Wear behavior and microhardness studies of tantalum (Ta)-coated 316L stainless steel by DC magnetron sputtering for the orthopedic applications
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Geringer J, Tatkiewicz W, Rouchouse G (2011) Wear behavior of PAEK, poly(aryl-ether-ketone), under physiological conditions, outlooks for performing these materials in the field of hip prosthesis. Wear 271(11–12):2793–2803. https://doi.org/10.1016/j.wear.2011.05.03410.1016/j.wear.2011.05.034 ↗
2. Dincel Ö, Şimşek İ, Özyürek D (2021) Investigation of the wear behavior in simulated body fluid of 316L stainless steels produced by mechanical alloying method. Eng Sci Technol Int J 24(1):35–40. https://doi.org/10.1016/j.jestch.2020.12.00110.1016/j.jestch.2020.12.001 ↗
3. Navarro CH, Martínez MF, Carvajal EEC, Reséndiz LPR, Bustos EDG (2021) Analysis of the wear behavior of multilayer coatings of TaZrN/TaZr produced by magnetron sputtering on AISI-316L stainless steel. Int J Adv Manuf Technol 117(5–6):1565–1573. https://doi.org/10.1007/s00170-021-07655-610.1007/s00170-021-07655-6 ↗
4. Jourani A, Bouvier S (2015) Friction and wear mechanisms of 316L stainless steel in dry sliding contact: effect of abrasive particle size. Tribol Trans 58(1):131–139. https://doi.org/10.1080/10402004.2014.95522910.1080/10402004.2014.955229 ↗
5. Li HF, Huang JY, Lin GC, Wang PY (2021) Recent advances in tribological and wear properties of biomedical metallic materials. Rare Met 40(11):3091–3106. https://doi.org/10.1007/s12598-021-01796-z10.1007/s12598-021-01796-z ↗
6. Uwais ZA, Hussein MA, Samad MA, Al-Aqeeli N (2017) Surface modification of metallic biomaterials for better tribological properties: a review. Arab J Sci Eng 42(11):4493–4512. https://doi.org/10.1007/s13369-017-2624-x10.1007/s13369-017-2624-x ↗
7. Jaiswal D, Singh V, Pathote D, Behera CK (2021) Electrochemical behaviour of lead-free Sn–0.7Cu–xIn solders alloys in 3.5 wt% NaCl solution. J Mater Sci Mater Electron 32(18):23371–23384. https://doi.org/10.1007/s10854-021-06824-310.1007/s10854-021-06824-3 ↗
8. Pathote D, Jaiswal D, Singh V, Behera CK (2022) Optimization of electrochemical corrosion behavior of 316L stainless steel as an effective biomaterial for orthopedic applications. Mater Today Proc 57:265–269. https://doi.org/10.1016/J.MATPR.2022.02.50110.1016/J.MATPR.2022.02.501 ↗
9. Weeden SH, Schmidt RH (2007) The use of tantalum porous metal implants for Paprosky 3A and 3B defects. J Arthroplasty 22(6 SUPPL.):151–155. https://doi.org/10.1016/j.arth.2007.04.02410.1016/j.arth.2007.04.024 ↗
10. Rosen C (2011) Principles and practices. 52(204). doi:https://doi.org/10.46692/9781447343264.00410.46692/9781447343264.004 ↗
11. Benz K et al (2012) Rheological and biological properties of a hydrogel support for cells intended for intervertebral disc repair. BMC Musculoskelet Disord 13:1–13. https://doi.org/10.1186/1471-2474-13-5410.1186/1471-2474-13-54 ↗
12. Bonitatibus PJ, Torres AS, Goddard GD, Fitzgerald PF, Kulkarni AM (2010) Synthesis, characterization, and computed tomography imaging of a tantalum oxide nanoparticle imaging agent. Chem Commun 46(47):8956–8958. https://doi.org/10.1039/c0cc03302b10.1039/c0cc03302b ↗
13. Janowski M, Bulte JWM, Walczak P (2012) Personalized nanomedicine advancements for stem cell tracking. Adv Drug Deliv Rev 64(13):1488–1507. https://doi.org/10.1016/j.addr.2012.07.00810.1016/j.addr.2012.07.008 ↗
14. Kumar S, Jaiswal D, Behera CK, Mahobia GS (2022) Potentiodyanmic corrosion behavior of Fe–18Cr–21Mn-0. 65 N austenitic stainless steel exposed at 400–700 °C. Mater Chem Phys, 290(May): 126568. doi:https://doi.org/10.1016/j.matchemphys.2022.12656810.1016/j.matchemphys.2022.126568 ↗
