This study investigated the influence of continuous extrusion speed on the microstructure and mechanical properties of Al-4.8Cu-0.45Mn-0.19Cd-0.18Ti-0.17Zr-0.14V alloy wires. By modulating the extrusion speed, the coupled effects of deformation temperature and strain rate on grain structure, dynamic recrystallization (DRX), and texture evolution were examined. The results indicate that as extrusion speed increases, grain size initially decreases and then elevates, with optimal grain refinement observed at 3 rpm. The DRX fraction initially increases then decreases with extrusion speed, peaking at 65% (4 rpm). At 5 rpm, excessive strain rate suppresses recrystallization, reducing the DRX fraction to 27.3%.Texture analysis reveals a transition from deformation textures (Copper and S') to recrystallization (Cube) and shear textures (Goss and T1) with increasing speed. Mechanical testing shows a maximum yield strength of 163 MPa at 3 rpm and a peak elongation of 19.94% at 4 rpm. Quantitative analysis confirms that strength improvements are primarily attributed to grain boundary and fine-grain strengthening, while DRX-induced softening contributes to enhanced ductility.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgy and Material Forming · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Lightweight composite materials in automotive engineering: state-of-the-ar and future trends10.1016/j.aej.2024.12.002 ↗
2. Advanced lightweight materials for automobiles: a review10.1016/j.matdes.2022.110994 ↗
3. High strength aluminum alloys in car manufacturing10.1088/1757-899X/418/1/012033 ↗
4. Experimental analysis of Al-Cu-Si metal matrix composite by powder-metallurgy process
5. Friction stir welding of wire arc additively manufactured 205A aluminum alloy: microstructure and mechanical properties10.1016/j.msea.2023.145154 ↗
6. Investigation of growth behavior of Al-Cu intermetallic compounds in Cu wire bonding10.1016/j.microrel.2010.09.034 ↗
7. Effect of pressure on microstructures and mechanical properties of Al-Cu-based alloy prepared by squeeze casting10.1016/S1003-6326(07)60122-8 ↗
8. Quantifying the effects of Sc and Ag on the microstructure and mechanical properties of Al–Cu alloys
9. The synergistic role of Mn and Zr/Ti in producing θ ′/L12 co-precipitates in Al-Cu alloys10.1016/j.actamat.2020.05.043 ↗
10. Coupled segregation mechanisms of Sc, Zr and Mn at θ′ interfaces enhances the strength and thermal stability of Al-Cu alloys
11. Simultaneous refinement in θ’ precipitation and corrosion behavior of a 2xxx series Al–Cu alloys modified via the sole or joint addition of Cr, Mn and Zr10.1016/j.mtcomm.2024.109578 ↗
12. The effects of Cr addition on microstructure, hardness and tensile properties of as-cast Al–3.8wt.%Cu–(Cr) alloys10.1016/j.jmrt.2020.04.054 ↗
13. Dissimilar friction stir welding of AA2198 and AA7475: effect of solution treatment and aging on the microstructure and mechanical strength10.1016/j.jmapro.2020.07.037 ↗
14. Effects of solution treatment on the microstructure and mechanical properties of naturally aged EN AW 2024 Al alloy sheet10.1016/j.jallcom.2020.153943 ↗
15. Refinement of second-phase particles and grain structures of 2219 Al-Cu alloy forgings using an improved thermomechanical treatment process10.1016/j.matchar.2021.110927 ↗
16. Microstructures and mechanical properties evolution of an Al–Fe–Cu alloy processed by repetitive continuous extrusion forming10.1016/j.msea.2014.06.038 ↗
17. High electrical conductivity Al-Ag-Sc-Zr alloy with ultrafine grains processed by accumulative continuous extrusion10.1016/j.matlet.2020.129227 ↗
18. Microstructure, mechanical properties, and strengthening mechanisms of ultra-high strength Al-Zn-Mg-Cu alloy prepared by continuous extrusion forming process10.1016/j.matdes.2024.112985 ↗
19. Deformation mechanisms and mechanical properties of the high-strength and ductile Al-Zn-Mg-Cu alloys processed by repetitive continuous extrusion forming process with different heat treatments10.1016/j.jallcom.2023.171006 ↗
