Abstract
Abstract The influence of grain growth inhibition by pearlite on hydrogen embrittlement (HE) behavior of ultra-low carbon ferritic steels was studied. The Fe-0.02C alloy has a considerable sensitivity to HE, while the Fe and Fe-0.1C materials have lower HE sensitivity. The high fraction of high-angle grain boundaries (HAGB) is responsible for the shift of the peak to a higher temperature in the Fe-0.1C alloy. The trapping of hydrogen by HAGBs was observed by hydrogen mapping. Higher density of HAGBs contributes to higher trap density in Fe-0.1C alloy and lower H diffusion coefficient. The coexistence of hydrogen enhanced decohesion (HEDE) and hydrogen-enhanced localized plasticity (HELP) mechanisms was identified and discussed. The results indicate that HEDE is active in the initial stage of the tensile loading during crack initiation and HELP in the rest of tensile testing duration that controls the crack propagation. Due to the reduction in grain size caused by the addition of pearlite, the normalized hydrogen content per HAGB length is significantly lower than Fe-0.1C, which means that the critical amount of local hydrogen required for crack initiation is less likely to accumulate due to the weakening of cohesive interatomic strength. In Fe-0.02C alloy, the ciritcal local content was built up at HAGBs, and resulting in activation of HEDE mechanism for crack initiation. In Fe-0.1C, a lower possibility of accumulating the critical H concentration at HAGBs, resulting in limited activation of HEDE-based crack initiation at HAGB and less crack propagation events based on the HELP mechanism.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Obama B (2017) The irreversible momentum of clean energy. Science 355:126–129. https://doi.org/10.1126/science.aam628410.1126/science.aam6284 ↗
2. Mallouk TE (2013) Divide and conquer. Nat Chem 5:362–36310.1038/nchem.1634 ↗
3. Xu K (2012) Hydrogen embrittlement of carbon steels and their welds. Gaseous hydrogen embrittlement of materials in energy technologies. Elsevier, Amsterdam, pp 526–56110.1533/9780857093899.3.526 ↗
4. Moshtaghi M, Safyari M (2022) Temperature mitigates the hydrogen embrittlement sensitivity of martensitic steels in slow strain rates. Vacuum 202:111187. https://doi.org/10.1016/j.vacuum.2022.11118710.1016/j.vacuum.2022.111187 ↗
5. San Marchi C, Somerday BP, Nibur KA et al (2010) Fracture and fatigue of commercial grade API pipeline steels in gaseous hydrogen. ASME 2010 pressure vessels and piping conference, vol 6. Parts A and B. ASMEDC, Bellevue, Washington, USA, pp 939–94810.1115/PVP2010-25825 ↗
6. Nanninga NE, Levy YS, Drexler ES et al (2012) Comparison of hydrogen embrittlement in three pipeline steels in high pressure gaseous hydrogen environments. Corros Sci 59:1–9. https://doi.org/10.1016/j.corsci.2012.01.02810.1016/j.corsci.2012.01.028 ↗
7. Michler T, Naumann J (2010) Microstructural aspects upon hydrogen environment embrittlement of various bcc steels. Int J Hydrog Energy 35:821–832. https://doi.org/10.1016/j.ijhydene.2009.10.09210.1016/j.ijhydene.2009.10.092 ↗
8. Ishikawa N, Sueyoshi H, Nagao A (2016) Hydrogen microprint analysis on the effect of dislocations on grain boundary hydrogen distribution in steels. ISIJ Int 56:413–417. https://doi.org/10.2355/isijinternational.ISIJINT-2015-32910.2355/isijinternational.ISIJINT-2015-329 ↗
9. Park C, Kang N, Liu S (2017) Effect of grain size on the resistance to hydrogen embrittlement of API 2W Grade 60 steels using in situ slow-strain-rate testing. Corros Sci 128:33–41. https://doi.org/10.1016/j.corsci.2017.08.03210.1016/j.corsci.2017.08.032 ↗
10. Takasawa K, Ikeda R, Ishikawa N (2010) Ishigaki R (2012) Effects of grain size and dislocation density on the susceptibility to high-pressure hydrogen environment embrittlement of high-strength low-alloy steels. AIChE Annu Meet Top Conf Hydrog Prod Storage Spec Issue 37:2669–2675. https://doi.org/10.1016/j.ijhydene.2011.10.09910.1016/j.ijhydene.2011.10.099 ↗
