Abstract

The wetting and reaction between Si melt and SiO2 substrate were investigated as a function of the atmosphere, temperature, and degree of vacuum. The results revealed that below 2 Torr with an Ar flow, the wetting angle is finally 90°. The Si droplet was stationary at a wetting angle of 90°. Videos indicated that the droplets moved and vibrated; Above 20 Torr, the Si droplet vibrated up and down with a frequency of approximately 2 Hz, thereby changing the wetting angle. Further, the droplet remained stationary on a substrate on which grooves with a width of 100 μm and depth of 100 μm were etched with a pitch of 1 mm. The presence of grooves or dimples on the substrates facilitated the leakage of SiO gas; as a result, the Si droplet did not vibrate. A vibration model was proposed in which the SiO gas produced at the interface between the Si droplet and the substrate according to the reaction Si + SiO = 2SiO expands and leaks continuously.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fluid Dynamics and Thin Films · Fluid Dynamics and Heat Transfer · Heat Transfer and Boiling Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Niu Z, Mukai K, Shiraishi Y, Hibiya T, Kakimoto K, Koyama M (1996) J Jpn Crystal Growth 23(5):374
2. Mukai K et al (2000) Mater Trans JIM 41(5):63910.2320/matertrans1989.41.639 ↗
3. Fujii H, Yamamoto M, Hara S, Nogi K (1999) J Mater Sci 34:316510.1023/A:1004673605025 ↗
4. Sugihara S, Okazaki K (1992) Materia Japan 31(3):197
5. Aksay IA, Hoge CE, Pask JA (1974) J Phys Chem 78(12):117810.1021/j100605a009 ↗
6. Marumo C, Pask JA (1977) J Mater Sci 12:22310.1007/BF00566262 ↗
7. Standage AE, Gani MS (1967) J Am Ceram Soc 50(2):10110.1111/j.1151-2916.1967.tb15049.x ↗
8. Prabriputaloong K, Piggott MR (1973) J Am Ceram Soc 56(4):18410.1111/j.1151-2916.1973.tb12451.x ↗
9. Nagesh VK, Pask JA (1983) J Mater Sci 18:266510.1007/BF00547582 ↗
10. Ogino K et al (1982) J Jpn Inst Metal 46(10):95710.2320/jinstmet1952.46.10_957 ↗
11. Tomsia AP, Pask JA (1986) Dent Mater 2:1010.1016/S0109-5641(86)80063-X ↗
12. Sangiorgi R, Muolo ML, Ceramic developments (1988) In: Sorrel CC, Ben-Nissan B (eds) Mater Sci Forum 34–36:42710.4028/www.scientific.net/MSF.34-36.427 ↗
13. Champion JA et al (1969) J Mater Sci 4:3910.1007/BF00555046 ↗
14. Pask JA (1987) Ceramic Bull 66(11):1587
15. Sugihara S, Hirose Y (1994) J Ceram Soc Jpn 102(3):21710.2109/jcersj.102.217 ↗
16. Levi G, Kaplan WD (2002) Acta Mater 50:7510.1016/S1359-6454(01)00333-0 ↗
17. Taimatsu H et al (1985) J Jpn Inst Mater 49(7):52310.2320/jinstmet1952.49.7_523 ↗
18. Sugihara S, Okazaki K (1993) J Mater Sci 28:245510.1007/BF01151679 ↗
19. Sugihara S (1990) J Jpn Soc Powder Powder Metall 37(7):105210.2497/jjspm.37.1052 ↗
20. Sugihara S, Okazaki K, Terashima Y, Kisamori K (1991) Jpn J Appl Phys 30(9B):241310.1143/JJAP.30.2413 ↗
21. Sugihara S et al (1998) J Korean Phys Soc 32(2):S1119
22. Sugihara S, Yamamoto M, Isobe T, Yutoh Y (2003) Adv Quant Chem 42:46510.1016/S0065-3276(03)42069-8 ↗