Abstract
Fracture behaviour of virgin and six times recycled isotactic polypropylene (PP) has been studied. Instrumented Charpy impact tests have been carried out to characterise the fracture parameters and scanning electron microscopy was used to study the fracture surfaces. Recycled PP presents slightly smaller spherulites and lower fracture toughness than virgin one. Fractography analysis reveals that crazing is the dominant fracture micromechanism for both materials, and that the difference in fracture toughness is a consequence of the smaller plastically deformed volume at the notch tip of the recycled polypropylene.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Polymer crystallization and properties · Fiber-reinforced polymer composites · Natural Fiber Reinforced Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. C. D. Papaspyrides and J.G. Poulakis, in “The Polymeric Materials Encyclopedia,” edited by J. C. Salomone (CRC Press, Inc, 1996) p. 7403.
2. V. A. GonzÁlez GonzÁlez, G. Neira-VelÁzquez and J. L. Angulo SÁnchez, Polym. Degrad. Stab. 60 (1998) 33.10.1016/S0141-3910(96)00233-9 ↗
3. B. E. Tiganis, R. A. Shanks and Y. Long, J. Appl. Polym. Sci. 59 (1996) 663.10.1002/(SICI)1097-4628(19960124)59:4<663::AID-APP12>3.0.CO;2-R ↗
4. Q. Ying, Y. Zhao and Y. Liu, Makromol. Chem. 192 (1991) 1041.10.1002/macp.1991.021920503 ↗
5. V. M. Gol'Dberg and G. E. Zaikov, Polym. Degrad. Stab. 19 (1987) 221.10.1016/0141-3910(87)90057-7 ↗
6. H. Hinsken, S. Moss J. R. Pauquet and H. Zweifel, ibid. 34 (1991) 279.10.1016/0141-3910(91)90123-9 ↗
7. J. Aurrekoetxea, M. A. Sarrionandia, I. Urrutibeascoa and M. LL. Maspoch, J. Mater. Sci., in press.
8. R. H. Olley and D. C. Bassett, Polymer 23 (1982) 1707.10.1016/0032-3861(82)90110-0 ↗
9. J. G. Williams, “Fracture Mechanics of Polymers” (Ellis Horwood, Chichester, 1987).
10. J. L. Way, J. R. Atkinson and J. Nutting, J. Mater. Sci. 9 (1974) 293.10.1007/BF00550954 ↗
11. K. Friedrich, Progr. Colloid Polymer Sci. 64 (1978) 103.10.1007/BFb0117509 ↗
12. M. Ouederni and P. J. Phillips, J. Polym. Sci. B Polym. Phys. 33 (1995) 1313.10.1002/polb.1995.090330901 ↗
13. M. Sugimoto, M. Ishikawa and K. Hatada, Polymer 36 (1995) 3675.10.1016/0032-3861(95)93769-I ↗
14. Z. Bratczak, A. Galeski, E. Mastrucelli and H. Janik, ibid. 26 (1985) 1843.10.1016/0032-3861(85)90013-8 ↗
15. J. F. Kalthoff, Int. J. Fract. 27 (1987) 277.10.1007/BF00017973 ↗
16. A. Van Der Wal, Ph.D thesis, University of Twente, 1996.
17. S. C. Tjong, J. S. Shen and R. K. Y. Li, Polymer 37 (1996) 2309.10.1016/0032-3861(96)85340-7 ↗
18. R. Greco and G. Ragosta, J. Mater. Sci. 23 (1988) 4171.10.1007/BF01106853 ↗
19. A. O. Ibhadon, J. Appl. Polym. Sci. 69 (1998) 2657.10.1002/(SICI)1097-4628(19980926)69:13<2657::AID-APP16>3.0.CO;2-R ↗
20. K. Friedrich, in “Crazing in Polymers,” edited H. H. Kausch (Springler-Verlag, Berlin, 1983) p. 225.10.1007/BFb0024059 ↗
21. J. Karger-Kocsis, J. Varga and G. W. Ehrenstein, J. Appl. Polym. Sci. 64 (1997) 2057.10.1002/(SICI)1097-4628(19970613)64:11<2057::AID-APP1>3.0.CO;2-I ↗
22. A. Van Der Wal, J. J. Mulder, H. A. Thijs and R. J. Gaymans, Polymer 39 (1998) 5467.10.1016/S0032-3861(97)10278-6 ↗
23. J. Varga, J. Mater. Sci. 27 (1992) 2557.10.1007/BF00540671 ↗
24. M. Ishikawa, K. Ushui, Y. Kondo, K. Hatada and S. Gima, Polymer 37 (1996) 5375.10.1016/S0032-3861(96)00364-3 ↗
25. R. Gensler, C. J. G. Plummer, C. Grein and H. H. Kausch, ibid. 41 (2000) 3809.10.1016/S0032-3861(99)00593-5 ↗