journal article·2022-10

Correlation microstructural evolution with creep-rupture properties of a novel directionally solidified Ni-based superalloy M4706

P. Zhang, Y. Yuan, Q. Niu, P. Liu, J. Li, X. F. Gong, X. L. Song, Y. F. Gu

Journal of Materials Science· Volume 57· Issue 37
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High Temperature Alloys and Creep · Intermetallics and Advanced Alloy Properties · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Pollock TM (2016) Alloy design for aircraft engines. Nature Mater 15(8):809–81510.1038/nmat4709 ↗
2. Cailletaud G, Cormier J, Eggeler G, Maurel V, Nazé L (2022) Nickel base single crystals across length scales. Elsevier
3. Jackson MP, Reed RC (1999) Heat treatment of UDIMET 720Li: the effect of microstructure on properties. Mater Sci Eng A 259:85–9710.1016/S0921-5093(98)00867-3 ↗
4. Sluytman JSV, Pollock TM (2012) Optimal precipitate shapes in nickel-base γ–γ′ alloys. Acta Mater 60:1771–178310.1016/j.actamat.2011.12.008 ↗
5. Tian C, Han G, Cui C, Sun X (2014) Effects of stacking fault energy on the creep behaviors of Ni-base superalloy. Mater Des 64:316–32310.1016/j.matdes.2014.08.007 ↗
6. Grant BMB, Francis EM, Quinta da Fonseca J, Daymond MR, Preuss M (2012) Deformation behaviour of an advanced nickel-based superalloy studied by neutron diffraction and electron microscopy. Acta Mater 60:6829–684110.1016/j.actamat.2012.09.005 ↗
7. Wang J, Zhou L, Sheng L, Guo J (2012) The microstructure evolution and its effect on the mechanical properties of a hot-corrosion resistant Ni-based superalloy during long-term thermal exposure. Mater Des 39:55–6210.1016/j.matdes.2012.02.020 ↗
8. Zhang P, Yuan Y, Zhong L et al (2021) Microstructural stability and tensile properties of a new γ′-hardened Ni-Fe-base superalloy. Materialia 16:10106110.1016/j.mtla.2021.101061 ↗
9. Jianting G (2010) The current situation of application and development of superalloys in the fileds of energy industry. Acta Metall Sin 46:513–52710.3724/SP.J.1037.2009.00860 ↗
10. Zhang P, Li J, Gong XF, Yuan Y, Gu YF, Wang JC, Yan JB, Yin HF (2019) Creep behavior and deformation mechanisms of a novel directionally solidified Ni-base superalloy at 900 °C. Mater Charact 148:201–20710.1016/j.matchar.2018.12.023 ↗
11. Zhang P, Yuan Y, Shen SC, Li B, Zhu RH, Yang GX, Song XL (2017) Tensile deformation mechanisms at various temperatures in a new directionally solidified Ni-base superalloy. J Alloys Compds 694:502–50910.1016/j.jallcom.2016.09.303 ↗
12. Zhang P, Yuan Y, Li B, Guo SW, Yang GX, Song XL (2016) Tensile deformation behavior of a new Ni-base superalloy at room temperature. Mater Sci Eng A 655:152–15910.1016/j.msea.2015.12.089 ↗
13. Zhang P, Yuan Y, Li J, Xu YF, Song X, Yang G (2017) Tensile deformation mechanisms in a new directionally solidified Ni-base superalloy containing coarse γ′ precipitates at 650 °C. Mater Sci Eng A 702:343–34910.1016/j.msea.2017.07.025 ↗
14. CS Press, GB/T 14999.T-2010, Test methods for grain sizes, primary dendrite spacing and microshrinkage of superalloy castings. China Standard Press, Beijing, China, 2010.
