending strength of composites developed with pitch-coated green coke improved significantly due to the enhanced binding of the constituents by the pitch.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Fiber-reinforced polymer composites · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Fitzer E (1987) Carbon 25:16310.1016/0008-6223(87)90116-3 ↗
2. Gee M, Little JA (1991) J Mater Sci 26:1093. doi: https://doi.org/10.1007/BF0057679210.1007/BF00576792 ↗
3. Kobayashi K, Maeda K, Sano K, Uchiyama H (1995) Carbon 33:39710.1016/0008-6223(94)00164-U ↗
4. Ogawa I, Kobayashi K, Nishikawa S (1988) J Mater Sci 23:1363. doi: https://doi.org/10.1007/BF0115460110.1007/BF01154601 ↗
5. Raman V, Bhatia G, Aggarwal RK, Sengupta PR, Mishra A (2002) J Mater Sci Lett 21:31710.1023/A:1017992308395 ↗
6. Kobayashi K, Miyazaki K, Ogawa I, Hagino T, Yoshida H (1988) Mater Des 9:1010.1016/0261-3069(88)90049-0 ↗
7. Raman V, Bhatia G, Mishra A, Sengupta PR, Shah M, Rashmi (2005) Mater Sci Eng A 412:3110.1016/j.msea.2005.08.058 ↗
8. Kaur M, Kumar S, Sengupta PR, Raman V, Bhatia G (2009) J Mater Sci 44:2128. doi: https://doi.org/10.1007/s10853-009-3307-010.1007/s10853-009-3307-0 ↗
9. Eick BM, Youngblood JP (2009) J Mater Sci 44:1159. doi: https://doi.org/10.1007/s10853-009-3249-610.1007/s10853-009-3249-6 ↗
10. Zahang WG, Cheng HM, Sano H, Uchiyama Y, Koboyasni K, Zhou LJ, Shen ZH, Znou BL (1996) Carbon 36:159110.1016/S0008-6223(98)00128-6 ↗
11. Quanli J, Haijun Z, Suping L, Xiaolin J (2007) Ceram Int 33:30910.1016/j.ceramint.2005.09.014 ↗
12. Vaben R, Stover D (1994) J Mater Sci 29:3791. doi: https://doi.org/10.1007/BF0035735010.1007/BF00357350 ↗
13. McKee DW, Spiro L, Lamby EJ (1984) Carbon 22:50710.1016/0008-6223(84)90083-6 ↗
14. Guo Q, Song J, Liu L, Zhang B (1999) Carbon 37:3310.1016/S0008-6223(98)00184-5 ↗