journal article·2026-03Open access

Effect of phase transformation and porosity formation on the mechanical behavior of continuous wave Nd: YAG laser beam welded Ti–6Al–4V

Isaac Dinaharan, Jebaraj David Raja Selvam, Peter Madindwa Mashinini, Soundararaja Perumal Vigneshwaran

Abstract

Ti–6Al–4V sheets with a thickness of 3 mm were welded using Nd:YAG laser beam welding (LBW). The scanning speed of the laser beam was changed from 3.5 m/min to 6 m/min. The microstructure of the welded region was assessed by various microscopic techniques. The fusion zone geometry exhibited an X shape, and the increase in scanning speed improved the aspect ratio. The heat-affected zone (HAZ) underwent an α′ martensitic phase transformation with a heterogeneous distribution. More ά martensite phase transformation was observed in the fusion zone. Slower scanning speeds produced blocky α phase along with ά martensite. Faster scanning speeds resulted in higher acicular ά martensite. A network of spherical pores was observed. Increased scanning speed reduced pore content. The martensite phase transformation generated a number of dislocations. The weld zone was hardened due to martensite formation. The tensile strength was dictated by both the phase transformation and the porosity content. Faster scanning speed produced joints that matched the base metal strength. The increment in scanning speed changed the fracture mode from brittle to ductile.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Advanced Welding Techniques Analysis · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Experimental realisation of build orientation effects on the mechanical properties of truly as-built Ti-6Al-4V SLM parts10.1016/j.jmapro.2021.01.027 ↗
2. Fundamental investigation into mass transfer process and microstructural transformation pathways in Ti-6Al-4V via underwater wire-laser directed energy deposition
3. Flow behaviour of Ti-6Al-4V alloy in a wide range of strain rates and temperatures under tensile, compressive and flexural loads10.1016/j.ijimpeng.2023.104549 ↗
4. Rapid screening of creep resistance in additive manufactured Ti-6Al-4V alloy10.1016/j.msea.2024.146999 ↗
5. Corrosion resistance improvement of Ti-6Al-4V alloy by anodization in the presence of inhibitor ions10.1016/S1003-6326(22)65917-X ↗
6. Recent advances in Ti-6Al-4V additively manufactured by selective laser melting for biomedical implants: prospect development10.1016/j.jallcom.2021.163072 ↗
7. Micro-crystallographically unraveling strength-enhanced behaviors of the heavy-thick Ti-6Al-4V welded joint10.1016/j.matchar.2022.111893 ↗
8. Gas Tungsten arc welding of Ti-6Al-4V sheet for pressure vessels used in aerospace application: a detailed characterization of weldment10.1016/j.ijpvp.2022.104787 ↗
9. Impression creep behaviour of different zones of pulsed gas tungsten arc welded Ti-6Al-4V alloy
10. Microstructure evolution and mechanical properties of wrought/wire arc additive manufactured Ti-6Al-4V joints by electron beam welding10.1016/j.matchar.2022.112090 ↗
11. Improving fatigue life and toughness in electron beam welded Ti–6Al–4V achieved through beta heat treatment for microstructure uniformity10.1016/j.jmrt.2025.01.055 ↗
12. Numerical simulation of rotary friction welding of Ti-6Al-4V tubes10.1007/s40194-023-01597-1 ↗
13. Heat-pattern induced non-uniform radial microstructure and properties of Ti-6Al-4V joint prepared by rotary friction welding10.1016/j.matchar.2022.112536 ↗
14. Linear friction welding of Ti-6Al-4V alloy fabricated below β-phase transformation temperature10.1016/j.scriptamat.2020.09.013 ↗
15. Effect of the welding parameters on microstructure and mechanical properties of linear friction welded Ti-6Al-4V alloy10.1016/j.jmapro.2022.01.033 ↗
