Effect of Cr:Fe ratio on the mechanical properties of (Cr,Fe)7C3 ternary carbides in abrasion-resistant white cast irons
Source abstract
Abstract
Abstract (Cr,Fe)7C3 ternary carbides constitute the majority of eutectic carbides in abrasion-resistant white cast irons. Density functional theory models have predicted these carbides to have a combination of metallic, covalent and ionic bonding, in proportions depending on the carbide’s Cr:Fe ratio. However, experimental research to validate these predictions has been lacking. This study investigates the characteristics of the carbides as a function of Cr:Fe ratio, which was manipulated from Fe-rich to Cr-rich by varying the Cr:C ratio of the bulk alloy. The carbides’ crystalline structure, hardness, Young’s modulus, fracture toughness and abrasion performance have been assessed through techniques including nano-indentation, HR-TEM and the inner circumference abrasion test (ICAT). Fe-rich M3C formed at very low bulk Cr:C ratio was found to have an orthorhombic crystal structure. In all other alloys, with Cr:C ratios above 2.7, M7C3 was formed and found to have a hexagonal structure. Hardness, Young’s modulus and calculated fracture toughness of M7C3 all increase with Cr:Fe ratio, from (Fe5,Cr2)C3 up to a maximum for (Cr4,Fe3)C3 (in 18Cr–6.8Cr:C WCI). This gave the highest hardness (22.9 GPa) and Young’s modulus (315 GPa), but also the highest fracture toughness (4.5 MPa.m0.5). The peak fracture toughness at carbide composition of (Cr4,Fe3)C3 in this study is consistent with the prediction of DFT models in the literature; while the peak hardness at the same carbide composition shows a marginal deviation from the predictions. Abrasion performance generally increased with carbide hardness and fracture toughness, with one exception: (Cr4.3,Fe2.7)C3. Although (Cr4.3,Fe2.7)C3 showed marginally lower inherent fracture toughness than (Cr4.0,Fe3.0)C3, the higher Cr:Fe carbides imparted the highest abrasion performance, associated with modified eutectic morphology.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Laird G, Gundlach R, Röhrig K (2000) Abrasion-resistant cast iron handbook. American Foundry Society, Illinois
2. Laird G (1991) Microstructures of nickel-hard I nickel-hard IV and high-chromium white cast irons. Ninety-Fifth Annual Meeting American Foundrymen’s Society, Columbus
3. Kootsookos A, Gates JD (2004) The effect of the reduction of carbon content on the toughness of high chromium white irons in the as-cast state. J Mater Sci 39(1):73–84. https://doi.org/10.1023/B:JMSC.0000007730.00517.6510.1023/B:JMSC.0000007730.00517.65 ↗
4. Heino V, Kallio M, Valtonen K, Kuokkala VT (2017) The role of microstructure in high stress abrasion of white cast irons. Wear 388:119–125. https://doi.org/10.1016/j.wear.2017.04.02910.1016/j.wear.2017.04.029 ↗
5. Kang M, Suh Y, Oh YJ, Lee YK (2014) The effects of vanadium on the microstructure and wear resistance of centrifugally cast Ni-hard rolls. J Alloys Compd 609:25–32. https://doi.org/10.1016/j.jallcom.2014.04.18410.1016/j.jallcom.2014.04.184 ↗
6. Kootsookos A, Gates JD (2008) The role of secondary carbide precipitation on the fracture toughness of a reduced carbon white iron. Mater Sci Eng A 490(1–2):313–318. https://doi.org/10.1016/j.msea.2008.01.03610.1016/j.msea.2008.01.036 ↗
