Abstract

RuO2 thin films deposited by reactive DC sputtering were heat-treated in a 0.3%-H2 atmosphere at 200°C in order to investigate the reduction property of RuO2. The films were selectively reduced (starting from the interface) because of insufficient oxidation. When the as-deposited RuO2/Si structure was hydrogen-reduced, the RuO2 film was broken into fragments because of poor mechanical strength. On the other hand, the RuO2 film heat-treated once in O2 at 700°C cracked into a star shape as a result of vapor generation and volume shrinkage. The star-shape cracking was still observed even when the RuO2 film was covered with a 90-nm-thick BST film. The mechanical strength and the adhesion of RuO2 were improved to some extent by post-oxidation at high temperatures. However, a way to prevent the morphological destruction could not be found because of the thermodynamic equilibrium during the hydrogen reduction process.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Gas Sensing Nanomaterials and Sensors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. M. L. Green, M. E. Gross, L. E. Papa, K. J. Schnoes and D. BRasen, J. Electrochem. Soc. 132 (1985) 2677.10.1149/1.2113647 ↗
2. Q. X. Jia, X. D. Wu, S. R. Foltyn, A. T. Findikoglu, P. Tiwari, J. P. Zheng and T. R. Jow, Appl. Phys. Lett. 67 (1995) 1677.10.1063/1.115054 ↗
3. J. S. Lee, H. J. Kwon, Y. W. Jeong, H. H. Kim and C. Y. Kim, J. Mater. Res. 11 (1996) 2681.10.1557/JMR.1996.0337 ↗
4. A. Grill, W. Kane, J. Viggiano, M. Brady and R. Laibowitz, ibid. 7 (1992) 3260.10.1557/JMR.1992.3260 ↗
5. E. Kolawa, F. C. T. So, E. T.-S. Pan and M.-A. Nicolet, Appl. Phys. Lett. 50 (1987) 854.10.1063/1.98012 ↗
6. L. K.-Elbaum and M. Wittmer and D. S. Yee, ibid. 50 (1987) 1879.10.1063/1.97673 ↗
7. S. Saito and K. Kuramasu, Jpn. J. Appl. Phys. 31 (1992) 135.10.1143/JJAP.31.135 ↗
8. K. Tokashiki, K. Sato, K. Takemura, S. Yamamichi, P.-Y. Lesaicherre, H. Miyamoto, E. Ikawa and Y. Miyasaka, in Proc. 15th Symp. Dry Process, Tokyo, 1994 (Institute of Electrical Engineers of Japan, Tokyo, 1994) p. 73.
9. K. Takemura, H. Yamaguchi, P.-Y. Lesaicherre, K. Tokashiki, H. Miyamoto, H. Ono, Y. Miyasaka and M. Yoshida, Jpn. J. Appl. Phys. 34 (1995) 5224.10.1143/JJAP.34.5224 ↗
10. Y. T. Kim and C. W. Lee, ibid. 35 (1996) 6153.10.1143/JJAP.35.6153 ↗
11. J.-H. Ahn, W.-Y. Choi, W.-J. Lee and H.-G. Kim, ibid. 37 (1998) 284.10.1143/JJAP.37.284 ↗
12. W. F. McClune (ed.), “Powder Diffraction File” (JCPDS, Swarthmore, 1985).
13. J. A. Rard, Chemical Reviews 85 (1985) 1.10.1021/cr00065a001 ↗