Supersonic particle bombardment of additive manufactured Ti6Al4V-induced gradient microstructure with prominent tribology and corrosion resistance
Source abstract
Abstract
The effects of supersonic particle bombardment (SFPB) on the microstructure, microhardness and wear property of Ti6Al4V alloy prepared by laser metal deposition (LMD) were investigated in this paper. The electrochemical corrosion behaviors of the LMDed Ti6Al4V alloy samples before and after SFPB treatment in 3.5% NaCl solution were measured. The results showed that a gradient severe deformation layer of ~ 350 μm thickness was formed with refined equiaxed grains oriented in various directions on the surface of LMDed Ti6Al4V alloy after SFPB treatment. The microhardness of the deformation layer was significantly increased due to the plastic deformation, grain refinement, dislocations and deformation twins increment. After SFPB treatment, the LMDed Ti6Al4V exhibited higher wear resistance which is about 55.6% decrease in wear loss than that of the untreated sample. Moreover, the corrosion resistance and corrosion rate of the SFPB-treated samples in 3.5% NaCl solution improved due to the finer hexagonal grains and high density of grain boundary in the severe deformation layer.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Surface Treatment and Residual Stress · High-Velocity Impact and Material Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Gao ZN, Shi HZ, Yang XY, Lyu FY, Wang LL, Zhan XH (2022) Influence of heat accumulation on the distribution uniformity of microstructure and mechanical properties of laser additive manufacturing joint of 80 mm thick Ti6Al4V titanium alloy plate. Mater Process Tech 310:11777410.1016/j.jmatprotec.2022.117774 ↗
2. Prakash C, Singh S, Pruncu C, Mishra V, Królczyk G, Pimenov DY, Pramanik A (2019) Surface modification of Ti-6Al-4V alloy by electrical discharge coating process using partially sintered Ti–Nb electrode. Materials 12:100610.3390/ma12071006 ↗
3. Schmidt M, Merklein M, Bourell D, Dimitrov D, Hausotte T, Wegener K, Overmeyer L, Vollertsen F, Levy GN (2017) Laser based additive manufacturing in industry and academia. Cirp Ann-Manuf Techn 66:561–58310.1016/j.cirp.2017.05.011 ↗
4. Chen XL, Liang ZL, Guo YH, Sun ZG, Wang YQ, Zhou L (2021) A study on the grain refinement mechanism of Ti-6Al-4V alloy produced by wire arc additive manufacturing using hydrogenation treatment processes. J Alloy Compd 890:161634
5. Bermingham MJ, StJohn DH, Krynen J, Tedman-Jones S, Dargusch MS (2019) Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing. Acta Mater 168:261–27410.1016/j.actamat.2019.02.020 ↗
6. Vrancken B, Thijs L, Kruth JP (2012) Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties. J Alloy Compd 541:177–18510.1016/j.jallcom.2012.07.022 ↗
7. Andrey B, Evgeny G, Evgeny Z (2019) The effect of preprocessing on surface quality in the chemical polishing of parts from titanium alloy produced by SLM. Mater Today Proc 19:2291–229410.1016/j.matpr.2019.07.671 ↗
8. Qiu C, Adkins NJE, Attallah MM (2013) Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti-6Al-4V. Mat Sci Eng A 578:230–23910.1016/j.msea.2013.04.099 ↗
9. Mironov S, Sato YS, Kokawa H (2018) Friction-stir welding and processing of Ti-6Al-4V titanium alloy: a review. J Mater Sci Technol 34:58–7210.1016/j.jmst.2017.10.018 ↗
