Effect of Co addition on hardness and electrical conductivity of Cu–Si alloys

Chenhui Lei, Huiya Yang, Feng Zhao, Xiaoyang Fang, Youtong Fang, Liang Meng, Jiabin Liu, Hongtao Wang

Journal of Materials Science· Volume 56· Issue 26
Publisher page

Abstract

High-strength and high-conductivity Cu alloys are widely required in railway and lead frames. As a conventional element, Si reduces the electrical conductivity of Cu alloys significantly. In this work, Co is introduced into Cu–Si alloys for improving the mechanical and electrical properties. The results show that the Co-containing alloy possesses much higher hardness and conductivity than the Co-free alloys. The added Co reacts with Si to produce high density of CoSi nanoprecipitates that have a semi-coherent interface with the Cu matrix in the aged Cu–Co–Si alloy. The presence of CoSi nanoprecipitates is sufficiently verified by X-ray, energy-dispersive spectrometer and electron diffraction pattern. The formation of CoSi nanoprecipitates can pin dislocation motion, prevent the recrystallization and reduce the Si solute concentration in the Cu matrix. The effects of precipitate hardening and precipitation purification from CoSi phase result in the better performance of the aged Co-containing alloy than the Co-free alloys. The success in Cu–Co–Si alloys opens a door to overcome the disadvantage of Si alloying in Cu-based alloys.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Chalon J, Guerin JD, Dubar L, Dubois A, Puchi-Cabrera ES (2016) Characterization of the hot-working behavior of a Cu-Ni-Si alloy. Mater Sci Eng A 667:77–86. https://doi.org/10.1016/j.msea.2016.04.06110.1016/j.msea.2016.04.061 ↗
2. Semboshi S, Sato S, Iwase A, Takasugi T (2016) Discontinuous precipitates in age-hardening Cu-Ni-Si alloys. Mater Charact 115:39–45. https://doi.org/10.1016/j.matchar.2016.03.01710.1016/j.matchar.2016.03.017 ↗
3. Choi JH (2012) Aging behavior and precipitate analysis of copper-rich Cu-Fe-Mn-P alloy. Mater Sci Eng A 550:183–190. https://doi.org/10.1016/j.msea.2012.04.05510.1016/j.msea.2012.04.055 ↗
4. Batra IS, Dey GK, Kulkarni UD, Banerjee S (2001) Microstructure and properties of a Cu-Cr-Zr alloy. J Nucl Mater 299(2):91–100. https://doi.org/10.1016/s0022-3115(01)00691-210.1016/s0022-3115(01)00691-2 ↗
5. Zinkle SJ (2016) Applicability of copper alloys for DEMO high heat flux components. Phys Scr. https://doi.org/10.1088/0031-8949/2015/t167/01400410.1088/0031-8949/2015/t167/014004 ↗
6. Guo X, Xiao Z, Qiu W, Li Z, Zhao Z, Wang X, Jiang Y (2019) Microstructure and properties of Cu-Cr-Nb alloy with high strength, high electrical conductivity and good softening resistance performance at elevated temperature. Mater Sci Eng A 749:281–290. https://doi.org/10.1016/j.msea.2019.02.03610.1016/j.msea.2019.02.036 ↗
7. Wang W, Kang H, Chen Z, Chen Z, Zou C, Li R, Yin G, Wang T (2016) Effects of Cr and Zr additions on microstructure and properties of Cu-Ni-Si alloys. Mater Sci Eng A 673:378–390. https://doi.org/10.1016/j.msea.2016.07.02110.1016/j.msea.2016.07.021 ↗
