Effect of the incorporation of graphene reinforcement layers on the microstructure and mechanical properties of AX20 laminated composites processed by accumulative roll bonding
Source abstract
Abstract
To address the limitations and deficiencies of traditional processing technologies, this study achieves the uniform dispersion of graphene nanoplatelets (GNPs) in AX20 magnesium alloy via an innovative electrophoretic deposition (EPD)-accumulative roll bonding (ARB) hybrid process. By synergizing the strengthening effect of GNPs and the microstructure regulation advantage of multi-pass severe plastic deformation (SPD), this work systematically clarifies the interfacial evolution law, grain refinement mechanism, and deformation coordination strengthening mechanism of the composite during ARB processing. Key findings demonstrate that the two-pass GNPs-reinforced composite (ARB-G2) forms a lamellar bimodal microstructure characterized by the coexistence of coarse subgrains and fine dynamically recrystallized grains. Its yield strength reaches 253.19 MPa, which is 20.41% higher than that of the two-pass pure AX20 alloy (ARB-2), while maintaining relatively stable ductility compared to the single-pass GNPs-reinforced sample (ARB-G1). This strength-ductility synergy originates from three core mechanisms: First, GNPs induce grain refinement via the particle-stimulated nucleation (PSN) effect and inhibit grain coarsening. Meanwhile, multi-pass ARB further increases the dislocation density and optimizes the dispersion of GNPs, alleviating the deformation incompatibility between the matrix and the reinforcement. Furthermore, the efficient activation of the pyramidal slip system provides additional deformation degrees of freedom. This study offers a feasible technical route for the controllable preparation of high-performance lightweight magnesium matrix composites.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Enhanced ductility and strength of Mg-1Zn-1Sn-0.3Y-0.2 Ca alloy achieved by novel micro-texture design10.1016/j.scriptamat.2021.114119 ↗
2. Large hardening response mediated by room-temperature dynamic solute clustering behavior in a dilute mg-zn-ca-sn-mn alloy10.1016/j.actamat.2022.118308 ↗
3. Effect of sheet thickness on the microstructural evolution of an Mg AZ61 alloy during large strain hot rolling10.1016/j.scriptamat.2003.11.015 ↗
4. Role of Ca content on microstructure, mechanical properties and strain evolution of as-rolled mg-al-ca-zn-mn alloy10.1016/j.jma.2024.06.010 ↗
5. Effect of heat treatment and severe plastic deformation on the mechanical properties of graphene-reinforced AM60B magnesium alloys
6. High temperature mechanical behavior of AZ61 magnesium alloy reinforced with graphene nanoplatelets10.1016/j.matdes.2015.10.101 ↗
7. Development of graphene nanoplatelet-reinforced AZ91 magnesium alloy by solidification processing10.1007/s11665-018-3391-x ↗
8. Effect of minor additions of graphene and copper on magnesium alloy AZ31 by stir casting
9. Interfacial bonding mechanism of graphene nanoplatelets reinforced AZ91D magnesium alloy prepared by semi-solid injection molding10.1016/j.jallcom.2024.176171 ↗
10. Production of high strength Al–Al2O3 composite by accumulative roll bonding10.1016/j.compositesa.2011.10.015 ↗
11. DIC-based experimental study of fracture toughness through R-curve tests in a multi-layered Al-Mg (LZ91) composite fabricated by ARB10.1016/j.jallcom.2021.160843 ↗
12. Microstructure and mechanical properties of Mg-14Li-1Al/MWCNTs composites prepared by electrophoretic deposition and accumulative roll bonding10.1016/j.jmapro.2021.10.040 ↗
13. Simultaneous achievement of high electromagnetic shielding effectiveness (X-band) and strength in Mg-Li-Zn-Gd/MWCNTs composite10.1016/j.jallcom.2021.160524 ↗
14. Effect of large thickness-reduction on microstructure evolution and tensile properties of Mg-9Al-1Zn alloy processed by hard-plate rolling10.1016/j.jmst.2021.01.050 ↗
15. A comparative study of carbon nanotubes and graphene for metal matrix composites: insights from simulation and experimentation10.1016/j.vacuum.2025.114429 ↗
16. Reinforcement of aluminum metal matrix composites through graphene and graphene-like monolayers: a first-principles study10.1039/D4MA00888J ↗
17. Measurement of the elastic properties and intrinsic strength of monolayer graphene10.1126/science.1157996 ↗
18. Ductility enhancement by activating non-basal slip in as-extruded Mg alloys with dilute Sc addition10.1016/j.jmrt.2022.12.083 ↗
19. Transitions in mechanical behavior and in deformation mechanisms enhance the strength and ductility of Mg-3Gd10.1016/j.actamat.2019.11.034 ↗
20. Estimation of micro-HallPetch coefficients for prismatic slip system in Mg-4Al as a function of grain boundary parameters10.1016/j.actamat.2021.117613 ↗
21. Significant lattice-distortion effect on compressive deformation in Mo-added CoCrFeNi-based high-entropy alloys10.1016/j.msea.2021.142295 ↗
22. Dynamic tensile properties and microstructural evolution of extruded EW75 magnesium alloy at high strain rates10.1016/j.jma.2020.02.013 ↗
23. Achieving high heat-resistant property in dilute Mg-0.2 Ce wrought alloy by retarding recrystallization process10.1016/j.jallcom.2023.170410 ↗
24. Unexpectedly formed strong basal texture in a rolled mg-zn-ca-mn alloy sheet10.1016/j.matchar.2023.113101 ↗
25. Effect of deformation mode on double-peak texture evolution in pre-twinning Mg-3Al-1Zn alloy during high-speed impacting loading10.1016/j.jallcom.2023.172122 ↗
26. Pyramidal slips in high cycle fatigue deformation of a rolled Mg-3Al-1Zn magnesium alloy10.1016/j.msea.2017.05.092 ↗
27. Effect of grain size distribution and texture on the cold extrusion behavior and mechanical properties of AZ31 Mg alloy10.1016/j.msea.2011.01.020 ↗
28. Effects of grain size, texture and twinning on mechanical properties and work-hardening behaviors of pure Mg10.1016/j.msea.2013.04.094 ↗
29. Deformation modes during room temperature tension of fine-grained pure magnesium10.1016/j.actamat.2021.116648 ↗
30. Strength and ductility with {10-11}-{10-12} double twinning in a magnesium alloy10.1038/ncomms11068 ↗
31. Grain size effect on tensile properties and slip systems of pure magnesium10.1016/j.actamat.2020.116604 ↗
32. Effect of grain size on prismatic slip in Mg- 3Al-1Zn alloy10.1016/j.scriptamat.2012.05.017 ↗
33. Evolution of sub-micron grain size and weak texture in magnesium alloy Mg-3Al-0.4Mn by a modified multi-axial forging process10.1016/j.scriptamat.2011.10.008 ↗
34. Influence of texture and grain size on the roomtemperature ductility and tensile behavior in a mg-gd-zn alloy processed by rolling and forging10.1016/j.matdes.2012.04.033 ↗
35. Strengthening in Mg-Li matrix composites10.1016/j.compscitech.2006.10.007 ↗
36. Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al-Li alloys: a review10.1016/j.jare.2017.12.004 ↗
37. Mixed-mode (I and II) fracture behavior of a basal-textured magnesium alloy10.1016/j.actamat.2020.03.023 ↗
38. Tensile fracture prediction of AZ31 cast-rolled sheet based on hot working map10.1016/j.jmrt.2023.01.223 ↗