On the anisotropy in room-temperature mechanical properties of laser powder bed fusion processed Ti6Al4V-ELI alloy for aerospace applications
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Tamirisakandala S, Vedam BV, Bhat RB (2003) Recent advances in the deformation processing of titanium alloys. J Mater Eng Perform 12:661–673. https://doi.org/10.1361/10599490332269246610.1361/105994903322692466 ↗
2. Anil Kumar V, Gupta RK, Prasad MJNV, Narayana Murty SVS (2021) Recent advances in processing of titanium alloys and titanium aluminides for space applications: a review. J Mater Res 36:689–716. https://doi.org/10.1557/s43578-021-00104-w10.1557/s43578-021-00104-w ↗
3. Liu S, Shin YC (2019) Additive manufacturing of Ti6Al4V alloy: a review. Mater Des 164:107552. https://doi.org/10.1016/j.matdes.2018.10755210.1016/j.matdes.2018.107552 ↗
4. Huang R, Riddle M, Graziano D et al (2016) Energy and emissions saving potential of additive manufacturing: the case of lightweight aircraft components. J Clean Prod 135:1559–1570. https://doi.org/10.1016/j.jclepro.2015.04.10910.1016/j.jclepro.2015.04.109 ↗
5. Gibson I, Rosen D, Stucker B (2015) Additive manufacturing technologies. Springer, New York10.1007/978-1-4939-2113-3 ↗
6. Agius D, Kourousis K, Wallbrink C (2018) A review of the as-built SLM Ti–6Al–4V mechanical properties towards achieving fatigue resistant designs. Metals (Basel) 8:75. https://doi.org/10.3390/met801007510.3390/met8010075 ↗
7. Seifi M, Salem A, Beuth J et al (2016) Overview of materials qualification needs for metal additive manufacturing. JOM 68:747–764. https://doi.org/10.1007/s11837-015-1810-010.1007/s11837-015-1810-0 ↗
8. Gorsse S, Hutchinson C, Gouné M, Banerjee R (2017) Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti–6Al–4V and high-entropy alloys. Sci Technol Adv Mater 18:584–610. https://doi.org/10.1080/14686996.2017.136130510.1080/14686996.2017.1361305 ↗
9. Galarraga H, Warren RJ, Lados DA et al (2017) Effects of heat treatments on microstructure and properties of Ti–6Al–4V ELI alloy fabricated by electron beam melting (EBM). Mater Sci Eng A 685:417–428. https://doi.org/10.1016/j.msea.2017.01.01910.1016/j.msea.2017.01.019 ↗
10. Cui C, Hu B, Zhao L, Liu S (2011) Titanium alloy production technology, market prospects and industry development. Mater Des 32:1684–1691. https://doi.org/10.1016/j.matdes.2010.09.01110.1016/j.matdes.2010.09.011 ↗
11. Uhlmann E, Kersting R, Klein TB et al (2015) Additive manufacturing of titanium alloy for aircraft components. Procedia CIRP 35:55–60. https://doi.org/10.1016/j.procir.2015.08.06110.1016/j.procir.2015.08.061 ↗
12. Herzog D, Seyda V, Wycisk E, Emmelmann C (2016) Additive manufacturing of metals. Acta Mater 117:371–392. https://doi.org/10.1016/j.actamat.2016.07.01910.1016/j.actamat.2016.07.019 ↗
13. Yusuf SM, Gao N (2017) Influence of energy density on metallurgy and properties in metal additive manufacturing. Mater Sci Technol 33:1269–1289. https://doi.org/10.1080/02670836.2017.128944410.1080/02670836.2017.1289444 ↗
14. Wang M, Lin X, Huang W (2016) Laser additive manufacture of titanium alloys. Mater Technol. https://doi.org/10.1179/1753555715Y.000000007910.1179/1753555715Y.0000000079 ↗
15. Frazier WE (2014) Metal additive manufacturing: a review. J Mater Eng Perform 23:1917–1928. https://doi.org/10.1007/s11665-014-0958-z10.1007/s11665-014-0958-z ↗
16. Kannan GB, Rajendran DK (2017) A review on status of research in metal additive manufacturing. In: Ian Wimpenny D, Pandey PM, Jyothish Kumar L (ed) Advances in 3D printing and additive manufacturing technologies. Springer, Singapore, pp 95–10010.1007/978-981-10-0812-2_8 ↗
17. Yang Z, Xu Y, Sisson RD, Liang J (2020) Factors influencing the corrosion behavior of direct metal laser sintered Ti–6Al–4V for biomedical applications. J Mater Eng Perform 29:3831–3839. https://doi.org/10.1007/s11665-020-04904-910.1007/s11665-020-04904-9 ↗
18. Traini T, Mangano C, Sammons RL et al (2008) Direct laser metal sintering as a new approach to fabrication of an isoelastic functionally graded material for manufacture of porous titanium dental implants. Dent Mater 24:1525–1533. https://doi.org/10.1016/j.dental.2008.03.02910.1016/j.dental.2008.03.029 ↗