8. Li Y, Xiao Z, Li Z, Zhou Z, Yang Z, Lei Q (2017) Microstructure and properties of a novel Cu-Mg-Ca alloy with high strength and high electrical conductivity. J Alloys Compd 723:1162–1170. https://doi.org/10.1016/j.jallcom.2017.06.15510.1016/j.jallcom.2017.06.155 ↗
9. Lee E, Han S, Euh K, Lim S, Kim S (2011) Effect of Ti addition on tensile properties of Cu-Ni-Si alloys. Met Mater Int 17(4):569–576. https://doi.org/10.1007/s12540-011-0807-710.1007/s12540-011-0807-7 ↗
10. Jiang L, Fu H, Wang C, Li W, Xie J (2020) Enhanced mechanical and electrical properties of a Cu-Ni-Si alloy by thermo-mechanical processing. Metall Mater Trans A 51(1):331–341. https://doi.org/10.1007/s11661-019-05507-310.1007/s11661-019-05507-3 ↗
11. Hu T, Chen JH, Liu JZ, Liu ZR, Wu CL (2013) The crystallographic and morphological evolution of the strengthening precipitates in Cu-Ni-Si alloys. Acta Mater 61(4):1210–1219. https://doi.org/10.1016/j.actamat.2012.10.03110.1016/j.actamat.2012.10.031 ↗
12. Zhang K, Yang J, Li J, Chen X, Zhou H, Liu P (2021) Effect of deformation and aging treatment on the microstructure and properties of Cu-0.45Cr-0.14Ti (wt.%) alloy. J Alloys Compd. https://doi.org/10.1016/j.jallcom.2020.15677610.1016/j.jallcom.2020.156776 ↗
13. Krupinska B, Borek W, Krupinski M, Karkoszka T (2020) The influence of Ag on the microstructure and properties of Cu-Ni-Si alloys. Materials. https://doi.org/10.3390/ma1315341610.3390/ma13153416 ↗
14. Lei Q, Li Z, Dai C, Wang J, Chen X, Xie JM, Yang WW, Chen DL (2013) Effect of aluminum on microstructure and property of Cu-Ni-Si alloys. Mater Sci Eng A 572:65–74. https://doi.org/10.1016/j.msea.2013.02.02410.1016/j.msea.2013.02.024 ↗
15. Li Z, Xiao Z, Jiang Y, Lei Q, Xie J (2019) Composition design, phase transition and fabrication of copper alloys with high strength and electrical conductivity. Chin J Nonferr Met 29(9):2009–2049
16. Soldi L, Laplace A, Roskosz M, Gosse S (2019) Phase diagram and thermodynamic model for the Cu-Si and the Cu-Fe-Si systems. J Alloys Compd 803:61–70. https://doi.org/10.1016/j.jallcom.2019.06.23610.1016/j.jallcom.2019.06.236 ↗
17. Connetable D, Thomas O (2011) First-principles study of nickel-silicides ordered phases. J Alloys Compd 509(6):2639–2644. https://doi.org/10.1016/j.jallcom.2010.10.11810.1016/j.jallcom.2010.10.118 ↗
18. Cao Y, Han SZ, Choi E-A, Ahn JH, Mi X, Lee S, Shin H, Kim S, Lee J (2020) Effect of inclusion on strength and conductivity of Cu-Ni-Si alloys with discontinuous precipitation. J Alloys Compd. https://doi.org/10.1016/j.jallcom.2020.15600610.1016/j.jallcom.2020.156006 ↗
19. Cheng JY, Tang BB, Yu FX, Shen B (2014) Evaluation of nanoscaled precipitates in a Cu-Ni-Si-Cr alloy during aging. J Alloys Compd 614:189–195. https://doi.org/10.1016/j.jallcom.2014.06.08910.1016/j.jallcom.2014.06.089 ↗
20. Lei Q, Li Z, Wang MP, Zhang L, Gong S, Xiao Z, Pan ZY (2011) Phase transformations behavior in a Cu-8.0Ni-1.8Si alloy. J Alloys Compd 509(8):3617–3622. https://doi.org/10.1016/j.jallcom.2010.12.11510.1016/j.jallcom.2010.12.115 ↗
