Tribological behavior of nanostructured AlSi10Mg fabricated by laser powder bed fusion/high-pressure torsion hybrid
Source abstract
Abstract
The hybrid laser powder bed fusion/high-pressure torsion (LPBF/HPT) approach has emerged as an effective method to enhance the mechanical properties of metals/alloys via the ultrafine and/or nanoscale grain refinement route. However, most studies on this approach have largely focused on the investigation of microstructure and mechanical properties, while studies on tribological performance are significantly limited despite its importance in many engineering applications. Thus, in this study, the tribological behavior of a nanostructured AlSi10Mg alloy (AlSi10Mg being a critical material for key automotive components) fabricated by the hybrid LPBF/HPT approach is investigated for the first time. The results of dry sliding wear tests conducted in reciprocating linear pin-on-disk mode demonstrate enhancement in the tribological performance after HPT processing, as indicated by the comprehensive reductions in coefficient of friction (COF), mass loss, m , and specific wear rate, k values with increasing number of HPT revolutions, amounting to improvements of ~ 25, ~ 64, and ~ 71%, respectively, after 10 revolutions relative to the as-received condition. The overall enhanced tribological performance can be ascribed to the significantly high hardness attained due to the extreme grain refinement resulting from the HPT-imposed torsional strains.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Surface Treatment and Residual Stress · High Entropy Alloys Studies · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Gadlegaonkar N, Bansod PJ, Lakshmikanthan A, Bhole K (2025) A Review on additively manufactured AlSi10Mg alloy: mechanical, tribological, and microstructure properties. J Min Met Fuels. https://doi.org/10.18311/jmmf/2025/4662110.18311/jmmf/2025/46621 ↗
2. Van Cauwenbergh P, Samaee V, Thijs L, Nejezchlebová J, Sedlák P, Iveković A, Schryvers D, Van Hooreweder B, Vanmeensel K (2021) Unravelling the multi-scale structure–property relationship of laser powder bed fusion processed and heat-treated AlSi10Mg. Sci Rep 11:1–15. https://doi.org/10.1038/s41598-021-85047-210.1038/s41598-021-85047-2 ↗
3. Zhu Z, Hu Z, Seet HL, Liu T, Liao W, Ramamurty U, Ling Nai SM (2023) Recent progress on the additive manufacturing of aluminum alloys and aluminum matrix composites: microstructure, properties, and applications. Int J Mach Tools Manuf 190:104047. https://doi.org/10.1016/j.ijmachtools.2023.10404710.1016/j.ijmachtools.2023.104047 ↗
4. Kladovasilakis N, Charalampous P, Tsongas K, Kostavelis I, Tzovaras D, Tzetzis D (2022) Influence of selective laser melting additive manufacturing parameters in Inconel 718 superalloy. Materials 15:1–19. https://doi.org/10.3390/ma1504136210.3390/ma15041362 ↗
5. Sabirov I, Murashkin MY, Valiev RZ (2013) Nanostructured aluminium alloys produced by severe plastic deformation: new horizons in development. Mater Sci Eng A 560:1–24. https://doi.org/10.1016/j.msea.2012.09.02010.1016/j.msea.2012.09.020 ↗
6. Valiev RZ, Sabirov I, Zhilyaev AP, Langdon TG (2012) Bulk nanostructured metals for innovative applications. JOM 64:1134–1142. https://doi.org/10.1007/s11837-012-0427-910.1007/s11837-012-0427-9 ↗
