On glass formation for a Na2O·4TeO2 melt: Effect of melting temperature, time, and raw material
Source abstract
Abstract
The effect of melting temperature, time, and the type of raw material, NaNO3 or Na2CO3, as a source for Na2O on the glass formation for a Na2O·4TeO2(NT4) melt was investigated. Melting with NaNO3 at 750°C for a short time (15 min) produced a glass that is slightly more chemically durable and more resistant to crystallization than glasses melted at a higher temperature (800°C), or for a longer time (60 min), or using Na2CO3. A thin surface layer (<1.5 nm) that contains some nitrogen and a higher concentration of bridging oxygen is suspected to be the reason for the higher chemical durability and higher resistance to crystallization for this glass. However, melting at 800°C for 60 min produced a glass, whose properties were independent of the type of raw material, NaNO3 or Na2CO3, used.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Luminescence Properties of Advanced Materials · Solid-state spectroscopy and crystallography
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. J. E. Stanworth, J. Soc. Glass Technol. 36 (1952) 217.
2. H. Burger, W. Vogel and V. Kozhukharov, Infrared Phys. 25 (1985) 395.10.1016/0020-0891(85)90114-9 ↗
3. H. Nasu, O. Matsushita, K. Kamiya, H. Kobayashi and K. Kubodera, J. Non-Cryst. Solides 124 (1990) 275.10.1016/0022-3093(90)90274-P ↗
4. S. H. Kim, T. Yoko and S. Sakka, J. Amer. Ceram. Soc. 76 (1993) 865.10.1111/j.1151-2916.1993.tb05307.x ↗
5. Idem. J. Amer. Ceram. Soc. ibid. 76 (1993) 2486.10.1111/j.1151-2916.1993.tb03970.x ↗
6. A. A. Bahgat, E. E. Shaisha and A. I. Sabry, J. Mater. Sci. 22 (1987) 1323.10.1007/BF01233128 ↗
7. C. S. Ray, D. E. Day, M. Makihara and J. Hayakawa, in “19th ISTS,” edited by M. Hinada (Hakushinsha Co., Tokyo, Japan, 1994) p. 651.
8. D. Zhu, W. Zhou and C. S. Ray, J. Mater. Sci. Lett. 20 (2001) 1961.10.1023/A:1013190903871 ↗
9. J. Heo, D. Lam, G. H. Sigel, E. A. Mendoza and D. A. Hensley, J. Amer. Ceram. Soc. 75 (1992) 77.10.1111/j.1151-2916.1992.tb08176.x ↗
10. S. K. Lee, M. Tatsumisago and T. Minami, Phys. Chem. Glass. 35 (1994) 226.
11. A. MoguŠ–Milankovi Ć, A. Š antiĆ, K. FuriĆ, C. S. Ray and D. E. Day, J. Eur. Ceram. Soc. (in press).
12. T. Sekiya, N. Mochida, A. Ohtsuka and M. Tanokawa, J. Non-Cryst. Solids 144 (1992) 128.10.1016/S0022-3093(05)80393-X ↗
13. S. L. Tagg, R. E. Youngman and J. W. Zwanziger, J. Phys. Chem. 99 (1995) 5111.10.1021/j100014a035 ↗
14. N. Kitamura, M. Makihara, T. Sato, M. Hamai, I. Moge, S. Awaji, K. Watanabe and M. Motokawa, JASMA 17 (2000) 102.
15. B. P. Troitskii, A. K. Yakhkind and N. S. Martyshchenko, Izv. Akad. Nauk SSSR, Neorg. Mater. 3 (1967) 741.
16. A. Dietzel, Glastechn. Ber. 22 (1948/1949) 41.
17. Y. Messaddeq and M. Poulain, J. Non-Cryst. Solids 140 (1992) 41.10.1016/S0022-3093(05)80738-0 ↗
18. N. P. Bansal, A. J. Bruce, R. H. Doremus and C. T. Moynihan, ibid. 70 (1985) 379.10.1016/0022-3093(85)90108-5 ↗
19. A. Hr üby, J. Phys. B22 (1972) 1187.
20. D. E. Day and M. R. Reidmeyer, J. Non-Cryst. Solids 181 (1995) 201.10.1016/S0022-3093(94)00511-7 ↗
21. D. E. Day, ibid. 112 (1989) 7.10.1016/0022-3093(89)90488-2 ↗
22. D. E. Day, M. R. Reidmeyer and R. K. Brow, ibid. 177 (1994) 208.10.1016/0022-3093(94)90532-0 ↗
23. Y. Himei, Y. Miura, T. Nanba and A. Osaka, ibid. 211 (1997) 64.10.1016/S0022-3093(96)00628-X ↗
24. T. Yoko, K. Kamiya, H. Yamada and K. Tanaka, J. Amer. Ceram. Soc. 71 (1988) C70.10.1111/j.1151-2916.1988.tb05832.x ↗
25. Y. Dimitriev, V. Dimitrov and M. Arnaudov, J. Mater. Sci. 18 (1983) 1353.10.1007/BF01111954 ↗
26. T. Uchino and T. Yoko, J. Non-Cryst. Solids 204 (1996) 243.10.1016/S0022-3093(96)00423-1 ↗
27. R. A. El-mallawany, Infrared Phys. 29 (1989) 781.10.1016/0020-0891(89)90125-5 ↗
28. International Center For Diffraction Data, PCPDFWIN Version 2.01, 1998.