21. Wu Y, Li Y, Lu J, Tan S, Jiang F, Sun J (2019) Effects of pre-deformation on precipitation behaviors and properties in Cu-Ni-Si-Cr alloy. Mater Sci Eng A 742:501–507. https://doi.org/10.1016/j.msea.2018.11.04510.1016/j.msea.2018.11.045 ↗
22. Wang C, Zhu J, Lu Y, Guo Y, Liu X (2014) Thermodynamic description of the Cu-Ni-Si system. J Ph Equilibria Diffus 35(1):93–104. https://doi.org/10.1007/s11669-013-0277-310.1007/s11669-013-0277-3 ↗
23. Li J, Huang G, Mi X, Peng L, Xie H, Kang Y (2019) Influence of the Ni/Co mass ratio on the microstructure and properties of quaternary Cu-Ni-Co-Si alloys. Materials. https://doi.org/10.3390/ma1218285510.3390/ma12182855 ↗
24. Geng Y, Li X, Zhou H, Zhang Y, Jia Y, Tian B, Liu Y, Volinsky AA, Zhang X, Song K, Wang G, Li L, Hou J (2020) Effect of Ti addition on microstructure evolution and precipitation in Cu-Co-Si alloy during hot deformation. J Alloys Compd. https://doi.org/10.1016/j.jallcom.2019.15351810.1016/j.jallcom.2019.153518 ↗
25. Sun X, Jie J, Wang P, Qin B, Ma X, Wang T, Li T (2019) Effects of Co and Si additions and cryogenic rolling on structure and properties of Cu-Cr alloys. Mater Sci Eng A 740:165–173. https://doi.org/10.1016/j.msea.2018.10.09310.1016/j.msea.2018.10.093 ↗
26. Zhao Z, Zhang Y, Tian B, Jia Y, Liu Y, Song K, Volinsky AA (2019) Co effects on Cu-Ni-Si alloys microstructure and physical properties. J Alloys Compd 797:1327–1337. https://doi.org/10.1016/j.jallcom.2019.05.13510.1016/j.jallcom.2019.05.135 ↗
27. Chen Y, Dai A, Zhu Z (2016) Solution and aging treatment of Cu-Co-Si-Zr alloy. Spec Cast Nonferr Alloys 36(7):781–784
28. Toda T (1970) Critical cooling rates determined by Jominy tests in age-hardening Cu-Cr, Cu-Be and Cu-Co2Si alloys. Trans Jpn Inst Met 11(1):24–29. https://doi.org/10.2320/matertrans1960.11.2410.2320/matertrans1960.11.24 ↗
29. Lendvai J, Ungar T, Kovacs I, Albert B (1988) Precipitation processes in Cu-Co-Si alloys. J Mater Sci 23(11):4059–4065. https://doi.org/10.1007/bf0110683510.1007/bf01106835 ↗
30. Kubista J, Vrest’al J (2000) Thermodynamics of the liquid Co-Cu system and calculation of phase diagram. J Ph Equilib 21(2):125–129. https://doi.org/10.1361/10549710077034016510.1361/105497100770340165 ↗
31. Zhang L, Du Y, Xu H, Pan Z (2006) Experimental investigation and thermodynamic description of the Co-Si system. Calphad 30(4):470–481. https://doi.org/10.1016/j.calphad.2006.06.00110.1016/j.calphad.2006.06.001 ↗
32. Shin D, Saal JE, Liu Z-K (2008) Thermodynamic modeling of the Cu-Si system. Calphad 32(3):520–526. https://doi.org/10.1016/j.calphad.2008.05.00310.1016/j.calphad.2008.05.003 ↗
33. Yan XY, Chang YA (2000) A thermodynamic analysis of the Cu-Si system. J Alloys Compd 308:221–229. https://doi.org/10.1016/s0925-8388(00)00983-x10.1016/s0925-8388(00)00983-x ↗
34. Li M, Wang H, Guo Y, Wang H, Zheng D, Shan J, Chang Y (2020) Microstructures and mechanical properties of the novel Cu-Cr-Zr-Fe-Ti-Y alloy for fusion reactor. J Nucl Mater. https://doi.org/10.1016/j.jnucmat.2020.15206310.1016/j.jnucmat.2020.152063 ↗