15. Frigg A, Dougall H, Boyd S, Nigg B (2010) Can porous tantalum be used to achieve ankle and subtalar arthrodesis?: A pilot study. Clin Orthop Relat Res 468(1):209–216. https://doi.org/10.1007/s11999-009-0948-x10.1007/s11999-009-0948-x ↗
16. Ma J, Sun W, Gao F, Guo W, Wang Y, Li Z (2016) Porous tantalum implant in treating osteonecrosis of the femoral head: still a viable option? Sci Rep 6:1–10. https://doi.org/10.1038/srep2822710.1038/srep28227 ↗
17. Singh V, Jaiswal D, Pathote D, Behera CK (2022) Drop calorimetric measurement of In-Zn system for Lead-Free solder applications. Mater Today Proc 57:285–288. https://doi.org/10.1016/j.matpr.2022.02.60110.1016/j.matpr.2022.02.601 ↗
18. Jaiswal D, Pathote D, Singh V, Behera CK (2022) Electrochemical behaviour of lead-free Sn–In–Al solders alloys in 3.5 wt.% NaCl solution. Mater Today Proc. doi:https://doi.org/10.1016/j.matpr.2022.02.31510.1016/j.matpr.2022.02.315 ↗
19. Zhang Y, Ahn PB, Fitzpatrick DC, Heiner AD, Poggie RA, Brown TD (1999) Interfacial frictional behavior: cancellous bone, cortical bone, and a novel porous tantalum biomaterial. J Musculoskelet Res 3(4):245–251. https://doi.org/10.1142/S021895779900026910.1142/S0218957799000269 ↗
20. Shirazi-Adl A, Dammak M, Paiement G (1993) Experimental determination of friction characteristics at the trabecular bone/porous-coated metal interface in cementless implants. J Biomed Mater Res 27(2):167–175. https://doi.org/10.1002/jbm.82027020510.1002/jbm.820270205 ↗
21. Sagomonyants KB, Hakim-Zargar M, Jhaveri A, Aronow MS, Gronowicz G (2011) Porous tantalum stimulates the proliferation and osteogenesis of osteoblasts from elderly female patients. J Orthop Res 29(4):609–616. https://doi.org/10.1002/jor.2125110.1002/jor.21251 ↗
22. White CJ, Ramee SR, Banks AK, Mesa JE, Chokshi S, Isner JM (1992) A new balloon-expandable tantalum coil stent: angiographic patency and histologic findings in an atherogenic swine model. J Am Coll Cardiol 19(4):870–876. https://doi.org/10.1016/0735-1097(92)90534-T10.1016/0735-1097(92)90534-T ↗
23. Jaiswal D, Pathote D, Singh V, Behera CK (2022) Effect of Al addition on electrochemical behavior of Sn-0.7Cu-xAl lead-free solders alloys in 3.5 wt.% NaCl solution. J Mater Eng Perform. doi:https://doi.org/10.1007/s11665-022-06771-y10.1007/s11665-022-06771-y ↗
24. dos Santos GA (2017) The importance of metallic materials as biomaterials. Adv Tissue Eng Regen Med Open Access 3(1):300–302. https://doi.org/10.15406/atroa.2017.03.0005410.15406/atroa.2017.03.00054 ↗
25. Rai VK, Kumar MR, Singh V, Jaiswal D, Behera CK (2019) Analysis of corrosion behavior and its characterization of In–Sn–Bi alloy. Mater Today Proc 18:2322–2328. https://doi.org/10.1016/j.matpr.2019.07.01510.1016/j.matpr.2019.07.015 ↗
26. Kumar MR, Singh V, Rai VK, Jaiswal D, Behera CK (2019) Investigation on mixing heat effect of Bi–In and In–Sn system at 730 K. Mater Today Proc 18:2917–2923. https://doi.org/10.1016/j.matpr.2019.07.16110.1016/j.matpr.2019.07.161 ↗
27. Rai PK et al (2017) Wear behavior of harmonic structured 304L stainless steel. J Mater Eng Perform 26(6):2608–2618. https://doi.org/10.1007/s11665-017-2719-210.1007/s11665-017-2719-2 ↗
28. Raposo M, Ferreira Q, Ribeiro PA (2007) A guide for atomic force microscopy analysis of soft-condensed matter. Mod Res Educ Top Microsc, pp 758–769. doi:https://doi.org/10.1002/sia.229410.1002/sia.2294 ↗
29. Wang R et al (2019) Using atomic force microscopy to measure thickness of passive film on stainless steel immersed in aqueous solution. Sci Rep 9(1):1–11. https://doi.org/10.1038/s41598-019-49747-010.1038/s41598-019-49747-0 ↗
