The effect of grain size on the flow stress determined from spherical microindentation of die-cast magnesium AM60B alloy
Source abstract
Abstract
Spherical microindentation tests were performed on samples cut from an AM60B magnesium alloy die casting to determine the effects of grain size on the local flow stress. Five samples were indented in the skin region (finer grain sizes), two samples in the core region (larger grain sizes and dendrites), and one sample was indented in both the skin and core region of the die-casting. It was determined that the Hall-Petch equation is applicable for predicting the initial yield point and the flow stress at several levels of plastic strain only in the skin region, and not the core region, of the die-casting. The Hall-Petch slope and intercept stress, determined from spherical indentation in the skin region, compare accurately with previously published results. Possible reasons for indentation results from the core region deviating from the Hall-Petch relationship are discussed. The Hall-Petch slope follows a linearly increasing relation with the square root of plastic strain; however, no conclusions can be drawn concerning this because of the small range of plastic strain tested.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. E. O. Hall, Proc Phys. Soc. B64 (1951) 747.10.1088/0370-1301/64/9/303 ↗
2. N. J. PETCH, J. Iron Steel Inst. 174 (1953) 25.
3. E. O. Hall, Nature 173 (1954) 948.10.1038/173948b0 ↗
4. Z. Shan and A. M. Gokhale, Mater. Sci. Engg. A361 (2003) 267.10.1016/S0921-5093(03)00529-X ↗
5. D. RODRIGO, M. MURRAY, H. MAO, J. BREVICK, C. MOBLEY and R. ESDAILE, in Proceedings of the 20th International NADCA Congress, World of Die Casting (NADCA, Cleveland, OH, 1999) p. 219.
6. A. Wahlberg, J. Iron Steel Inst. 59 (1901) 243.
7. H. O'Neill, Proc. Inst. Mech. Eng. 151 (1944) 116.10.1243/PIME_PROC_1944_151_022_02 ↗
8. D. Tabor, in “The Hardness of Metals” (Clarendon Press, Oxford, United Kingdom, 1951) pp. 12, 46.
9. K. L. Johnson, J. Mech. Phys. Sol. 18 (1970) 115.10.1016/0022-5096(70)90029-3 ↗
10. S. D. Mesarovic and N. A. Fleck, Proc. Royal Soc. Lond., Series A 455 (1999) 2707.10.1098/rspa.1999.0423 ↗
11. J.-H. Ahn and D. Kwon, J. Mater. Res. 16 (2001) 3170.10.1557/JMR.2001.0437 ↗
12. M. Beghini, L. Bertini and V. Fontanari, Intern. J. Comp. Appl. Technol. 15 (2002) 168.10.1504/IJCAT.2002.000292 ↗
13. F. M. HAGGAG, U.S. Patent #4852397 (1990).
14. Y. Y. Lim and M. M. Chaudhri, Philos Mag. A. 82 (2002) 2071.10.1080/01418610208235717 ↗
15. M. Furukawa, Z. Horita, M. Nemoto, R. Z. Valiev and T. G. Langdon, Acta Mater. 44 (1996) 4619.10.1016/1359-6454(96)00105-X ↗
16. A. Couture and J. W. Meier, Mines Bran. Res. Rep. R 153. (Canada Department of Mines and Technical Surveys, 1965), p. 1.
17. T. M. Yue, H. U. Ha and N. J. Musson, J. Mater. Sci. 30 (1995) 2277.10.1007/BF01184573 ↗
18. W. C. Oliver and G. M. Pharr, J. Mater. Res. 7 (1992) 1564.10.1557/JMR.1992.1564 ↗
19. J. Alcala, A. C. Barone and M. Anglada, Acta Mater. 48 (2000) 3451.10.1016/S1359-6454(00)00140-3 ↗
20. D. Yin, in “Microstructural characterization of a magnesium die-casting”, M.E.Sc. Thesis (University of Western Ontario, London, Ontario, 2004).
21. B. J. Coultes, in “Mechanical Property Variation in a Magnesium High-pressure Die-cast Component”, M.E.Sc. Thesis (University of Western Ontario, London, Ontario, 2004).
22. B. J. COULTES, J. T. WOOD, G. WANG and R. BERKMORTEL, in “Magnesium Technology 2003”, edited by H. I. Kaplan (TMS, Warrendale, PA, 2003) p. 45.
23. G. Mima and Y. Tanaka, J. Jpn. Inst. Met. 35 (1971) 319.10.2320/jinstmet1952.35.4_319 ↗
24. W. P. SEQUEIRA, G. L. DUNLOP and M. T. MURRAY, in Proceedings of the 3rd International Magnesium Conference, edited by G. W. Lorimer (The Institute of Metals, Manchester, UK, 1996) p. 63.
25. J. P. WEILER, J. T. WOOD, R. J. KLASSEN, R. BERKMORTEL and G. WANG, in “Magnesium Technology 2005”, edited by N. R. Neelameggham, H. I. Kaplan and B. R. Powell (TMS, Warrendale, PA, 2005) p. 191.
26. B. E. Carlson, in “The Effects of Strain Rate and Temperature on the Deformation of Die Cast AM60B (950425)” (SAE, 1995) p. 343.10.4271/950425 ↗
27. A. L. Bowles, J. R. Griffiths, and C. J. Davidson, in “Magnesium Technology 2001”, edited by J. Hryn (TMS, Warrendale, PA, 2001) p. 161.10.1002/9781118805497.ch29 ↗
28. T. WEISS and P. DAVIES, Trans. Inst. Metal Finish. 78 (2000) 65.10.1080/00202967.2000.11871309 ↗
29. T. Abbott, M. Easton and W. Song, Mater. Sci. Forum. 419–422 (2003) 141.10.4028/www.scientific.net/MSF.419-422.141 ↗
30. P. Andersson, C. H. Caceres and J. Koike, ibid. 419-422 (2003) 123.10.4028/www.scientific.net/MSF.419-422.123 ↗
31. F. E. Hauser, P. R. Landon and J. E. Dorn, Trans. Amer. Inst. Min. Metall. Petrol. Eng. 206 (1956) 589.
32. D. J. LLOYD and S. A. COURT, Mater Sci Technol 19 (2003) 1349.10.1179/026708303225006088 ↗
33. U. F. KOCKS, Metall. Trans. 1 (1970) 1121.10.1007/BF02900224 ↗
34. R. P. CARREKER and W. R. HIBBARD, Acta. Metall. 1 (1953) 654.10.1016/0001-6160(53)90022-4 ↗