10. Zheng XY, Zhang YR, Zhang BR (2017) Effect of N-ion implantation and diamond-like carbon coating on fretting wear behaviors of Ti6Al7Nb in artificial saliva. T Nonferr Metal Soc 27:1071–108010.1016/S1003-6326(17)60125-0 ↗
11. Karimi A, Amini S (2016) Steel 7225 surface ultrafine structure and improvement of its mechanical properties using surface nanocrystallization technology by ultrasonic impact. Int J Adv Manuf Tech 83:1127–113410.1007/s00170-015-7619-8 ↗
12. Yan X, Yin S, Chen C, Jenkins R, Lupoi R, Bolot R, Ma WY, Kuang M, Liao HL, Lu J, Liu M (2019) Fatigue strength improvement of selective laser melted Ti6Al4V using ultrasonic surface mechanical attrition. Mater Res Lett 7:327–33310.1080/21663831.2019.1609110 ↗
13. Zhang XC, Zhang YK, Lu JZ, Xuan FZ, Wang ZD, Tu ST (2010) Improvement of fatigue life of Ti-6Al-4V alloy by laser shock peening. Mater Sci Eng A 527:3411–341510.1016/j.msea.2010.01.076 ↗
14. Wang ZB, Tao NR, Li S (2003) Effect of surface nanocrystallization on friction and wear properties in low carbon steel. Mater Sci Eng A 352:144–14910.1016/S0921-5093(02)00870-5 ↗
15. Eyzat Y, Chemkhi M, Portell Q (2019) Characterization and mechanical properties of As-Built SLM Ti-6Al-4V subjected to surface mechanical post-treatment. Procedia CIRP 81:1225–122910.1016/j.procir.2019.03.298 ↗
16. Slawik S, Bernarding S, Lasagni F, Navarro C, Mücklich F (2021) Microstructural analysis of selective laser melted Ti6Al4V modified by laser peening and shot peening for enhanced fatigue characteristics. Mater Charact 173:11093510.1016/j.matchar.2021.110935 ↗
17. Zhang Q, Duan BB, Zhang ZQ, Wang JB, Si CR (2011) Effect of ultrasonic shot peening on microstructure evolution and corrosion resistance of selective laser melted Ti6Al4V alloy. Mater Lett 65:1268–127110.1016/j.matlet.2011.01.041 ↗
18. Bagherifard S, Fernandez-Pariente I, Ghelichi R, Guagliano M (2013) Fatigue behavior of notched steel samples with nanocrystallized surface obtained by severe shot peening. Mater Des 45:497–50310.1016/j.matdes.2012.09.025 ↗
19. Shi L, Cui XF, Li J, Jin G, Zhang XR, Wen X, Tian HL (2022) Enhanced impact and wear properties of gear steel by supersonic fine particle bombardment modification technology. Mater Charact 194:11236810.1016/j.matchar.2022.112368 ↗
20. Wu YL, Xiong Y, Liu W, Chen ZG, Zhang X, Wang SB, Cao W (2021) Effect of supersonic fine particle bombardment on microstructure and fatigue properties of Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy at different temperatures. Surf Coat Tech 421:12747310.1016/j.surfcoat.2021.127473 ↗
21. Ma GZ, Xu BS, Wang HD, Si HJ, Yang DX (2011) Effect of surface nanocrystallization on the tribological properties of 1Cr18Ni9Ti stainless steel. Mater Lett 65:1268–127110.1016/j.matlet.2011.01.041 ↗
22. Wang Z, Liu ZQ, Gao CF, Wong KH, Ye SJ, Xiao ZY (2020) Modified wear behavior of selective laser melted Ti6Al4V alloy by direct current assisted ultrasonic surface rolling process. Surf Coat Tech 381:12512210.1016/j.surfcoat.2019.125122 ↗
23. Yang JJ, Yu HC, Yin J, Yao JH, Cai J, Luo KY (2016) Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting. Mater Design 108:308–31810.1016/j.matdes.2016.06.117 ↗