19. Dutta B, Froes FH (2017) The additive manufacturing (AM) of titanium alloys. Met Powder Rep 72:96–106. https://doi.org/10.1016/j.mprp.2016.12.06210.1016/j.mprp.2016.12.062 ↗
20. Castells R DMLS vs SLM 3D Printing for Metal Manufacturing. https://www.element.com/nucleus/2016/dmls-vs-slm-3d-printing-for-metal-manufacturing
21. AMS4930L (2020) Titanium alloy bars, wire, forgings, and rings 6Al–4V, extra low interstitial annealed. SAE Int https://doi.org/10.4271/AMS4930K10.4271/AMS4930K ↗
22. Specification for Titanium Alloy Ti6Al4V ELI Forgings, Rods, Rings and Blocks (Annealed), VSSC: MMPS: 3103F:2011
23. Vrancken B, Thijs L, Kruth J-P, Van Humbeeck J (2012) Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties. J Alloys Compd 541:177–185. https://doi.org/10.1016/j.jallcom.2012.07.02210.1016/j.jallcom.2012.07.022 ↗
24. Moletsane MG, Krakhmalev P, Kazantseva N et al (2016) Tensile properties and microstructure of direct metal laser-sintered Ti6Al4V (ELI) alloy. South Afr J Ind Eng. https://doi.org/10.7166/27-3-166710.7166/27-3-1667 ↗
25. Yadroitsev I, Krakhmalev P, Yadroitsava I, Du Plessis A (2018) Qualification of Ti6Al4V ELI alloy produced by laser powder bed fusion for biomedical applications. JOM 70:372–377. https://doi.org/10.1007/s11837-017-2655-510.1007/s11837-017-2655-5 ↗
26. van Zyl I, Moletsane M, Krakhmalev P et al (2016) Validation of miniaturised tensile testing on DMLS Ti6Al4V (ELI) Specimens. S Afr J Ind Eng. https://doi.org/10.7166/27-3-166610.7166/27-3-1666 ↗
27. Muiruri AM, Maringa M, du Preez W, Masu L (2018) Variation of impact toughness of as-built dmls Ti6Al4V (ELI) specimens with temperature. S Afr J Ind Eng. https://doi.org/10.7166/29-3-207610.7166/29-3-2076 ↗
28. Muiruri A, Maringa M, du Preez W, Masu L (2020) Effects of stress-relieving heat treatment on impact toughness of direct metal laser sintering (DMLS)-produced Ti6Al4V (ELI) parts. JOM 72:1175–1185. https://doi.org/10.1007/s11837-019-03862-510.1007/s11837-019-03862-5 ↗
29. Galarraga H, Lados DA, Dehoff RR et al (2016) Effects of the microstructure and porosity on properties of Ti–6Al–4V ELI alloy fabricated by electron beam melting (EBM). Addit Manuf 10:47–57. https://doi.org/10.1016/j.addma.2016.02.00310.1016/j.addma.2016.02.003 ↗
30. (2016) EOS Titanium Ti64ELI, Material data sheet
31. ASTM-F3001 (2014) Standard Specification for Additive Manufacturing Titanium-6 Aluminum-4 Vanadium ELI (Extra Low Interstitial) with Powder Bed Fusion. In: ASTM book of Standards
32. Monaheng LF, du Preez WB, Polese C (2021) Towards qualification in the aviation industry: impact toughness of Ti6Al4V(ELI) specimens produced through laser powder bed fusion followed by two-stage heat treatment. Metals (Basel) 11:1736. https://doi.org/10.3390/met1111173610.3390/met11111736 ↗
33. E94/E94M (2017) Designation: E94/E94M-17 Standard Guide for Radiographic Examination Using Industrial Radiographic Film 1. In: ASTM Book of Standards, pp 1–13
34. ASTM-E8 (2018) Standard test methods for tension testing of metallic materials. In: ASTM book of standards
35. ASTM-E23 (2018) Standard test methods for notched bar impact testing of metallic materials. In: ASTM book of standards
36. ASTM-E399 (2020) Standard test method for linear-elastic plane-strain fracture toughness of metallic materials. In: ASTM book of standards
37. E3 (2017) E 3-11 preparation of metallographic specimens. In: ASTM Book of standards, pp 1–12
38. E112 (2013) E112-13 Standard test methods for determining average grain size. In: ASTM book of standards, pp 1–28
39. Yan Q, Chen B, Kang N et al (2020) Comparison study on microstructure and mechanical properties of Ti–6Al–4V alloys fabricated by powder-based selective-laser-melting and sintering methods. Mater Charac 164:110358. https://doi.org/10.1016/j.matchar.2020.11035810.1016/j.matchar.2020.110358 ↗
40. Xu W, Sun S, Elambasseril J et al (2015) Ti–6Al–4V additively manufactured by selective laser melting with superior mechanical properties. JOM 67:668–673. https://doi.org/10.1007/s11837-015-1297-810.1007/s11837-015-1297-8 ↗