11. Luppo MI, Ovejero-Garcia J (1991) The influence of microstructure on the trapping and diffusion of hydrogen in a low carbon steel. Corros Sci 32:1125–1136. https://doi.org/10.1016/0010-938X(91)90097-910.1016/0010-938X(91)90097-9 ↗
12. Wei FG, Tsuzaki K (2012) Gaseous HE of materials in energy technologies. Gaseous Hydrog Embrittlement Mater Energy Technol 1:493e525
13. Bhadeshia HKDH (2016) Prevention of hydrogen embrittlement in steels. ISIJ Int 56:24–36. https://doi.org/10.2355/isijinternational.ISIJINT-2015-43010.2355/isijinternational.ISIJINT-2015-430 ↗
14. Takashima K, Han R, Yokoyama K, Funakawa Y (2019) Hydrogen embrittlement induced by hydrogen charging during deformation of ultra-high strength steel sheet consisting of ferrite and nanometer-sized precipitates. ISIJ Int 59:2327–2333. https://doi.org/10.2355/isijinternational.ISIJINT-2019-21910.2355/isijinternational.ISIJINT-2019-219 ↗
15. Lee HG, Lee J-Y (1984) Hydrogen trapping by TiC particles in iron. Acta Metall 32:131–136. https://doi.org/10.1016/0001-6160(84)90210-410.1016/0001-6160(84)90210-4 ↗
16. Pressouyre GM, Bernstein IM (1978) A quantitative analysis of hydrogen trapping. Metall Trans A 9:1571–1580. https://doi.org/10.1007/BF0266193910.1007/BF02661939 ↗
17. Wei FG, Tsuzaki K (2006) Quantitative analysis on hydrogen trapping of TiC particles in steel. Metall Mater Trans A 37:331–353. https://doi.org/10.1007/s11661-006-0004-310.1007/s11661-006-0004-3 ↗
18. Wei FG, Hara T, Tsuzaki K (2004) Precise determination of the activation energy for desorption of hydrogen in two Ti-added steels by a single thermal-desorption spectrum. Metall Mater Trans B 35:587–597. https://doi.org/10.1007/s11663-004-0057-x10.1007/s11663-004-0057-x ↗
19. Asahi H, Hirakami D, Yamasaki S (2003) Hydrogen trapping behavior in vanadium-added steel. ISIJ Int 43:527–533. https://doi.org/10.2355/isijinternational.43.52710.2355/isijinternational.43.527 ↗
20. Wei F-G, Hara T, Tsuzaki K (2011) Nano-preciptates design with hydrogen trapping character in high strength steel. Advanced steels. Springer, NY, pp 87–9210.1007/978-3-642-17665-4_11 ↗
21. Choo WY, Lee JY (1982) Thermal analysis of trapped hydrogen in pure iron. Metall Trans A 13:135–140. https://doi.org/10.1007/BF0264242410.1007/BF02642424 ↗
22. Moshtaghi M, Loder B, Safyari M et al (2022) Hydrogen trapping and desorption affected by ferrite grain boundary types in shielded metal and flux-cored arc weldments with Ni addition. Int J Hydrog Energy. https://doi.org/10.1016/j.ijhydene.2022.04.26010.1016/j.ijhydene.2022.04.260 ↗
23. Moshtaghi M, Safyari M, Kuramoto S, Hojo T (2021) Unraveling the effect of dislocations and deformation-induced boundaries on environmental hydrogen embrittlement behavior of a cold-rolled Al–Zn–Mg–Cu alloy. Int J Hydrog Energy 46:8285–8299. https://doi.org/10.1016/j.ijhydene.2020.12.02810.1016/j.ijhydene.2020.12.028 ↗
24. Safyari M, Moshtaghi M, Kuramoto S (2021) On the role of traps in the microstructural control of environmental hydrogen embrittlement of a 7xxx series aluminum alloy. J Alloys Compd 855:157300. https://doi.org/10.1016/j.jallcom.2020.15730010.1016/j.jallcom.2020.157300 ↗
25. Devanathan MAV, Stachurski Z (1962) The adsorption and diffusion of electrolytic hydrogen in palladium. Proc R Soc Lond Ser Math Phys Sci 270:90–102. https://doi.org/10.1098/rspa.1962.020510.1098/rspa.1962.0205 ↗
26. Moshtaghi M, Safyari M, Mori G (2022) Hydrogen absorption rate and hydrogen diffusion in a ferritic steel coated with a micro- or nanostructured ZnNi coating. Electrochem Commun 134:107169. https://doi.org/10.1016/j.elecom.2021.10716910.1016/j.elecom.2021.107169 ↗
27. Addach H, Berçot P, Rezrazi M, Wery M (2005) Hydrogen permeation in iron at different temperatures. Mater Lett 59:1347–1351. https://doi.org/10.1016/j.matlet.2004.12.03710.1016/j.matlet.2004.12.037 ↗
28. Kassner ME, Barrabes SR (2005) New developments in geometric dynamic recrystallization. Mater Sci Eng A 410:152–15510.1016/j.msea.2005.08.052 ↗