16. Deformation induced microstructure and texture evolution in additively manufactured Ti-6Al-4V sheets via friction stir welding10.1016/j.msea.2025.148043 ↗
17. A specific analytical study of friction stir welded Ti-6Al-4V grade 5 alloy: stir zone microstructure and mechanical properties10.1016/j.jmapro.2022.02.036 ↗
18. A comprehensive review on recent laser beam welding process: geometrical, metallurgical, and mechanical characteristic modeling10.1007/s00170-023-12536-1 ↗
19. A review: suppression of the solidification cracks in the laser welding process by controlling the grain structure and chemical compositions
20. Microstructure and texture evolution of Ti–6Al–4V alloy T-joint fabricated by dual laser beam bilateral synchronous welding10.1016/j.msea.2021.141426 ↗
21. Microstructure and properties of underwater laser welding of TC4 titanium alloy
22. Progress and perspectives of in-situ optical monitoring in laser beam welding: sensing, characterization and modeling10.1016/j.jmapro.2022.01.044 ↗
23. Microstructure and corrosion resistance of fusion zone in Ti-6Al-4V alloy welded using pulsed- and continuous-wave lasers10.1016/j.corsci.2023.111269 ↗
24. Impact of microstructure evolution on the corrosion behaviour of the Ti–6Al–4V alloy welded joint using high-frequency pulse wave laser10.1016/j.jmrt.2023.04.077 ↗
25. Effects of groove clearance size on gap bridging capacity in PWLBW of Ti6Al4V alloy sheet assembled in butt joint configuration: numerical simulation and experimental assessment10.1016/j.optlastec.2022.108527 ↗
26. Effect of ultrasonic rolling on crack propagation behavior of Ti6Al4V titanium alloy laser welded joints
27. Effect of synchronous gas cooling method on microstructure and mechanical properties of laser welded joint for Ti6Al4V titanium alloy
28. Effect of heat treatment on microstructures and properties of vacuum laser welding Ti–6Al–4V titanium alloy10.1016/j.jmrt.2024.04.265 ↗
29. The evolution characteristics of solidification microstructure in laser welding of Ti-6Al-4V titanium alloy by considering transient flow field10.1016/j.optlastec.2023.110195 ↗
30. Unravelling the mechanism of columnar-to-equiaxed transition and grain refinement in ultrasonic vibration assisted laser welding of Ti6Al4V titanium alloy10.1016/j.ultras.2024.107342 ↗
31. Microstructure and mechanical properties of laser welded Ti-6Al-4V (TC4) titanium alloy joints10.1016/j.optlastec.2023.110320 ↗
32. Determination of beam oscillating pattern for tailoring melt flow and microstructural characteristics of laser welded Ti–6Al–4V alloy10.1016/j.ijthermalsci.2024.109156 ↗
33. Microstructure and mechanical properties of Ti6Al4V titanium alloy fiber-diode laser hybrid welded joint10.1016/j.optlastec.2025.113191 ↗
34. Mechanical properties and gradient distributed microstructure of laser welded joints of LPBF/LDED Ti6Al4V alloy10.1016/j.jmapro.2025.03.073 ↗
35. Influence of crystallographic texture on the microstructure, tensile properties and residual stress state of laser-welded titanium joints10.1016/j.matdes.2016.03.148 ↗
36. Parametric optimisation and microstructural analysis on high power Yb-fibre laser welding of Ti–6Al–4V10.1016/j.optlaseng.2016.06.002 ↗
37. Deformation behavior and microstructure characteristics of the laser-welded Ti-6Al-4V joint under variable amplitude fatigue10.1016/j.matchar.2022.112606 ↗
38. Porosity and microstructure in pulsed Nd:YAG laser welded Ti6Al4V sheet10.1016/j.jmatprotec.2014.01.015 ↗
39. Keyhole formation and thermal fluid flow-induced porosity during laser fusion welding in titanium alloys: experimental and modelling10.1016/j.actamat.2016.12.062 ↗
40. Phase transformations during cooling in α + β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
41. Microstructural evolution of fusion zone in laser beam welds of pure titanium10.1016/j.matchar.2011.12.010 ↗