30. Geringer J, Pellier J, Cleymand F, Forest B (2012) Atomic force microscopy investigations on pits and debris related to fretting-corrosion between 316L SS and PMMA. Wear 292–293:207–217. https://doi.org/10.1016/j.wear.2012.05.00810.1016/j.wear.2012.05.008 ↗
31. Wang XY, Wu YS, Zhang L, Yu ZY (2001) Atomic force microscopy and x-ray photoelectron spectroscopy study on the passive film for type 316L stainless steel. Corrosion 57(6):540–546. https://doi.org/10.5006/1.329038010.5006/1.3290380 ↗
32. Li X, Wang X, Bondokov R, Morris J, An YH, Sudarshan TS (2005) Micro/nanoscale mechanical and tribological characterization of SiC for orthopedic applications. J Biomed Mater Res Part B Appl Biomater 72(2):353–361. https://doi.org/10.1002/jbm.b.3016810.1002/jbm.b.30168 ↗
33. Attabi S, Himour A, Laouar L, Motallebzadeh A (2021) Mechanical and wear behaviors of 316L stainless steel after ball burnishing treatment. J Mater Res Technol 15:3255–3267. https://doi.org/10.1016/j.jmrt.2021.09.08110.1016/j.jmrt.2021.09.081 ↗
34. Gao X-W, Davies T, Beskos D (2003) Boundary element programming in mechanics. Appl Mech Rev 56(1):B1–B1. https://doi.org/10.1115/1.152335010.1115/1.1523350 ↗
35. Eliaz N (2019) Corrosion of metallic biomaterials: a review. Materials (Basel), 12(3). doi:https://doi.org/10.3390/ma1203040710.3390/ma12030407 ↗
36. Jenczyk P, Gawrońska M, Dera W, Chrzanowska-Giżyńska J, Denis P, Jarząbek DM (2019) Application of SiC particles coated with a protective Ni layer for production of Ni/SiC co-electrodeposited composite coatings with enhanced tribological properties. Ceram Int 45(17):23540–23547. https://doi.org/10.1016/j.ceramint.2019.08.06310.1016/j.ceramint.2019.08.063 ↗
37. Liu LL, Xu J, Lu X, Munroe P, Xie ZH (2016) Electrochemical corrosion behavior of nanocrystalline β-Ta coating for biomedical applications. ACS Biomater Sci Eng 2(4):579–594. https://doi.org/10.1021/acsbiomaterials.5b0055210.1021/acsbiomaterials.5b00552 ↗
38. Gao J, et al (2022) Wear, corrosion, and biocompatibility of 316L stainless steel modified by well-adhered Ta coatings. J Mater Eng Perform, no. Ref 15. doi:https://doi.org/10.1007/s11665-022-06928-910.1007/s11665-022-06928-9 ↗
39. Sikdar K, Shekhar S, Balani K (2014) Fretting wear of Mg–Li–Al based alloys. Wear 318(1–2):177–187. https://doi.org/10.1016/j.wear.2014.06.01210.1016/j.wear.2014.06.012 ↗
40. Fellah M, Labaïz M, Assala O, Lost A, Dekhil L (2013) Tribological behaviour of AISI 316L stainless steel for biomedical applications. Tribol - Mater Surfaces Interfaces 7(3):135–149. https://doi.org/10.1179/1751584X13Y.000000003210.1179/1751584X13Y.0000000032 ↗
41. García-León RA, Martínez-Trinidad J, Campos-Silva I, Figueroa-López U, Guevara-Morales A (2021) Wear maps of borided AISI 316L steel under ball-on-flat dry sliding conditions. Mater Lett 282:17–18. https://doi.org/10.1016/j.matlet.2020.12884210.1016/j.matlet.2020.128842 ↗
42. Cohen J (1967) Biomaterials in orthopedic surgery. Am J Surg 114(1):31–41. https://doi.org/10.1016/0002-9610(67)90037-210.1016/0002-9610(67)90037-2 ↗
43. Du S et al (2018) Optimizing the tribological behavior of tantalum carbide coating for the bearing in total hip joint replacement. Vacuum 150:222–231. https://doi.org/10.1016/j.vacuum.2018.01.05010.1016/j.vacuum.2018.01.050 ↗
44. Zhang TF et al (2015) Wear and corrosion properties of diamond like carbon (DLC) coating on stainless steel, CoCrMo and Ti6Al4V substrates. Surf Coatings Technol 273(1):12–19. https://doi.org/10.1016/j.surfcoat.2015.03.03110.1016/j.surfcoat.2015.03.031 ↗