24. Lu JZ, Lu HF, Xu X, Yao J, Luo K (2020) High-performance integrated additive manufacturing with laser shock peening –induced microstructural evolution and improvement in mechanical properties of Ti6Al4V alloy components. Int J Mach Tool Manu 148:10347510.1016/j.ijmachtools.2019.103475 ↗
25. Charlotte DF, Sébastien M, Olivier R, Lionel G, Stéphane G (2016) Electron beam melted Ti-6Al-4V: microstructure, texture and mechanical behavior of the as-built and heat-treated material. Mater Sci Eng A 652:105–11910.1016/j.msea.2015.11.052 ↗
26. Zhu KY, Vassel A, Brisset F, Lu K, Lu J (2004) Nanostructure formation mechanism of a-titanium using SMAT. Acta Mater 52:4101–411010.1016/j.actamat.2004.05.023 ↗
27. Liu Y, Xu HZ, Peng BY, Wang XF, Li SX, Wang Q, Li ZG, Wang YG (2022) Effect of heating treatment on the microstructural evolution and dynamic tensile properties of Ti-6Al-4V alloy produced by selective laser melting. J Manuf Process 74:244–25510.1016/j.jmapro.2021.12.035 ↗
28. Ma JK, Zhang YS, Li JJ, Wang ZJ, Wang JC (2022) Variant selection within one β grain in laser solid formed Ti-6Al-4V alloys. Mater Charact 185:11174410.1016/j.matchar.2022.111744 ↗
29. Liu Y, Pang ZC, Li M, Wang YG, Wang D, Song CH, Li SX (2019) Investigation into the dynamic mechanical properties of selective laser melted Ti-6Al-4V alloy at high strain rate tensile loading. Mater Sci Eng A 745:440–44910.1016/j.msea.2019.01.010 ↗
30. Yin MG, Cai ZB, Li ZY, Zhou ZR, Wang WJ, He WF (2019) Improving impact wear resistance of Ti-6Al-4V alloy treated by laser shock peening. T Nonferr Metal Soc 29:1439–144810.1016/S1003-6326(19)65051-X ↗
31. Guo W, Sun RJ, Song BW, Zhu Y, Li F, Che ZG, Li B, Guo C, Liu L, Peng P (2018) Laser shock peening of laser additive manufactured Ti6Al4V titanium alloy. Surf Coat Tech 349:503–51010.1016/j.surfcoat.2018.06.020 ↗
32. Pramod K, Mahobia GS, Kausik C (2020) Surface nanocrystallization of β-titanium alloy by ultrasonic shot peening. Mater Today Proc 28:486–49010.1016/j.matpr.2019.10.174 ↗
33. Chen JW, Zhang CH, Zhou FQ, Zhang S, Chen HT, Wang Q (2021) Microstructural, electrochemical and wear-corrosion characterization of TC4-5Cu alloy fabricated by selective laser melting. J Alloy Compd 874:15995310.1016/j.jallcom.2021.159953 ↗
34. Zhou LJ, Deng H, Chen LQ, Qiu WB, Wei YQ, Peng HQ, Hu ZD, Lu D, Cui XD, Tang J (2021) Morphological effects on the electrochemical dissolution behavior of forged and additive manufactured Ti-6Al-4V alloys in runway deicing fluid. Surf Coat Tech 414:12709610.1016/j.surfcoat.2021.127096 ↗
35. Jelliti S, Richard C, Retraint D, Roland T, Chemkhi M, Demangel C (2013) Effect of surface nanocrystallization on the corrosion behavior of Ti-6Al-4V titanium alloy. Surf Coat Tech 224:82–8710.1016/j.surfcoat.2013.02.052 ↗
36. Martin É, Azzi M, Salishchev GA, Szpunar J (2010) Influence of microstructure and texture on the corrosion and tribocorrosion behavior of Ti-6Al-4V. Tribol Int 43:91810.1016/j.triboint.2009.12.055 ↗
37. Heidarbeigy M, Karimzadeh F, Saatchi A (2008) Corrosion and galvanic coupling of heat treated Ti-6Al-4V alloy weldment. Mater Lett 62:1575–157810.1016/j.matlet.2007.09.045 ↗
38. Liu RY, Yu S, Lin NM, Zeng QF, Wang ZH, Wu YC (2021) Application of ultrasonic nanocrystal surface modification (UNSM) technique for surface strengthening of titanium and titanium alloys: a mini review. J Mater Res Technol 11:351–37710.1016/j.jmrt.2021.01.013 ↗