Study on friction and sliding wear behavior of woven S-glass fiber reinforced vinylester composites manufactured with different comonomers
Source abstract
Abstract
The effect of variations in sliding velocity and applied normal load on the friction and sliding wear behavior of glass–vinylester composite (G–V) is studied by measuring the weight change and observing the surface features of worn specimens using scanning electron microscopy (SEM). The G–V composites were manufactured with Bi-directional woven S-glass fibers (65 wt%) reinforced with vinylester resin with different comonomers. Friction and wear experiments were carried at ambient conditions on a Pin on disc machine arrangement. The wear in the experiment was determined from the weight loss measured after running against steel disc at sliding velocities of 1, 2, 3, and 4 m/s and applied normal load of 10, 20, 30, and 40 N. The experimental findings show increase in specific wear rate with increase the applied load. Specific wear rate was maximum for the sample A (Styrene as Comonomer), intermediate for sample B (Methyl acrylate as comonomer), and least for sample C (Butyl acrylate as comonomer). It was also observed that increasing normal load and sliding velocity the coefficient of friction decreases. The scanning pictures show features like tendency for the matrix to adhere towards the fiber, debris formation, network of cracks, agglomeration of debris, and broken fibers depending on the load and velocity employed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Tribology and Wear Analysis · Mechanical stress and fatigue analysis · Natural Fiber Reinforced Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Kishore P, Sampathkumaran S, Seetharamu S, Murali A, Kumar RK (1999) J Reinf Plast Compos 18(1):5510.1177/073168449901800106 ↗
2. Kishore P, Sampathkumaran S, Seetharamu S, Vynatheya S, Murali A, Kumar RK (2000) Wear 237:2010.1016/S0043-1648(99)00300-2 ↗
3. Collyer AA (1994) Rubber toughened engineering materials. Chapman & Hall, London
4. Pıhtılı H, Tosun N (2002) Compos Sci Technol 62(3):36710.1016/S0266-3538(01)00196-8 ↗
5. El-Tayep NS, Gadelrap RM (1996) Wear 192:11210.1016/0043-1648(95)06770-1 ↗
6. Chand N, Naik A, Neogi S (2000) Wear 242:3810.1016/S0043-1648(00)00398-7 ↗
7. Kukureka SN, Hooke CJ, Rao M, Liao P, Chen YK (1999) Tribol Int 32:10710.1016/S0301-679X(99)00017-1 ↗
8. Mallick PK (1988) Fiber-reinforced composites: materials, manufacturing, and design. Marcel Dekker, New York
9. Piggot MR (1980) Load bearing fiber composites. Pergamon Press, Oxford
10. Pihtili H, Tosun N (2002) Wear 252:97910.1016/S0043-1648(02)00062-5 ↗
11. Bijwe J, Indumathi J, John Rajesh J, Fahim M (2001) Wear 249:71510.1016/S0043-1648(01)00696-2 ↗
12. Hutchings IM (1992) Tribology: friction and wear of engineering materials. CRC press, London, p 156
13. Harsha AP, Tewari US (2002) Polym Test 21:69710.1016/S0142-9418(01)00145-3 ↗
14. Mutlu I, Eldagon O, Findik F (2006) Tribol Int 39(4):31710.1016/j.triboint.2005.02.002 ↗
15. Mutlu I, Oner C, Cevik I, Findik F (2007) Ind Lubr Tribol 59(1):3810.1108/00368790710723124 ↗
16. Mody PB, Chou TW, Fredrich K (1988) J Mater Sci 23:4319. doi:https://doi.org/10.1007/BF0055192610.1007/BF00551926 ↗
17. Suresha B, Chandramohan G, Prakash JN, Balusamy V, Sankaranarayanasamy K (2006) J Miner Mater Charact Eng 5:87
18. Shivakumar KN, Gowtham S, Sharpe M, Reinf J (2006) Plast Compos 25:110110.1177/0731684406065194 ↗
19. Suresha B, Chandramohan G, Sampathkumaran P, Seetharamu S, Vynatheya S, Reinf J (2006) Plast Compos 25:77110.1177/0731684406063540 ↗
20. Chauhan S, Kumar A, Patnaik A, Satapathy A, Singh I (2008) J Reinf Plast Compos. doi:https://doi.org/10.1177/073168440809382310.1177/0731684408093823 ↗
21. Suresha B, Chandramohan G, Siddaramaiah Sampathkumaran P, Seetharamu S (2008) J Mater Sci Eng A 480:57310.1016/j.msea.2007.07.011 ↗