20. Microstructural evolution and strengthening mechanism of Al–Mg alloys with fine grains processed by accumulative continuous extrusion forming10.1016/j.jmst.2022.03.032 ↗
21. Effect of billet preheating temperature on continuous extrusion forming of Al-Sr alloy10.1016/j.proeng.2017.10.794 ↗
22. Effect of extrusion parameters on microstructure, texture and mechanical property anisotropy of spray deposited 2195 Al–Li alloy profile10.1016/j.msea.2021.141406 ↗
23. Microstructure evolution and mechanical properties of 2196 Al-Li alloy in hot extrusion process
24. Effect of hot extrusion and subsequent T6 treatment on the microstructure evolution and tensile properties of an Al-6Si-2Cu-0.5Mg alloy10.1016/j.msea.2017.10.052 ↗
25. Effects of secondary phase and coarse grain defects on mechanical behavior of near-equiatomic Al alloy during extrusion at different temperatures and speeds10.1016/j.jmrt.2025.02.186 ↗
26. Abnormal grain growth behavior and mechanism of 6005A aluminum alloy extrusion profile10.1016/j.jmst.2023.02.013 ↗
27. Effects of extrusion temperature and extrusion ratio on the microstructure and properties of Mg–5Sn–1Ca alloy prepared by continuous squeeze casting-extrusion process10.1016/j.msea.2024.146360 ↗
28. Influence of extrusion parameters on microstructure, texture, and second-phase particles in an Al-Mg-Si alloy10.1016/j.jmatprotec.2019.03.014 ↗
29. EBSD analysis on restoration mechanism of as-extruded AA2099 Al-Li alloy after various thermomechanical processes10.1016/j.matchemphys.2017.01.044 ↗
30. Texture evolution induced by extrusion parameters and its effect on strengthening-toughening mechanisms of Al-Mg-Si-Cu-Mn alloys10.1016/j.msea.2024.147377 ↗
31. Enhanced fracture toughness in an annealed Al-Cu-Mg alloy by increasing goss/brass texture ratio10.1016/j.matchar.2016.07.015 ↗
32. Fatigue crack growth behavior of X2095 Al–Li alloy10.1016/S0142-1123(99)00087-0 ↗
33. Deformation mechanisms and evolution of grain boundaries in hot extruded heterogeneous Al-Cu-Mg alloys10.1016/j.jallcom.2025.179409 ↗
34. The dynamic recrystallization microstructure characteristics and the effects on static recrystallization and mechanical properties of Al–Mg–Si alloy10.1016/j.msea.2024.146454 ↗
35. Recrystallization behavior and texture evolution during annealing of cryogenic-rolled 3003 aluminum alloy10.1016/j.jallcom.2024.174818 ↗
36. Coincidence site lattice boundary mechanism for the preferred growth of goss and cube grains during annealing in an Al-Cu-Mg alloy10.1016/j.matchar.2018.04.030 ↗
37. Texture evolution in twin-roll strip cast non-oriented electrical steel with strong cube and goss texture10.1016/j.actamat.2020.08.048 ↗
38. Investigating formation behavior of P and goss grains and mechanical properties of Al-Cu-Li alloy via well-designed annealing treatments10.1016/j.msea.2025.147967 ↗
39. The role of goss-oriented texture for brass-type texture in nickel-based metals during cold rolling10.1016/j.mtcomm.2024.110823 ↗
40. Bi-directional dynamic recrystallization behavior of AZ31 alloy by Al-RE precipitation control10.1016/j.ijplas.2025.104289 ↗
41. Grain boundary mobility during recrystallization of copper10.1007/s11661-997-0061-2 ↗
42. Effect of extrusion process on grain structure, texture type and mechanical properties of 2195 Al-Li alloy wire rods10.1016/j.jallcom.2025.178889 ↗
43. Enhanced grain refinement and texture weakening in Al–Mg–Si alloy through a novel thermomechanical processing10.1016/j.jallcom.2022.166654 ↗
44. Current issues in recrystallization: a review10.1016/S0921-5093(97)00424-3 ↗
45. Growth rates and misorientation relationships between growing nuclei/grains and the surrounding deformed matrix during recrystallization10.1016/0956-7151(95)00111-8 ↗
46. Enhanced strength-plasticity combination in an Al–Cu–Mg alloy——atomic scale microstructure regulation and strengthening mechanisms10.1016/j.msea.2020.139447 ↗
47. Hall–Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