Recrystallization and fracture characteristics of thin copper wire

Fei-Yi Hung, Truan-Sheng Lui, Li-Hui Chen, Yuan-Tin Wang

Journal of Materials Science· Volume 42· Issue 14
Publisher page

Abstract

In this study, the annealed effect (at 150 °C ∼ 250 °C for 1 h) on the tensile mechanical properties of thin copper wires with φ = 25 μm (1 mil) was investigated. The microstructural characteristics and the mechanical properties before and after an electric flame-off (EFO) were also studied. Results indicate that with annealing temperatures of more than 200 °C, the wires possessed a fully annealed structure, the tensile strength and the hardness decreased, and the elongation was raised significantly. Through recrystallization, equiaxed grains and a few annealed twins formed in the matrix structure. The microstructures of the free air ball (FAB) of the various wires after EFO contained column-like grains. The column-like grains grew from the heat-affected zone (HAZ) to the Cu ball, and the preferred orientation was . According to Weibull’s reliability analysis, the failure rates of all the specimens were the modus of wear-failure. The tensile strength and the reliability of both the 200 °C and 250 °C annealed wires in the HAZs showed the highest values of all.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical stress and fatigue analysis · Electrical Contact Performance and Analysis · Electronic Packaging and Soldering Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. Wulff F, Breach CD, Dittmer K (2003) J Mater Sci Lett 22:137310.1023/A:1025751714880 ↗
2. Murali N, Srikanth N, Vath CJ III (2003) Mater Res Bull 38:63710.1016/S0025-5408(03)00004-7 ↗
3. Srikanth N, Murali S, Wong YM, Vath CJ III (2004) Thin Solid Films 462:33910.1016/j.tsf.2004.05.116 ↗
4. Baker H, Benjamin D, Kirkpatrick CW (1979) Properties and selection: nonferrous alloys and pure metals, Metals Handbook, 9th edn. vol 2
5. Ho HM, Lam W, Stoukatch S, Ratchev P, Vath CJ III, Beyne E (2003) Microelectron Reliab 43:91210.1016/S0026-2714(03)00074-X ↗
6. Murali S, Srikanth N, Vath CJ III (2003) Mater Charact 50:3910.1016/S1044-5803(03)00102-5 ↗
7. Saboui A (1991) Wire bounding limitation for high density fine pitch plastic packages, IEEE/CHMT IEMT Symposium, 75–7910.1109/IEMT.1991.279750 ↗
8. Weibull W (1951) J Appl Mech 18:29310.1115/1.4010337 ↗
9. Reliability in Engineering Design, Sons KC, John Wiley & Sons, 1977, Chap. 1–6
10. Faucher B, Tyson WR (1998) J Mater Sci Lett 7:119910.1007/BF00722337 ↗
11. Li XD, Edwards L (1996) Eng Fract Mech 20:3510.1016/0013-7944(95)00206-5 ↗