Contributions of sub-surface intergranular phases on fatigue crack initiation in additively manufactured austenitic stainless steel
Source abstract
Abstract
Abstract Fatigue failures in additively manufactured 316L austenitic stainless steel produced using laser powder bed fusion processes are often attributed to the presence of process-related defects or surface roughness. To better investigate the role of surface roughness on fatigue properties, internal pores were mitigated using hot isostatic pressing, and strain-controlled fatigue testing was performed with the surface in the as-deposited condition. In the absence of internal defects, crack initiation was expected to occur at the surface, which displayed arithmetic mean surface roughness (Sa) values between 10 and 40 µm as the build angle decreased from a vertical (90°) to a 45° orientation. Even though a decrease in average fatigue life with this increase in surface roughness was observed, there was no evidence of fatal cracks initiating from as-deposited surface asperities. Instead, widespread brittle intergranular fracture occurred within fine-grained sub-surface regions in the contour passes along the specimen perimeter that were populated by sub-micrometer-sized Cr2N particles and nanometer-sized α-tridymite oxides that decorated the austenite grain boundaries. The width of these brittle fracture regions increased by 100 µm as the build angle changed from 90° to 45°. At the same time, the fraction of decorated grain boundaries (30–45%) and precipitate length (up to 10 µm) within these wider contour regions increased, driving the observed decreases in the fatigue life. Graphical abstract
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Andreau O, Pessard E, Koutiri I, Peyre P, Saintier N (2021) Influence of the position and size of various deterministic defects on the high cycle fatigue resistance of a 316L steel manufactured by laser powder bed fusion. Int J Fatigue 143:105930. https://doi.org/10.1016/j.ijfatigue.2020.10593010.1016/j.ijfatigue.2020.105930 ↗
2. Andreau O, Pessard E, Koutiri I, Penot JD, Dupuy C, Saintier N, Peyre P (2019) A competition between the contour and hatching zones on the high cycle fatigue behaviour of a 316L stainless steel: analyzed using X-ray computed tomography. Mater Sci Eng, A 757:146–159. https://doi.org/10.1016/j.msea.2019.04.10110.1016/j.msea.2019.04.101 ↗
3. Shrestha R, Simsiriwong J, Shamsaei N (2019) Fatigue behavior of additive manufactured 316L stainless steel parts: effects of layer orientation and surface roughness. Addit Manuf 28:23–38. https://doi.org/10.1016/j.addma.2019.04.01110.1016/j.addma.2019.04.011 ↗
4. Shrestha R, Simsiriwong J, Shamsaei N (2021) Fatigue behavior of additive manufactured 316L stainless steel under axial versus rotating-bending loading: synergistic effects of stress gradient, surface roughness, and volumetric defects. Int J Fatigue 144:106063. https://doi.org/10.1016/j.ijfatigue.2020.10606310.1016/j.ijfatigue.2020.106063 ↗
5. Solberg K, Guan S, Razavi SMJ, Welo T, Chan KC, Berto F (2019) Fatigue of additively manufactured 316L stainless steel: the influence of porosity and surface roughness. Fatigue Fract Eng Mater Struct 42:2043–2052. https://doi.org/10.1111/ffe.1307710.1111/ffe.13077 ↗
6. Solberg K, Hovig EW, Sørby K, Berto F (2021) Directional fatigue behaviour of maraging steel grade 300 produced by laser powder bed fusion. Int J Fatigue 149:106229. https://doi.org/10.1016/j.ijfatigue.2021.10622910.1016/j.ijfatigue.2021.106229 ↗
7. ASTM, Standard Test Method for Strain-Controlled Fatigue Testing - E606, (2012). https://doi.org/10.1520/E0606-04E01.Copyright.10.1520/E0606-04E01.Copyright ↗
8. Li P, Warner DH, Pegues JW, Roach MD, Shamsaei N, Phan N (2019) Investigation of the mechanisms by which hot isostatic pressing improves the fatigue performance of powder bed fused Ti-6Al-4V. Int J Fatigue 120:342–352. https://doi.org/10.1016/j.ijfatigue.2018.10.01510.1016/j.ijfatigue.2018.10.015 ↗
