Preparation and luminescence of terbium and cerium-doped silica xerogels
Source abstract
Abstract
Sol-gel chemistry offers a possibility for preparation of optical materials like xerogels, aerogels, or thin films doped with rare earth ions [1–5]. In the case of silicabased materials the physical properties of the produced xerogels depend on the physicochemical processes accompanying the hydrolysis and gelation of tetraethylorthosilicate (TEOS) at different temperatures and time durations. In our previous contributions we demonstrate a higly efficient germanium–terbium energy transfer in silica sol-gel derived glasses [4, 5], the synthesis of transparent holmium-doped silica xerogels [3], as well as the luminescence of silica gels doped with terbium benzoate complexes [4]. The aim of the present investigation is the study of the preparation and luminescence of Ce3+/Tb3+ codoped silica xerogels. Optical materials containing Tb3+ and Ce3+ are important green emitting phosphors due to Ce3+ (5d1) → Tb3+ (4f75d1) energy transfer [6–8]. Despite the intense investigations of polycrystalline Ce3+/Tb3+-doped materials [8], the luminescence of amorphous xerogels remains unexplained so far. The silica xerogels in the present contribution were prepared by acid-catalyzed hydrolyzation of TEOS dissolved in ethanol (EtOH), and then gelation and drying (Techne 3D dry block with 5.6 ml starting amount of TEOS for all samples). Both ethanol addition and doping, followed by hydrolysis with HCl at pH 2 were performed under stirring. The molar ratios were TEOS:EtOH:H2O:HCl = 1:1:4:0.003. The pH of the 0.45 M Tb3+ nitrate solution is 4–5. For the cerium codoping a 1.8 M Ce3+ nitrate solution with pH 4–5 was added to the terbium containing sol. The duration and temperature conditions for all samples of the different sol-gel steps following the cerium codoping are: hydrolysis—1 hr at room temperature, gelation—48 hr at 50 ◦C and drying—120 hr at 50 ◦C. Samples containing 1 mol% Tb/Si and codoped with 0.5, 1, 2, 3, 4, 5, and 7.5 mol% Ce/Si as well as 1, 2, and 5 mol% Ce/Si were
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Lanthanide and Transition Metal Complexes · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. H. R. LI, H. J. ZHANG, J. LIN, S. B. WANG and K. Y. YANG, J. Non-Cryst. Solids 278 (2000) 218.10.1016/S0022-3093(00)00349-5 ↗
2. T. BRANKOVA, V. BEKIARI and P. LIANOS, Chem. Mater. 15 (2003) 1885.10.1021/cm0212055 ↗
3. S. GUTZOV, C. BERGER, M. BREDOL and C. L. LENGAUER, J. Mater. Sci. Lett. 21 (2002) 1105.10.1023/A:1016510600747 ↗
4. M. BREDOL, T. H. JüSTEL and S. GUTZOV, Opt. Mater. 18 (2001) 337.10.1016/S0925-3467(01)00173-2 ↗
5. M. BREDOL and S. GUTZOV, ibid. 20 (2002) 233.10.1016/S0925-3467(02)00094-0 ↗
6. T. H. JüSTEL, D. U. WIECHERT, C. LAU, D. SENDOR and U. KYNAST, Adv. Funct. Mater. 11(2) (2001) 105.10.1002/1616-3028(200104)11:2<105::AID-ADFM105>3.0.CO;2-J ↗
7. B. HENDERSON and G. F. IMBUSCH, “Optical Spectroscpopy of Inorganic Solids” (Oxford: Calderon Press, 1989) p. 380.
8. G. BLASSE and B. C. GRABMAIER, “Luminescent Materials” (New York: Springer-Verlag, 1994) p. 20.10.1007/978-3-642-79017-1 ↗
9. S. GUTZOV, J. PONAHLO, C. L. LENGAUER and A. BERAN, J. Amer. Ceram. Soc. 77 (1994) 1649.10.1111/j.1151-2916.1994.tb09769.x ↗
10. M. BREDOL, S. GUTZOV and T. H. JüSTEL, J. Non-Cryst. Solids 321 (2003) 225.10.1016/S0022-3093(03)00225-4 ↗
11. S. GUTZOV, F. WASGESTIAN, T. H. BARTHEL and W. ASSMUS, Z. Phys. Chem. 205 (1998) 41.10.1524/zpch.1998.205.Part_1.041 ↗
12. S. X. LIAN, M. REN, J. H. LIN, Z. N. GU and M. Z. SU, J. Mater. Sci. Lett. 19 (2000) 1603.10.1023/A:1006741405154 ↗
13. N. SABBATINI, S. DELLONTE and G. BLASSE, Chem. Phys. Lett. 129 (1986) 541.10.1016/0009-2614(86)80397-9 ↗