Al–Ti powder produced through mechanical alloying for different times
Source abstract
Abstract
A powder mixture of aluminum, 10 wt% titanium, and 1.5 wt% of a wax acting as process control agent (PCA), has been attrition-milled for 2–20 h. Titanium powder had been previously ground to a lower particle size to make it similar to the as-received aluminum particle size. The overall aim of this work was to achieve a metastable titanium solution in the aluminum matrix. Changes with milling time of particle size and shape, microstructure, hardness and other powder characteristics have been studied. Given the used experimental-conditions, a process time of 10 h has been selected for the mechanical alloying (MA) of Al–10Ti powder, attaining a compromise between uniform microstructure development and a not so long processing time. At this milling time aluminum dissolves about 9 wt% Ti, increasing its Vickers microhardness (202 VH20) more than 10 times with reference to the starting Al powder (20 VH20). Milled particle size is smaller than the starting one (17 vs. 44 μm). Increasing milling for longer times, up to 20 h, does not produce important changes in powders structure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Benjamin JS (1970) Met Trans 1(10):294310.1007/BF03037835 ↗
2. Benjamin JS, Bomford MJ (1977) Met Trans 8A(8):1302
3. Jangg G (1975) Aluminium 51(10):641 (in German)10.2307/2615915 ↗
4. Gilman PS (1979) Ph.D. Thesis, Stanford University, USA
5. Singer RF, Oliver WC, Nix WD (1980) Met Trans 11A(11):189510.1007/BF02655106 ↗
6. Bloch EA (1961) Met Rev 6:19310.1179/095066061790425983 ↗
7. Froes FH, Suryanarayana C (1994) Metal Powder Rep 49(1):1410.1016/0026-0657(94)91437-0 ↗
8. Moon KI, Park HS, Lee KS (2002) Mater Sci Eng A 323:29310.1016/S0921-5093(01)01388-0 ↗
9. Ma E, Atzmon M, Pinkerton FE (1993) J Appl Phys 74(2):95510.1063/1.354837 ↗
10. Zhang F, Lu L, Lai MO (2000) J Alloys Comp 297(1–2):21110.1016/S0925-8388(99)00568-X ↗
11. Szegvari A, Patent No. 2,764,359 (Sept. 25, 1956)10.1136/bmj.2.4995.764 ↗
12. Rodríguez JA, (1992) Ph. D. Thesis, University of Seville, Spain
13. Young RA, (ed.) (2000) The Rietveld method (International Union of Crystallography), Oxford University Press, Oxford, UK
14. Benjamin JS, Volin TE (1974) Met Trans 5(8):192910.1007/BF02644161 ↗
15. Araki H, Saji S, Okabe T, Minamino Y, Yamane T, Miyamoto Y (1995) Mater Trans JIM 36(3):46510.2320/matertrans1989.36.465 ↗
16. Cuevas FG, (2004) Ph.D. Thesis, University of Seville, Spain
17. Ma E, Thompson CV, Clevenger LA (1991) J Appl Phys 69(4):221110.1063/1.348722 ↗
18. Ryu HJ, Hong SH, Baek WH (1997) J Mater Process Techol 63:29210.1016/S0924-0136(96)02638-6 ↗
19. Suryanarayana C (2001) Prog Mater Sci 46:110.1016/S0079-6425(99)00010-9 ↗