Production of sintered materials from air pollution control residues from waste incineration
Source abstract
Abstract
Air pollution control residues from waste incineration have been washed to remove excess chloride and other soluble salts and blended with combinations of soda lime glass and waste electrostatic precipitator dust containing boric oxide from the fibre-glass industry. Homogenous fine powder mixes have been pressed and sintered at temperatures between 900 and 1000 °C. The physical properties and microstuctural characteristics of the glass–ceramics formed have been assessed. The results show that it is possible to produce a dense glass–ceramic material containing wollastonite and gehlenite crystalline phases with a hardness of 4.5 GPa. The high density and hardness means that the glass–ceramic may have a potential use in high value construction products.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycling and utilization of industrial and municipal waste in materials production · Glass properties and applications · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Environmental Services Association (2005) Draft APC residue case study, DEFRA, https://doi.org/www.defra.gov.uk/environment/waste/hazforum/pdf/hwf-3-5iv.pdf, as on March 2005
2. Abanades S, Flamant G, Gagnepain B, Gauthier D (2002) Waste Manage Res 20(1):5510.1177/0734242X0202000107 ↗
3. Lee PH, Nasserzadeh V, Swithenbank J, Laming JV, Goodfellow J, Mcleod C, Argent BB, Lawrence D, Garrod N (1999) Process Saf Environ Protect 77(B4):21210.1205/095758299530099 ↗
4. He P-J, Zhang H, Zhang C-G, Lee D-J (2004) J Hazard Mater B116:22910.1016/j.jhazmat.2004.09.009 ↗
5. European Waste Catalogue (2000) In: 2000/532/EC
6. Geysen D, Vandecasteele C, Jaspers M, Wauters G (2004) J Hazard Mater 107(3):13110.1016/j.jhazmat.2003.12.001 ↗
7. Alba N, Vazquez E, Gasso S, Baldasano JM (2001) Waste Manage 21(4):31310.1016/S0956-053X(00)00082-9 ↗
8. Todorovic J, Ecke H, Lagerkvist A (2003) Waste Manage 23(7):62110.1016/S0956-053X(03)00106-5 ↗
9. Barna R, Rethy Z, Imyim A, Perrodin Y, Moszkowicz P, Tiruta-Barna L (2000) Waste Manage 20(8):74110.1016/S0956-053X(00)00032-5 ↗
10. Rouchotas E (2001) MSc thesis, Department of Civil and Environmental Engineering, Imperial College London
11. Wang KS, Chiang KY, Lin KL, Sun CJ (2001) Hydrometallurgy 62(2):7310.1016/S0304-386X(01)00186-4 ↗
12. Chimenos JM, Fernandes AI, Cervantes A, Miralles L, Fernandes MA, Espiell F (2005) Waste Manage 25(7):68610.1016/j.wasman.2004.12.014 ↗
13. Abbas Z, Moghaddam AP, Steenari BM (2003) Waste Manage 23(4):29110.1016/S0956-053X(02)00154-X ↗
14. Boccaccini AR, Wu JP, Rawlings RD (2006) J Mater Sci 41(3):733. doi:https://doi.org/10.1007/s10853-006-6554-310.1007/s10853-006-6554-3 ↗
15. Colombo P, Brusatin G, Bernardo E, Scarinci G (2003) Curr Opin Solid State Mat Sci 7(3):22510.1016/j.cossms.2003.08.002 ↗
16. Boccaccini AR, Bucker M, Bossert J, Marszalek K (1997) Waste Manage 17(1):3910.1016/S0956-053X(97)00035-4 ↗
17. Barbieri L, Lancellotti I, Manfredini T, Queralt I, Rincon JM, Romero M (1999) Fuel 78(2):27110.1016/S0016-2361(98)00134-3 ↗
18. Olgun A, Erdogan Y, Ayhan Y, Zeybek B (2005) Ceram Int 31:15310.1016/j.ceramint.2004.04.007 ↗
19. Shao H, Liang K, Peng F, Zhou F, Hu A (2005) Minerals Eng 18(6):63510.1016/j.mineng.2004.09.007 ↗
20. Catarino L, Sousa J, Martins IM, Vieira MT, Oliveira MM (2003) J Mater Process Technol 143:84310.1016/S0924-0136(03)00341-8 ↗
21. Pisciella P, Crisucci S, Karamanov A, Pelino M (2001) Waste Manage 21:110.1016/S0956-053X(00)00077-5 ↗
22. Rozenstrauha I, Wu JP, Boccaccini AR (2005) Glass Technol 46(3):248
23. Yun YH, Yoon CH, Kim YH, Kim CK, Kim SB, Kwon JT, Kang BA, Hwang KS (2002) Ceram Int 28(5):50310.1016/S0272-8842(02)00002-0 ↗
24. Barbieri L, Corradi A, Lancellotti I, Pellacani GC, Boccaccini AR (2003) Glass Technol 44(5):184
25. Boccaccini AR, Schawohl J, Hern H, Schunck B, Rincon JM, Romero M (2000) Glass Technol 41(3):99
26. Boccaccini AR, Kopf M, Stumpfe W (1995) Ceram Int 21(4):23110.1016/0272-8842(95)99787-C ↗
27. Romero M, Rincon JM, Rawlings RD, Boccaccini AR (2001) Mater Res Bull 36(1–2):38310.1016/S0025-5408(01)00501-3 ↗
28. Rincon JM, Romero M, Boccaccini AR (1999) J Mater Sci 34(18):4413. doi:https://doi.org/10.1023/A:100462081800110.1023/A:1004620818001 ↗
29. Hollander HI, Plumley AL, Decesare RS (1996) J Hazard Mater 47(1–3):36910.1016/0304-3894(95)00113-1 ↗
30. Kim JM, Kim HS (2004) J European Ceram Soc 24:237310.1016/j.jeurceramsoc.2003.08.001 ↗
31. Wexell D, Vitrification of ash from waste-to-energy incinerators, Part II. Cold crown melting and parameters for scale-up, Pollution Prevention Resource Center Corning Inc., https://doi.org/www.pprc.org/pprc/rpd/statefnd/nyschwm/vitrific.html, as on 05/08/2005,
32. Cheeseman CR, Monteiro Da Rocha S, Sollars C, Bethanis S, Boccaccini AR (2003) Waste Manage 23(10):90710.1016/S0956-053X(03)00039-4 ↗
33. Rawlings RD, Boccaccini AR (2004) Glass Technol 45(2):108
34. Borax Consolidated Limited (1965) In: Glasses, 3rd ed., London, Borax Consolidated London, p 83
35. Lundtorp K, Jensen DL, Sorensen MA, Christensen TH, Mogensen EPB (2002) Waste Manage Res 20(1):6910.1177/0734242X0202000108 ↗
36. Cheeseman CR, Sollars CJ, Mcentee S (2003) Resour Conserv Recycl 40(1):1310.1016/S0921-3449(03)00022-3 ↗
37. Tsai C-C, Wang K-S, Chiou I-J (2006) J Hazard Mater 134(1–3):8710.1016/j.jhazmat.2005.10.035 ↗
38. Romero M, Rawlings RD, Rincon JM (1999) J Eur Ceram Soc 19(12):204910.1016/S0955-2219(99)00011-4 ↗
39. Esposito L, Tucci A, Naldi D (2005) J Eur Ceram Soc 25(9):148710.1016/j.jeurceramsoc.2004.05.030 ↗