15. Roskosz S, Adamiec J (2009) Methodology of quantitative evaluation of porosity, dendrite arm spacing and grain size in directionally solidified blades made of CMSX-6 nickel alloy. Mater Charact 60:1120–112610.1016/j.matchar.2009.01.024 ↗
16. Shao C, Liu H, Li JT, Ma ZL, Zhao M (2012) Applications of hot isostatic pressing on cast superalloy. Mater Rev 26:121–135
17. Kozar RW, Suzuki A, Milligan WW, Schirra JJ, Savage MF, Pollock TM (2009) Strengthening mechanisms in polycrystalline multimodal nickel-base superalloys. Metall Mater Trans A 40:1588–160310.1007/s11661-009-9858-5 ↗
18. Zhang P, Yuan Y, Gao ZH, Gu YF, Lu JT (2020) Strain-rate insensitive yield strength and deformation mechanisms of Ni-base superalloy CM247LC at 600 °C. J Alloys Compds 45:158478
19. Lvov G, Levit VI, Kaufman MJ (2004) Mechanism of primary MC carbide decomposition in Ni-base superalloys. Metall Mater Trans A 35:1669–167910.1007/s11661-004-0076-x ↗
20. Qin XZ, Guo JT, Yuan C, Chen CL, Ye HQ (2007) Effects of long-term thermal exposure on the microstructure and properties of a cast Ni-base superalloy. Metall Mater Trans A 38:3014–302210.1007/s11661-007-9381-5 ↗
21. Hou JS, Guo JT, Yang GX, Zhou LZ, Qin XZ, Ye HQ (2008) The microstructural instability of a hot corrosion resistant superalloy during long-term exposure. Mater Sci Eng A 498:349–35810.1016/j.msea.2008.08.005 ↗
22. Wang T, Sheng G, Liu ZK, Chen LQ (2008) Coarsening kinetics of γ′ precipitates in the Ni-Al-Mo system. Acta Mater 56:5544–555110.1016/j.actamat.2008.07.024 ↗
23. Philippe T, Voorhees PW (2013) Ostwald ripening in multicomponent alloys. Acta Mater 61:4237–424410.1016/j.actamat.2013.03.049 ↗
24. Martens V, Nembach E (1975) Strengthening of the nimonic alloy PE 16 by ordered particles of Ni3(Al, Ti). Acta Metall 23:149–15310.1016/0001-6160(75)90178-9 ↗
25. Zhang P, Yuan Y, Yan JB, Wang JC, Song XL, Yang GX (2018) Morphological evolution of γ′ precipitates in superalloy M4706 during thermal aging. Mater Letts 211:107–10910.1016/j.matlet.2017.09.096 ↗
26. Zhang P, Ma L, Yang G, Song X (2016) Extraordinary plastic behaviour of the γ′ precipitate in a directionally solidified nickel-based superalloy. Phil Mag Letts 96:19–2610.1080/09500839.2015.1134832 ↗
27. Li L, Gong X, Wang C et al (2021) Correlation between phase stability and tensile properties of the Ni-based superalloy MAR-M247. Acta Metall Sin 34:872–88410.1007/s40195-020-01139-4 ↗
28. Lifshitz IM, Slyozov VV (1961) The kinetics of precipitation from supersaturated solid solutions. J Phys Chem Solids 19:35–5010.1016/0022-3697(61)90054-3 ↗
29. Wagner C (1961) Theorie der Alterung von Niederschägen durch Umlösen (Ostwald-Reifung). Z Metall 65:581–591
30. Moshtaghin RS, Asgari S (2003) Growth kinetics of γ′ precipitates in superalloy IN-738LC during long term aging. Mater Des 24:325–33010.1016/S0261-3069(03)00061-X ↗
31. Jiang XW, Wang D, Xie G, Li H, Lou LH, Zhang J (2014) The effect of long-term thermal exposure on the microstructure and stress rupture property of a directionally solidified Ni-based superalloy. Metall Mater Trans A 45:6016–602610.1007/s11661-014-2559-8 ↗
32. Ardell AJ, Nicholson R (1966) On the modulated structure of aged Ni-Al alloys. Acta Metall 14:1295–130910.1016/0001-6160(66)90247-1 ↗
33. Fährmann M, Fratzl P, Paris O, Fährmann E, Johnson WC (1995) Influence of coherency stress on microstructural evolution in model Ni-Al-Mo alloys. Acta Metall Mater 43:1007–102210.1016/0956-7151(94)00337-H ↗
34. Fährmann M, Wolf JG, Pollock TM (1996) The influence of microstructure on the measurement of γ-γ′ lattice mismatch in single-crystal Ni-base superalloys. Mater Sci Eng A 210:8–1510.1016/0921-5093(95)10073-3 ↗
