Degradation behaviors of PLA-matrix composite with 20 vol% magnesium alloy wires under static loading conditions

Chenglin Chu, Xuan Li, Weidong Yu, Linyuan Han, Jing Bai, Feng Xue

Journal of Materials Science· Volume 54· Issue 6
Publisher page

Abstract

Influence of static compression loading on the degradation behaviors of polylactic acid-based composite reinforced with 20 vol% magnesium alloy wires (MAWs) is investigated. The external stress would enhance the degradation of the composite. As the applied stress is increased from 1 to 3 MPa, the overall degradation rate goes up. After immersion for 30 days, the degradation rate of PLA matrix in the composite at the stress level of 3 MPa is about 1.46 and 2.4 times those at 1 and 0 MPa (unloading condition) while the bending strength retention is 0.73 and 0.63 times those of the latter ones. The relationship between the degradation rate of PLA matrix in the composite and the external compression stress is further elucidated. The external stress deteriorates the strength retention of the composite but a high MAWs content could mitigate the deterioration.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Orthopaedic implants and arthroplasty · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Claes LE, Heigele CA, Neidlinger-Wilke C, Kaspar D, Seidl W, Margevicius KJ, Peter Augat (1998) Effects of mechanical factors on the fracture healing process. Clin Orthop Relat Res 355:S132–S14710.1097/00003086-199810001-00015 ↗
2. Südkamp N, Bayer J, Hepp P, Voigt C, Oestern H, Kääb M, Luo C, Plecko M, Wendt K, Köstler W (2009) Open reduction and internal fixation of proximal humeral fractures with use of the locking proximal humerus plate. J Bone Joint Surg Am 91:1320–132810.2106/JBJS.H.00006 ↗
3. Perren S (1979) Physical and biological aspects of fracture healing with special reference to internal fixation. Clin Orthop Relat Res 138:175–196
4. Zheng YF, Gu XN, Witte F (2014) Biodegradable metals. Mater Sci Eng R 77:1–3410.1016/j.mser.2014.01.001 ↗
5. Törne K, Örnberg A, Weissenrieder J (2017) Influence of strain on the corrosion of magnesium alloys and zinc in physiological environments. Acta Biomater 48:541–55010.1016/j.actbio.2016.10.030 ↗
6. Li X, Chu C, Chu PK (2016) Effects of external stress on biodegradable orthopedic materials: a review. Bioact Mater 1:77–8410.1016/j.bioactmat.2016.09.002 ↗
7. Li X, Chu CL, Liu L, Liu XK, Bai J, Guo C, Xue F, Lin PH, Chu PK (2015) Biodegradable poly-lactic acid based-composite reinforced unidirectionally with high-strength magnesium alloy wires. Biomaterials 49:135–14410.1016/j.biomaterials.2015.01.060 ↗
8. Wu YH, Li N, Cheng Y, Zheng YF, Han Y (2013) In vitro study on biodegradable AZ31 magnesium alloy fibers reinforced PLGA composite. J Mater Sci Technol 29:545–55010.1016/j.jmst.2013.03.004 ↗
9. Oosterbeek RN, Seal CK, Staiger MP, Hyland MM (2015) Topologically ordered magnesium-biopolymer hybrid composite structures. J Biomed Mater Res A 103:311–31710.1002/jbm.a.35175 ↗
10. Uppstu P, Paakki C, Rosling A (2015) In vitro hydrolysis and magnesium release of poly(d, l-lactide-co-glycolide)-based composites containing bioresorbable glasses and magnesium hydroxide. J Appl Polym Sci 132:42646. https://doi.org/10.1002/app.4264610.1002/app.42646 ↗
11. Liu H, Wang R, Chu HK, Sun D (2015) Design and characterization of a conductive nanostructured polypyrrole-polycaprolactone coated magnesium/PLGA composite for tissue engineering scaffolds. J Biomed Mater Res A 103:2966–297310.1002/jbm.a.35428 ↗
12. Cifuentes SC, Gavilán R, Lieblich M, Benavente R, González-Carrasco JL (2016) In vitro degradation of biodegradable polylactic acid/magnesium composites: relevance of Mg particle shape. Acta Biomater 32:348–35710.1016/j.actbio.2015.12.037 ↗
