Phase transformation, oxidation stability, and electrical conductivity of TiO2-polysiloxane derived ceramics

Kathy Lu, Donald Erb, Mengying Liu

Journal of Materials Science· Volume 51· Issue 22
Publisher page

Abstract

There have been increasing needs for high-thermal stability and high-electrical conductivity materials. In this study, we in situ synthesized silicon oxycarbide (SiOC)–TiC x O y composites based on the pyrolysis of polysiloxane and carbothermal reaction between TiO2 nanoparticles and free carbon in SiOC. The TiO2 to TiC x O y conversion is dependent on the pyrolysis temperature. Higher pyrolysis temperature leads to more TiC formation but lower thermal stability. With more homogeneous distribution of TiO2, the thermal stability of the SiOC–TiC x O y composite increases. This family of SiOC composite also demonstrates high electrical conductivity. The highest electrical conductivity is 5.03 S cm−1 at 400 °C measurement temperature, the highest for air atmosphere condition. The key issue for tuning the SiOC–TiC x O y system for both thermal stability and electrical conductivity is to avoid the destabilization of the SiOC system.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Greil P (1995) Active-filler-controlled pyrolysis of preceramic polymers. J Am Ceram Soc 78:835–84810.1111/j.1151-2916.1995.tb08404.x ↗
2. Colombo P, Mera G, Riedel R, Soraru GD (2010) Polymer-derived ceramics: 40 years of research and innovation in advanced ceramics. J Am Ceram Soc 93:1805–183710.1111/j.1551-2916.2010.03876.x ↗
3. Greil P (2000) Polymer derived engineering ceramics. Adv Eng Mater 2:339–34810.1002/1527-2648(200006)2:6<339::AID-ADEM339>3.0.CO;2-K ↗
4. Ionescu E, Linck C, Fasel C, Muller M, Kleebe HJ, Riedel R (2010) Polymer-derived Sioc/Zro2 ceramic nanocomposites with excellent high-temperature stability. J Am Ceram Soc 93:241–25010.1111/j.1551-2916.2009.03395.x ↗
5. Ionescu E, Papendorf B, Kleebe HJ, Poli F, Muller K, Riedel R (2010) Polymer-derived silicon oxycarbide/hafnia ceramic nanocomposites. Part I: phase and microstructure evolution during the ceramization process. J Am Ceram Soc 93:1774–178210.1111/j.1551-2916.2009.03395.x ↗
6. Ionescu E, Papendorf B, Kleebe HJ, Riedel R (2010) Polymer-derived silicon oxycarbide/hafnia ceramic nanocomposites. Part II: Stability Toward decomposition and microstructure evolution at T ≫ 1000 degrees C. J Am Ceram Soc 93:1783–178910.1111/j.1551-2916.2009.03395.x ↗
7. Greil P (1998) near net shape manufacturing of polymer derived ceramics. J Eur Ceram Soc 18:1905–191410.1016/S0955-2219(98)00129-0 ↗
8. Ma QS, Chen ZH (2007) Electrical resistivity of silicon oxycarbide ceramics fabricated via polysiloxane pyrolysis. Rare Metal Mater Eng 36:619–621
9. Cordelair J, Greil P (2000) Electrical conductivity measurements as a microprobe for structure transitions in polysiloxane derived si–o–c ceramics. J Eur Ceram Soc 20:1947–195710.1016/S0955-2219(00)00068-6 ↗
10. Volkmann E, Evangelista LL, Tushtev K, Koch D, Wilhelmi C, Rezwan K (2014) Oxidation-induced microstructural changes of a polymer-derived nextel (tm) 610 ceramic composite and impact on the mechanical performance. J Mater Sci 49:710–719. doi: 10.1007/s10853-013-7752-410.1007/s10853-013-7752-4 ↗
11. Wang KW, Ma BS, Li XQ, Wang YG, An LN (2014) Effect of pyrolysis temperature on the structure and conduction of polymer-derived sic. J Am Ceram Soc 97:2135–213810.1111/jace.12931 ↗
12. Ahn D, Raj R (2011) Cyclic stability and c-rate performance of amorphous silicon and carbon based anodes for electrochemical storage of lithium. J Power Sources 196:2179–218610.1016/j.jpowsour.2010.09.086 ↗
13. Schulz M (2009) Polymer derived ceramics in MEMS/NEMS—a review on production processes and application. Adv Appl Ceram 108:454–46010.1179/174367609X422171 ↗
14. Reinold LM, Graczyk-Zajac M, Gao Y, Mera G, Riedel R (2013) Carbon-rich sicn ceramics as high capacity/high stability anode material for lithium-ion batteries. J Power Sour 236:224–22910.1016/j.jpowsour.2013.02.046 ↗