7. Langdon TG (2013) Twenty-five years of ultrafine-grained materials: achieving exceptional properties through grain refinement. Acta Mater 61:7035–7059. https://doi.org/10.1016/j.actamat.2013.08.01810.1016/j.actamat.2013.08.018 ↗
8. Edalati K, Bachmaier A, Beloshenko VA, Beygelzimer Y, Blank VD, Botta WJ, Bryła K, Čížek J, Divinski S, Enikeev NA, Estrin Y, Faraji G, Figueiredo RB, Fuji M, Furuta T, Grosdidier T, Gubicza J, Hohenwarter A, Horita Z, Huot J, Ikoma Y, Janeček M, Kawasaki M, Král P, Kuramoto S, Langdon TG, Leiva DR, Levitas VI, Mazilkin A, Mito M, Miyamoto H, Nishizaki T, Pippan R, Popov VV, Popova EN, Purcek G, Renk O, Révész Á, Sauvage X, Sklenicka V, Skrotzki W, Straumal BB, Suwas S, Toth LS, Tsuji N, Valiev RZ, Wilde G, Zehetbauer MJ, Zhu X (2022) Nanomaterials by severe plastic deformation: review of historical developments and recent advances. Mater Res Lett 10:163–256. https://doi.org/10.1080/21663831.2022.202977910.1080/21663831.2022.2029779 ↗
9. Edalati K, Ahmed AQ, Akrami S, Ameyama K, Aptukov V, Asfandiyarov RN, Ashida M, Astanin V, Bachmaier A, Beloshenko V, Bobruk EV, Bryła K, Cabrera JM, Carvalho AP, Chinh NQ, Choi IC, Chulist R, Cubero-Sesin JM, Davdian G, Demirtas M, Divinski S, Durst K, Dvorak J, Edalati P, Emura S, Enikeev NA, Faraji G, Figueiredo RB, Floriano R, Fouladvind M, Fruchart D, Fuji M, Fujiwara H, Gajdics M, Gheorghe D, Gondek L, González-Hernández JE, Gornakova A, Grosdidier T, Gubicza J, Gunderov D, He L, Higuera OF, Hirosawa S, Hohenwarter A, Horita Z, Horky J, Huang Y, Huot J, Ikoma Y, Ishihara T et al (2024) Severe plastic deformation for producing superfunctional ultrafine-grained and heterostructured materials: an interdisciplinary review. J Alloys Compd. https://doi.org/10.1016/j.jallcom.2024.17466710.1016/j.jallcom.2024.174667 ↗
10. Yusuf SM, Nie M, Chen Y, Yang S, Gao N (2018) Microstructure and corrosion performance of 316L stainless steel fabricated by selective laser melting and processed through high-pressure torsion. J Alloys Compd 763:360–375. https://doi.org/10.1016/j.jallcom.2018.05.28410.1016/j.jallcom.2018.05.284 ↗
11. Mohd Yusuf S, Chen Y, Yang S, Gao N (2020) Microstructural evolution and strengthening of selective laser melted 316L stainless steel processed by high-pressure torsion. Mater Charact 159:110012. https://doi.org/10.1016/j.matchar.2019.11001210.1016/j.matchar.2019.110012 ↗
12. Mohd Yusuf S, Chen Y, Yang S, Gao N (2020) Micromechanical response of additively manufactured 316L stainless steel processed by high-pressure torsion. Adv Eng Mater 22(10):2000052. https://doi.org/10.1002/adem.20200005210.1002/adem.202000052 ↗
13. Yusuf SM, Lim D, Chen Y, Yang S, Gao N (2021) Tribological behaviour of 316L stainless steel additively manufactured by laser powder bed fusion and processed via high-pressure torsion. J Mater Process Technol 290:116985. https://doi.org/10.1016/j.jmatprotec.2020.11698510.1016/j.jmatprotec.2020.116985 ↗
14. Yusuf SM, Hoegden M, Gao N (2020) Effect of sample orientation on the microstructure and microhardness of additively manufactured AlSi10Mg processed by high-pressure torsion. Int J Adv Manuf Technol 106:4321–4337. https://doi.org/10.1007/s00170-019-04817-510.1007/s00170-019-04817-5 ↗