35. Xia PC, Yu JJ, Sun XF, Guan HR, Hu ZQ (2007) The influence of thermal exposure on the microstructure and stress rupture property of DZ951 nickel-base alloy. J Alloys Compds 443:125–13110.1016/j.jallcom.2006.09.123 ↗
36. Zhang JX, Wang JC, Harada H, Koizumi Y (2005) The effect of lattice misfit on the dislocation motion in superalloys during high-temperature low-stress creep. Acta Mater 53:4623–463310.1016/j.actamat.2005.06.013 ↗
37. Zhang JX, Harada H, Koizumi Y, Kobayashi T (2010) Dislocation motion in the early stages of high-temperature low-stress creep in a single-crystal superalloy with a small lattice misfit. J Mater Sci 45:523–532. https://doi.org/10.1007/s10853-009-3970-110.1007/s10853-009-3970-1 ↗
38. Tang Y, Huang M, Xiong J, Li J, Zhu J (2017) Evolution of superdislocation structures during tertiary creep of a nickel-based single-crystal superalloy at high temperature and low stress. Acta Mater 126:336–34510.1016/j.actamat.2016.12.072 ↗
39. Pollock TM, Argon AS (1992) Creep resistance of CMSX-3 nickel base superalloy single crystals. Acta Metall Mater 40:1–3010.1016/0956-7151(92)90195-K ↗
40. Carry C, Strudel JL (1977) Apparent and effective creep parameters in single crystals of a nickel base superalloy-I Incubation period. Acta Metall 25:767–77710.1016/0001-6160(77)90092-X ↗
41. Carry C, Strudel JL (1978) Apparent and effective creep parameters in single crystals of a nickel base superalloy-II. Secondary creep Acta Metall 26:859–87010.1016/0001-6160(78)90035-4 ↗
42. Blum W, Reppich B (1985) Creep of particle-strengthened alloys. In: Wilshire B, Evans RW (eds) Creep behavior of crystalline solids. Pineridge Press, pp 83–135
43. Link T, Feller-Kniepmeier M (1992) Shear mechanisms of the γ′ phase in single-crystal superalloys and their relation to creep. Metall Trans A 23:99–10510.1007/BF02660857 ↗
44. Wang C, Guo Y, Guo J, Zhou L (2016) Microstructural changes and their effect on tensile properties of a Ni-Fe based alloy during long-term thermal exposure. Mater Sci Eng A 670:178–18710.1016/j.msea.2016.06.018 ↗
45. Pollock TM, Argon AS (1994) Directional coarsening in nickel-base single crystals with high volume fractions of coherent precipitates. Acta Metall Mater 42:1859–187410.1016/0956-7151(94)90011-6 ↗
46. Nabarro FRN (1996) Rafting in Superalloys. Metall Mater Trans A 27:513–53010.1007/BF02648942 ↗
47. Guo JT, Yuan C, Yang HC, Lupinc V, Maldini M (2001) Creep-rupture behavior of a directionally solidified nickel-base superalloy. Metall Mater Trans A 32:1103–111010.1007/s11661-001-0121-y ↗
48. Monkman FC, Grant NJ (1956) An empirical relationship between rupture life and minimum creep rate in creep-rupture tests. Rroc. ASTM: 595–603.
49. Reppich B, Schepp P, Wehner G (1982) Some new aspects concerning particle hardening mechanisms in γ’ precipitating nickel-base alloys-II. Experiments Acta Metallu 30:95–10410.1016/0001-6160(82)90049-9 ↗
50. Ardell AJ (1995) Intermetallics compounds as precipitates and dispersoids in high-strength alloys. In: Westbrook JH, Fleischer RL (eds) in: IntermetallicCompounds. John Wiley and Sons, pp 257–286
51. Heilmaier M, Leetz U, Reppich B (2001) Order strengthening in the cast nickel-based superalloy IN 100 at room temperature. Mater Sci Eng A 319–321:375–37810.1016/S0921-5093(01)00989-3 ↗
52. Feller-Kniepmeier M, Link T, Poschmann I, Scheunemann-Frerker G, Schulze C (1996) Temperature dependence of deformation mechanisms in a single crystal nickel-base alloy with high volume fraction of γ′ phase. Acta Mater 44:2397–240710.1016/1359-6454(95)00354-1 ↗