Effects of thermal cycling and room-temperature ageing on bismuth precipitates in Sn-Ag-Cu-Bi solder joints
Source abstract
Abstract
Abstract The long-term stability of Bi-strengthened Sn–Ag–Cu solders is an important but insufficiently understood factor for the reliability of stored electronic assemblies. In this study, (Bi) precipitates in Sn-2.25Ag-0.5Cu-6Bi (wt.%) solder joints were examined in two ball grid array (BGA) packages after long-term (> 6 years) room-temperature ageing following reflow soldering and after harsh thermal cycling between − 55 and 125 °C. Significant differences are observed between bulk and surface (Bi) precipitates in their distribution, morphology, crystallographic orientation relationships (ORs) with β -Sn, and the formation of interfaces and ORs with Cu₆Sn₅. Three distinct ORs between (Bi) and β -Sn are identified, each with eight crystallographic variants in good agreement with calculated variants. The precipitates are plate-shaped, with the largest habit planes corresponding to the most coherent interfaces ( $${\{100\}}_{\beta \text{Sn}}\parallel {\{01\bar{1}2\} }_{\left(\text{Bi}\right)}$$ for OR1; $${\{011\}}_{\beta \text{Sn}}\parallel {\{01\bar{1}2\} }_{\left(\text{Bi}\right)}$$ for OR2), resulting in multiple precipitate alignments within the matrix. Notably, OR2 is preferentially observed for bulk precipitates. Two additional ORs are identified between (Bi) and Cu₆Sn₅. After prolonged room-temperature storage, however, the bulk (Bi) precipitates become coarsened and widely spaced (> 1 μm in size and > 9 μm spacing), and (Bi) is observed to accumulate adjacent to Cu₆Sn₅ and Ag₃Sn particles. These observations indicate over-ageing and significant microstructural evolution even at room temperature, suggesting a potential long-term reliability concern for Bi-strengthened solder joints in stored electronics. Graphical abstract
Source: crossref · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Copper Interconnects and Reliability · Metallurgical and Alloy Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (84)
Show source-provided references
1. Coyle R et al (2016) A collaborative industrial consortia program for characterizing thermal fatigue reliability of third generation Pb-free alloys. In: International SMTA (ed) Rosemont. USA, IL, pp 188–196
2. Bieler TR, Jiang H, Lehman LP, Kirkpatrick T, Cotts EJ, Nandagopal B (2008) Influence of Sn grain size and orientation on the thermomechanical response and reliability of Pb-free solder joints. IEEE Trans Compon Packag Technol 31(2):370–381. https://doi.org/10.1109/TCAPT.2008.91683510.1109/TCAPT.2008.916835 ↗
3. Xian JW, Xu YL, Stoyanov S, Coyle RJ, Dunne FPE, Gourlay CM (2024) The role of microstructure in the thermal fatigue of solder joints. Nat Commun 15(1):4258. https://doi.org/10.1038/s41467-024-48532-610.1038/s41467-024-48532-6 ↗
4. Keller J, Baither D, Wilke U, Schmitz G (2011) Mechanical properties of Pb-free SnAg solder joints. Acta Mater 59(7):2731–2741. https://doi.org/10.1016/j.actamat.2011.01.01210.1016/j.actamat.2011.01.012 ↗
5. Sundelin JJ, Nurmi ST, Lepistö TK, Ristolainen EO (2006) Mechanical and microstructural properties of SnAgCu solder joints. Mater Sci Eng A 420(1–2):55–62. https://doi.org/10.1016/j.msea.2006.01.06510.1016/j.msea.2006.01.065 ↗
6. Yin L, Wentlent L, Yang L, Arfaei B, Oasaimeh A, Borgesen P (2012) Recrystallization and precipitate coarsening in Pb-free solder joints during thermomechanical fatigue. J Electron Mater 41(2):241–252. https://doi.org/10.1007/s11664-011-1762-210.1007/s11664-011-1762-2 ↗