15. Hosseinzadeh A, Radi A, Richter J, Wegener T, Sajadifar SV, Niendorf T, Yapici GG (2021) Severe plastic deformation as a processing tool for strengthening of additive manufactured alloys. J Manuf Process 68:788–795. https://doi.org/10.1016/j.jmapro.2021.05.07010.1016/j.jmapro.2021.05.070 ↗
16. Snopiński P, Woźniak A, Pagáč M (2021) Microstructural evolution, hardness, and strengthening mechanisms in SLM AlSi10Mg alloy subjected to equal-channel angular pressing (ECAP). Materials. https://doi.org/10.3390/ma1424759810.3390/ma14247598 ↗
17. Mohd Yusuf S, Chen Y, Musa NH, Mazlan N, Nordin NA, Nazmi N, Mazlan SA, Gao N (2022) Elimination of porosity in additively manufactured 316L stainless steel by high-pressure torsion. Int J Adv Manuf Technol 123:1175–1187. https://doi.org/10.1007/s00170-022-10228-w10.1007/s00170-022-10228-w ↗
18. Yusuf SM, Chen Y, Gao N (2021) Influence of high-pressure torsion on the microstructure and microhardness of additively manufactured 316L stainless steel. Metals 11:1–12
19. Edalati K, Horita Z, Langdon TG (2009) The significance of slippage in processing by high-pressure torsion. Scr Mater 60:9–12. https://doi.org/10.1016/j.scriptamat.2008.08.04210.1016/j.scriptamat.2008.08.042 ↗
20. Gunderov D, Asfandiyarov R, Titov V, Gunderova S, Astanin V (2023) Some slippage issues in high-pressure torsion using Cu and Ti samples as an example. Materials 16:1–13. https://doi.org/10.3390/ma1601016210.3390/ma16010162 ↗
21. Sahu S, Ren Y, Kumar D, Hamilton AR, Gao N (2025) Microstructure, mechanical properties, and corrosion behavior of laser powder bed fused AlSi10Mg alloy after high-pressure torsion. J Mater Eng Perform. https://doi.org/10.1007/s11665-025-11821-210.1007/s11665-025-11821-2 ↗
22. Edalati K, Miresmaeili R, Horita Z, Kanayama H, Pippan R (2011) Significance of temperature increase in processing by high-pressure torsion. Mater Sci Eng A 528:7301–7305. https://doi.org/10.1016/j.msea.2011.06.03110.1016/j.msea.2011.06.031 ↗
23. Zhang Y, Shen D, Liu G, Tang B (2024) Effect of high-pressure torsion temperatures on the precipitation and properties of Cu-Cr alloy. Materials. https://doi.org/10.3390/ma1717442910.3390/ma17174429 ↗
24. Edalati K, Horita Z (2011) Significance of homologous temperature in softening behavior and grain size of pure metals processed by high-pressure torsion. Mater Sci Eng A 528:7514–7523. https://doi.org/10.1016/j.msea.2011.06.08010.1016/j.msea.2011.06.080 ↗
25. Edalati K, Horita Z (2016) A review on high-pressure torsion (HPT) from 1935 to 1988. Mater Sci Eng A 652:325–352. https://doi.org/10.1016/j.msea.2015.11.07410.1016/j.msea.2015.11.074 ↗
26. Thorvaldsen A (1997) The intercept method—1. evaluation of grain shape. Acta Mater 45:587–594. https://doi.org/10.1016/S1359-6454(96)00197-810.1016/S1359-6454(96)00197-8 ↗
27. Han JK, Lee HJ, Jang J, Kawasaki M, Langdon TG (2017) Micro-mechanical and tribological properties of aluminum-magnesium nanocomposites processed by high-pressure torsion. Mater Sci Eng A 684:318–327. https://doi.org/10.1016/j.msea.2016.12.06710.1016/j.msea.2016.12.067 ↗
28. Tucho WM, Cuvillier P, Sjolyst-Kverneland A, Hansen V (2017) Microstructure and hardness studies of Inconel 718 manufactured by selective laser melting before and after solution heat treatment. Mater Sci Eng A 689:220–232. https://doi.org/10.1016/j.msea.2017.02.06210.1016/j.msea.2017.02.062 ↗
