journal article·2026-05Open access

Synergistic densification and performance of Cf/ZrB2–SiC–ZrC composites via a hybrid HP-PIP strategy

Yushi Qi, Qinghua Liu, Hongge Li, Junchang Cao, Liping Jiang, Kai Jiang, Xusheng Chang, Wenbo Han, Houyi Bai, Gang Chen

Abstract

A hybrid process combining slurry infiltration, low-temperature hot-pressing (HP), and precursor infiltration and pyrolysis (PIP) was developed to fabricate continuous C f /ZrB 2 -SiC-ZrC composites. Optimized HP at 1200 °C (40 MPa, 15 min) established a robust porous skeleton, which significantly reduced the subsequent PIP cycles to six, achieving a high bulk density of 2.93 g/cm 3 and low open porosity of 8.45 %. The optimal composite exhibited a flexural strength of 109.47 MPa. Notably, while the fracture toughness was moderate (3.77 MPa·m 1/2 ), the material demonstrated exceptional damage tolerance with a high work of fracture (578.98 J/m 2 ), attributed to extensive fiber pull-out and crack deflection mechanisms. After oxidation at 1500 °C, a continuous ZrO 2 -SiO 2 scale formed, allowing the composite to retain 30 % of its strength and maintain structural integrity. This work offers a strategic pathway for balancing densification efficiency and damage tolerance in UHTCMCs.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Innovative fabrication pathways for ultra-high temperature ceramic matrix composites: progress, properties enhancements and future perspectives
2. Csf/SiBCN-ZrB2 composites prepared by in-situ reaction: plasma ablation behavior at different durations10.1016/j.jmrt.2025.12.140 ↗
3. Mechanical properties of ultra-high temperature ceramic matrix composites (UHTCMCs): a review10.1016/j.ceramint.2025.04.293 ↗
4. Processing and characterization of 2D woven ZrB2‐based ultrahigh‐temperature ceramic matrix composites10.1111/ijac.14528 ↗
5. Bioinspired C/C composites with long-duration ablation resistance for thermal protection up to 2400 °C10.1016/j.mser.2025.101157 ↗
6. Morphology-driven Cu gradient distribution induces varied anti-ablation performance in C/C-ZrC composites10.1016/j.carbon.2025.121063 ↗
7. Bioinspired vacuum-driven approach enables mechanically robust, ablation-resistant sharp leading-edge composites10.1016/j.mattod.2025.11.031 ↗
8. Ablation resistance of C/C–Hf1-xZrxC composites under an oxyacetylene flame at above 2700 °C10.1016/j.compositesb.2024.111855 ↗
9. Microstructure characterization of Cf/ZrC-ZrB2-SiC-C ultrahigh temperature ceramic matrix composites
10. High-performance ZrB2-SiC-Cf composite prepared by low-temperature hot pressing using nanosized ZrB2 powder10.1016/j.jeurceramsoc.2017.02.008 ↗
11. The ablation and mechanical behaviors of C/(SiC-ZrC)n multi-layer structure matrix composites by chemical vapor infiltration10.1016/j.jeurceramsoc.2022.04.026 ↗
12. Cyclic ablation behavior of C/C-ZrC-SiC-ZrB2 composites under oxyacetylene torch with two heat fluxes at the temperatures above 2000 °C10.1016/j.corsci.2020.109202 ↗
13. Effect of ZrB2 on the ablation behavior of Cf/ZrB2-ZrC-SiC sharp leading edge composites by PIP and RMI10.1016/j.matchar.2024.113898 ↗
14. Ablation behaviour and mechanical performance of ZrB2-ZrC-SiC modified carbon/carbon composites prepared by vacuum infiltration combined with reactive melt infiltration10.1016/j.carbon.2024.119517 ↗
15. Ablation behavior of three-dimensional Cf/SiC-ZrC-ZrB2 composites prepared by a joint process of sol-gel and reactive melt infiltration10.1016/j.corsci.2018.02.011 ↗