7. Xian JW, Belyakov SA, Gourlay CM (2021) Time-lapse imaging of Ag3Sn thermal coarsening in Sn-3Ag-0.5Cu solder joints. J Electron Mater 50(3):786–795. https://doi.org/10.1007/s11664-020-08498-910.1007/s11664-020-08498-9 ↗
8. Delhaise AM et al (2020) Thermal preconditioning and restoration of bismuth-containing, lead-free solder alloys. J Electron Mater 49(1):116–127. https://doi.org/10.1007/s11664-019-07666-w10.1007/s11664-019-07666-w ↗
9. Choudhury P et al (2015) Development of Lead-Free Alloys with Ultre-High Thermo-Mechanical Reliability. In: International SMTA (ed) Rosemont. USA, IL, pp 128–133
10. AZ (2010) Miric New developments in high-temperature, high-performance lead-free solder alloys. In SMTA International Orlando, FL, USA
11. Ali HE, El-Taher AM, Algarni H (2024) Influence of bismuth addition on the physical and mechanical properties of low silver/lead-free Sn-Ag-Cu solder. Mater Today Commun 39:109113. https://doi.org/10.1016/j.mtcomm.2024.10911310.1016/j.mtcomm.2024.109113 ↗
12. Liang J et al (2026) Strength improvement and ductility preservation of Sn-Ag-Cu solder alloy induced by Bi and Mn microalloying. Mater Sci Eng, A 958:150010. https://doi.org/10.1016/j.msea.2026.15001010.1016/j.msea.2026.150010 ↗
13. Tien J, Xie L, Blendell J, Handwerker CA, Bahr DF (2026) Bi addition increases strength and strain-softening behavior in SAC305. Mater Res Lett. https://doi.org/10.1080/21663831.2026.263416010.1080/21663831.2026.2634160 ↗
14. Y Liu, F Sun, X Liu (2010) Improving Sn-0.3Ag-0.7Cu low-Ag lead-free solder performance by adding Bi element In International Forum on Strategic Technol IEEE https://doi.org/10.1109/IFOST.2010.5667986.10.1109/IFOST.2010.5667986 ↗
15. El-Daly AA, El-Taher AM, Gouda S (2015) Development of new multicomponent Sn–Ag–Cu–Bi lead-free solders for low-cost commercial electronic assembly. J Alloys Compd 627:268–275. https://doi.org/10.1016/j.jallcom.2014.12.03410.1016/j.jallcom.2014.12.034 ↗
16. Shen J, Pu Y, Wu D, Tang Q, Zhao M (2015) Effects of minor Bi, Ni on the wetting properties, microstructures, and shear properties of Sn–0.7Cu lead-free solder joints. J Mater Sci: Mater Electron 26(3):1572–1580. https://doi.org/10.1007/s10854-014-2577-810.1007/s10854-014-2577-8 ↗
17. Vianco PT, Rejent JA (1999) Properties of ternary Sn-Ag-Bi solder alloys: Part II - wettability and mechanical properties analyses. J Electron Mater 28(10):1138–1143. https://doi.org/10.1007/s11664-999-0251-310.1007/s11664-999-0251-3 ↗
18. He M, Ekpenuma SN, Acoff VL (2008) Microstructure and creep deformation of Sn-Ag-Cu-Bi/Cu solder joints. J Electron Mater 37(3):300–306. https://doi.org/10.1007/s11664-007-0368-110.1007/s11664-007-0368-1 ↗
19. Hodúlová E, Palcut M, Lechovič E, Šimeková B, Ulrich K (2011) Kinetics of intermetallic phase formation at the interface of Sn–Ag–Cu–X (X = Bi, In) solders with Cu substrate. J Alloys Compd 509(25):7052–7059. https://doi.org/10.1016/j.jallcom.2011.03.16410.1016/j.jallcom.2011.03.164 ↗
20. Kim KS, Yu CH, Yang JM (2006) Behavior of tin whisker formation and growth on lead-free solder finish. Thin Solid Films 504(1–2):350–354. https://doi.org/10.1016/J.TSF.2005.09.08810.1016/J.TSF.2005.09.088 ↗
21. Jadhav N, Williams M, Pei F, Stafford G, Chason E (2013) Altering the mechanical properties of Sn films by alloying with Bi: mimicking the effect of Pb to suppress whiskers. J Electron Mater 42(2):312–318. https://doi.org/10.1007/s11664-012-2267-310.1007/s11664-012-2267-3 ↗
