journal article·2025-09Open access

An efficient strategy for evaluating the hydrogen embrittlement via micro-pillar compression in compositional gradient high-strength steel

Heng Dong, Chunlei Shang, Yifei Zha, Yiqun Li, Xilin Xiong, Kewei Gao, Honghui Wu, Rongjian Shi, Xiaolu Pang, Xinping Mao

Abstract

Evaluating the effect of microalloying elements on hydrogen embrittlement (HE) in high-strength steels is essential for material design. In this work, we propose a novel strategy to assess the HE behavior of compositional gradient high-strength steels using micro-pillar compression tests. Experimental results reveal that hydrogen significantly influences the mechanical properties of the micropillars with different solid solution alloying elements. Specifically, V exhibits optimal HE resistance at approximately 0.2 wt%, while Cr and Mo reflect an increase in HE resistance with increasing concentrations within in the 0–0.6 wt% range. These findings provide a new perspective for the composition optimization of HE-resistant high-strength steels, suggesting that the microscale HE evaluation method could guide the design of high-strength HE-resistant materials.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Atomic-scale investigation of deep hydrogen trapping in NbC/α-Fe semi-coherent interfaces10.1016/j.actamat.2020.09.031 ↗
2. Observation of hydrogen trapping at dislocations,grain boundaries, and precipitates10.1126/science.aaz0122 ↗
3. Direct observation of hydrogen-trapping sites in vanadium carbide precipitation steel by atom probe tomography10.1016/j.scriptamat.2012.04.022 ↗
4. Effect of niobium precipitation behavior on microstructure and hydrogen induced cracking of press hardening steel 22MnB510.1016/j.msea.2018.02.021 ↗
5. Effect of V–Ti multi-microalloying on enhancing hydrogen embrittlement resistance in hot-stamping steel10.1016/j.jmrt.2024.10.232 ↗
6. Effects of Ti alloying on resistance to hydrogen embrittlement in (Nb+Mo)-alloyed ultra-high-strength hot-stamping steels10.1016/j.msea.2020.139763 ↗
7. Effect of alloy element on hydrogen-induced grain boundary embrittlement in BCC iron10.1016/j.jmrt.2024.11.264 ↗
8. Effect of Mo addition on hydrogen segregation at α-Fe grain boundaries: a first-principles investigation of the mechanism by which Mo addition improves hydrogen embrittlement resistance in high-strength steels10.1016/j.commatsci.2022.111951 ↗
9. Effects of solid solution and grain-boundary segregation of Mo on hydrogen embrittlement in 32MnB5 hot-stamping steels10.1016/j.actamat.2021.116661 ↗
10. Effect of Mo on intergranular corrosion behavior in super-austenitic stainless steel10.1016/j.corsci.2024.111986 ↗
11. Effect of vanadium on hydrogen embrittlement susceptibility of high-strength hot-stamped steel10.1007/s42243-020-00469-y ↗
12. Effects of vanadium carbides on hydrogen embrittlement of tempered martensitic steel10.1007/s12540-016-5631-7 ↗
13. Effect of V/Mo ratio on the evolution of carbide precipitates and hydrogen embrittlement of tempered martensitic steel10.1016/j.corsci.2020.108929 ↗
14. On the suitability of slow strain rate tensile testing for assessing hydrogen embrittlement susceptibility10.1016/j.corsci.2019.108291 ↗
15. Limitations of the slow strain rate test for stress corrosion cracking testing
16. Effect of the loading mode and temperature on hydrogen embrittlement behavior of 15Cr for steam turbine last stage blade steel10.1016/j.ijhydene.2022.10.061 ↗
17. Comparison of constant load, SSRT and CSRT methods for hydrogen embrittlement evaluation using round bar specimens of high strength steels10.2355/isijinternational.ISIJINT-2015-565 ↗
18. Development of a methodology to study the hydrogen embrittlement of steels by means of the small punch test10.1016/j.msea.2014.12.083 ↗
19. Small punch test methodologies for the analysis of the hydrogen embrittlement of structural steels10.1016/j.tafmec.2016.09.005 ↗
