Effect of crosshead speed on the fracture toughness of Soda-lime glass, Al2O3 and Si3N4 ceramics determined by the surface crack in flexure (SCF) method
Source abstract
Abstract
The fracture toughness of soda-lime glass, Al2O3 and Si3N4 specimens was measured by the surface crack in flexure method. For the soda-lime glass specimens, the fracture toughness was calculated from the initial crack size and flexure strength, and the value increased with increasing crosshead speed. This trend seems to be related to the difficulty in determining the critical crack size at fracture, since slow crack growth occurs during bending test. For the Al2O3 specimens, a halo region (stable crack growth region) was formed around the initial precrack during bending test. The halo size increased and the resultant flexure strength decreased with decreasing in the crosshead speed. The halo region, however, could not be observed in the Si3N4 specimens. Despite of the difference in the appearance of halo region, the fracture toughness of the Al2O3 and Si3N4 specimens was constant irrespective of the crosshead speed when the values were calculated with the critical crack sizes at fracture (halo incorporated crack sizes). The constant fracture toughness with the crosshead speed could be explained by the relation between the changes of halo size (thus critical crack size at fracture) and resultant flexure strength.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Concrete and Cement Materials Research · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. P. Kenny, Powder Met. 14 (1971) 22.10.1179/pom.1971.14.27.002 ↗
2. K. R. Kinsman, in“Deformation of Ceramic Materials,” edited by R. C. Bradt and R. E. Tressler (Plenum Press, New York, 1975) p. 465.10.1007/978-1-4613-4431-5_26 ↗
3. J. J. Petrovic, L. A. Jacobson, P. A. Talty and A. K. Vasudevan, J. Amer.Ceram. Soc. 58 (1975) 113.10.1111/j.1151-2916.1975.tb19571.x ↗
4. J. J. Petrovic, R. A. Dirks, L. A. Jacobson and M.G. Mendiratta, ibid. 59 (1976) 177.10.1111/j.1151-2916.1976.tb09468.x ↗
5. J. C. Newman. Jr., I. S. Raju, Eng. Fract. Mech. 15 (1981) 185.10.1016/0013-7944(81)90116-8 ↗
6. C. A. Tracy and G. D. Quinn, Ceram.Eng. Sci. Proc. 15 (1994) 837.
7. G. D. Quinn, R. J. Gettings and J. J. KÜbler,ibid. 15 (1994) 846.10.1002/9780470314555.ch30 ↗
8. Idem., in “Ceramic Transactions,” Vol. 64,edited by J. R. Varner, V. D. Frechette and G. D. Quinn (American Ceramic Society, Westerville, OH, 1996) p. 107.
9. J. J. Swab and G. D. Quinn, J. Amer. Ceram. Soc. 81 (1998) 2261.10.1111/j.1151-2916.1998.tb02620.x ↗
10. ISO/TC 206/SC, N209, New Work Item Proposal (1998).
11. G. D. Quinn, J.J. KÜbler and R. J. Gettings, in “VAMAS Technical Report” (National Institute of Standards and Technology, Gaithersburg, MD, June, 1994) #17.
12. ASTM C 1161, “Annual Book of ASTM Standards,” Vol.15.01 (ASTM, West Conshohoken, PA., 1997) p. 324.
13. S. M. Wiederhorn and L.H. Boltz, J. Amer. Ceram. Soc. 53 (1970) 543.10.1111/j.1151-2916.1970.tb15962.x ↗
14. A. G. Evans, Int. J. Fract. 10(1974) 251.10.1007/BF00113930 ↗
15. J. J. Mecholsky, A. C. Gonzalez and S. W. Freiman, J. Amer. Ceram. Soc.62 (1979) 577.10.1111/j.1151-2916.1979.tb12735.x ↗
16. B. J. Pletka and S. M. Wiederhorn, J. Mater. Sci. 17 (1982)1257.10.1007/BF00752234 ↗
17. R. K. Govila, J. Amer. Ceram. Soc. 63 (1980) 319.10.1111/j.1151-2916.1980.tb10730.x ↗
18. F. F. Lange,ibid. 57 (1974) 84.10.1111/j.1151-2916.1974.tb10819.x ↗