22. Liu Y, Sun F, Liu Y, Li X (2014) Effect of Ni, Bi concentration on the microstructure and shear behavior of low-Ag SAC–Bi–Ni/Cu solder joints. J Mater Sci: Mater Electron 25(6):2627–2633. https://doi.org/10.1007/s10854-014-1921-310.1007/s10854-014-1921-3 ↗
23. Al Athamneh R, Hamasha S (2020) Fatigue behavior of SAC-Bi and SAC305 solder joints with aging. IEEE Trans Compon Packag Manuf Technol 10(4):611–620. https://doi.org/10.1109/TCPMT.2019.294971910.1109/TCPMT.2019.2949719 ↗
24. Hamasha K, Hamasha MM, Hamasha S (2026) Effect of bismuth addition to SAC305 on the microstructure and mechanical properties of solder joints. J Electron Packag. https://doi.org/10.1115/1.407051510.1115/1.4070515 ↗
25. Das R et al (2025) Superior reliability of SAC305-SnBi solder joints formed in a 150 °C reflow. Mater Sci Eng A. https://doi.org/10.1016/j.msea.2025.14859810.1016/j.msea.2025.148598 ↗
26. Das R et al (2025) Post-annealing of hybrid SAC305-SnBi solder joints formed with a 150 °C reflow to improve fatigue resistance. J Mater Sci Mater Electron 36(5):321. https://doi.org/10.1007/s10854-025-14379-w10.1007/s10854-025-14379-w ↗
27. Zhao J, Qi L, Wang XM, Wang L (2004) Influence of Bi on microstructures evolution and mechanical properties in Sn-Ag-Cu lead-free solder. J Alloys Compd 375(1–2):196–201. https://doi.org/10.1016/j.jallcom.2003.12.00510.1016/j.jallcom.2003.12.005 ↗
28. KR Hassan, J Wu, MS. Alam, JC Suhling, P Lal (2021) Mechanical behavior and reliability of SAC+Bi lead free solders with various levels of bismuth, IEEE 71st Electronic Components and Technology Conference (ECTC), IEEE 937–945. https://doi.org/10.1109/ECTC32696.2021.0015510.1109/ECTC32696.2021.00155 ↗
29. M Al Ahsan, SMK Hasan, A Fahim, JC Suhling, P Lall (2021) Mechanical property evolution in SAC+Bi lead free solders subjected to various thermal exposures. In 2021 20th IEEE Intersociety Conference on Thermal and Thermomechanical Phenomena in Electronic Systems (iTherm), IEEE. 700–7007 https://doi.org/10.1109/ITherm51669.2021.950317510.1109/ITherm51669.2021.9503175 ↗
30. El-Taher AM et al (2025) Microstructural and mechanical enhancements in Sn–Ag–Cu solder alloys via nickel and bismuth additions. J Mater Sci Mater Electron 36(27):1752. https://doi.org/10.1007/s10854-025-15640-y10.1007/s10854-025-15640-y ↗
31. Witkin D (2012) Creep behavior of Bi-containing lead-free solder alloys. J Electron Mater 41(2):190–203. https://doi.org/10.1007/s11664-011-1748-010.1007/s11664-011-1748-0 ↗
32. Shukla V, Ahmed O, Su P, Jiang T (2024) Reliability risk mitigation in advanced packages by aging-induced precipitation of Bi in water-quenched Sn–Ag–Cu–Bi solder. Materials Basel 17(14):3602. https://doi.org/10.3390/ma1714360210.3390/ma17143602 ↗
33. Juarez JM et al (2015) Manufacturability and reliability screening of lower melting point, Pb-free alloys containing bismuth. J Microelectron Electron Packag 12(1):1–28. https://doi.org/10.4071/imaps.44110.4071/imaps.441 ↗
34. JH Lee, S Kumar, HJ Kim, YW Lee, JT Moon (2014) High thermo-mechanical fatigue and drop impact resistant Ni-Bi doped lead free solder In 2014 IEEE 64th Electronic Components and Technology Conference (ECTC), IEEE 712–716 https://doi.org/10.1109/ECTC.2014.689736210.1109/ECTC.2014.6897362 ↗
35. R Coyle, M Anselm C Feng R Popowich (2024)The Effect of extended dwell time on thermal cycling performance of hybrid low temperature solder joints. In 2024 IEEE 74th Electronic Components and Technology Conference (ECTC), IEEE 1452–1459. https://doi.org/10.1109/ECTC51529.2024.00236.10.1109/ECTC51529.2024.00236 ↗
