Investigation of vulcanization fouling behavior of biomimetic liquid-infused slippery surfaces
Source abstract
Abstract
Mold fouling during vulcanization is a widespread issue faced by tire industry that urgently needed to be addressed as it can degrade comprehensive performance of molded products and increase production time for cleaning mold, resulting in tremendous economic loss and resource consumption. Here, a novel and promising fouling mitigation strategy inspired by nature is presented, and its antifouling behavior in vulcanization conditions is investigated. The inspired slippery liquid-infused surfaces were successfully designed on aluminum alloy by anodic oxidation, followed by myristic acid modification and impregnation with perfluorinated oil. The prepared surfaces showed a water contact angle of 112.3° and sliding angle of 0.5°, accompanying with self-cleaning ability, stability for repelling hot water and under high-pressure condition as well as excellent corrosion resistance in 0.05 M H2SO4 corrosive medium. Moreover, remarkable antifouling performance was obtained for slippery liquid-infused surfaces as no trace of fouling was observed after vulcanization test and thus a potential strategy for practical industrial applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Modification and Superhydrophobicity · Marine Biology and Environmental Chemistry · Polymer Surface Interaction Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Mai YJ, Jie XH, Liu LL, Yu N, Zheng XX (2012) The study on vulcanization fouling behavior of nanocrystalline layer. Surf Interface Anal 44(3):282–287. https://doi.org/10.1002/sia.379910.1002/sia.3799 ↗
2. Chen L, Zeng R, Xiang L, Luo Z, Wang Y (2012) Polydopamine-graft-PEG antifouling coating for quantitative analysis of food proteins by CE. Anal Methods 4(9):2852–2859. https://doi.org/10.1039/C2AY25129A10.1039/C2AY25129A ↗
3. Li F, Meng J, Ye J, Yang B, Tian Q, Deng C (2014) Surface modification of PES ultrafiltration membrane by polydopamine coating and poly (ethylene glycol) grafting: morphology, stability, and anti-fouling. Desalination 344:422–430. https://doi.org/10.1016/j.desal.2014.04.01110.1016/j.desal.2014.04.011 ↗
4. Fang J, Kelarakis A, Wang D, Giannelis EP, Finlay JA, Callow ME, Callow JA (2010) Fouling release nanostructured coatings based on PDMS-polyurea segmented copolymers. Polymer 51(12):2636–2642. https://doi.org/10.1016/j.polymer.2010.04.02410.1016/j.polymer.2010.04.024 ↗
5. Zhang X, Lin M, Lin L, Zhuang M, Ye L, Yang W, Jiang B (2015) Sol–gel preparation of fluoro-containing ORMOSIL antireflective coating with resistance simultaneously to hydrophilic and oleophilic pollutants. J Sol-Gel Sci Techn 74(3):698–706. https://doi.org/10.1007/s10971-015-3651-210.1007/s10971-015-3651-2 ↗
6. Latthe SS, Sutar RS, Kodag VS, Bhosale A, Kumar AM, Sadasivuni KK, Xing R, Liu S (2019) Self–cleaning superhydrophobic coatings: potential industrial applications. Prog Org Coat 128:52–58. https://doi.org/10.1016/j.porgcoat.2018.12.00810.1016/j.porgcoat.2018.12.008 ↗
7. Dalawai SP, Aly MAS, Latthe SS, Xing R, Sutar RS, Nagappan S, Ha CS, Sadasivuni KK, Liu S (2020) Recent advances in durability of superhydrophobic self-cleaning technology: a critical review. Prog Org Coat 138:1–15. https://doi.org/10.1016/j.porgcoat.2019.10538110.1016/j.porgcoat.2019.105381 ↗
8. Zhang D, Wu G, Li H, Cui Y, Zhang Y (2021) Superamphiphobic surfaces with robust self-cleaning, abrasion resistance and anti-corrosion. Chem Eng J 406:1–9. https://doi.org/10.1016/j.cej.2020.12675310.1016/j.cej.2020.126753 ↗
9. Wu Y, Zhao W, Wang W, Sui W (2016) Fabricating binary anti-corrosion structures containing superhydrophobic surfaces and sturdy barrier layers for Al alloys. Rsc Adv 6(6):5100–5110. https://doi.org/10.1039/C5RA25153B10.1039/C5RA25153B ↗
10. Lafuma A, Quéré D (2003) Superhydrophobic states. Nat Mater 2(7):457–460. https://doi.org/10.1038/nmat92410.1038/nmat924 ↗
