Studies of calcium-precipitating oral bacterial adhesion on TiN, TiO2 single layer, and TiN/TiO2 multilayer-coated 316L SS
Source abstract
Abstract
Titanium nitride (TiN), titanium oxide (TiO2) single layer, and TiN/TiO2 multilayer coatings were deposited on a 316L stainless steel substrate using reactive magnetron sputtering process with the aim of preventing bacterial adhesion. The crystal structures of as-prepared coatings were evaluated using X-ray diffraction analysis. The cubic structure of TiN, anatase, and rutile structure of TiO2 was noticed. Atomic force microscopy images exhibited a relatively smooth surface for all coatings. The surface wettability studies confirmed that the coatings were hydrophilic in nature. The rate of bacterial adhesion was evaluated using scanning electron microscopy and epifluorescence microscopy. These results demonstrated that the coated substrates could help to effectively reduce the bacterial adhesion and biofilm formations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Dental materials and restorations · Advanced Photocatalysis Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Scarano A, Piattelli M, Vrespa G, Caputi S, Piattelli A (2003) Bacterial adhesion on titanium nitride-coated and uncoated implants: an in vivo human study. J Oral Implantol 29(2):80–8510.1563/1548-1336(2003)029<0080:BAOTNA>2.3.CO;2 ↗
2. Pablos C, van Grieken R, Marugan J, Chowdhury I, Walker SL (2013) Study of bacterial adhesion onto immobilized TiO2: effect on the photocatalytic activity for disinfection applications. Catal Today 209:140–14610.1016/j.cattod.2012.12.010 ↗
3. Ramadoss A, Kim SJ (2013) Nanostructured TiO2/TiN multilayer coatings on AISI 316L stainless steel for biomedical applications. Sci Adv Mater 5:1168–117810.1166/sam.2013.1569 ↗
4. So S, Harris IA, Naylor JM, Adie S, Mittal R (2011) Correlation between metal allergy and treatment outcomes after ankle fracture fixation. J Orthop Surg 19:309–31310.1177/230949901101900309 ↗
5. Garg N, Rajpurohit N, Webel R (2011) AngioSeal device malfunction: a case report of dilator tip fracture and successful endovascular retrieval. EJVES Extra 22:49–5110.1016/j.ejvsextra.2011.06.010 ↗
6. Cahill TJ, Choji K, Kardos A (2014) Fluoroscopy-guided snare retrieval of the celt ACD metallic vascular closure device following failed deployment. Cathet Cardiovasc Interv 83:556–55910.1002/ccd.25229 ↗
7. Khan SN, Rapacchi S, Levi DS, Finn JP (2013) Pediatric cardiovascular interventional devices: effect on CMR images at 1.5 and 3 Tesla. J Cardiovasc Magn Reson 15:2–1410.1186/1532-429X-15-2 ↗
8. Kajander EO, Ciftcioglu N (1998) Nanobacteria: an alternative mechanism for pathogenic intra- and extra-cellular calcification and stone formation. Proc Natl Acad Sci USA 95:8274–827910.1073/pnas.95.14.8274 ↗
9. Knoll AH, Swett K (1990) Carbonate deposition during the late Proterozoic Era: an example from Spitzbergen. Am J Sci 290A:104–132
10. Hubler R, Cozza A, Marcondes TL, Souza RB, Fiori FFL (2001) Wear and corrosion protection of 316-L femoral implants by deposition of thin films. Surf Coat Technol 142:1078–108310.1016/S0257-8972(01)01321-4 ↗
11. Rosu RA, Serban VA, Bucur AI, Dragos U (2012) Deposition of titanium nitride and hydroxyapatite-based biocompatible composite by reactive plasma spraying. Appl Surf Sci 258:3871–387610.1016/j.apsusc.2011.12.049 ↗
12. Arshi N, Lu J, Joo YK, Lee CG, Yoon JH, Ahmed F (2012) Study on structural, morphological and electrical properties of sputtered titanium nitride films under different argon gas flow. Appl Surf Sci 134:839–844