13. Wen W, Zou Z, Luo B, Zhou C (2017) In vitro degradation and cytocompatibility of g-MgO whiskers/PLLA composites. J Mater Sci 52:2329–2344. https://doi.org/10.1007/s10853-016-0525-010.1007/s10853-016-0525-0 ↗
14. Fan YB, Li P, Zeng L, Huang XJ (2008) Effects of mechanical load on the degradation of poly(d, l-lactic acid) foam. Polym Degrad Stab 93:677–68310.1016/j.polymdegradstab.2007.12.015 ↗
15. Guo M, Chu Z, Yao J, Feng W, Wang Y, Wang L, Fan Y (2016) The effects of tensile stress on degradation of biodegradable PLGA membranes: a quantitative study. Polym Degrad Stab 124:95–10010.1016/j.polymdegradstab.2015.12.019 ↗
16. Gutman EM (1998) Mechanochemistry of materials. Cambridge Int Science Publishing, Cambridge
17. Gutman EM (1994) Mechanochemistry of solid surfaces. World Scientific, Singapore10.1142/2373 ↗
18. Baláž P (2003) Mechanical activation in hydrometallurgy. Int J Miner Pro 72:341–35410.1016/S0301-7516(03)00109-1 ↗
19. Bonora PL, Andrei M, Eliezer A, Gutman EM (2002) Corrosion behaviour of stressed magnesium alloys. Corros Sci 44:729–74910.1016/S0010-938X(01)00101-9 ↗
20. Chu CL, Han X, Bai J, Xue F, Chu PK (2012) Fabrication and degradation behavior of micro-arc oxidized biomedical magnesium alloy wires. Surf Coat Technol 213:307–31210.1016/j.surfcoat.2012.10.078 ↗
21. Kirkland NT, Birbilis N (2014) Magnesium biomaterials: design, testing, and best practice. Springer, Cham10.1007/978-3-319-02123-2 ↗
22. Schindler A, Harper D (1979) Polylactide. II. Viscosity–molecular weight relationships and unperturbed chain dimensions. J Polym Sci Pol Phys Ed 17:2593–259910.1002/pol.1979.170170831 ↗
23. Piemonte V, Gironi F (2013) Kinetics of hydrolytic degradation of PLA. J Polym Environ 21:313–31810.1007/s10924-012-0547-x ↗
24. Codari F, Lazzari S, Soos M, Storti G, Morbidelli M, Moscatelli D (2012) Kinetics of the hydrolytic degradation of poly(lactic acid). Polym Degrad Stab 97:2460–246610.1016/j.polymdegradstab.2012.06.026 ↗
25. Deng M, Zhou J, Chen G, Burkley D, Xu Y, Jamiolkowski D, Barbolt T (2005) Effect of load and temperature on in vitro degradation of poly(glycolide-co-l-lactide) multifilament braids. Biomaterials 26:4327–433610.1016/j.biomaterials.2004.09.067 ↗
26. Kharazi AZ, Fathi MH, Bahmani F, Fanian H (2012) Nonmetallic textile composite bone plate with desired mechanical properties. J Compos Mater 46:2753–276110.1177/0021998311431997 ↗
27. Fan Y, Li P, Yuan X (2010) Influence of mechanical loads on degradation of scaffolds. In: Lim CT, Goh JCH (eds). 6th world congress of biomechanics (WCB 2010) August 1–6, 2010 Springer, Berlin, pp 549–55210.1007/978-3-642-14515-5_140 ↗
28. Rapoport NY, Gennadii EZ (1983) Kinetics and mechanism of the oxidation of polymers in a stressed state. Russ Chem Rev 52:897–91610.1070/RC1983v052n09ABEH002899 ↗
29. Ward IM, Sweeney J (2012) Mechanical properties of solid polymers. Wiley, New York10.1002/9781119967125 ↗
30. Li X, Chu C, Zhou L, Bai J, Guo C, Xue F, Lin P, Chu Paul K (2017) Fully degradable PLA-based composite reinforced with 2D-braided Mg wires for orthopedic implants. Compos Sci Technol 142:180–18810.1016/j.compscitech.2017.02.013 ↗
31. Li X, Chu C, Wei Y, Qi C, Bai J, Guo C, Lin P, Chu Paul K (2017) In vitro degradation kinetics of pure PLA and Mg/PLA composite: effects of immersion temperature and compression stress. Acta Biomater 48:468–47810.1016/j.actbio.2016.11.001 ↗
32. Zhang Y, Zale S, Sawyer L, Bernstein H (1997) Effects of metal salts on poly(DL-lactide-co-glycolide) polymer hydrolysis. J Biomed Mater Res 34:531–53810.1002/(SICI)1097-4636(19970315)34:4<531::AID-JBM13>3.0.CO;2-F ↗
33. Mobedi H, Nekoomanesh M, Orafaei H, Mivehchi H (2006) Studying the degradation of poly(L-lactide) in presence of magnesium hydroxide. Iran Polym J 15:31–39