29. Tucho WM, Lysne VH, Austbø H, Sjolyst-Kverneland A, Hansen V (2018) Investigation of effects of process parameters on microstructure and hardness of SLM manufactured SS316L. J Alloys Compd 740:910–925. https://doi.org/10.1016/j.jallcom.2018.01.09810.1016/j.jallcom.2018.01.098 ↗
30. Kawasaki M, Lee HJ, Ahn B, Zhilyaev AP, Langdon TG (2014) Evolution of hardness in ultrafine-grained metals processed by high-pressure torsion. J Mater Res Technol 3:311–318. https://doi.org/10.1016/j.jmrt.2014.06.00210.1016/j.jmrt.2014.06.002 ↗
31. Al-Zubaydi ASJ, Gao N, Wang S, Reed PAS (2022) Microstructural and hardness evolution of additively manufactured Al–Si–Cu alloy processed by high-pressure torsion. J Mater Sci 57:8956–8977. https://doi.org/10.1007/s10853-022-07234-410.1007/s10853-022-07234-4 ↗
32. Kawasaki M (2014) Different models of hardness evolution in ultrafine-grained materials processed by high-pressure torsion. J Mater Sci 49:18–34. https://doi.org/10.1007/s10853-013-7687-910.1007/s10853-013-7687-9 ↗
33. Archard JF (1953) Contact and rubbing of flat surfaces. J Appl Phys 24:98110.1063/1.1721448 ↗
34. El Aal MIA, Kim HS (2014) Wear properties of high pressure torsion processed ultrafine grained Al-7%Si alloy. Mater Des 53:373–382. https://doi.org/10.1016/j.matdes.2013.07.04510.1016/j.matdes.2013.07.045 ↗
35. Edalati K, Ashida M, Horita Z, Matsui T, Kato H (2014) Wear resistance and tribological features of pure aluminum and Al-Al2O3 composites consolidated by high-pressure torsion. Wear 310:83–89. https://doi.org/10.1016/j.wear.2013.12.02210.1016/j.wear.2013.12.022 ↗
36. Kayaba T, Hokkirigawa K, Kato K (1986) Analysis of the abrasive wear mechanism by successive observations of wear processes in a scanning electron microscope. Wear 110:419–43010.1016/0043-1648(86)90115-8 ↗
37. Kato H, Todaka Y (2017) Microstructure and wear properties of high-pressure torsion processed iron. Mater Sci Forum 890:371–374. https://doi.org/10.4028/www.scientific.net/MSF.890.37110.4028/www.scientific.net/MSF.890.371 ↗
38. Gode C, Yilmazer H, Ozdemir I, Todaka Y (2014) Microstructural refinement and wear property of Al-Si-Cu composite subjected to extrusion and high-pressure torsion. Mater Sci Eng A 618:377–384. https://doi.org/10.1016/j.msea.2014.09.01110.1016/j.msea.2014.09.011 ↗
39. Yusuf SM, Lazim NH, Nordin NA, Mazlan SA, Gao N (2024) Synthesis of an ultra-high hardness nanostructured AlSi10Mg alloy via a hybrid laser powder bed fusion/high-pressure torsion approach. J Adv Res Micro Nano Eng 21(1):66–74. https://doi.org/10.37934/armne.21.1.667410.37934/armne.21.1.6674 ↗
40. Liu M, Roven HJ, Liu X, Murashkin M, Valiev RZ, Ungár T, Balogh L (2010) Grain refinement in nanostructured Al-Mg alloys subjected to high pressure torsion. J Mater Sci 45:4659–4664. https://doi.org/10.1007/s10853-010-4604-310.1007/s10853-010-4604-3 ↗
41. Kawasaki M, Langdon TG (2012) Developing hardness and microstructural homogeneity in high-pressure torsion. Mater Sci Forum 706–709:1805–1810. https://doi.org/10.4028/www.scientific.net/MSF.706-709.180510.4028/www.scientific.net/MSF.706-709.1805 ↗