11. Wong TS, Kang SH, Tang SKY, Smythe EJ, Hatton BD, Grinthal A, Aizenberg J (2011) Bioinspired self-repairing slippery surfaces withpressure-stable omniphobicity. Nature 477:443-447. https://doi.org/10.1038/nature1044710.1038/nature10447 ↗
12. Epstein AK, Wong T-S, Belisle RA, Boggs EM, Aizenberg J (2012) Liquid-infused structured surfaces with exceptional anti-biofouling performance. Surf Coat Tech 109(33):13182–13187. https://doi.org/10.1073/pnas.120197310910.1073/pnas.1201973109 ↗
13. Wang J, Kato K, Blois AP, Wong TS (2016) Bioinspired omniphobic coatings with a thermal self-repair function on industrial materials. Acs Appl Mater Inter 8(12):8265–8271. https://doi.org/10.1021/acsami.6b0019410.1021/acsami.6b00194 ↗
14. MacCallum N, Howell C, Kim P, Sun D, Friedlander R, Ranisau J, Ahanotu O, Lin JJ, Vena A, Hatton B (2015) Liquid-infused silicone as a biofouling-free medical material. Acs Biomater Sci Eng 1(1):43–51. https://doi.org/10.1021/ab500057810.1021/ab5000578 ↗
15. Yu M, Liu M, Hou Y, Fu S, Zhang L, Li M, Wang D (2020) Facile fabrication of biomimetic slippery lubricant-infused transparent and multifunctional omniphobic surfaces. J Mater Sci 55(10):4225–4237. https://doi.org/10.1007/s10853-019-04243-810.1007/s10853-019-04243-8 ↗
16. Cui J, Zhu H, Tu Z, Niu D, Liu G, Bei Y, Zhu Q (2019) Effect of the texture geometry on the slippery behavior of liquid-infused nanoporous surfaces. J Mater Sci 54(3):2729–2739. https://doi.org/10.1007/s10853-018-2972-210.1007/s10853-018-2972-2 ↗
17. Sun J, Wang C, Song J, Huang L, Sun Y, Liu Z, Zhao C, Li Y (2018) Multi-functional application of oil-infused slippery Al surface: from anti-icing to corrosion resistance. J Mate Sci 53(23):16099–16109. https://doi.org/10.1007/s10853-018-2760-z10.1007/s10853-018-2760-z ↗
18. Xie M, Zhao W, Wu Y (2021) Preventing algae biofilm formation via designing long-term oil storage surfaces for excellent antifouling performance. Appl Surf Sci 554:1–9. https://doi.org/10.1016/j.apsusc.2021.14961210.1016/j.apsusc.2021.149612 ↗
19. Wang P, Zhang D, Lu Z, Sun S (2016) Fabrication of slippery lubricant-infused porous surface for inhibition of microbially influenced corrosion. Acs Appl Mater Inter 8(2):1120–1127. https://doi.org/10.1021/acsami.5b0845210.1021/acsami.5b08452 ↗
20. Li J, Kleintschek T, Rieder A, Cheng Y, Baumbach T, Obst U, Schwartz T, Levkin PA (2013) Hydrophobic liquid-infused porous polymer surfaces for antibacterial applications. Acs Appl Mater Inter 5(14):6704–6711. https://doi.org/10.1021/am401532z10.1021/am401532z ↗
21. Manabe K, Kyung K-H, Shiratori S (2015) Biocompatible slippery fluid-infused films composed of chitosan and alginate via layer-by-layer self-assembly and their antithrombogenicity. Acs Appl Mater Inter 7(8):4763–4771. https://doi.org/10.1021/am508393n10.1021/am508393n ↗
22. Yin J, Mei ML, Li Q, Xia R, Zhang Z, Chu CH (2016) Self-cleaning and antibiofouling enamel surface by slippery liquid-infused technique. Sci Rep 6:1–14. https://doi.org/10.1038/srep2592410.1038/srep25924 ↗
23. Liu Z, Pan N, Tao H, Lin J (2021) Temperature-dependent wetting characteristics of micro–nano-structured metal surface formed by femtosecond laser. J Mater Sci 56(4):3525–3534. https://doi.org/10.1007/s10853-020-05457-x10.1007/s10853-020-05457-x ↗
24. Nakajima D, Kikuchi T, Yoshioka T, Matsushima H, Ueda M, Suzuki RO, Natsui S (2019) A superhydrophilic aluminum surface with fast water evaporation based on anodic alumina bundle structures via anodizing in pyrophosphoric acid. Materials 12(21):1–12. https://doi.org/10.3390/ma1221349710.3390/ma12213497 ↗
25. Kim Y, Lee S, Cho H, Park B, Kim D, Hwang W (2012) Robust superhydrophilic/hydrophobic surface based on self-aggregated Al2O3 nanowires by single-step anodization and self-assembly method. Acs Appl Mater Inter 4(10):5074–5078. https://doi.org/10.1021/am301411z10.1021/am301411z ↗
