Fibre-reinforced geopolymer concrete with ambient curing for in situ applications

Mark Reed, Weena Lokuge, Warna Karunasena

Journal of Materials Science· Volume 49· Issue 12
Publisher page

Abstract

Geopolymer concrete is proven to have excellent engineering properties with a reduced carbon footprint. It not only reduces the greenhouse gas emissions (compared to Portland cement-based concrete) but also utilises a large amount of industrial waste materials such as fly ash and slag. Due to these positive attributes, it is becoming an increasingly popular construction material. Previous studies on geopolymer concrete report that heat curing plays an important role in gaining higher compressive strength values (as opposed to ambient curing), and hence the application of this material could be limited to precast members. Therefore, this research was aimed at investigating the effect of heat curing by comparing the mechanical properties such as compressive strength and ductility of ambient cured and heat cured geopolymer concrete samples. It is worth noting that there was marginal strength change due to heat curing. In Australia, fibre-reinforced geopolymer concrete is being used in precast panels in underground constructions. Commercially available geopolymer cement and synthetic fibres are effectively being used to produce elements that are more durable than what is currently used in industry. As a result, this research investigated the effects of polypropylene fibres in geopolymer concrete using 0.05 and 0.15 % fibres (by weight). The addition of polypropylene fibres enhances the compressive strength and the ductility of geopolymer concrete.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Concrete Properties and Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. McLellan BC, Williams RP, Lay J, Riessen A, Corder GD (2011) Costs and carbon emissions for geopolymer pastes in comparison to Ordinary Portland Cement. J Clean Prod 19:1080–109010.1016/j.jclepro.2011.02.010 ↗
2. Rangan BV (2008) Fly ash-based geopolymer concrete. Curtin University of Technology, Perth
3. Wallah SE (2010) Creep behaviour of fly ash-based geopolymer concrete. Civil Eng Dimens 12:73–78
4. Intelligence M (2013) World Cement Consumption. http://www.betonabq.org/images/imguser/WorldReport_Aug_2013final__01__cement.pdf . Accessed 4 Feb 2014
5. Davidovits J (1988) Geopolymer chemistry and properties. Proceedings of Geopolymer ‘88, First European Conference on Soft Mineralurgy, The Geopolymer Institute, Compiegne, 25–48.
6. Deevasan KK, Ranganath RV (2010) Geopolymer concrete using industrial byproducts. Constr Mater 164:43–5010.1680/coma.900034 ↗
7. Hardjito D, Wallah SE, Sumajouw DMJ, Rangan BV (2005) Fly ash based geopolymer concrete. Aust J Struct Eng 6:77–8510.1080/13287982.2005.11464946 ↗
8. Memon FA, Nuruddin MF, Demie S, Shafiq N (2011) Effect of curing conditions on strength of fly ash-based self-compacting geopolymer concrete. World Acad Sci Eng Technol 80:860–863
9. Pan Z, Sanjayan JG, Rangan BV (2011) Fracture properties of geopolymer paste and concrete. Mag Concr Res 63:763–77110.1680/macr.2011.63.10.763 ↗
10. Neville A, Brooks J (2004) Concrete technology. Pearson Education, Essex
11. Karahan O, Tanyildizi H, Atis C (2009) Statistical analysis for strength properties of polypropylene-fibre-reinforced fly ash concrete. Mag Concr Res 61:557–56610.1680/macr.2007.00033 ↗
12. Swamy RN, Bahia HM (1985) The effectiveness of steel fibres as shear reinforcement. Concr Int 7:35–40
13. Sabir B (2001) Toughness and tortuosity of polypropylene fibre reinforced concrete. Mag Concr Res 53:163–17010.1680/macr.2001.53.3.163 ↗
14. Wimpenny D, Duxson P, Cooper T, Provis J, Zeuschner R (2011) Fibre reinforced geopolymer concrete products for underground infrastructure. http://www.halcrow.com/Documents/australia/FRGC_products_for_undergound_infrastructure.pdf . Accessed 4 Oct 2013
15. Chindaprasirt P, Chareerat T, Sirivivatnanon V (2007) Workability and strength of coarse high calcium fly ash geopolymer. Cement Concr Compos 29:224–22910.1016/j.cemconcomp.2006.11.002 ↗
16. Guo X, Shi H, Dick WA (2010) Compressive strength and microstructural characteristics of class C fly ash geopolymer. Cement Concr Compos 32:142–14710.1016/j.cemconcomp.2009.11.003 ↗
17. Olivia M, Nikraz H (2012) Properties of fly ash geopolymer concrete designed by Taguchi method. Mater Des 36:191–19810.1016/j.matdes.2011.10.036 ↗
18. Zhao R, Sanjayan JG (2011) Geopolymer and Portland cement concretes in simulated fire. Mag Concr Res 63:163–17310.1680/macr.9.00110 ↗
19. Australia S (1999) Method of testing concrete, Method 9: determination of the compressive strength of concrete specimens, pp. 13
20. Concrete Institute of Australia (2011) Recommended practice: geopolymer concrete. Concrete Institute of Australia, West Perth
21. Vijai K, Kumutha R, Vishnuram B (2012) Experimental investigations on mechanical properties of geopolymer concrete composites. Asian J Civ Eng (Build Hous) 13:89–96
22. Collins MP, Mitchell D, MacGregor JG (1993) Structural design considerations for high strength concrete. ACI Concr Int 15:27–34
23. Ahn JM, Shin SW (2007) An evaluation of ductility of high-strength reinforced concrete columns subjected to reversed cyclic loads under axial compression. Mag Concr Res 59:29–4410.1680/macr.2007.59.1.29 ↗
24. Paultre P, Eid R, Robles HI, Bouaanani N (2009) Seismic performance of circular high-strength concrete columns. ACI Struct J 106:395–404
25. Rui J, Jin-qing J, Shi-lang X (2007) Seismic ductility of very-high-strength-concrete short columns subject to combined axial loading and cyclic lateral loading. J Chongqing Univ: English Edition 6:205–212
26. Woods JM, Kiousis PD, Ehsani MR, Saadatmanesh H (2007) Bending ductility of rectangular high strength concrete columns. Eng Struct 29:1783–179010.1016/j.engstruct.2006.09.024 ↗
27. Pan Z, Sanjayan JG, Rangan BV (2009) An investigation of the mechanisms for strength gain or loss of geopolymer mortar after exposure to elevated temperature. J Mater Sci 44:1873–1880. doi: 10.1007/s10853-009-3243-z10.1007/s10853-009-3243-z ↗
28. Foster S, Kilpatrick AE, Warner RF (2010) In reinforced concrete basics analysis and design of reinforced concrete structures, 2nd edn. Frenchs Forest, NSW