journal article·2022-02Open access

Development of TiB and nanocrystalline Ti-reinforced novel hybrid Ti nanocomposite produced by powder metallurgy

D. A. Angel, T. Mikó, F. Kristály, M. Benke, Z. Gácsi

Journal of Materials Science· Volume 57· Issue 6

Abstract

Abstract Titanium monoboride (TiB) whisker-reinforced titanium (Ti) matrix composites were produced by powder metallurgy, through vacuum sintering. TiB is formed by thermal decomposition of TiB2 precursor. In addition, a new hybrid composite was developed by admixing nanograined and nanocrystalline (more important) Ti to enhance the transformation mechanism of TiB2 to TiB phase. The morphology and particle size of the initial powders, mixtures and the microstructure of the composites have been studied by scanning electron microscopy (SEM). The phase analysis and transformation monitoring were performed by X-ray diffraction (XRD). The sintered composites were also subjected to compressive strength and hardness measurements. According to XRD results, through the addition of nanocrystalline Ti, a probable enhancement of the TiB2 → TiB transformation occurred producing more TiB whiskers in the hybrid composites. All samples of the hybrid composites exhibited improved yield strength (1365 MPa) and hardness (358 HV) compared to the non-hybrid ones 927 MPa and 254 HV, respectively. Graphical abstract
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Tjong SC, Ma ZY (2000) Microstructural and mechanical characteristics of in situ metal matrix composites. Mater Sci Eng R 29:49–113. https://doi.org/10.1016/S0927-796X(00)00024-310.1016/S0927-796X(00)00024-3 ↗
2. Norgate TE, Wellwood G (2006) The potential applications for titanium metal powder and their life cycle impacts. J Min Met Mat S 58:58–63. https://doi.org/10.1007/s11837-006-0084-y10.1007/s11837-006-0084-y ↗
3. Geetha M, Singh AK, Asokamani R, Gogia AK (2009) Ti based biomaterials, the ultimate choice for orthopaedic implants – A review. Prog Mater Sci 54:397–425. https://doi.org/10.1016/j.pmatsci.2008.06.00410.1016/j.pmatsci.2008.06.004 ↗
4. Elias CN, Meyers MA, Valiev RZ, Monteiro SN (2013) Ultrafine grained titanium for biomedical applications: an overview of performance. J Mater Res Tech 2:340–350. https://doi.org/10.1016/j.jmrt.2013.07.00310.1016/j.jmrt.2013.07.003 ↗
5. Basu B, Raju GB, Suri AK (2006) Processing and properties of monolithic TiB2 based materials. Int Mater Rev 51:352–374. https://doi.org/10.1179/174328006X10252910.1179/174328006X102529 ↗
6. Munro RG (2000) Material properties of titanium diboride. J Res of the Natl Inst Stan 105:709–720. https://doi.org/10.6028/jres.105.05710.6028/jres.105.057 ↗
7. Ravichandran KS, Panda KB, Sahay SS (2004) TiBw-reinforced Ti composites: Processing, properties, application prospects, and research needs. J Min Met Mat S 56:42–48. https://doi.org/10.1007/s11837-004-0127-110.1007/s11837-004-0127-1 ↗
8. Alman DE, Hawk JA (1999) The abrasive wear of sintered titanium matrix–ceramic particle reinforced composites. Wear 225–229:629–639. https://doi.org/10.1016/s0043-1648(99)00065-410.1016/s0043-1648(99)00065-4 ↗
9. Saito T (2004) The automotive application of discontinuously reinforced TiB-Ti composites. J Min Met Mat S 56:33–36. https://doi.org/10.1007/s11837-004-0125-310.1007/s11837-004-0125-3 ↗
10. Yi M, Zhang X, Liu G, Wang B, Shao H, Qiao G (2018) Comparative investigation on microstructures and mechanical properties of (TiB + TiC)/Ti-6Al-4V composites from Ti-B4C-C and Ti-TiB2-TiC systems. Mater Charact 140:281–289. https://doi.org/10.1016/j.matchar.2018.04.01010.1016/j.matchar.2018.04.010 ↗
11. Li DX, Ping DH, Lu YX, Ye HQ (1993) Characterization of the microstructure in TiB-whisker reinforced Ti alloy matrix composite. Mater Lett 16:322–326. https://doi.org/10.1016/0167-577X(93)90201-810.1016/0167-577X(93)90201-8 ↗
12. Lu W, Zhang D, Zhang X, Wu R, Sakata T, Mori H (2001) HREM study of TiB/Ti interfaces in a TiB-TiC in situ composite. Scripta Mater 44:1069–1075. https://doi.org/10.1016/S1359-6462(01)00663-710.1016/S1359-6462(01)00663-7 ↗
13. Namini AS, Azadbeh M, Asl MS (2017) Effect of TiB2 content on the characteristics of spark plasma sintered Ti–TiBw composites. Adv Powder Technol 28:1564–1572. https://doi.org/10.1016/j.apt.2017.03.02810.1016/j.apt.2017.03.028 ↗
14. Mohammadzadeh A, Azadbeh M, Danninger H, Namini AS (2020) Ti-TiB2 composites consolidated by spark plasma sintering: reaction mechanism, characteristics of in-situ formed phases and densification behavior. Mater Chem Phys 242:122556. https://doi.org/10.1016/j.matchemphys.2019.12255610.1016/j.matchemphys.2019.122556 ↗