20. Establishment of an in-situ small punch test method for characterizing hydrogen embrittlement behaviors under hydrogen gas environments and new influencing factor10.1016/j.ijhydene.2019.07.029 ↗
21. The role of the testing rate on Small Punch tests for the estimation of fracture toughness in hydrogen embrittlement10.1016/j.prostr.2020.10.024 ↗
22. Hydrogen microprint technique in the study of hydrogen in steels10.1007/BF00556094 ↗
23. Quantitative evaluation of detection efficiency of the hydrogen microprint technique applied to steel10.1016/S0010-938X(02)00218-4 ↗
24. Examination of hydrogen embrittlement in FeAl by means of in situ electrochemical micropillar compression and nanoindentation techniques10.1016/j.intermet.2010.01.001 ↗
25. Influence of hydrogen on the deformation morphology of vanadium (100) micropillars in the α-phase of the vanadium–hydrogen system10.1016/j.scriptamat.2012.09.020 ↗
26. Hydrogen-enhanced deformation in pearlite10.1016/j.actamat.2024.120327 ↗
27. Hydrogenated vacancies lock dislocations in aluminium10.1038/ncomms13341 ↗
28. The diffusion-multiple approach to designing alloys10.1146/annurev.matsci.35.100303.111314 ↗
29. Compressive behaviour of carbon fibres micropillars by in situ SEM nanocompression10.1016/j.compositesa.2023.107699 ↗
30. Effect of Cr on the phase transformation and interphase nanoprecipitation behaviours of high-strength microalloyed steels10.1016/j.matchar.2023.113504 ↗
31. Strengthening mechanisms in vanadium-microalloyed medium-Mn steels
32. Enhancing the hydrogen embrittlement resistance with cementite/VC multiple precipitates in high-strength steel10.1016/j.msea.2023.145084 ↗
33. Quantification of hydrogen trapping in multiphase steels: Part I – point traps in martensite10.1016/j.actamat.2020.05.007 ↗
34. Effect of crystallographic orientations on the hydrogen-induced cracking resistance improvement of API 5L X70 pipeline steel under various thermomechanical processing10.1016/j.corsci.2016.05.003 ↗
35. Dual role of nanosized NbC precipitates in hydrogen embrittlement susceptibility of lath martensitic steel10.1016/j.corsci.2019.108345 ↗
36. Effect of Nb on the hydrogen-induced cracking of high-strength low-alloy steel10.1016/j.corsci.2018.04.041 ↗
37. A new understanding of intergranular stress corrosion cracking resistance of pipeline steel through grain boundary character and crystallographic texture studies10.1016/j.corsci.2008.10.006 ↗
38. Direct observation of individual hydrogen atoms at trapping sites in a ferritic steel10.1126/science.aal2418 ↗
39. Atomic-scale insights on hydrogen trapping and exclusion at incoherent interfaces of nanoprecipitates in martensitic steels10.1038/s41467-022-31665-x ↗
40. Effect of Laves-decorated dendrite structure on hydrogen embrittlement in selective laser-melted nickel-based alloy10.1016/j.jmst.2025.03.051 ↗
41. High-throughput evaluation of alloying effect on hydrogen diffusion of ultra-high strength steel10.1016/j.scriptamat.2025.116791 ↗
42. Improving the hydrogen embrittlement resistance by straining the ferrite/cementite interfaces10.1016/j.actamat.2024.119850 ↗
43. Probing the effect of solute hydrogen and hydrides on the prismatic slip of [21‾1‾0]-orientated alpha titanium using in-situ micropillar compression10.1016/j.scriptamat.2025.116859 ↗
44. Effect of hydrogen on deformation behavior of Alloy 725 revealed by in-situ bi-crystalline micropillar compression test10.1016/j.jmst.2020.08.006 ↗
45. Hydrogen trapping and embrittlement in metals – a review
46. Effects of size on the mechanical response of metallic glasses investigated through in situ TEM bending and compression experiments10.1016/j.actamat.2009.08.070 ↗
47. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
48. Designing hydrogen embrittlement-resistant grain boundary in steel by alloying elements segregation: first-principles calculations10.1016/j.apsusc.2024.159684 ↗