9. Hastie JC, Kartal ME, Carter LN, Attallah MM, Mulvihill DM (2020) Classifying shape of internal pores within AlSi10Mg alloy manufactured by laser powder bed fusion using 3D X-ray micro computed tomography: Influence of processing parameters and heat treatment. Mater Charact 163:110225. https://doi.org/10.1016/j.matchar.2020.11022510.1016/j.matchar.2020.110225 ↗
10. Lavery NP, Cherry J, Mehmood S, Davies H, Girling B, Sackett E, Brown SGR, Sienz J (2017) Effects of hot isostatic pressing on the elastic modulus and tensile properties of 316L parts made by powder bed laser fusion. Mater Sci Eng, A 693:186–213. https://doi.org/10.1016/j.msea.2017.03.10010.1016/j.msea.2017.03.100 ↗
11. Beddoes J, Bibby MJ (2003) Principles of metal manufacturing processes. Elsevier Butterworth-Heinemann, Boston
12. Iams AD, Keist JS, Palmer TA (2020) Formation of austenite in additively manufactured and post-processed duplex stainless steel alloys. Metall Mater Trans A Phys Metall Mater Sci 51:982–999. https://doi.org/10.1007/s11661-019-05562-w10.1007/s11661-019-05562-w ↗
13. Wietecha-Reiman IJ, Sabol SM, Palmer TA (2024) Developing statistical tools to analyze historical stress-controlled fatigue data in additively manufactured austenitic stainless steel. Mater Sci Eng: A 902:146580. https://doi.org/10.1016/j.msea.2024.14658010.1016/j.msea.2024.146580 ↗
14. Mower TM, Long MJ (2016) Mechanical behavior of additive manufactured, powder-bed laser-fused materials. Mater Sci Eng, A 651:198–213. https://doi.org/10.1016/j.msea.2015.10.06810.1016/j.msea.2015.10.068 ↗
15. Spierings AB, Starr TL, Wegener K (2013) Fatigue performance of additive manufactured metallic parts. Rapid Prototyp J 19:88–94. https://doi.org/10.1108/1355254131130293210.1108/13552541311302932 ↗
16. Uhlmann E, Fleck C, Gerlitzky G, Faltin F (2017) Dynamical fatigue behavior of additive manufactured products for a fundamental life cycle approach. Procedia CIRP 61:588–593. https://doi.org/10.1016/j.procir.2016.11.13810.1016/j.procir.2016.11.138 ↗
17. Voloskov B, Evlashin S, Dagesyan S, Abaimov S, Akhatov I, Sergeichev I (2020) Very high cycle fatigue behavior of additively manufactured 316L stainless steel. Materials 13:1–11. https://doi.org/10.3390/ma1315329310.3390/ma13153293 ↗
18. Zhang M, Sun CN, Zhang X, Goh PC, Wei J, Hardacre D, Li H (2017) Fatigue and fracture behaviour of laser powder bed fusion stainless steel 316L: influence of processing parameters. Mater Sci Eng, A 703:251–261. https://doi.org/10.1016/j.msea.2017.07.07110.1016/j.msea.2017.07.071 ↗
19. Zhang M, Sun CN, Zhang X, Goh PC, Wei J, Hardacre D, Li H (2018) Effect of heat treatment on fatigue crack initiation of laser powder bed fusion stainless steel 316L. MATEC Web Conf 165:1–6. https://doi.org/10.1051/matecconf/20181652200610.1051/matecconf/201816522006 ↗
20. Zhang M, Sun CN, Zhang X, Wei J, Hardacre D, Li H (2019) High cycle fatigue and ratcheting interaction of laser powder bed fusion stainless steel 316L: fracture behaviour and stress-based modelling. Int J Fatigue 121:252–264. https://doi.org/10.1016/j.ijfatigue.2018.12.01610.1016/j.ijfatigue.2018.12.016 ↗
21. Elangeswaran C, Cutolo A, Muralidharan GK, de Formanoir C, Berto F, Vanmeensel K, Van Hooreweder B (2019) Effect of post-treatments on the fatigue behaviour of 316L stainless steel manufactured by laser powder bed fusion. Int J Fatigue 123:31–39. https://doi.org/10.1016/j.ijfatigue.2019.01.01310.1016/j.ijfatigue.2019.01.013 ↗
22. Blinn B, Klein M, Gläßner C, Smaga M, Aurich JC, Beck T (2018) An investigation of the microstructure and fatigue behavior of additively manufactured AISI 316L stainless steel with regard to the influence of heat treatment. Metals (Basel) 8:220. https://doi.org/10.3390/met804022010.3390/met8040220 ↗
23. Kumar P, Jayaraj R, Suryawanshi J, Satwik UR, McKinnell J, Ramamurty U (2020) Fatigue strength of additively manufactured 316L austenitic stainless steel. Acta Mater 199:225–239. https://doi.org/10.1016/j.actamat.2020.08.03310.1016/j.actamat.2020.08.033 ↗