7. Laird G, Nielsen R, Macmillan N (1991) On the nature of eutectic carbides in Cr–Ni white cast irons. Metall Trans A 22(8):1709–1719. https://doi.org/10.1007/BF0264649410.1007/BF02646494 ↗
8. Röhrig K (1996) Ni-hard material data and applications. Nickel Development Institute, Columbus
9. Jokari-Sheshdeh M, Ali Y, Gallo SC, Lin W, Gates JD (2022) Comparing the abrasion performance of NiHard-4 and high-Cr–Mo white cast irons: The effects of chemical composition and microstructure. Wear 492–493:204208–204208–11. https://doi.org/10.1016/j.wear.2021.20420810.1016/j.wear.2021.204208 ↗
10. Jokari-Sheshdeh M, Ali Y, Le Nué C et al (2022) Evaluation of silicon effects on abrasion performance, microstructure and crystalline structure of NiHard-4 white cast iron using synchrotron X-ray diffraction. Mater 21:101332–101332–11. https://doi.org/10.1016/j.mtla.2022.10133210.1016/j.mtla.2022.101332 ↗
11. Yilmaz SO (2007) Wear behavior of TiB2 inoculated 20Cr–3Mo–4C high chromium white cast irons. J Mater Sci 42(16):6769–6778. https://doi.org/10.1007/s10853-006-1430-810.1007/s10853-006-1430-8 ↗
12. Coronado JJ (2011) Effect of (Fe,Cr)7C3 carbide orientation on abrasion wear resistance and fracture toughness. Wear 270(3–4):287–293. https://doi.org/10.1016/j.wear.2010.10.07010.1016/j.wear.2010.10.070 ↗
13. Casellas D, Caro J, Molas S, Prado JM, Valls I (2007) Fracture toughness of carbides in tool steels evaluated by nanoindentation. Acta Mater 55(13):4277–4286. https://doi.org/10.1016/j.actamat.2007.03.02810.1016/j.actamat.2007.03.028 ↗
14. Zum Gahr KH (1980) Fracture analysis of white cast iron. IJMR 71(2):103–109. https://doi.org/10.1515/ijmr-1980-71020810.1515/ijmr-1980-710208 ↗
15. Franco SD, Sinatora A (1994) Determinacão da tenacidade à fratura de carbonetos M7C3 usando o método da indentac ão, in: XI Congresso Brasileiro de Engenharia e Ciência dos Materiais, Águas de São Pedro, pp 247–250. https://repositorio.usp.br/item/000876946. Accessed 06 Jan. 2023
16. Berns H (1995) Microstructural properties of wear-resistant alloys. Wear 181:271–279. https://doi.org/10.1016/0043-1648(95)90034-910.1016/0043-1648(95)90034-9 ↗
17. Laugier M (1987) New formula for indentation toughness in ceramics. J Mater Sci Lett 6(3):355–356. https://doi.org/10.1007/BF0172935210.1007/BF01729352 ↗
18. Pei Y, Song R, Zhang Y et al (2020) The relationship between fracture mechanism and substructures of primary M7C3 under the hot compression process of self-healing hypereutectic high chromium cast iron. Mater Sci Eng A 779:139150–139150–8. https://doi.org/10.1016/j.msea.2020.13915010.1016/j.msea.2020.139150 ↗
19. Wang J, Guo W, Sun H, Li H, Gou H, Zhang J (2016) Plastic deformation behaviors and hardening mechanism of M7C3 carbide. Mater Sci Eng A 662:88–94. https://doi.org/10.1016/j.msea.2016.03.06210.1016/j.msea.2016.03.062 ↗
20. Li Y, Wang X, Yuan G, Han P, Zhu X (2021) Hot compression deformation and microstructure evolution of high chromium cast iron based on canning compression. J Mater Sci 56(30):17296–17305. https://doi.org/10.1007/s10853-021-06379-y10.1007/s10853-021-06379-y ↗
21. Kagawa A, Kawashima S, Ohta Y (1992) Wear properties of (Fe, Cr)7C3 carbide bulk alloys. Mater Trans JIM 33(12):1171–1177. https://doi.org/10.2320/matertrans1989.33.117110.2320/matertrans1989.33.1171 ↗
