High-temperature wear and microstructural degradation of CrN/CrAlSiN/TiC multilayer coatings deposited on Orvar 2 M hot-work tool steel
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Surface Treatment and Coatings · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Hutchings · 2017
2. Effect of solution and artificial aging heat treatment on the hardness, friction and wear properties of laser cladding and roll-formed 18Ni300 materials10.2478/msp-2024-0017 ↗
3. Roberts · 1998
4. 2016
5. 1995
6. Evaluation of the possibility of improving the durability of tools made of X153CrMoV12 steel used in the extrusion of a clay band in ceramic roof tile production10.2478/msp-2023-0011 ↗
7. Straffelini · 2015
8. Wear of hot-work tool steels under sliding contact
9. High temperature wear mechanisms of tool steels
10. Tribological behavior of hot-work tool steel under dry sliding
11. Friction and wear in metal forming
12. Wear and friction evaluation of different tool steels for hot stamping10.1155/2018/3296398 ↗
13. Influence of the grade of hot work tool steels and its microstructural features on the durability of punches used in the closed die precision forging of valve forgings made of nickel-chrome steel
14. Tribological performance of hot work steels
15. Tribological performance of Orvar 2m tool steel coated with Alwin XC for improved forging tool durability10.2478/msp-2025-0045 ↗
16. Effect of retained austenite on the wear resistance of C80W1 and 90CrSi5 tool steels
17. Study on microscopic characteristics and wear testing of steel surface after ultrasonic impact treatment
18. 2017
19. 2012
20. Recent advances in PVD coatings for high-temperature tribological applications
21. Calculation and analytical prediction of coating wear during tribological tests based on models of contact fatigue failure
22. Generalized assessment of wear resistance of polymer materials and coating tribological properties under sliding conditions10.3103/S1068366625700011 ↗
23. Influence of ceramic counterpart material on tribological behaviour of thin hard coatings
24. High-temperature tribological behaviour of advanced PVD coatings: a review
25. Analysis of selected aspects of improving the durability of ceramic roof tile forming tools with consideration of numerical modeling10.1016/j.triboint.2026.111700 ↗
26. Friction and wear of coatings at elevated temperatures
27. Topographical analysis of wear tracks on thin films using 3D areal parameters
28. Wear mechanisms and durability of advanced PVD coatings under severe tribological loading
29. Influence of the application of a PN+Cr/CrN hybrid layer on the improvement of the lifetime of hot forging tools10.1016/j.jmatprotec.2018.03.029 ↗
30. Analysis of the wear of forging tools surface layer after hybrid surface treatment10.1016/j.ijmachtools.2016.12.010 ↗
31. Formation and evolution of tribo-oxide layers on hard coatings at elevated temperatures
32. Analysis of the destruction of a die insert used in the industrial process of hot die forging to produce a yoke forging10.1016/j.engfailanal.2024.108661 ↗
33. Oxidative wear behavior of H13 steel under dry sliding conditions at elevated temperatures
34. Effect of tempering conditions on wear resistance in various wear mechanisms of H13 steel
35. The search for novel, superhard materials10.1116/1.581977 ↗
36. Hard and superhard nanocomposite coatings10.1016/S0257-8972(99)00586-1 ↗
37. Mechanical and structural properties of CrAlSiN nanocomposite coatings10.3390/coatings10010041 ↗
38. Microstructure and properties of CrAlSiN coatings deposited by HiPIMS and DC magnetron sputtering10.3390/coatings9080512 ↗
39. (Cr1-xAlx)N coating deposition by short-pulse high-power dual magnetron sputtering10.3390/ma15228237 ↗
40. High-temperature mechanical properties and friction-wear performance of CrAlN coatings prepared by arc ion plating via Mo doping10.3390/met16020152 ↗
41. Structure and properties of CrAlSiN nanocomposite coatings deposited by lateral rotating cathode arc10.1016/j.tsf.2010.10.022 ↗
42. A concept for the design of novel superhard coatings10.1016/0040-6090(95)06695-0 ↗
43. Analysis of the possibilities of increasing the durability of forging tools used in the production of forgings for the automotive industry by applying the ALWIN XC hard coating10.1016/j.ijrmhm.2025.107288 ↗
44. Harish
45. Protective effectiveness of a nanocomposite coating with low-friction layers under sliding friction at ambient temperature
46. Study on microstructure, mechanical properties, tribological properties and service performance of CrAlN and CrAlBN coatings deposited on powder metallurgy high-speed steel by arc ion plating technique10.3390/coatings14040486 ↗
47. Friction and wear properties of TiN, TiAlN, AlTiN and CrAlN PVD nitride coatings10.1016/j.ijrmhm.2011.09.010 ↗
48. Effects of PVD CrAlN/(CrAlB)N/CrAlN coating on pin–disc friction properties at elevated temperatures10.3390/met14060662 ↗