Abstract
The resultant thermoelectric properties of welded Cu/Bi-Te/Cu composites were measured at 298 K as a function of relative thickness x of Bi-Te compound by changing the interval s between two thermocouples and compared with those calculated as a function of x by treating it as an electrical and thermal circuit. These composites were prepared by welding with eutectic solder of Pb-Sn, after one end surface of the as-grown p- and n-type Bi-Te ingots were plated with Ni. It was found that the observed ZT of composites has a local maximum at an optimum x even when s was changed, as in the case of Cu/Bi-Sb/Cu and Ni/Bi-Sb/Ni composites with various relative thicknesses. Appearance of a local maximum in ZT is owing to the barrier thermo-emf generated by a sharp temperature drop at the interface between Bi-Te compound and copper. It may be caused by the separation of non-equilibrium carriers at the interface between them. The observed maximum ZT values at 298 K of the p- and n-type composites reached surprisingly great values of 1.53 and 1.66 at x=0.98, which correspond to about twice as large as those of commercially utilized Bi-Te compounds. This enhancement of ZT is available for generators, but may be not utilizable as a Peltier module. The composite materials were thus found to be utilizable as useful means of further increase in ZT of macroscopic bulk materials.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Thermal properties of materials · Thermal Radiation and Cooling Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. C. WOOD, Prog. Phys. 51 (1988) 459.10.1088/0034-4885/51/4/001 ↗
2. G. MAHAN, B. SALES and J. SHARP, Phys. Today 50 (1997) 42.10.1063/1.881752 ↗
3. L. D. HICKS and M. S. DRESSELHAUS, Phys. Rev. B47 (1993) 12727.10.1103/PhysRevB.47.12727 ↗
4. L. D. HICKS, T. C. HARMAN and M. S. DRESSELHAUS, Appl. Phys. Lett. 63 (1993) 3230.10.1063/1.110207 ↗
5. D. A. BROIDO and T. L. REINECKE, Appl. Phys. Lett. 67 (1995) 1170.10.1063/1.114998 ↗
6. H. J. GOLDSMID, in “Thermoelectric Refrigeration” (Plenum, NewYork, 1964).10.1007/978-1-4899-5723-8 ↗
7. T. KOGA, O. RABIN and M. S. DRESSELHAUS, Phys. Rev. B62 (2000) 16703.10.1103/PhysRevB.62.16703 ↗
8. T. KOGA, S. B. CRONIN, M. S. DRESSELHAUS, J. L. LIU and K. L. WANG, Appl. Phys. Lett. 77 (2000) 1490.10.1063/1.1308271 ↗
9. R. VENKATASUBRAMANIAN, E. SIIVOLA, T. COLPITTS and B. O’QUINN, Nature 413 (2001) 597.10.1038/35098012 ↗
10. D. J. BERGMAN and O. LEVY, J. Appl. Phys. 70 (1991) 6821.10.1063/1.349830 ↗
11. Z. M. DASHEVSKY, A. I. KASIYAN and N. V. KOLOMOETS, in Proceedings of the 8th International Conference on Thermoelectric Energy Conversion (Nancy, France, 1989) p. 200.
12. I. I. BALMUSH, Z. M. DASHEVSKY and A. I. KASIYAN, Semiconductors 29 (1995) 937.
13. O. YAMASHITA, K. SATOU, H. ODAHARA and S. TOMIYOSHI, J. Appl. Phys. 98 (2005) 073707.10.1063/1.2081113 ↗
14. H. ODAHARA, O. YAMASHITA, K. SATOU, S. TOMIYOSHI, J. TANI and H. KIDO, J. Appl. Phys. 97 (2005) 103722.10.1063/1.1895468 ↗
15. O. YAMASHITA, H. ODAHARA, K. SATOU and S. TOMIYOSHI, J. Mater. Sci. (in press).
16. O. YAMASHITA and S. TOMIYOSHI, J. Appl. Phys. 95 (2004) 6277.10.1063/1.1712013 ↗
17. Idem., ibid. 95 (2004) 161.
18. W. M. YIM and F. D. ROSI, Solid State Electron. 15 (1972) 1121.10.1016/0038-1101(72)90172-4 ↗
19. C. KITTEL, in “Introduction to Solid State Physics” (John Wiley & Sons, NewYork, 1996).