15. Liu L, Minasyan T, Ivanov R, Aydinyan S, Hussainova I (2020) Selective laser melting of TiB2-Ti composite with high content of ceramic phase. Ceram Int 46:21128–21135. https://doi.org/10.1016/j.ceramint.2020.05.18910.1016/j.ceramint.2020.05.189 ↗
16. Atri RR, Ravichandran KS, Jha SK (1999) Elastic properties of in-situ processed Ti–TiB composites measured by impulse excitation of vibration. Mater Sci Eng A 271:150–159. https://doi.org/10.1016/S0921-5093(99)00198-710.1016/S0921-5093(99)00198-7 ↗
17. Sahay SS, Ravichandran KS, Atri RR, Chen B, Rubin J (1999) Evolution of microstructure and phases in in situ processed Ti–TiB composites containing high volume fractions of TiB whiskers. J Mater Res 14:4214–4223. https://doi.org/10.1557/JMR.1999.057110.1557/JMR.1999.0571 ↗
18. Mikó T, Kristály F, Pethő D, Svéda M, Karacs G, Gergely G, Gácsi Z, Roósz A (2021) Investigation of nanocrystalline sintered W-25 w% Cu composite. Int J Refract Met H 95:105438. https://doi.org/10.1016/j.ijrmhm.2020.10543810.1016/j.ijrmhm.2020.105438 ↗
19. Young RA (1995) The rietveld method. Oxford University Press
20. Dinnebier RE, Leineweber A, Evans JSO (2018) Rietveld refinement: practical powder diffraction pattern analysis using TOPAS. De Gruyter. https://doi.org/10.1515/978311046138110.1515/9783110461381 ↗
21. McCusker LB, Von Dreele RB, Cox DE, Louër D, Scardi P (1999) Rietveld refinement guidelines. J App Crystallogr 32:36–50. https://doi.org/10.1107/S002188989800985610.1107/S0021889898009856 ↗
22. Wang G, Li J, Lv K, Zhang W, Ding X, Yang G, Liu X, Jiang X (2016) Surface thermal oxidation on titanium implants to enhance osteogenic activity and in vivo osseointegration. Sci Rep-UK 6:31769. https://doi.org/10.1038/srep3176910.1038/srep31769 ↗
23. Liu X, Chu PK, Ding C (2004) Surface modification of titanium, titanium alloys, and related materials for biomedical applications. Mat Sci Eng R 47:49–121. https://doi.org/10.1016/j.mser.2004.11.00110.1016/j.mser.2004.11.001 ↗
24. Hardness conversion chart -https://steelselector.sij.si/calculators/hardness/hardness_table.html. Accessed 29 July 2021
25. Panda KB, Ravi Chandran KS (2003) Titanium-titanium boride (Ti-TiB) functionally graded materials through reaction sintering: Synthesis, microstructure, and properties. Metall Mater Trans A 34:1993–2003. https://doi.org/10.1007/s11661-003-0164-310.1007/s11661-003-0164-3 ↗
26. Huang LJ, Yang FY, Hu HT, Rong XD, Geng L, Wu LZ (2013) TiB whiskers reinforced high temperature titanium Ti60 alloy composites with novel network microstructure. Mater Design 51:421–426. https://doi.org/10.1016/j.matdes.2013.04.04810.1016/j.matdes.2013.04.048 ↗
27. Feng H, Meng Q, Zhou Y, Jia D (2005) Spark plasma sintering of functionally graded material in the Ti–TiB2–B system. Mat Sci Eng A 397:92–97. https://doi.org/10.1016/j.msea.2005.02.00310.1016/j.msea.2005.02.003 ↗
28. Attar H, Löber L, Funk A, Calin M, Zhang LC, Prashanth KG, Scudino S, Zhang YS, Eckert J (2015) Mechanical behavior of porous commercially pure Ti and Ti–TiB composite materials manufactured by selective laser melting. Mat Sci Eng A 625:350–356. https://doi.org/10.1016/j.msea.2014.12.03610.1016/j.msea.2014.12.036 ↗
29. Attar H, Bönisch M, Calin M, Zhang LC, Scudino S, Eckert J (2014) Selective laser melting of in situ titanium–titanium boride composites: Processing, microstructure and mechanical properties. Acta Mater 76:13–22. https://doi.org/10.1016/j.actamat.2014.05.02210.1016/j.actamat.2014.05.022 ↗
30. Attar H, Bönisch M, Calin M, Zhang LC, Zhuravleva K, Funk A, Scudino S, Yang C, Eckert J (2014) Comparative study of microstructures and mechanical properties of in situ Ti–TiB composites produced by selective laser melting, powder metallurgy, and casting technologies. J Mater Res 29:1941–1950. https://doi.org/10.1557/jmr.2014.12210.1557/jmr.2014.122 ↗
31. Han C, Rita B, Chua JDQ, Ramamurty U, Tor SB, Sun CN, Zhou K (2020) Microstructure and mechanical properties of (TiB+TiC)/Ti composites fabricated in situ via selective laser melting of Ti and B4C powders. Addit Man 36:101466. https://doi.org/10.1016/j.addma.2020.10146610.1016/j.addma.2020.101466 ↗
32. Namini AS, Dilawary SAA, Motallebzadeh A, Asl MS (2019) Effect of TiB2 addition on the elevated temperature tribological behavior of spark plasma sintered Ti matrix composite. Compos Part B-Eng 172:271–280. https://doi.org/10.1016/j.compositesb.2019.05.07310.1016/j.compositesb.2019.05.073 ↗
33. Otte JA, Zou J, Patel R, Lu M, Dargusch MS (2020) TiB nanowhisker reinforced titanium matrix composite with improved hardness for biomedical applications. Nanomaterials 10:2480. https://doi.org/10.3390/nano1012248010.3390/nano10122480 ↗