22. Xie JY, Chen NX, Shen J, Teng L, Seetharaman S (2005) Atomistic study on the structure and thermodynamic properties of Cr7C3, Mn7C3, Fe7C3. Acta Mater 53(9):2727–2732. https://doi.org/10.1016/j.actamat.2005.02.03910.1016/j.actamat.2005.02.039 ↗
23. Konyaeva M, Medvedeva N (2009) Electronic structure, magnetic properties, and stability of the binary and ternary carbides (Fe, Cr)3C and (Fe, Cr)7C3. Phys Solid State 51(10):2084–2089. https://doi.org/10.1134/S106378340910015110.1134/S1063783409100151 ↗
24. Xiao B, Feng J, Zhou C, Jiang Y, Zhou R (2011) Mechanical properties and chemical bonding characteristics of Cr7C3 type multicomponent carbides. J Appl Phys 109(2):023507–023507-9. https://doi.org/10.1063/1.353203810.1063/1.3532038 ↗
25. Shi Z, Shao W, Rao L et al (2021) Effects of Y dopant on mechanical properties and electronic structures of M7C3 carbide in Fe-Cr–C hardfacing coating. Appl Surf Sci 538:148108–148108-10. https://doi.org/10.1016/j.apsusc.2020.14810810.1016/j.apsusc.2020.148108 ↗
26. Chong X, Hu M, Wu P, Shan Q, Jiang YH, Feng J (2019) Tailoring the anisotropic mechanical properties of hexagonal M7X3 (M= Fe, Cr, W, Mo; X= C, B) by multialloying. Acta Mater 169:193–208. https://doi.org/10.1016/j.actamat.2019.03.01510.1016/j.actamat.2019.03.015 ↗
27. Music D, Kreissig U, Mertens R, Schneider J (2004) Electronic structure and mechanical properties of Cr7C3. Phys Lett A 326(5–6):473–476. https://doi.org/10.1016/j.physleta.2004.04.06810.1016/j.physleta.2004.04.068 ↗
28. Li Y, Gao Y, Xiao B et al (2011) The electronic, mechanical properties and theoretical hardness of chromium carbides by first-principles calculations. J Alloys Compd 509(17):5242–5249. https://doi.org/10.1016/j.jallcom.2011.02.00910.1016/j.jallcom.2011.02.009 ↗
29. Zhang P, Zhou Y, Yang J et al (2013) Optimization on mechanical properties of Fe7−xCrxC3 carbides by first-principles investigation. J Alloys Compd 560:49–53. https://doi.org/10.1016/j.jallcom.2013.01.10310.1016/j.jallcom.2013.01.103 ↗
30. Sobolev A, Mirzoev A (2019) Structure and stability of (Cr, Fe)7C3 ternary carbides in solid and liquid state. J Alloys Compd 804:566–572. https://doi.org/10.1016/j.jallcom.2019.06.28210.1016/j.jallcom.2019.06.282 ↗
31. Maratray F, Usseglio-Nanot R (1970) Factors affecting the structure of chromium and chromium-molybdenum white irons. https://www.osti.gov/biblio/4743555. Accessed 07 Jan. 2023
32. Oliver WC, Pharr GM (1992) An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J Mater Res 7(6):1564–1583. https://doi.org/10.1557/JMR.1992.156410.1557/JMR.1992.1564 ↗
33. Gautham S, Sasmal S (2019) Determination of fracture toughness of nano-scale cement composites using simulated nanoindentation technique. Theor Appl Fract Mech 103:102275–102275-13. https://doi.org/10.1016/j.tafmec.2019.10227510.1016/j.tafmec.2019.102275 ↗
34. Cheng YT, Li Z, Cheng CM (2002) Scaling relationships for indentation measurements. Philos Mag 82(10):1821–1829. https://doi.org/10.1080/0141861020823569310.1080/01418610208235693 ↗
35. Cai X, Xu Y, Zhong L, Liu M (2017) Fracture toughness of WC-Fe cermet in W-WC-Fe composite by nanoindentation. J Alloys Compd 728:788–796. https://doi.org/10.1016/j.jallcom.2017.09.07010.1016/j.jallcom.2017.09.070 ↗
36. Doğan Ö, Hawk J, Laird G (1997) Solidification structure and abrasion resistance of high chromium white irons. Met Mater Trans A 28(6):1315–1328. https://doi.org/10.1007/s11661-997-0267-310.1007/s11661-997-0267-3 ↗
