journal article·2017-10

Hydrogen sorption enhancement in cold-rolled and ball-milled CaNi5

Jacques Huot, Manuel Tousignant

Journal of Materials Science· Volume 52· Issue 20
Publisher page

Abstract

The effect of cold rolling and ball milling on the hydrogen sorption properties of CaNi5 was investigated with a special emphasis on the first hydrogenation. We compared cold rolling for 5, 12, and 25 rolling passes in the air with ball milling in argon for 30 and 60 min. Results show that 15 min of ball milling had a positive effect on the first hydrogen absorption, but further milling to 60 min made the sample almost impermeable to hydrogen. Cold rolling had a positive effect on first hydrogenation. We found that cold rolling greatly reduces the particle size as well as the crystallite size. We also found that dehydrogenation under 5 kPa of hydrogen at 323 K was not complete. Two partially hydride phases remained: CaNi5H and Ca2Ni7H x .
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen Storage and Materials · Ammonia Synthesis and Nitrogen Reduction · Muon and positron interactions and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Huot J (2012) Nanocrystalline metal hydrides obtained by severe plastic deformations. Metals 2:22–4010.3390/met2010022 ↗
2. Zhang LT, Ito K, Vasudevan VK, Yamaguchi M (2001) Hydrogen absorption and desorption in a B2 single-phase Ti-22Al-27Nb alloy before and after deformation. Acta Mater 49:751–75810.1016/S1359-6454(00)00400-6 ↗
3. Suganuma K, Miyamura H, Kikuchi S et al (2007) Hydrogen storage properties of Mg–Al alloy prepared by super lamination technique. Adv Mater Res 26–28:857–86010.4028/www.scientific.net/AMR.26-28.857 ↗
4. Takeichi N, Tanaka K, Tanaka H et al (2007) The hydrogen storage properties of Mg/Cu and Mg/Pd laminate composites and metallographic structure. J Alloy Compd 446–447:543–54810.1016/j.jallcom.2007.04.220 ↗
5. Tanaka K, Takeichi N, Tanaka H et al (2008) Investigation of micro-structural transition through disproportionation and recombination during hydrogenation and dehydrogenation in Mg/Cu super-laminates. J Mater Sci 43:3812–3816. doi: 10.1007/s10853-007-2134-410.1007/s10853-007-2134-4 ↗
6. Tousignant M, Huot J (2014) Hydrogen sorption enhancement in cold rolled LaNi5. J Alloy Compd 595:22–2710.1016/j.jallcom.2014.01.169 ↗
7. Edalati K, Matsuda J, Iwaoka H, Toh S, Akiba E, Horita Z (2013) High-pressure torsion of TiFe intermetallics for activation of hydrogen storage at room temperature with heterogeneous nanostructure. Int J Hydrog Energy 38:4622–462710.1016/j.ijhydene.2013.01.185 ↗
8. Edalati K, Matsuda J, Yanagida A, Akiba E, Horita Z (2014) Activation of TiFe for hydrogen storage by plastic deformation using groove rolling and high-pressure torsion: similarities and differences. Int J Hydrog Energy 39:15589–1559410.1016/j.ijhydene.2014.07.124 ↗
9. Jorge AM Jr, Ferreira G, de Lima MR, Triques Martins et al (2014) Correlation between hydrogen storage properties and textures induced in magnesium through ECAP and cold rolling. Int J Hydrog Energy 39:3810–382110.1016/j.ijhydene.2013.12.154 ↗
10. Révész Á, Gajdics M, Varga LK, Krállics G, Péter L, Spassov T (2014) Hydrogen storage of nanocrystalline Mg–Ni alloy processed by equal-channel angular pressing and cold rolling. Int J Hydrog Energy 39:9911–991710.1016/j.ijhydene.2014.01.059 ↗
11. Sandrock GD, Murray JJ, Post ML, Taylor JB (1982) Hydrides and deuterides of CaNi5. Mater Res Bull 17:887–89410.1016/0025-5408(82)90008-3 ↗
12. Yoshikawa A, Uyenishi Y, Iizumi H, Matsumoto T, Takano N, Terasaki F (1998) Determination of the position and occupancy of deuterium in CaNi5 deuterides by neutron diffraction. J Alloy Compd 280:204–20810.1016/S0925-8388(98)00704-X ↗
13. Pitt MP, Brinks HW, Jensen JO, Hauback BC (2004) An in situ neutron diffraction study of the ageing of CaNi 5Dx at 80 °C and 9 bar. J Alloy Compd 372:190–19610.1016/j.jallcom.2003.10.025 ↗
14. Seta S, Uchida H (1995) Hydrogen solubility in LaNi5. J Alloy Compd 231:448–45310.1016/0925-8388(95)01874-3 ↗
15. Uchida H, Sato M, Moriwaki O (1997) Hydrogen absorption and desorption isotherms in the solid solution regions of the LaNi5–H system. J Alloy Compd 253–254:235–23710.1016/S0925-8388(96)02946-5 ↗
16. Termsuksawad P, Niyomsoan S, Mishra B, Olson DL, Gavra Z, Kaydanov VI (2005) Prediction of hydrogen absorption behavior in AB5 hydrogen storage alloys by electronic techniques. Mater Sci Eng B Solid State Mater Adv Technol 117:45–5110.1016/j.mseb.2004.10.014 ↗
17. Hanada N, Nakagawa T, Asada H et al (2015) Dependence of constituent elements of AB5 type metal hydrides on hydrogenation degradation by CO2 poisoning. J Alloy Compd 647:19810.1016/j.jallcom.2015.05.253 ↗
18. Tagawa T (2011) Process intensification of dehydrogenation reactions by pressure swing reactor. J Jpn Pet Inst 54:310–31910.1627/jpi.54.310 ↗
19. Cheary RW, Coelho AA, Cline JP (2004) Fundamental parameters line profile fitting in laboratory diffractometers. J Res Natl Inst Stand Technol 109:110.6028/jres.109.002 ↗
20. Chen J, Takeshita HT, Tanaka H et al (2000) Hydriding properties of LaNi3 and CaNi3 and their substitutes with PuNi3-type structure. J Alloy Compd 302:304–31310.1016/S0925-8388(00)00694-0 ↗
21. Si TZ, Pang G, Zhang QA, Liu DM, Liu N (2009) Solid solubility of Mg in Ca2Ni7 and hydrogen storage properties of (Ca2−x Mg x )Ni7 alloys. Int J Hydrog Energy 34:4833–483710.1016/j.ijhydene.2009.03.055 ↗
22. Iwase K, Sakaki K, Nakamura Y, Akiba E (2013) In situ XRD study of La2Ni7Hx during hydrogen absorption–desorption. Inorg Chem 52:10105–1011110.1021/ic401419n ↗
23. Calvert LD, Murray JJ, Gainsford GJ, Taylor JB (1984) Crystal structure of CaNi5H using X-ray diffraction with in situ hydriding. Mater Res Bull 19:107–11310.1016/0025-5408(84)90016-3 ↗
24. Westlake DG (1983) Site occupancies and stoichiometries in hydrides of intermetallic compounds: geometric considerations. J Less Common Metals 90:251–27310.1016/0022-5088(83)90075-9 ↗
25. Kamble A, Sharma P, Huot J (2017) Effect of doping and particle size on hydrogen absorption properties of BCC solid solution 52Ti-12V-36Cr. Int J Hydrogen Energ 42:1152310.1016/j.ijhydene.2017.02.137 ↗