15. Graczyk-Zajac M, Toma L, Fasel C, Riedel R (2012) Carbon-rich sioc anodes for lithium-ion batteries: Part I. Influence of material UV-Pre-treatment on high power properties. Solid State Ionics 225:522–52610.1016/j.ssi.2011.12.007 ↗
16. Hauser R, Francis A, Theismann R, Riedel R (2008) Processing and magnetic properties of metal-containing sicn ceramic micro- and nano-composites. J Mater Sci 43:4042–4049. doi: 10.1007/s10853-007-2143-310.1007/s10853-007-2143-3 ↗
17. Zhou C, Yang L, Geng H et al (2012) Preparation of Si-C-N-Fe magnetic ceramic derived from iron-modified polysilazane. Ceram Int 38:6815–682210.1016/j.ceramint.2012.05.080 ↗
18. Chen XJ, Su ZM, Zhang L, Tang M, Yu Y, Zhang L, Chen L (2010) Iron nanoparticle-containing silicon carbide fibers prepared by pyrolysis of Fe(Co)(5)-doped polycarbosilane fibers. J Am Ceram Soc 93:89–9510.1111/j.1551-2916.2009.03369.x ↗
19. Yurkov GY, Astaf’ev DA, Nikitin LN, Koksharovc YA, Kataevaa NA, Shtykovad EV, Dembod KA, Volkovd AA, Khokhlovb AR, Gubina SP (2006) Fe-containing nanoparticles in siloxane rubber matrices. Inorg Mater 42:496–50210.1134/S0020168506050098 ↗
20. Vakifahmetoglu C, Pippel E, Woltersdorf J, Colombo P (2010) Growth of one-dimensional nanostructures in porous polymer-derived ceramics by catalyst-assisted pyrolysis. Part I: Iron catalyst. J Am Ceram Soc 93:959–96810.1111/j.1551-2916.2009.03448.x ↗
21. Vakifahmetoglu C, Colombo P, Carturan SM, Pippel E, Woltersdorf J (2010) Growth of one-dimensional nanostructures in porous polymer-derived ceramics by catalyst-assisted pyrolysis. Part II: Cobalt catalyst. J Am Ceram Soc 93:3709–371910.1111/j.1551-2916.2010.03974.x ↗
22. Guo AR, Roso M, Colombo P, Liu JC, Modesti M (2015) In situ carbon thermal reduction method for the production of electrospun metal/sioc composite fibers. J Mater Sci 50:2735–2746. doi: 10.1007/s10853-015-8827-110.1007/s10853-015-8827-1 ↗
23. Cordelair J, Greil P (2001) Electrical characterization of polymethylsiloxane/Mosi2-derived composite ceramics. J Am Ceram Soc 84:2256–225910.1111/j.1151-2916.2001.tb00998.x ↗
24. Kim DP (2001) Preparation of electrically conducting sic/mosi2 composites from metal mixtures of preceramic polymer. Mater Res Bull 36:2497–250510.1016/S0025-5408(01)00704-8 ↗
25. Liu WP, DuPont JN (2003) Fabrication of functionally graded tic/ti composites by laser engineered net shaping. Scr Mater 48:1337–134210.1016/S1359-6462(03)00020-4 ↗
26. Swift GA, Koc R (1999) Formation studies of tic from carbon coated TiO2. J Mater Sci 34:3083–3093. doi: 10.1023/A:100469271459510.1023/A:1004692714595 ↗
27. Woo Y-C, Kang H-J, Kim DJ (2007) Formation of TiC particle during carbothermal reduction of TiO2. J Eur Ceram Soc 27:719–72210.1016/j.jeurceramsoc.2006.04.090 ↗
28. Cho D, Park JH, Jeong Y, Joo YL (2015) Synthesis of titanium carbide-carbon nanofibers via carbothermal reduction of titania with carbon. Ceram Int 41:10974–1097910.1016/j.ceramint.2015.05.041 ↗
29. Dewan MAR, Zhang G, Ostrovski O (2008) Carbothermal reduction of titania in different gas atmospheres. Metall Mater Trans B 40:62–6910.1007/s11663-008-9205-z ↗
30. Gadiou R, Serverin S, Gibot P, Vix-Guterl C (2008) The Synthesis of SiC and TiC protective coatings for carbon fibers by the reactive replica process. J Eur Ceram Soc 28:2265–227410.1016/j.jeurceramsoc.2008.02.022 ↗
31. Lu K, Erb D, Liu M (2016) Thermal stability and electrical conductivity of carbon-enriched silicon oxycarbide. J Mater Chem C 4:1829–183710.1039/C6TC00069J ↗
32. Peña-Alonso R, Sorarù GD, Raj R (2006) Preparation of ultrathin-walled carbon-based nanoporous structures by etching pseudo-amorphous silicon oxycarbide ceramics. J Am Ceram Soc 89:2473–248010.1111/j.1551-2916.2006.01117.x ↗
33. Wilson AM, Zank G, Eguchi K, Xing W, Yates B, Dahn JR (1997) Pore creation in silicon oxycarbides by rinsing in dilute hydrofluoric acid. Chem Mater 9:2139–214410.1021/cm970224p ↗
34. Martinez-Crespiera S, Ionescu E, Kleebe HJ, Riedel R (2011) pressureless synthesis of fully dense and crack-free sioc bulk ceramics via photo-crosslinking and pyrolysis of a polysiloxane. J Eur Ceram Soc 31:913–91910.1016/j.jeurceramsoc.2010.11.019 ↗
35. Robertson J (1986) Amorphous-carbon. Adv Phys 35:317–37410.1080/00018738600101911 ↗