37. Çöl M, Koç FG, Öktem H, Kır D (2016) The role of boron content in high alloy white cast iron (Ni-Hard 4) on microstructure, mechanical properties and wear resistance. Wear 348:158–165. https://doi.org/10.1016/j.wear.2015.12.00710.1016/j.wear.2015.12.007 ↗
38. Thorpe WR, Chicco B (1981) On the formation of duplex eutectic carbides in commercially important white irons. Mater Sci Eng 51(2):P11–P19. https://doi.org/10.1016/0025-5416(81)90210-X10.1016/0025-5416(81)90210-X ↗
39. Scandian C, Boher C, De Mello J, Rezai-Aria F (2009) Effect of molybdenum and chromium contents in sliding wear of high-chromium white cast iron: the relationship between microstructure and wear. Wear 267(1–4):401–408. https://doi.org/10.1016/j.wear.2008.12.09510.1016/j.wear.2008.12.095 ↗
40. Al-Rubaie KS, Pohl M (2014) Heat treatment and two-body abrasion of Ni-hard 4. Wear 312(1–2):21–28. https://doi.org/10.1016/j.wear.2014.01.01310.1016/j.wear.2014.01.013 ↗
41. Pintaude G, Bernardes F, Santos M, Sinatora A, Albertin E (2009) Mild and severe wear of steels and cast irons in sliding abrasion. Wear 267(1–4):19–25. https://doi.org/10.1016/j.wear.2008.12.09910.1016/j.wear.2008.12.099 ↗
42. Coronado JJ (2011) Effect of load and carbide orientation on abrasive wear resistance of white cast iron. Wear 270(11–12):823–827. https://doi.org/10.1016/j.wear.2011.02.00910.1016/j.wear.2011.02.009 ↗
43. Jiang C (2008) First-principles study of structural, elastic, and electronic properties of chromium carbides. Appl Phys Lett 92(4):041909. https://doi.org/10.1063/1.283834510.1063/1.2838345 ↗
44. Xiao B, Xing J, Feng J et al (2008) Theoretical study on the stability and mechanical property of Cr7C3. Phys B Condens Matter 403(13–16):2273–2281. https://doi.org/10.1016/j.physb.2007.12.01210.1016/j.physb.2007.12.012 ↗
45. Gates JD, Gore G (1995) Wear of metals: philosophies and practicalities. Mater Forum Inst Met Mater Aust 124:3052
46. Liu S, Wang Z, Shi Z, Zhou Y, Yang Q (2017) Experiments and calculations on refining mechanism of NbC on primary M7C3 carbide in hypereutectic Fe-Cr–C alloy. J Alloys Compd 713:108–118. https://doi.org/10.1016/j.jallcom.2017.04.16710.1016/j.jallcom.2017.04.167 ↗
47. Liu S, Zhou Y, Xing X, Wang J, Yang Q (2017) Refining effect of TiC on primary M7C3 in hypereutectic FeCrC harden-surface welding coating: experimental research and first-principles calculation. J Alloys Compd 691:239–249. https://doi.org/10.1016/j.jallcom.2016.08.13310.1016/j.jallcom.2016.08.133 ↗
48. Zhi X, Liu J, Xing J, Ma S (2014) Effect of cerium modification on microstructure and properties of hypereutectic high chromium cast iron. Mater Sci Eng A 603:98–103. https://doi.org/10.1016/j.msea.2014.02.08010.1016/j.msea.2014.02.080 ↗
49. Gates JD, Gore G, Hermand MP, Guerineau MP, Martin P, Saad J (2007) The meaning of high stress abrasion and its application in white cast irons. Wear 263(1–6):6–35. https://doi.org/10.1016/j.wear.2006.12.03310.1016/j.wear.2006.12.033 ↗
50. Ali Y, Garcia-Mendoza C, Gates JD (2019) Effects of ‘impact’and abrasive particle size on the performance of white cast irons relative to low-alloy steels in laboratory ball mills. Wear 426:83–100. https://doi.org/10.1016/j.wear.2019.01.04810.1016/j.wear.2019.01.048 ↗