13. Groessner-Schreiber B, Neubert A, Muller WD, Hopp M, Griepentrog M, Lange KP (2003) Fibroblast growth on surface-modified dental implants: an in vitro study. J Biomed Mater Res A 15(64A):591–59910.1002/jbm.a.10417 ↗
14. Zhang S (1993) TiN coating of tool steels: a review. J Mater Process Technol 39:165–17710.1016/0924-0136(93)90016-Y ↗
15. Zega B, Kornmann M, Amiguet J (1977) Hard decorative TiN coatings by ion plating. Thin Solid Films 45:577–58210.1016/0040-6090(77)90249-8 ↗
16. Al Jabbari YS, Fehrman J, Barnes AC, Zapf AM, Zinelis S, Berzins DW (2012) Titanium nitride and nitrogen ion implanted coated dental materials. Coatings 2:160–17810.3390/coatings2030160 ↗
17. Ananthakumar R, Subramanian B, Yugeswaran S, Jayachandran M (2012) Effect of substrate temperature on structural, morphological and optical properties of crystalline titanium dioxide films prepared by DC reactive magnetron sputtering. J Mater Sci Mater Electron 23:1898–190410.1007/s10854-012-0681-1 ↗
18. Andersson M, Sterlund LO, Ljungstrom S, Palmqvist A (2002) Preparation of nanosize anatase and rutile TiO2 by hydrothermal treatment of microemulsions and their activity for photocatalytic wet oxidation of phenol. J Phys Chem B 106:10674–1067910.1021/jp025715y ↗
19. Benk G, Myllyperki P, Pan J, Yartsev AP, Sundstrom V (2003) Photoinduced electron injection from Ru(dcbpy)2(NCS)2 to SnO2 and TiO2 nanocrystalline films. J Am Chem Soc 125:1118–111910.1021/ja029025j ↗
20. Sonmezoglu S, Arslan A, Seri T, Serin N (2011) The effects of film thickness on the optical properties of TiO2–SnO2 compound thin films. Phys Scr 84:065602–06560710.1088/0031-8949/84/06/065602 ↗
21. Krishna DSR, Sun Y, Chen Z (2011) Magnetron sputtered TiO2 films on a stainless steel substrate: selective rutile phase formation and its tribological and anti-corrosion performance. Thin Solid Films 519:4860–486410.1016/j.tsf.2011.01.042 ↗
22. Huang N, Yang P, Leng YX, Chen JY, Sun H, Wang J, Wang GJ, Ding PD, Xi TF, Leng Y (2003) Hemocompatibility of titanium oxide films. Biomaterials 24:2177–218710.1016/S0142-9612(03)00046-2 ↗
23. Chenglong L, Dazhi Y, Guoqiang L, Min Q (2005) Corrosion resistance and hemocompatibility of multilayered Ti/TiN-coated surgical AISI 316L stainless steel. Mater Lett 59:3813–381910.1016/j.matlet.2005.06.058 ↗
24. Leng YX, Chu PK (2002) Structure and properties of biomedical TiO2 films synthesized by dual plasma deposition. Surf Coat Technol 156:295–30010.1016/S0257-8972(02)00092-0 ↗
25. Leng YX, Chen JY, Yang P, Wang J, Zhao AS, Wan GJ, Sun H, Huang N (2006) The microstructure and mechanical properties of TiN and TiO2/TiN duplex films synthesized by plasma immersion ion implantation and deposition on artificial heart valve. Surf Coat Technol 201:1012–101610.1016/j.surfcoat.2006.01.024 ↗
26. Hultman L, Engstrom C, Oden M (2000) Mechanical and thermal stability of TiN/NbN superlattice thin films. Surf Coat Technol 133–134:227–23310.1016/S0257-8972(00)00935-X ↗
27. An J, Zhang QY (2007) Structure, hardness and tribological properties of nanolayered TiN/TaN multilayer coatings. Mater Charact 58:439–44610.1016/j.matchar.2006.06.012 ↗
28. Apse P, Ellen RP, Overall CM, Zarb GA (1989) Microbiota and crevicular fluid collagenase activity in the osseointegrated dental implant sulcus: a comparison of sites in edentulous and partially edentulous patients. J Periodontal Res 24:96–10510.1111/j.1600-0765.1989.tb00863.x ↗
