The dynamic rheological behavior and morphology of nylon/elastomer blends

Wanjie Wang, Qiang Zheng

Journal of Materials Science· Volume 40· Issue 20
Publisher page

Abstract

In the recent decades, there has been an increasing interest in preparing novel polymeric blending materials with combined and additional characteristics of each component. Having a relatively high modulus, toughness and strength, low creep, and good temperature resistance, nylons have been widely applied in the automotive industry, machinery, electronic equipment, and military applications [1]. It is well-known that blends consisting of nylon and elastomer possess excellent toughness; however, due to its highly polar amide end-groups, nylon is incompatible with elastomer. In general, it is believed that functionalization of the elastomer is a preferred approach to enhance the interfacial properties between these polymers. Research concerning nylon/functionalized elastomer blends has mostly focused on the aspects of mechanical and thermal properties. To our knowledge, only a few reports have dealt with dynamic rheological behavior of their melts [2–4]. The rheological measurements not only give much useful information for material moulding and processing, but also is an important way to characterize the structure and properties of polymer materials [5, 6]. The aim of this article is to study the influence of the graft reaction between nylon1212 and SEBS-gMA on dynamic rheological behavior and morphology of their blends. Nylon1212 (melt-flow index = 22.43 g/min) used here was obtained from Shandong Dongchen Engineering Plastic Co., Ltd., China. The elastomer, a triblock copolymer styrene-b-(ethylene-co-butylene)-b-styrene (SEBS 4033) was supplied by the Yuyao Huiju Polymer Co., Ltd. China. The maleated triblock copolymer styrene-b-(ethylene-co-butylenes)-b-styrene (SEBS-gMA) was supplied by Yuyao Yongcheng Engineering plastics Co., Ltd., China. The grafting ratio of maleic anhydride is 1.84 wt%. Both SEBS and SEBSg-MA consist of 30 wt% polystyrene end-blocks. The nylon1212/SEBS blends and nylon1212/SEBS-g-MA blends including 1 wt% antioxidant (1010) were prepared in a corotating twin-screw extruder (PRISM TES 16TC, UK) at 210 ◦C. All the samples were compression-moulded into disks of 25 mm in diameter and 1.2 mm in thickness at 180 ◦C, 50 MPa. Melt rheological tests were conducted in an ARES Rheometer
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Polymer crystallization and properties · Polymer Nanocomposites and Properties · Rheology and Fluid Dynamics Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. M. I. KOHAN, “Nylon Plastic Handbook” (Carl Hanser Verlag, Munich, 1995).
2. A. J. OSHINSKI, H. KESKKULA and D. R. PAUL, Polymer 23 (1992) 268.10.1016/0032-3861(92)90984-5 ↗
3. R. J. M. BORGGREVE, R. J. GAYMANS and H. M. EICHEMWALD, ibid. 30 (1989) 78.10.1016/0032-3861(89)90386-8 ↗
4. E. M. ARAUJO, Jr. E. HAGE and A. J. F. CARVALHO, J. Mater. Sci. 38 (2003) 3515.10.1023/A:1025648508152 ↗
5. Q. ZHENG and T. J. ZHAO, Chin. J. Mater. Res. 12 (1998) 225.
6. Q. ZHENG, B. B. YANG, G. WU and L. W. LI, Chem. J. Chin. Univ. 20 (1999) 1483.
7. J. D. FEERY, “Viscoelastic Properties of Polymers” (Wiley Press, New York, 1980) p. 56.
8. SNOOPY GEORGE, K. RAMAMURTHY and J. S. ANAND, Polymer 40 (1999) 4325.10.1016/S0032-3861(98)00681-8 ↗
9. Q. ZHENG, Y. X. CAO and M. DU, J. Mater. Sci. Lett. 39 (2004) 1813.10.1023/B:JMSC.0000016192.33456.06 ↗
10. C. D. HAN and J. K. KIM, Macromolecules 22 (1989) 4292.10.1021/ma00201a026 ↗
11. S. H. JAFARI, P. POTSCHKE, M. STEPHAN, H. WARTH and H. ALBERTS, Polymer 43 (2002) 6985.10.1016/S0032-3861(02)00614-6 ↗
12. S. STEINMANN, W. GRONSKI and C. FRIEDRICH, Rheo. Acta 41 (2002) 77.10.1007/s003970200007 ↗
13. B. MAJUMDAR, H. KESKKULA and D. R. PAUL, Polymer 35 (1994) 1386.10.1016/0032-3861(94)90338-7 ↗