26. Gao X, Jiang L (2004) Water-repellent legs of water striders. Nature 432(7013):36–36. https://doi.org/10.1038/432036a10.1038/432036a ↗
27. Smith JD, Dhiman R, Anand S, Reza-Garduno E, Cohen RE, McKinley GH, Varanasi KK (2013) Droplet mobility on lubricant-impregnated surfaces. Soft Matter 9(6):1772–1780. https://doi.org/10.1039/C2SM27032C10.1039/C2SM27032C ↗
28. Nosonovsky M, Bhushan B (2012) Lotus versus rose: biomimetic surface effects. Green Tribology. https://doi.org/10.1007/978-3-642-23681-5_210.1007/978-3-642-23681-5_2 ↗
29. Vargaftik NB, Volkov BN, Voljak LD (1983) International tables of the surface tension of water. J Phys Chem Ref Data 12(3):817–820. https://doi.org/10.1063/1.55568810.1063/1.555688 ↗
30. Zhu L, Shi P, Xue J, Wang Y, Chen Q, Ding J, Wang Q (2014) Superhydrophobic stability of nanotube array surfaces under impact and static forces. Acs Appl Mater Interfaces 6(11):8073–8079. https://doi.org/10.1021/am500261c10.1021/am500261c ↗
31. Bi P, Li H, Zhao G, Ran M, Cao L, Guo H, Xue Y (2019) Robust super-hydrophobic coating prepared by electrochemical surface engineering for corrosion protection. Coatings 9(7):1–28. https://doi.org/10.3390/coatings907045210.3390/coatings9070452 ↗
32. Liang J, Srinivasan PB, Blawert C, Dietzel W (2010) Influence of chloride ion concentration on the electrochemical corrosion behaviour of plasma electrolytic oxidation coated AM50 magnesium alloy. Electrochim Acta 55(22):6802–6811. https://doi.org/10.1016/j.electacta.2010.05.08710.1016/j.electacta.2010.05.087 ↗
33. Cao Y, Zheng D, Li X, Lin J, Wang C, Dong S, Lin C (2018) Enhanced corrosion resistance of superhydrophobic layered double hydroxide films with long-term stability on Al substrate. Acs Appl Mater Inter 10(17):15150–15162. https://doi.org/10.1021/acsami.8b0228010.1021/acsami.8b02280 ↗
34. Poornima T, Jagannatha N, Shetty AN (2010) Studies on corrosion of annealed and aged 18 Ni 250 grade maraging steel in sulphuric acid medium. Port Electrochim Acta 28(3):173–188. https://doi.org/10.4152/pea.20100317310.4152/pea.201003173 ↗
35. Zhang J, Gu C, Tu J (2017) Robust slippery coating with superior corrosion resistance and anti-icing performance for AZ31B Mg alloy protection. Acs Appl Mater Inter 9(12):11247–11257. https://doi.org/10.1021/acsami.7b0097210.1021/acsami.7b00972 ↗
36. Song F, Wu C, Chen H, Liu Q, Liu J, Chen R, Li R, Wang J (2017) Water-repellent and corrosion-resistance properties of superhydrophobic and lubricant-infused super slippery surfaces. Rsc Adv 7(70):44239–44246. https://doi.org/10.1039/C7RA04816E10.1039/C7RA04816E ↗
37. Yang S, Qiu R, Song H, Wang P, Shi Z, Wang Y (2015) Slippery liquid-infused porous surface based on perfluorinated lubricant/iron tetradecanoate: Preparation and corrosion protection application. Appl Surf Sci 328:491–500. https://doi.org/10.1016/j.apsusc.2014.12.06710.1016/j.apsusc.2014.12.067 ↗
38. Rosmaninho R, Santos O, Nylander T, Paulsson M, Beuf M, Benezech T, Yiantsios S, Andritsos N, Karabelas A, Rizzo G (2007) Modified stainless steel surfaces targeted to reduce fouling–Evaluation of fouling by milk components. J Food Eng 80(4):1176–1187. https://doi.org/10.1016/j.jfoodeng.2006.09.00810.1016/j.jfoodeng.2006.09.008 ↗
39. Brady RF Jr, Singer IL (2000) Mechanical factors favoring release from fouling release coatings. Biofouling 15(1–3):73–81. https://doi.org/10.1080/0892701000938629910.1080/08927010009386299 ↗
40. Zouaghi S, Six T, Bellayer S, Moradi S, Hatzikiriakos SG, Dargent T, Thomy V, Coffinier Y, André C, Delaplace G (2017) Antifouling biomimetic liquid-infused stainless steel: application to dairy industrial processing. Acs Appl Mater Inter 9(31):26565–26573. https://doi.org/10.1021/acsami.7b0670910.1021/acsami.7b06709 ↗
41. Boveri G, Corozzi A, Veronesi F, Raimondo M (2021) Different approaches to low-wettable materials for freezing environments: design, performance and durability. Coatings 11(1):1–16. https://doi.org/10.3390/coatings1101007710.3390/coatings11010077 ↗