Abstract

The aim of the present study was to investigate the effect of moisture content and temperature on the fracture behaviour of thermally modified Norway spruce (Picea abies [L.] Karst.) in the transverse plane. Spruce was thermally modified at two heat treatment temperatures, 190 and 210 °C. Mode I fracture tests were carried out at temperatures of 22 and 50 °C on air-dried and fully water-saturated (>fibre saturation point) material. Small CT specimens were used, and load–CMOD curves were recorded. Characteristic fracture parameters were calculated. The fracture surfaces were subsequently examined using optical microscopy. Thermal modification altered all the calculated fracture parameter values and the changes increased as the severity of heat treatment increased. The parameters were altered more in the radial-tangential (RT) than in tangential-radial (TR) orientation. The failure mode changed due to heat treatment in the TR orientation but in the RT orientation the failure mode of unmodified and heat treated material differs only at high moisture content and elevated temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Wood Treatment and Properties · Bamboo properties and applications · Natural Fiber Reinforced Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Esteves B, Pereira H (2009) Wood modification by heat treatment: a review. BioResources 4:370–40410.15376/biores.4.1.Esteves ↗
2. Borrega M (2011) Mechanisms affecting the structure and properties of heat-treated and high-temperature dried Norway spruce (Picea abies) wood, PhD dissertation. University of Eastern Finland10.14214/df.134 ↗
3. Hughes M, Hill C, Pfriem A (2015) The toughness of hygrothermally modified wood—a review. COST action FP0904 2010-2014: thermo-hydro-mechanical wood behavior and processing. Holzforschung. doi: 10.1515/hf-2014-018410.1515/hf-2014-0184 ↗
4. Bourgois J, Guyonnet R (1988) Characterization and analysis of torrefied wood. Wood Sci Technol 22:143–15510.1007/BF00355850 ↗
5. Zaman A, Alén R, Kotilainen R (2000) Thermal behavior of scots pine (Pinus Sylvestris) and silver birch (Betula Pendula) at 200–230°C. Wood Fiber Sci 32:138–143
6. Burmester A (1975) Zur Dimensionsstabilisierung von Holz. Holz als Roh-und Werkstoff 33:333–33510.1007/BF02612789 ↗
7. Borrega M, Kärenlampi PP (2010) Three mechanisms affecting the mechanical properties of spruce wood dried at high temperatures. J Wood Sci 56:87–9410.1007/s10086-009-1076-7 ↗
8. Bergander A, Salmén L (2002) Cell wall properties and their effects on the mechanical properties of fibers. J Mater Sci 37:151–156. doi: 10.1023/A:101311592567910.1023/A:1013115925679 ↗
9. Reiterer A, Sinn G (2002) Fracture behaviour of modified spruce wood: a study using linear and non linear fracture mechanics. Holzforschung 56:191–19810.1515/HF.2002.032 ↗
10. Murata K, Watanabe Y, Nakano T (2013) Effect of thermal treatment on fracture properties and adsorption properties of spruce wood. Materials 6:4186–419710.3390/ma6094186 ↗
11. Majano-Majano A, Hughes M, Fernandez-Cabo JL (2012) The fracture toughness and properties of thermally modified beech and ash at different moisture contents. Wood Sci Technol 46:5–2110.1007/s00226-010-0389-4 ↗
12. Pleschberger H, Teischinger A, Müller U, Hansmann C (2014) Change in fracturing and colouring of solid spruce and ash wood after thermal modification. Wood Mater Sci Eng 9:92–10110.1080/17480272.2014.895418 ↗
13. Tukiainen P, Hughes M (2015) The effect of temperature and moisture content on fracture behaviour of spruce and birch. Holzforschung. doi: 10.1515/hf-2015-0017
14. Schachner H, Reiterer A, Stanzl-Tschegg S (2000) Orthotropic fracture toughness of wood. J Mater Sci Lett 19:1783–1785. doi: 10.1023/A:100670371803210.1023/A:1006703718032 ↗
15. Borrega M, Kärenlampi PP (2008) Effect of relative humidity on thermal degradation of Norway spruce (Picea abies) wood. J Wood Sci 54:323–32810.1007/s10086-008-0953-9 ↗
16. Esteves B, Domingos I, Pereira H (2008) Pine wood modification by heat treatment in air. BioResources 3:142–15410.15376/biores.3.1.142-154 ↗
17. Keunecke D, Stanzl-Tschegg S, Niemz P (2007) Fracture characterisation of yew (Taxus baccata L.) and spruce (Picea abies [L.] Karst.) in the radial-tangential and tangential-radial crack propagation system by a micro wedge splitting test. Holzforschung 61:582–58810.1515/HF.2007.089 ↗
18. Thuvander F, Berglund L (2000) In situ observations of fracture mechanisms for radial cracks in wood. J Mater Sci 35:6277–6283. doi: 10.1023/A:102677862215610.1023/A:1026778622156 ↗
19. Vasic S, Stanzl-Tschegg S (2007) Experimental and numerical investigation of wood fracture mechanisms at different humidity levels. Holzforschung 61:367–37410.1515/HF.2007.056 ↗
20. Thuvander F, Jernkvist L, Gunnars J (2000) Influence of repetitive stiffness variation on crack growth behaviour in wood. J Mater Sci 35:6259–6266. doi: 10.1023/A:102676620350110.1023/A:1026766203501 ↗
21. Borrega M, Kärenlampi PP (2011) Radial mechanical properties of high-temperature dried Norway spruce (Picea abies) wood. Wood Mater Sci Eng 6:147–15410.1080/17480272.2011.561017 ↗
22. Ashby M, Easterling K, Harrysson R, Maiti S (1985) The fracture and toughness of woods. Proc R Soc Lond A 398:261–28010.1098/rspa.1985.0034 ↗
23. Fengel D, Wegener G (1989) Wood: chemistry, ultrastructure, reactions. Walter de Gruyter, Berlin
24. Perilä O (1961) The chemical composition of carbohydrates of wood cells. J Polym Sci 51:19–2610.1002/pol.1961.120510103 ↗