36. Belhadi MEA, Hamasha S, Alahmer A, Zhao R, Prorok BC, Alavi S (2024) The impact of Bi content on the coarsening kinetics of IMC particles and creep deformation under thermal cycling. J Electron Mater 53(1):380–393. https://doi.org/10.1007/s11664-023-10780-510.1007/s11664-023-10780-5 ↗
37. Hsieh CL, Coyle RJ, Belyakov SA, Xian JW, Gourlay CM (2025) Effects of bismuth on the microstructure and crack propagation in Sn–Ag–Cu-Bi solder joints during thermal cycling. J Mater Sci Mater Electron 36(30):1926. https://doi.org/10.1007/s10854-025-15979-210.1007/s10854-025-15979-2 ↗
38. Huang ML, Wang L (2005) Effects of Cu, Bi, and In on microstructure and tensile properties of Sn-Ag-X(Cu, Bi, In) solders. Metall Mater Trans A 36(6):1439–1446. https://doi.org/10.1007/s11661-005-0236-710.1007/s11661-005-0236-7 ↗
39. Sayyadi R, Naffakh-Moosavy H (2018) Physical and mechanical properties of synthesized low Ag/lead-free Sn–Ag–Cu–xBi (x = 0, 1, 2.5, 5 wt%) solders. Mater Sci Eng A 735:367–377. https://doi.org/10.1016/j.msea.2018.08.07110.1016/j.msea.2018.08.071 ↗
40. Celikin M, Maalekian M, Pekguleryuz M (2018) Effect of Bi additions on the creep behaviour of SAC solder alloys. J Electron Mater 47(10):5842–5849. https://doi.org/10.1007/s11664-018-6458-410.1007/s11664-018-6458-4 ↗
41. Wu JA, Luktuke A, Chawla N (2023) Surface precipitation and growth of bismuth particles in Sn–Ag–Cu–Bi solder joints. J Electron Mater 52(2):801–809. https://doi.org/10.1007/s11664-022-10126-710.1007/s11664-022-10126-7 ↗
42. Belhadi MEA, Hamasha S, Alahmer A (2023) Effect of Bi content and aging on solder joint shear properties considering strain rate. Microelectron Reliab 146:115020. https://doi.org/10.1016/J.MICROREL.2023.11502010.1016/J.MICROREL.2023.115020 ↗
43. M Sampathkumar, S Rajesnayagham, SM Ramkumar, SJ Anson (2005) Investigation of the performance of SAC and SACBi lead-free solder alloys with OSP and immersion silver PCB finish. In SMTA International 25–2910.37665/smBBIZW74626 ↗
44. G Yuan, X Yang, X Shu (2009) Effects of strain rate and temperature on mechanical behavior of SACB solder alloy. In 2009 IEEE International Conference on Electronic Packaging Technology & High Density Packaging (ICEPT-HDP) 1186–1189 https://doi.org/10.1109/ICEPT.2009.527061610.1109/ICEPT.2009.5270616 ↗
45. Hu SH et al (2021) Effects of bismuth additions on mechanical property and microstructure of SAC-Bi solder joint under current stressing. Microelectron Reliab 117:114041. https://doi.org/10.1016/j.microrel.2021.11404110.1016/j.microrel.2021.114041 ↗
46. V Shukla, O Ahmed, G Jalilvand, A Mehta, P Su, T Jiang (2021) Effects of aging on microstructure and mechanical properties of Sn–Ag–Cu–Bi solder alloys. In 2021 IEEE 71st Electronic Components and Technology Conference (ECTC), IEEE 667–672 https://doi.org/10.1109/ECTC32696.2021.0011610.1109/ECTC32696.2021.00116 ↗
47. L Pan et al (2024) Advanced prediction model for SACQ solder reliability assessment for automotive memory applications In 2024 IEEE 26th Electronics Packaging Technology Conference (EPTC), Institute of Electrical and Electronics Engineers Inc. 855–858 https://doi.org/10.1109/EPTC62800.2024.1090997710.1109/EPTC62800.2024.10909977 ↗
48. Belhadi MEA, Wentlent L, Al-Athamneh R, Hamasha S (2019) Mechanical properties of SAC-Bi solder alloys with aging. In: International SMTA (ed) Rosemont. USA, IL, pp 431–438
49. Vianco PT, Neilsen MK, Williams S, Bradley DR, Diebold TW (2023) Elastic modulus and coefficient of thermal expansion of 91.84Sn-3.33Ag-4.83Bi Pb-Free solder. J Electron Mater 52(3):2116–2138. https://doi.org/10.1007/S11664-022-10159-Y/FIGURES/2410.1007/S11664-022-10159-Y/FIGURES/24 ↗