41. Xu W, Brandt M, Sun S et al (2015) Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition. Acta Mater 85:74–84. https://doi.org/10.1016/j.actamat.2014.11.02810.1016/j.actamat.2014.11.028 ↗
42. Wu B, Pan Z, Ding D et al (2018) Effects of heat accumulation on microstructure and mechanical properties of Ti6Al4V alloy deposited by wire arc additive manufacturing. Addit Manuf 23:151–160. https://doi.org/10.1016/j.addma.2018.08.00410.1016/j.addma.2018.08.004 ↗
43. Cain V, Thijs L, Van Humbeeck J et al (2015) Crack propagation and fracture toughness of Ti6Al4V alloy produced by selective laser melting. Addit Manuf 5:68–76. https://doi.org/10.1016/j.addma.2014.12.00610.1016/j.addma.2014.12.006 ↗
44. Gupta A, Bennett CJ, Sun W (2021) The role of defects and characterisation of tensile behaviour of EBM Additive manufactured Ti–6Al–4V: an experimental study at elevated temperature. Eng Fail Anal 120:105115. https://doi.org/10.1016/j.engfailanal.2020.10511510.1016/j.engfailanal.2020.105115 ↗
45. Phutela C, Aboulkhair NT, Tuck CJ, Ashcroft I (2020) The effects of feature sizes in selectively laser melted Ti–6Al–4V parts on the validity of optimised process parameters. Materials (Basel) 13:117. https://doi.org/10.3390/ma1301011710.3390/ma13010117 ↗
46. Antonysamy AA (2012) Microstructure, texture and mechanical property evolution during additive manufacturing of Ti6Al4V alloy for aerospace applications. The University of Manchester, London
47. Vilardell AM, Fredriksson G, Yadroitsev I, Krakhmalev P (2019) Fracture mechanisms in the as-built and stress-relieved laser powder bed fusion Ti6Al4V ELI alloy. Opt Laser Technol 109:608–615. https://doi.org/10.1016/j.optlastec.2018.08.04210.1016/j.optlastec.2018.08.042 ↗
48. ASM, Aerospace Specification Metals Inc. http://asm.matweb.com/search/SpecificMaterial.asp?bassnum=MTP643. 26 May, 2021
49. Lizzul L, Sorgato M, Bertolini R et al (2021) Anisotropy effect of additively manufactured Ti6Al4V titanium alloy on surface quality after milling. Precis Eng 67:301–310. https://doi.org/10.1016/j.precisioneng.2020.10.00310.1016/j.precisioneng.2020.10.003 ↗
50. Kok Y, Tan XP, Wang P et al (2018) Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review. Mater Des 139:565–586. https://doi.org/10.1016/j.matdes.2017.11.02110.1016/j.matdes.2017.11.021 ↗
51. Yadollahi A, Shamsaei N (2017) Additive manufacturing of fatigue resistant materials: Challenges and opportunities. Int J Fatigue 98:14–31. https://doi.org/10.1016/j.ijfatigue.2017.01.00110.1016/j.ijfatigue.2017.01.001 ↗
52. Yadollahi A, Shamsaei N, Thompson SM et al (2017) Effects of building orientation and heat treatment on fatigue behavior of selective laser melted 17–4 PH stainless steel. Int J Fatigue 94:218–235. https://doi.org/10.1016/j.ijfatigue.2016.03.01410.1016/j.ijfatigue.2016.03.014 ↗
53. Edwards P, O’Conner A, Ramulu M (2013) Electron beam additive manufacturing of titanium components: properties and performance. J Manuf Sci Eng. https://doi.org/10.1115/1.402577310.1115/1.4025773 ↗
54. Prasad K, Obana M, Ito A, Torizuka S (2021) Synchrotron diffraction characterization of dislocation density in additively manufactured IN 718 superalloy. Mater Charact 179:111379. https://doi.org/10.1016/j.matchar.2021.11137910.1016/j.matchar.2021.111379 ↗
55. Prasad K, Horita Y, Ito A, Torizuka S (2021) In situ synchrotron diffraction study of a crack-free additively manufactured Ni base superalloy. Scr Mater 200:113896. https://doi.org/10.1016/j.scriptamat.2021.11389610.1016/j.scriptamat.2021.113896 ↗
56. Narayana Murty SVS, Torizuka S, Nagai K et al (2008) Effects of strain on grain boundary characteristics and their correlation to mechanical properties in low carbon steel processed by warm multipass calibre rolling. Mater Sci Technol 24:1167–1173. https://doi.org/10.1179/174328407X21323310.1179/174328407X213233 ↗
57. Van Hooreweder B, Moens D, Boonen R et al (2012) Analysis of fracture toughness and crack propagation of Ti6Al4V produced by selective laser melting. Adv Eng Mater 14:92–97. https://doi.org/10.1002/adem.20110023310.1002/adem.201100233 ↗