Abstract
The effect of pre-rolling prior to the high strain rate rolling (HSRR) on the dynamic recrystallization (DRX), dynamic precipitation and mechanical properties of Mg–6Zn–1Mn (ZM61) was investigated. Aiming this, a set of pre-rolling tests were carried out at the temperature of 300 °C with pre-rolling strain of 20 and 40%. The results show that pre-rolling treatment greatly homogenize the microstructure and refine DRX grains. The original twins induced by pre-rolling accelerate the DRX process and provide more nucleation sites for DRX grains. The precipitates induced by pre-rolling increase the precipitation density and lead to a strong interaction between DRX grains and precipitates. The ZM61 alloy sheet prepared with 20% pre-rolling strain at 300 °C followed by HSRR at 300 °C exhibits the UTS of 392 MPa and elongation of 16.8%. The advanced mechanical properties can be ascribed to the combined effect of grain refinement hardening and nano-precipitation strengthening.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Luo AA, Neelameggham NR et al (2016) Materials comparison and potential applications of magnesium in automobiles. In: Essential readings in magnesium technology. Springer International Publishing, Berlin, pp 25–3410.1007/978-3-319-48099-2_4 ↗
2. Kubota K, Mabuchi M, Higashi K (1999) Review processing and mechanical properties of fine-grained magnesium alloys. J Mater Sci 34(10):2255–2262. doi: 10.1023/A:100456120562710.1023/A:1004561205627 ↗
3. Zhu SQ, Yan HG, Xia WJ et al (2009) Influence of different deformation processing on the AZ31 magnesium alloy sheets. J Mater Sci 44(14):3800–3806. doi: 10.1007/s10853-009-3513-910.1007/s10853-009-3513-9 ↗
4. Zhu SQ, Yan HG, Chen JH et al (2012) Feasibility of high strain-rate rolling of a magnesium alloy across a wide temperature range. Scr Mater 67(4):404–40710.1016/j.scriptamat.2012.05.036 ↗
5. Song B, Guo N, Liu T et al (2014) Improvement of formability and mechanical properties of magnesium alloys via pre-twinning: a review. Mater Des 62(10):352–36010.1016/j.matdes.2014.05.034 ↗
6. Hong SG, Park SH, Chong SL (2010) Role of {10–12} twinning characteristics in the deformation behavior of a polycrystalline magnesium alloy. Acta Mater 58(18):5873–588510.1016/j.actamat.2010.07.002 ↗
7. Xin Y, Wang M, Zeng Z et al (2012) Strengthening and toughening of magnesium alloy by {10–12} extension twins. Scr Mater 66(1):25–2810.1016/j.scriptamat.2011.09.033 ↗
8. Changizian P, Zarei-Hanzaki A, Abedi HR (2012) On the recrystallization behavior of homogenized AZ81 magnesium alloy: the effect of mechanical twins and γ precipitates. Mater Sci Eng A 558(558):44–5110.1016/j.msea.2012.07.054 ↗
9. Murr LE, Esquivel EV (2004) Observations of common microstructural issues associated with dynamic deformation phenomena: twins, microbands, grain size effects, shear bands, and dynamic recrystallization. J Mater Sci 39(4):1153–1168. doi: 10.1023/B:JMSC.0000013870.09241.c010.1023/B:JMSC.0000013870.09241.c0 ↗
10. Nie JF (2012) Precipitation and hardening in magnesium alloys. Metall Mater Trans A 43(11):3891–393910.1007/s11661-012-1217-2 ↗
11. Sasaki TT, Yamamoto K, Honma T et al (2008) A high-strength Mg–Sn–Zn–Al alloy extruded at low temperature. Scr Mater 59(10):1111–111410.1016/j.scriptamat.2008.07.042 ↗
12. Appel F, Fischer FD, Clemens H (2007) Precipitation twinning. Acta Mater 55(14):4915–492310.1016/j.actamat.2007.05.007 ↗
13. Chaudhury PK, Rack HJ, Mikucki BA (1991) Effect of double-ageing on mechanical properties of Mg-6Zn reinforced with SiC particulates. J Mater Sci 26(9):2343–2347. doi: 10.1007/BF0113017910.1007/BF01130179 ↗
14. Zhang DF, Shi GLG, Zhao XB (2011) Microstructure evolution and mechanical properties of Mg-x%Zn-1%Mn(x = 4,5,6,7,8,9) wrought magnesium alloys. Trans Nonferrous Met Soc China 21(1):15–2510.1016/S1003-6326(11)60672-9 ↗
15. Chen C, Chen JH, Yan HG et al (2016) Dynamic precipitation, microstructure and mechanical properties of Mg–5Zn–1Mn alloy sheets prepared by high strain-rate rolling. Mater Des 100:58–6610.1016/j.matdes.2016.03.129 ↗
16. Li JP, Lorimer GW, Robson JD et al (2005) Investigation on microstructures of heat treated Mg–Zr and Mg–Mn Alloys. Mater Sci Forum 488–489:189–192
17. Park SH, Kim HS, Bae JH et al (2013) Improving the mechanical properties of extruded Mg–3Al–1Zn alloy by cold pre-forging. Scr Mater 69(3):250–25310.1016/j.scriptamat.2013.04.011 ↗
18. Zhu SQ, Yan HG, Chen JH et al (2010) Effect of twinning and dynamic recrystallization on the high strain rate rolling process. Scr Mater 63(10):985–98810.1016/j.scriptamat.2010.07.029 ↗
19. Reed-Hill RE, Robertson WD (1957) Additional modes of deformation twinning in magnesium. Acta Metall 5(12):717–72710.1016/0001-6160(57)90074-3 ↗
20. Barnett MR, Keshavarz Z, Beer AG et al (2004) Influence of grain size on the compressive deformation of wrought Mg–3Al–1Zn. Acta Mater 52(17):5093–510310.1016/j.actamat.2004.07.015 ↗
21. Shi GL, Zhang DF, Zhang HJ et al (2013) Influence of pre-deformation on age-hardening response and mechanical properties of extruded Mg–6%Zn–1%Mn alloy. Trans Nonferrous Met Soc China 23(3):586–59210.1016/S1003-6326(13)62503-0 ↗
22. Song B, Xin R, Sun L et al (2013) Enhancing the strength of rolled ZK60 alloys via the combined use of twinning deformation and aging treatment. Mater Sci Eng A 582(2):68–7510.1016/j.msea.2013.06.047 ↗
23. Hall EO (1951) The deformation and ageing of mild steel: III discussion of results. Proc Phys Soc 643(9):747–75210.1088/0370-1301/64/9/303 ↗
24. Petch NJ (1953) The cleavage strength of polycrystals. J Iron Steel Inst 174(1):25–28
25. Nie JF (2003) Effects of precipitate shape and orientation on dispersion strengthening in magnesium alloys. Scr Mater 48(8):1009–101510.1016/S1359-6462(02)00497-9 ↗