50. Delhaise AM, Perovic DD (2018) Study of solid-state diffusion of Bi in polycrystalline Sn using electron probe microanalysis. J Electron Mater 47(3):2057–2065. https://doi.org/10.1007/s11664-017-6011-x10.1007/s11664-017-6011-x ↗
51. Belyakov SA et al (2019) Precipitation and coarsening of bismuth plates in Sn–Ag–Cu–Bi and Sn–Cu–Ni–Bi solder joints. J Mater Sci Mater Electron 30(1):378–390. https://doi.org/10.1007/s10854-018-0302-810.1007/s10854-018-0302-8 ↗
52. Shen Y-A (2023) Bi dispersion hardening in Sn-Bi alloys by solid-state aging. JOM 75(11):4922–4930. https://doi.org/10.1007/s11837-023-06079-910.1007/s11837-023-06079-9 ↗
53. Hsieh C-L, Coyle RJ, Gourlay CM (2025) Time-lapse imaging of Bismuth precipitation and coarsening on the surface of Sn–Ag–Cu–Bi solder joints after thermal cycling. J Electron Mater. https://doi.org/10.1007/s11664-025-11747-410.1007/s11664-025-11747-4 ↗
54. Yang KH, Choo WK (1994) The variants of the orientation relationship between austenite and cementite in Fe-30wt%Mn-1.0wt%C alloy. Acta Metall Mater 42(1):263–269. https://doi.org/10.1016/0956-7151(94)90068-X10.1016/0956-7151(94)90068-X ↗
55. Zhang RY et al (2022) γ variant-sensitive deformation behaviour of Inconel 718 superalloy. J Mater Sci Technol 126:169–181. https://doi.org/10.1016/j.jmst.2022.03.01810.1016/j.jmst.2022.03.018 ↗
56. Feng ZQ et al (2011) Variant selection and the strengthening effect of S precipitates at dislocations in Al–Cu–Mg alloy. Acta Mater 59(6):2412–2422. https://doi.org/10.1016/j.actamat.2010.12.04110.1016/j.actamat.2010.12.041 ↗
57. Nie JF (2012) Precipitation and hardening in magnesium alloys. Metall and Mater Trans A 43(11):3891–3939. https://doi.org/10.1007/S11661-012-1217-210.1007/S11661-012-1217-2 ↗
58. Jona F (1967) Low-energy electron diffraction study of surfaces of antimony and bismuth. Surf Sci 8(1–2):57–76. https://doi.org/10.1016/0039-6028(67)90073-810.1016/0039-6028(67)90073-8 ↗
59. Hofmann P (2006) The surfaces of bismuth: structural and electronic properties. Prog Surf Sci 81(5):191–245. https://doi.org/10.1016/j.progsurf.2006.03.00110.1016/j.progsurf.2006.03.001 ↗
60. H Arnold (2006) Transformations of the coordinate system (unit-cell transformations). In International Tables for Crystallography, Chester, England: International Union of Crystallography, 78–85 https://doi.org/10.1107/9780955360206000051010.1107/97809553602060000510 ↗
61. Martin S, Winkelmann A, Leineweber A (2022) Domain structure of pseudosymmetric η″-ordered Cu6Sn5 by EBSD analysis. Acta Mater 229:117828. https://doi.org/10.1016/j.actamat.2022.11782810.1016/j.actamat.2022.117828 ↗
62. Swanson HE, Tatge E (1953) Standard X-ray diffraction powder patterns, vol 1. National Bureau of Standards, Washington, DC
63. Rossi PJ, Zotov N, Mittemeijer EJ (2016) Redetermination of the crystal structure of the Ag 3 Sn intermetallic compound. Zeitschrift für Kristallographie - Crystalline Materials 231(1):1–9. https://doi.org/10.1515/zkri-2015-186710.1515/zkri-2015-1867 ↗
64. Gangulee A, Das GC, Bever MB (1973) An X-ray diffraction and calorimetric investigation of the compound Cu6Sn5. Mach Des 4(9):2063–2066. https://doi.org/10.1007/bf0264326810.1007/bf02643268 ↗
65. Larsson A-K, Stenberg L, Lidin S (1994) The superstructure of domain-twinned η’′-Cu6Sn 5. Acta Crystallogr B Struct Sci. https://doi.org/10.1107/S010876819400405210.1107/S0108768194004052 ↗
66. Cucka P, Barrett CS (1962) The crystal structure of Bi and of solid solutions of Pb, Sn, Sb and Te in Bi. Acta Crystallogr 15(9):865–872. https://doi.org/10.1107/s0365110x6200229710.1107/s0365110x62002297 ↗