29. Ingelström N, Ustimenko V (1975) The influence of porosity and carbon content on the fracture toughness of some sintered steels. Powder Metall 18:303–322. https://doi.org/10.1179/pom.1975.18.36.00410.1179/pom.1975.18.36.004 ↗
30. Xu K, Rana M (2008) Tensile and fracture properties of carbon and low alloy steels in high pressure hydrogen. 2008 International hydrogen conference (Materials Park. ASM International, OH, p 349
31. Merson E, Vinogradov A, Merson DL (2015) Application of acoustic emission method for investigation of hydrogen embrittlement mechanism in the low-carbon steel. J Alloys Compd 645:S460–S46310.1016/j.jallcom.2014.12.083 ↗
32. Shibata A, Momotani Y, Murata T et al (2017) Microstructural and crystallographic features of hydrogen-related fracture in lath martensitic steels. Mater Sci Technol 33:1524–1532. https://doi.org/10.1080/02670836.2017.131221010.1080/02670836.2017.1312210 ↗
33. Momotani Y, Shibata A, Terada D, Tsuji N (2017) Effect of strain rate on hydrogen embrittlement in low-carbon martensitic steel. Int J Hydrog Energy 42:3371–3379. https://doi.org/10.1016/j.ijhydene.2016.09.18810.1016/j.ijhydene.2016.09.188 ↗
34. Chen L, Xiong X, Tao X et al (2020) Effect of dislocation cell walls on hydrogen adsorption, hydrogen trapping and hydrogen embrittlement resistance. Corros Sci 166:108428. https://doi.org/10.1016/j.corsci.2020.10842810.1016/j.corsci.2020.108428 ↗
35. Thelning K-E (2014) Steel and its heat treatment, 2nd edn. Elsevier Science, Kent
36. Calado WR, Barbosa R (2013) Influence of carbon content and deformation temperature on ultra-grain refinement of plain carbon steels by means of torsion test. ISIJ Int 53:909–914. https://doi.org/10.2355/isijinternational.53.90910.2355/isijinternational.53.909 ↗
37. Pressouyre GM (1980) Trap theory of hydrogen embrittlement. Acta Metall 28:895–911. https://doi.org/10.1016/0001-6160(80)90106-610.1016/0001-6160(80)90106-6 ↗
38. Pressouyre GM (1979) A classification of hydrogen traps in steel. Metall Trans A 10:1571–1573. https://doi.org/10.1007/BF0281202310.1007/BF02812023 ↗
39. Akiyama E, Matsuoka S (2015) Hydrogen visualization in steels using ag decoration method. Mater Trans 56:793–797. https://doi.org/10.2320/matertrans.M201443110.2320/matertrans.M2014431 ↗
40. Troiano AR (2016) The role of hydrogen and other interstitials in the mechanical behavior of metals. Metallogr Microstruct Anal 5:557–569. https://doi.org/10.1007/s13632-016-0319-410.1007/s13632-016-0319-4 ↗
41. Gerberich WW, Oriani RA, Lji M-J et al (1991) The necessity of both plasticity and brittleness in the fracture thresholds of iron. Philos Mag A 63:363–37610.1080/01418619108204854 ↗
42. Oriani RA (1987) Whitney award lecture—1987: hydrogen—the versatile embrittler. Corrosion 43:390–39710.5006/1.3583875 ↗
43. Safyari M, Moshtaghi M, Kuramoto S (2021) Environmental hydrogen embrittlement associated with decohesion and void formation at soluble coarse particles in a cold-rolled Al–Cu based alloy. Mater Sci Eng A 799:139850. https://doi.org/10.1016/j.msea.2020.13985010.1016/j.msea.2020.139850 ↗
44. Martin ML, Fenske JA, Liu GS et al (2011) On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels. Acta Mater 59:1601–1606. https://doi.org/10.1016/j.actamat.2010.11.02410.1016/j.actamat.2010.11.024 ↗
45. Nagumo M, Matsuda H (2002) Function of hydrogen in intergranular fracture of martensitic steels. Philos Mag A 82:3415–3425. https://doi.org/10.1080/0141861020824045210.1080/01418610208240452 ↗
46. Robertson IM (1999) The effect of hydrogen on dislocation dynamics. Eng Fract Mech 64:649–673. https://doi.org/10.1016/S0013-7944(99)00094-610.1016/S0013-7944(99)00094-6 ↗
47. Huang H, Hui H, Peng J et al (2023) Prediction of hydrogen-assisted fracture under coexistence of hydrogen-enhanced plasticity and decohesion. Int J Hydrog Energy. https://doi.org/10.1016/j.ijhydene.2023.06.03310.1016/j.ijhydene.2023.06.033 ↗
48. Siegl, W (2021) Hydrogen Trapping in Iron and Iron-Based Alloys. [Doctoral Thesis, Montanuniversitaet Leoben]