29. Grossner-Schreiber B, Griepentrog M, Haustein I, Muller WD, Lange KP, Briedigkeit H, Gobel UB (2001) Plaque formation on surface modified dental implants: an in vitro study. Clin Oral Implants Res 12:543–55110.1034/j.1600-0501.2001.120601.x ↗
30. Hauser-Gerspach I, Kulik EM, Weiger R, Decker EM, Ohle CV, Meyer J (2007) Adhesion of Streptococcus sanguinis to dental implant and restorative materials in vitro. Dent Mater J 26:361–36610.4012/dmj.26.361 ↗
31. Subramanian B, Ananthakumar R, Jayachandran M (2011) Structural and tribological properties of DC reactive magnetron sputtered titanium/titanium nitride (Ti/TiN) multilayered coatings. Surf Coat Technol 205:3485–349210.1016/j.surfcoat.2010.12.016 ↗
32. Major L, Morgiel J, Major B, Lackner JM, Waldhauser W, Ebner R, Nistor L, Van Tendeloo G (2006) Crystallographic aspects related to advanced tribological multilayers of Cr/CrN and Ti/TiN types produced by pulsed laser deposition (PLD). Surf Coat Technol 200:6190–619510.1016/j.surfcoat.2005.11.021 ↗
33. Meng F, Lu F (2010) Characterization and photocatalytic activity of TiO2 thin films prepared by RF magnetron sputtering. Vacuum 85:84–8810.1016/j.vacuum.2010.04.006 ↗
34. Pulker HK, Paesold G, Ritter E (1979) Characterization of optical thin films. Appl Opt 18:1969–197710.1364/AO.18.001969 ↗
35. Subramanian B, Ananthakumar R, Vidhya VS, Jayachandran M (2011) Influence of substrate temperature on the materials properties of reactive DC magnetron sputtered Ti/TiN multilayered thin films. Mater Sci Eng B 176:1–710.1016/j.mseb.2010.08.004 ↗
36. Subramanian B, Govindan K, Swaminathan V, Jayachandran M (2009) Materials properties of electrodeposited NiFe and NiCoFe coatings. Trans Inst Met Finish 87:325–32910.1179/174591909X12554332311546 ↗
37. Lugscheider E, Bobzin K (2003) Wettability of PVD compound materials by lubricants. Surf Coat Technol 165:51–5710.1016/S0257-8972(02)00724-7 ↗
38. Contreras A, Bedolla E, Perez R (2004) Interfacial phenomena in wettability of TiC by Al–Mg alloys. Acta Mater 52:985–99410.1016/j.actamat.2003.10.034 ↗
39. Dhandapania P, MuraliKannan M, Anandkumar B, Maruthamuthu S, Manoharan SP (2014) Electrochemistry of calcium precipitating bacteria in orthodontic wire. Oral Sci Int 11:22–2910.1016/S1348-8643(13)00026-8 ↗
40. Laurent F, Grosgogeat B, Reclaru L, Dalard F, Lissac M (2001) Comparison of corrosion behaviour in presence of oral bacteria. Biomaterials 22:2273–228210.1016/S0142-9612(00)00416-6 ↗
41. Maruthamuthu S, Dhandapani P, Ponmariappan S, Sathiyanarayanan S, Muthukrishnan S, Palaniswamy N (2010) Scale formation by calcium-precipitating bacteria in cooling water system. J Fail Anal Prev 10:416–42610.1007/s11668-010-9377-0 ↗
42. Rehman I, Bonfield W (1997) Characterization of hydroxyapatite and carbonated apatite by photo acoustic FTIR spectroscopy. J Mater Sci Mater Med 8:1–410.1023/A:1018570213546 ↗
43. Mather JP, Penelope ER (1998) Introduction to cell and tissue culture: theory and technique. Plenum Press, New York. ISBN 0-306-45859-4
44. Subramanian B, Dhandapani P, Maruthamuthu S, Jayachandran M (2010) Biosynthesis of calcium hydroxylapatite coating on sputtered Ti/TiN nano multilayers and their corrosion behavior in simulated body solution. J Biomater Appl 26:687–70510.1177/0885328210377534 ↗
45. Fujishima A, Rao TN, Tryk DA (2001) Titanium dioxide photocatalysis. J Photochem Photobiol C 1:1–2110.1016/S1389-5567(00)00002-2 ↗
46. Almaguer-Flores A, Olivaves-Navarrete R, Lechuga-Bernal A, Ximenez-Fyvie LA, Rodil SE (2009) Oral bacterial adhesion on amorphous carbon films. Diamond Relat Mater 18:1179–118510.1016/j.diamond.2009.03.003 ↗