24. Leuders S, Lieneke T, Lammers S, Tröster T, Niendorf T (2014) On the fatigue properties of metals manufactured by selective laser melting - the role of ductility. J Mater Res 29:1911–1919. https://doi.org/10.1557/jmr.2014.15710.1557/jmr.2014.157 ↗
25. Liverani E, Toschi S, Ceschini L, Fortunato A (2017) Effect of selective laser melting (SLM) process parameters on microstructure and mechanical properties of 316L austenitic stainless steel. J Mater Process Technol 249:255–263. https://doi.org/10.1016/j.jmatprotec.2017.05.04210.1016/j.jmatprotec.2017.05.042 ↗
26. Riemer A, Leuders S, Thöne M, Richard HA, Tröster T, Niendorf T (2014) On the fatigue crack growth behavior in 316L stainless steel manufactured by selective laser melting. Eng Fract Mech 120:15–25. https://doi.org/10.1016/j.engfracmech.2014.03.00810.1016/j.engfracmech.2014.03.008 ↗
27. Rogers J, Qian M, Elambasseril J, Burvill C, Brice C, Wallbrink C, Brandt M, Leary M (2023) Fatigue test data applicability for additive manufacture: a method for quantifying the uncertainty of AM fatigue data. Mater Des 231:111978. https://doi.org/10.1016/j.matdes.2023.11197810.1016/j.matdes.2023.111978 ↗
28. Khonsari MM, Amiri M (2013) Introduction to thermodynamics of mechanical fatigue. Taylor & Francis, New York
29. Suresh S (2004) Fatigue of materials, 2nd edn. Cambridge University Press, New Yor
30. Mike Gedeon, Stress Life vs. Strain Life, Materion Brush Technical Tidbits (2014). https://materion.com/-/media/files/alloy/newsletters/technical-tidbits/issue-no-67---stress-life-vs-strain-life.pdf.
31. Falkowska A, Seweryn A, Tomczyk A (2018) Fatigue life and strength of 316L sintered steel of varying porosity. Int J Fatigue 111:161–176. https://doi.org/10.1016/j.ijfatigue.2018.02.02310.1016/j.ijfatigue.2018.02.023 ↗
32. Kluczyński J, Śnieżek L, Grzelak K, Torzewski J, Szachogłuchowicz I, Oziębło A, Perkowski K, Wachowski M, Małek M (2020) The influence of heat treatment on low cycle fatigue properties of selectively laser melted 316l steel. Materials 13:1–20. https://doi.org/10.3390/ma1324573710.3390/ma13245737 ↗
33. Unigovski YB, Lothongkum G, Gutman EM, Alush D, Cohen R (2009) Low-cycle fatigue behavior of 316L-type stainless steel in chloride solutions. Corros Sci 51:3014–3020. https://doi.org/10.1016/j.corsci.2009.08.03510.1016/j.corsci.2009.08.035 ↗
34. Sistaninia M, Niffenegger M (2015) Fatigue crack initiation and crystallographic growth in 316L stainless steel. Int J Fatigue 70:163–170. https://doi.org/10.1016/j.ijfatigue.2014.09.01010.1016/j.ijfatigue.2014.09.010 ↗
35. Suzuki K, Fukakura J, Kashiwaya H (1988) Cryogenic fatigue properties of 304L and 316L stainless steels compared to mechanical strength and increasing magnetic permeability. J Test Eval 16:190–197. https://doi.org/10.1520/jte11161j10.1520/jte11161j ↗
36. Blinn B, Ley M, Buschhorn N, Teutsch R, Beck T (2019) Investigation of the anisotropic fatigue behavior of additively manufactured structures made of AISI 316L with short-time procedures PhyBaL LIT and PhyBaL CHT. Int J Fatigue 124:389–399. https://doi.org/10.1016/j.ijfatigue.2019.03.02210.1016/j.ijfatigue.2019.03.022 ↗
37. Qu X, Li X, Zhang L, Yi D, Wang J, Wen C, Zhao Z, Gu X, Lin Y, Liu B, Cao Y, Bai P (2024) Effect of construction angles on the microstructure and mechanical properties of LPBF-fabricated 15–5 PH stainless steel. Mater Sci Eng: A 72:900. https://doi.org/10.1016/j.msea.2024.14642310.1016/j.msea.2024.146423 ↗
38. Cabanettes F, Joubert A, Chardon G, Dumas V, Rech J, Grosjean C, Dimkovski Z (2018) Topography of as built surfaces generated in metal additive manufacturing: a multi scale analysis from form to roughness. Precis Eng 52:249–265. https://doi.org/10.1016/j.precisioneng.2018.01.00210.1016/j.precisioneng.2018.01.002 ↗
39. Sanderson J (2019) Understanding light microscopy. John Wiley and Sons Ltd, Hoboken10.1002/9781118696736 ↗
40. ASME, (2019) ASME Standards Collection - ASME B46.1 2009 http://asmestandardscollection.org/PrinterFriendly.aspx?scope=DOCO, 1–124.
