Process and wear behavior of monolithic SiC and short carbon fiber-SiC matrix composite
Source abstract
Abstract
The process and wear behavior of monolithic SiC and 10 vol. % short carbon fiber-SiC matrix (C-SiC) composite have been studied. The results indicate that, among ethyl alcohol, acetone, n-hexane and n-octyl alcohol, n-octyl alcohol was the most effective dispersing agent in dispersing both SiC powder and short carbon fiber. Among AlN, Al2O3, B4C, graphite, AlN/B4C, AlN/graphite, B4C/graphite and Al2O3/B4C, the most effective sintering aid for the fabrication of SiC and C-SiC composite was a mixture of 2 wt% AlN and 0.5 wt% graphite. The monolithic SiC hot-pressed at 2100°C exhibited higher density but lower flexural strength than those hot-pressed at 2000°C due to a grain growth effect. For the C-SiC composite, both density and strength of the composite hot-pressed at 2100°C were generally higher than those hot-pressed at 2000°C. The density and strength of C-SiC composite were lower than those of monolithic SiC under the same hot pressing conditions due to a higher porosity level in the composite. When monolithic SiC slid against C-SiC composite, the weight losses of SiC and the composite were each less than that of self-mated SiC or self-mated C-SiC. In the self-mated SiC tribosystem, a mechanically stable film could not be established, resulting in an essentially constant wear rate. When sliding against C-SiC, a thin, smooth and adherent debris film was quickly formed on the SiC surface, resulting in a lower wear.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. K. Suganuma, G. Sasaki, T. Fujita, M. Okumura and K. Niihara, J. Mater. Sci. 28 (1991) 1175.10.1007/BF01191949 ↗
2. M. Landon and F. Thevenot, Ceram. Int. 17 (1991) 97.10.1016/0272-8842(91)90038-2 ↗
3. T. Takadoum, Z. Zsiga and C. R. Carmes, Wear 174 (1994) 239.10.1016/0043-1648(94)90107-4 ↗
4. T. Takadoum, Z. Zsiga, N. B. Rhouma and C. R. Carmes, J. Mater. Sci. Lett. 13 (1994) 474.10.1007/BF00540171 ↗
5. A. Blomberg, M. Olsson and S. Hogmark,Wear 171 (1994) 77.10.1016/0043-1648(94)90350-6 ↗
6. L. C. Erickson, A. Blomberg, S. Hogmark and J. Bratthcll, Tribo. Int. 26 (1993) 83.10.1016/0301-679X(93)90016-T ↗
7. A. Gangopadhyay and S. Jahanmir, Tribo. Trans. 34 (1991) 257.10.1080/10402009108982034 ↗
8. A. Skopp, M. Woydt, K. H. Habig, T. Klug and R. BrÑckner, Wear 169 (1993) 243.10.1016/0043-1648(93)90305-6 ↗
9. “Standard test method for water absorption, bulk density, apparent porosity, and apparent specific gravity of fired whiteware products,” 1984 Annual Book of ASTM Standards, vol. 15.02 C373 p. 182.
10. R. F. Pabst, in “Fracture Mechanics of Ceramics, Vol. 2, Mi-crostructure, Materials, and Applications,” edited by R. C. Bradt, D. P. H. Hasselman and F. F. lange (Plenum Press, New York, 1974) p. 555.10.1007/978-1-4615-7014-1_8 ↗
11. M. Okuyama, J. Am. Ceram. Soc. 72 (1989) 1918.10.1111/j.1151-2916.1989.tb06001.x ↗
12. S. Prochazka and R. M. Scanlan, ibid. 58 (1975) 72.10.1111/j.1151-2916.1975.tb18990.x ↗
13. D. R. Secrist, ibid. 47 (1964) 127.10.1111/j.1151-2916.1964.tb14369.x ↗
14. F. F. Lange, J. Mater. Sci. 10 (1975) 314.10.1007/BF00540356 ↗
15. W. Rafaniello, K. Cho and A. V. Virkar, ibid. 16 (1981) 3479.10.1007/BF00586311 ↗
16. R. A. Alliegro, L. B. Coffin and J. R. Tiinklepaugh, J. Am. Ceram. Soc. 39 (1956) 386.10.1111/j.1151-2916.1956.tb15609.x ↗
17. B. W. Lin, M. Imai, T. Yano and T. Iseki, ibid. 69 (1986) C-67.
18. E. Fitzer and R. Gadpw, Am. Ceram. Soc. Bull. 65 (1986) 326.