42. Gebril MA, Omar MZ, Mohamed IF, Othman NK, Irfan OM (2022) Combining heat treatment and high-pressure torsion to enhance the hardness and corrosion resistance of A356 alloy. Metals. https://doi.org/10.3390/met1205085310.3390/met12050853 ↗
43. Wang X, Nie M, Wang CT, Wang SC, Gao N (2015) Microhardness and corrosion properties of hypoeutectic Al-7Si alloy processed by high-pressure torsion. Mater Des 83:193–202. https://doi.org/10.1016/j.matdes.2015.06.01810.1016/j.matdes.2015.06.018 ↗
44. Mungole T, Nadammal N, Dawra K, Kumar P, Kawasaki M, Langdon TG (2013) Evolution of microhardness and microstructure in a cast Al-7 % Si alloy during high-pressure torsion. J Mater Sci 48:4671–4680. https://doi.org/10.1007/s10853-012-7061-310.1007/s10853-012-7061-3 ↗
45. Zhilyaev AP, García-Infanta JM, Carreño F, Langdon TG, Ruano OA (2007) Particle and grain growth in an Al-Si alloy during high-pressure torsion. Scr Mater 57:763–765. https://doi.org/10.1016/j.scriptamat.2007.06.02910.1016/j.scriptamat.2007.06.029 ↗
46. Muñoz JA, Komissarov A, Avalos M, Bolmaro RE, Zhu Y, Cabrera JM (2024) Improving density and strength-to-ductility ratio of a 3D-printed Al–Si alloy by high-pressure torsion. J Mater Sci 59:6024–6047. https://doi.org/10.1007/s10853-023-09298-210.1007/s10853-023-09298-2 ↗
47. Al-Zubaydi ASJ, Gao N, Džugan J, Podaný P, Chen Y, Reed PAS (2024) Fracture behaviour assessment of the additively manufactured and HPT-processed Al–Si–Cu alloy. Mater Sci Technol. https://doi.org/10.1177/0267083624126247710.1177/02670836241262477 ↗
48. Gu DD, Meiners W, Wissenbach K, Poprawe R (2012) Laser additive manufacturing of metallic components: materials, processes and mechanisms. Int Mater Rev 57:133–164. https://doi.org/10.1179/1743280411Y.000000001410.1179/1743280411Y.0000000014 ↗
49. Amanov A, Lee SW, Pyun YS (2017) Low friction and high strength of 316L stainless steel tubing for biomedical applications. Mater Sci Eng C Mater Biol Appl 71:176–185. https://doi.org/10.1016/j.msec.2016.10.00510.1016/j.msec.2016.10.005 ↗
50. Rezaei-Nejad SS, Abdollah-zadeh A, Hajian M, Kargar F, Seraj R (2015) Formation of nanostructure in AISI 316L austenitic stainless steel by friction stir processing. Procedia Mater Sci 11:397–402. https://doi.org/10.1016/j.mspro.2015.11.00810.1016/j.mspro.2015.11.008 ↗
51. Qin W, Kang J, Li J, Yue W, Liu Y, She D, Mao Q, Li Y (2018) Tribological behavior of the 316L stainless steel with heterogeneous lamella structure. Materials. https://doi.org/10.3390/ma1110183910.3390/ma11101839 ↗
52. Archard JF, Hirst W (1956) The wear of metals under unlubricated conditions. Proc R Soc A 236:397–410. https://doi.org/10.1098/rspa.1956.014410.1098/rspa.1956.0144 ↗
53. Hokkirigawa K, Kato K (1988) An experimental and theoretical investigation of ploughing, cutting and wedge formation during abrasive wear. Tribol Int. https://doi.org/10.1016/0301-679X(88)90128-410.1016/0301-679X(88)90128-4 ↗
54. Hutchings IM (1992) Tribology: friction and wear of engineering materials. Butterworth-Heinemann, London
55. Gao N, Wang CT, Wood RJK, Langdon TG (2012) Tribological properties of ultrafine-grained materials processed by severe plastic deformation. J Mater Sci 47:4779–4797. https://doi.org/10.1007/s10853-011-6231-z10.1007/s10853-011-6231-z ↗