16. Effects of SiC content on the microstructure and mechanical performance of stereolithography-based SiC ceramics10.1016/j.jmrt.2023.06.260 ↗
17. C/C-HfC-ZrC composites with excellent long-term ablation performance prepared by combining PIP and RMI10.1016/j.ceramint.2024.01.308 ↗
18. Effects of preform pore structure on infiltration kinetics and microstructure evolution of RMI-derived Cf/ZrC-ZrB2-SiC composite10.1016/j.jeurceramsoc.2019.11.020 ↗
19. Microstructure evolution of (Hf, Zr, Ti)C ceramic-modified C/C composites fabricated by reactive melt infiltration10.1016/j.ceramint.2025.09.281 ↗
20. Effects of polymer-derived ZiC interlayer on mechanical properties and ablation performance of C/C-ZiC-ZrC-SiC composites prepared by RMI10.1016/j.jeurceramsoc.2024.03.058 ↗
21. A novel vibration-assisted slurry impregnation to fabricate Cf/ZrB2-SiC composite with enhanced mechanical properties10.1016/j.jeurceramsoc.2018.10.029 ↗
22. 3D microstructure characterization of 2D Cf-ZrB2-SiC ultra-high temperature ceramic matrix composites using X-ray microscopy10.1016/j.ceramint.2023.11.183 ↗
23. Chemical reactions and thermal stress induced microstructure evolution in 2D-Cf/ZrB2-SiC composites10.1016/j.jmst.2020.12.054 ↗
24. Microstructures and mechanical properties of Cf/ZrB2-SiC composite fabricated by nano slurry brushing combined with low-temperature hot pressing10.1016/j.jallcom.2019.03.147 ↗
25. Binder jetting 3D printing preparation of SiC ceramics with low free silicon content and densification by PIP and LSI process10.1016/j.jmrt.2025.04.260 ↗
26. Tensile properties of 3D stitched C/C-SiC composites prepared by a hybrid chemical vapor infiltration (CVI) and polymer impregnation and pyrolysis (PIP) process10.1016/j.ceramint.2024.12.371 ↗
27. Ablation behavior of Cf/ZrC-SiC-based composites fabricated by an improved reactive melt infiltration10.1016/j.jeurceramsoc.2019.07.007 ↗
28. Insitu synthesis of ZrB2-ZrC-SiC ultra-high-temperature nanocomposites by a sol-gel process10.1080/17436753.2017.1412032 ↗
29. Spark plasma sintering of quadruplet ZrB2-SiC-ZrC-Cf composites10.1016/j.ceramint.2019.08.243 ↗
30. Characterization and mechanical properties of Cf/ZrB2-SiC composites fabricated by a hybrid technique based on slurry impregnation, polymer infiltration and pyrolysis and low-temperature hot pressing10.1016/j.ceramint.2018.12.001 ↗
31. Oxidation-resistant ZrB2-SiC composites at 2200 °C10.1016/j.compscitech.2007.08.017 ↗
32. High temperature oxidation and oxyacetylene ablation properties of ZrB2-ZrC-SiC ultra-high temperature composite ceramic coatings deposited on C/C composites by laser cladding10.3390/coatings13010173 ↗
33. Preparation of UHTCMCs by hybrid processes coupling polymer infiltration and pyrolysis with hot pressing and vice versa10.1016/j.jeurceramsoc.2021.12.039 ↗
34. Properties of Cf/SiC-ZrB2-TaxCy composite produced by reactive hot pressing and polymer impregnation pyrolysis (RHP/PIP)10.1016/j.jeurceramsoc.2019.02.025 ↗
35. Toughening effect of short carbon fibers in the ZrB2-ZrSi2 ceramic composites10.1016/j.matdes.2015.03.006 ↗
36. Oxidation behavior of ZrB2/SiC laminates: effect of composition on microstructure and mechanical strength10.1016/j.jeurceramsoc.2014.12.029 ↗
37. Development of UHTCMCs via water based ZrB2 powder slurry infiltration and polymer infiltration and pyrolysis10.1016/j.jeurceramsoc.2020.05.054 ↗