67. National Institute of Standards and Technology (2024) Phase diagram & computational thermodynamics. Accessed: Jul. 16, 2024. [Online]. Available: https://www.metallurgy.nist.gov/phase/solder/agcusn.html
68. Shen X, Zois A, Douglas JO, Gourlay CM (2025) Eutectic orientation relationships in Sn-Bi solder. J Alloys Compd 1035:181339. https://doi.org/10.1016/J.JALLCOM.2025.18133910.1016/J.JALLCOM.2025.181339 ↗
69. Lifshitz IM, Slyozov VV (1961) The kinetics of precipitation from supersaturated solid solutions. J Phys Chem Solids 19(1–2):35–50. https://doi.org/10.1016/0022-3697(61)90054-310.1016/0022-3697(61)90054-3 ↗
70. Wagner C (1961) Theorie der Alterung von Niederschlägen durch Umlösen (Ostwald‐Reifung). Zeitschrift für Elektrochemie, Berichte der Bunsengesellschaft für physikalische Chemie 65(7–8):581–591. https://doi.org/10.1002/bbpc.1961065070410.1002/bbpc.19610650704 ↗
71. Takajo S, Kaysser WA, Petzow G (1984) Analysis of particle growth by coalescence during liquid phase sintering. Acta Metall 32(1):107–113. https://doi.org/10.1016/0001-6160(84)90207-410.1016/0001-6160(84)90207-4 ↗
72. Bramfitt BL (1970) The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron. Metall Trans 1(7):1987–1995. https://doi.org/10.1007/BF0264279910.1007/BF02642799 ↗
73. Lee JA, Raynor GV (1954) The lattice spacings of binary tin-rich alloys. Proc Phys Soc B 67(10):737–747. https://doi.org/10.1088/0370-1301/67/10/30110.1088/0370-1301/67/10/301 ↗
74. Nabarro FRN (1940) The strains produced by precipitation in alloys. Proc R Soc Lond A Math Phys Sci 175(963):519–538. https://doi.org/10.1098/rspa.1940.007210.1098/rspa.1940.0072 ↗
75. Porter DA, Easterling KE, Sherif MY (2009) Phase transformations in metals and alloys (revised reprint). CRC press10.1201/9781439883570 ↗
76. Telang AU, Bieler TR, Zamiri A, Pourboghrat F (2007) Incremental recrystallization/grain growth driven by elastic strain energy release in a thermomechanically fatigued lead-free solder joint. Acta Mater 55(7):2265–2277. https://doi.org/10.1016/j.actamat.2006.11.02310.1016/j.actamat.2006.11.023 ↗
77. Delhaise AM, Chen Z, Perovic DD (2019) Solid-state diffusion of Bi in Sn: effects of β-Sn grain orientation. J Electron Mater 48(1):32–43. https://doi.org/10.1007/s11664-018-6621-y10.1007/s11664-018-6621-y ↗
78. Delhaise AM, Chen Z, Perovic DD (2019) Solid-state diffusion of Bi in Sn: effects of anisotropy, temperature, and high diffusivity pathways. JOM 71(1):133–142. https://doi.org/10.1007/s11837-018-3145-010.1007/s11837-018-3145-0 ↗
79. Shewmon P (2016) Diffusion in solids. Springer International Publishing, Cham. https://doi.org/10.1007/978-3-319-48206-410.1007/978-3-319-48206-4 ↗
80. Thermo-Calc (2022) TCSLD Database version 4.1
81. Lidin S (1998) Superstructure ordering of intermetallics: B8 structures in the pseudo-cubic regime. Acta Crystallogr B 54(2):97–108. https://doi.org/10.1107/S010876819701879X10.1107/S010876819701879X ↗
82. Xian JW et al (2018) Influence of Ni on the refinement and twinning of primary Cu6Sn5 in Sn-0.7Cu-0.05Ni. Intermetallics (Barking) 102:34–45. https://doi.org/10.1016/j.intermet.2018.08.00210.1016/j.intermet.2018.08.002 ↗
83. Leineweber A (2023) The Cu–Sn system: a comprehensive review of the crystal structures of its stable and metastable phases. J Phase Equilib Diffus 44(3):343–393. https://doi.org/10.1007/S11669-023-01041-310.1007/S11669-023-01041-3 ↗
84. Nogita K (2010) Stabilisation of Cu6Sn5 by Ni in Sn-0.7Cu-0.05Ni lead-free solder alloys. Intermetallics (Barking) 18(1):145–149. https://doi.org/10.1016/j.intermet.2009.07.00510.1016/j.intermet.2009.07.005 ↗