journal article·2000-08

Microstructural evolution on the sintered properties of W-8 pct Mo-7 pct Ni-3 pct Fe alloy

Tien-Yin Chan, Shun-Tian Lin

Journal of Materials Science· Volume 35· Issue 15
Publisher page

Abstract

The microstructure of W-8 pct Mo-7 pct Ni-3 pct Fe alloy has been found to evolve in concomitance with the reprecipitation of tungsten atoms from the matrix phase onto the grains. With increase in isothermal holding time at 1480°C, the concentration of tungsten in the matrix phase reduces from 53.7 wt pct for an isothermal holding time of 5 minutes, and gradually approaches an equilibrium value of about 18 wt pct. The continuous solid-liquid reactions result in gradual penetration of the liquid phase into the boundaries of the skeletal solid grains. Consequently, contiguity of the tungsten based grains drops sharply during the initial stage of isothermal holding, and reaches minimum after an isothermal holding time of 120 minutes. The contiguity subsequently increases again as the coalescence of grains commences. Simultaneous diminishing of the concentration of tungsten in the matrix phase along with decrease in contiguity of the grains result in an optimal combination of mechanical properties after an isothermal holding time of 120 minutes. Molybdenum has been found to bring about a substantial microstructural refinement, whereby a mean grain size of only 22 μm is attained from an isothermal holding time of as long as 240 minutes.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Injection Molding Process and Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. A. Bose and R. M. German, Metall. Trans. A 21A (1990) 1325.10.1007/BF02698261 ↗
2. R. M. German, in “Tungsten & Tungsten Alloys-1992,” edited by A. Bose and R. J. Dowding (Metal Powder Industries Federation, Princeton, New Jersey, 1993) p. 3.
3. A. Bose and R. M. German, Metall. Trans. A 19A (1988) 3100.10.1007/BF02647738 ↗
4. A. Bose, H. Zhang, P. Kemp and R. M. German, in “Advances in Powder Metallurgy, Vol. 2,” edited by E. R. Andreotti and P. J. McGeehan (Metal Powder Industries Federation, Princeton, New Jersey, 1990) p. 401.
5. R. M. German, A. Bose, P. K. Kemp and H. Zhang, in “Advances in Powder Metallurgy, Vol. 2,” edited by T. G. Gasbarre and W. F. Jandeska, Jr. (Metal Powder Industries Federation, Princeton, New Jersey, 1989) p. 401.
6. W. Qingquan and Z. Binru, in “Tungsten & Tungsten Alloys-1992,” edited by A. Bose and R. J. Dowding (Metal Powder Industries Federation, Princeton, New Jersey, 1993) p. 431.
7. T. Y. Chan and S. T. Lin, Metall. Mater. Trans. 29A (1998) 2885.10.1007/s11661-998-0195-x ↗
8. R. M. German, “Liquid Phase Sintering” (Plenum Publication Corporation, New York, 1985) p. 21.10.1007/978-1-4899-3599-1 ↗
9. P. Villars, A. Rubak and H. Okamoto, “Handbook of Ternary Alloy Phase Diagrams, Vol. 10” (ASM International, Materials Park, OH, 1995) p. 12555.
10. H. Riegger, J. A. Pask and H. E. Exner, in “Sintering Processes,” edited by G. C. Kuczynski (Plenum Press, New York, NY, 1980) p. 219.10.1007/978-1-4899-5301-8_19 ↗
11. A. Bose, G. Jerman and R. M. German, Powder Metall. Int. 21 (1989) 9.
12. P. L. Flaitz and J. A. Pask, J. Am. Ceram. Soc. 70 (1987) 449.10.1111/j.1151-2916.1987.tb05674.x ↗
13. Y. S. Zu, MS thesis, National Taiwan University of Science and Technology, May, 1994, p. 98.
14. P. B. Kemp and R. M. German, J. Less Comm. Met. 175 (1991) 353.10.1016/0022-5088(91)90022-V ↗
15. R. M. German Idem., Metall. Mater. Trans. A 26A (1995) 2187.10.1007/BF02670690 ↗
16. J. Gurland, Mater. Sci. Eng. 40 (1979) 59.10.1016/0025-5416(79)90008-9 ↗
17. R. M. German, J. E. Hanafee and S. L. Digiallonardo, Metall. Trans. A 15A (1984) 121.10.1007/BF02644393 ↗
18. M. Nakai, N. Okato, A. Kawasaki and R. Watanabe, in “Advances in Powder Metallurgy & Particulate Materials-1992, Vol. 3,” edited by J. M. Capus and R. M. German (Metal Powder Industries Federation, Princeton, NJ, 1992) p. 259.
19. Y. S. Zu and S. T. Lin, J. Mat. Proc. Tech. 71 (1997) 337.10.1016/S0924-0136(97)00095-2 ↗
20. J. W. Noh, E. P. Kim, H. S. Song, W. H. Baek, K. S. Churn and S. J. Kang, Metall. Trans. A 24A (1993) 2411.10.1007/BF02646520 ↗