41. Sheather SJ (2009) A modern approach to regression with R. Springer, New York10.1007/978-0-387-09608-7 ↗
42. Kutner M, Nachtsheim C, Neter J, Li W (2005) Applied linear statistical models, 5th edn. McGraw-Hill, New York
43. Ott RL, Longnecker M (2016) Statistical methods and data analysis, 7th edn. Cengage Learning, Boston
44. Vander Voort GF (1999) Metallography: principles and practice. ASM International, The Netherlands
45. Flewitt EJ, Peter RKW (2017) Physical methods for materials characterization, 3rd edn. CRC Press, Boca Raton10.1201/9781315382012 ↗
46. Giannuzzi LA, Stevie FA (2005) Introduction to focused ion beams: instrumentation theory techniques and practice. Springer, Berlin10.1007/b101190 ↗
47. Cliff G, Lorimer GW (1975) The quantitative analysis of thin specimens. J Microsc 103:203–20710.1111/j.1365-2818.1975.tb03895.x ↗
48. Wietecha-Reiman IJ, Segall A, Zhao X, Palmer TA (2023) Combining fractal and topological analyses to quantify fracture surfaces in additively manufactured Ti-6Al-4V. Int J Fatigue 166:107232. https://doi.org/10.1016/j.ijfatigue.2022.10723210.1016/j.ijfatigue.2022.107232 ↗
49. Brooks CR, Choudhury A (2002) Failure analysis of engineering materials. McGraw-Hill, New York
50. Lee S, Pegues JW, Shamsaei N (2020) Fatigue behavior and modeling for additive manufactured 304L stainless steel: the effect of surface roughness. Int J Fatigue 141:105856. https://doi.org/10.1016/j.ijfatigue.2020.10585610.1016/j.ijfatigue.2020.105856 ↗
51. Sunwoo H, Fine ME, Meshii M, Stone DH (1982) Cyclic deformation of pearlitic eutectoid rail steel. Metall Trans A 13:2035–2047. https://doi.org/10.1007/BF0264594910.1007/BF02645949 ↗
52. Sadeghi E, Karimi P, Israelsson N, Shipley J, Månsson T, Hansson T (2020) Inclusion-induced fatigue crack initiation in powder bed fusion of Alloy 718. Addit Manuf 36:101670. https://doi.org/10.1016/j.addma.2020.10167010.1016/j.addma.2020.101670 ↗
53. Singh UP, Banerjee S (1991) On the origin of pop-in crack extension. Acta Metall Mater 39:1073–108410.1016/0956-7151(91)90194-6 ↗
54. Murakami Y, Endo M (1994) Effects of defects, inclusions and inhomogeneities on fatigue strength. Int J Fatigue 16:163–182. https://doi.org/10.1016/0142-1123(94)90001-910.1016/0142-1123(94)90001-9 ↗
55. ASTM International, ASTM F3184 - 16, (2016) Standard specification for additive manufacturing stainless steel alloy (UNS S31603) with powder bed fusion, i 1–9. https://doi.org/10.1520/F318410.1520/F3184 ↗