journal article·2025-05Open access

Wetting behavior and interfacial reactions of Cu–20Sn–2Cr alloy on various carbon substrates

Wenjuan Ci, Likai Yang, Qiaoli Lin, Yu Shi

Abstract

The effect of different carbon sources (CS) and the underlying mechanisms on wetting behavior, interfacial reaction products, and spreading kinetics at the reactive wetting interface between Cu-based alloys and carbon materials during brazing and composites preparation remain unclear. This study investigates the reactive wetting behavior of a Cu–20Sn–2Cr alloy on various carbon substrates (graphite (C gr ), polycrystalline diamond (C PD ), vitreous carbon (C V ), and multi-walled carbon nanotubes Bucky paper (C MW )) at 1100 °C using a modified sessile drop method. The results indicate the equilibrium contact angle ( θ e ) of C gr (7°), C PD (8°), and C V (11°) are close to each other, whereas the θ e values of C MW-back (83°) and C MW-front (69°) are higher. The reaction product layer (RPL) in C gr , C PD , and C V consists of a continuous and dense chromium carbides (Cr m C n ); the interface of C MW exhibit an “alloy + nanoscale Cr 3 C 2 cluster" transition zone. The spreading kinetics of C gr , C PD and C MW are controlled diffusion of Cr atoms to the triple line (TL) front, while Cv is controlled first by the diffusion of Cr atoms to the TL front, then is controlled by the reaction between Cr and C atoms at the TL front.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced materials and composites · Electronic Packaging and Soldering Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (89)

Show source-provided references
1. Graphite and carbon powders for electrochemical applications10.1016/j.jpowsour.2006.02.064 ↗
2. A review on application of carbonaceous materials and carbon matrix composites for heat exchangers and heat sinks10.1016/j.ijrefrig.2011.09.001 ↗
3. Wettability and interface reaction of Sn–Cr powder alloy on poly-crystalline diamond (PCD)10.1088/1757-899X/423/1/012063 ↗
4. Naidich · 2007
5. Evolution of glassy carbon under heat treatment: correlation structure–mechanical properties10.1007/s10853-017-1753-7 ↗
6. A review on the use of glassy carbon in advanced technological applications10.1016/j.carbon.2021.10.022 ↗
7. Copper/carbon nanotube composites: research trends and outlook10.1098/rsos.180814 ↗
8. Carbon nanotube reinforced metal matrix composites – a review10.1179/095066009X12572530170543 ↗
9. Interface structure and strengthening behavior of graphene/CuCr composites10.1016/j.carbon.2018.03.018 ↗
10. Graphene reinforced metal and ceramic matrix composites: a review10.1080/09506608.2016.1219481 ↗
11. Wear and mechanical properties of carbon fiber reinforced copper alloy composites10.1016/j.matchar.2008.10.008 ↗
12. Pre-infiltration and brazing behaviors of Cf/C composites with high temperature TiSi eutectic alloy10.1016/j.carbon.2018.08.021 ↗
13. Inagaki · 2014
14. Chapter 9 – adsorbent storage for natural gas vehicles
15. Carbon science in 2016: status, challenges and perspectives10.1016/j.carbon.2015.11.060 ↗
16. Recent applications of carbon-based composites in defence industry: a review10.1016/j.dt.2022.03.006 ↗
17. A review of processing of Cu/C base plate composites for interfacial control and improved properties10.1088/2631-7990/ab61c5 ↗
18. Review of recent development in copper/carbon composites prepared by infiltration technique10.3390/en15145227 ↗
19. The role of van der Waals interactions on wetting and adhesion in metal/carbon systems10.1016/S1359-6462(99)00082-2 ↗
20. Diamond–metal interfaces in cutting tools: a review10.1007/s10853-011-6164-6 ↗
21. The wetting of carbon by copper and copper alloys10.1007/BF00554633 ↗
22. Effect of Cr on the wetting in Cu/graphite system10.1016/j.apsusc.2011.02.060 ↗
23. Reaction layer formation at the graphite/copper-chromium alloy interface10.1007/BF02669602 ↗
24. Wetting of graphite by molten Cu–xSn–yCr ternary alloys at 1373 K10.1016/j.carbon.2019.12.097 ↗
25. A new method of wettability measurement utilizing a small sample and its application to graphite or ALPHA–SiC and liquid Cu–Cr alloy systems10.2355/isijinternational.30.64 ↗
26. Investigation of the wetting of diamond and graphite by molten metals and alloys V. Carbide-formation kinetics at the graphite/metallic melt interface10.1007/BF00774308 ↗
27. Interaction between Ti or Cr containing copper alloys and porous graphite substrate
28. Mechanisms of reactive wetting: the question of triple line configuration10.1016/S1359-6454(96)00372-2 ↗
29. Diffusion-limited reactive wetting: study of spreading kinetics of Cu–Cr alloys on carbon substrates10.1016/S1359-6454(99)00008-7 ↗
30. Wettability of carbon by aluminum and aluminum alloys10.1016/S0921-5093(98)00759-X ↗
31. Wetting behavior and reactivity between AlTi6 alloy and carbon nanotubes10.1007/s11665-016-1919-5 ↗
32. Interaction between porous graphite substrate and liquid or semi-liquid aluminum alloys containing titanium10.4028/www.scientific.net/MSF.217-222.153 ↗
33. Wetting of molten cerium on typical carbon materials (graphite, CVD-diamond and NWCNT) and molten Cu–Ce alloys on graphite at 950 °C10.1016/j.jre.2020.02.021 ↗
34. Wettability characteristics of metal melts on graphite and glasslike carbon substrates and their relation to catalytic graphitization
35. The wetting and bonding of diamonds by copper-base binary alloys10.1007/BF00754470 ↗
36. Wetting behavior of graphite and CFC composites by Cu–Ti compacts10.1007/s11595-018-1782-3 ↗
37. Effect of matrix carbon species on interface wetting behavior of C/Cu composites
38. The wetting of alumina and vitreous carbon by copper-tin-titanium alloys10.1007/BF00553207 ↗
39. Reaction and wetting between molten Cu–Ti alloy and graphite
40. Reactive spontaneous infiltration and spreading wetting of graphite by Cu–aTi (a = 17, 34, 68 at. %) alloys at 1100 °C10.1016/j.vacuum.2024.113417 ↗
41. The wettability and interface thermal resistance of copper/graphite system with an addition of chromium10.1016/j.matchemphys.2011.03.003 ↗
42. The nature of the chemical bond in the carbides and nitrides of d metals10.1007/BF00518445 ↗
43. Carbide stoichiometry in TiCx and Cu–TiCx produced by self-propagating high-temperature synthesis, Scr
44. Enhanced mass transport in titanium carbide at large departures from stoichiometry, powder
45. Effect of reactant C/Ti ratio on the stoichiometry, morphology of TiCx and mechanical properties of TiCx–Ni composite10.1039/C2CE26767E ↗
46. A common regularity of stoichiometry-induced morphology evolution of transition metal carbides, nitrides, and diborides during self-propagating high-temperature synthesis10.1021/cg201604z ↗
47. Structure and properties of nanocrystalline TiC full-density bulk alloy consolidated from mechanically reacted powders10.1016/S0925-8388(00)00692-7 ↗
48. Characterization of a silicon carbide thin layer prepared by a self-propagating high temperature synthesis reaction10.1016/S0040-6090(00)01266-9 ↗
49. Microstructure and tribological properties of in-situ TiC–C/Cu nanocomposites synthesized using different carbon sources (graphite, carbon nanotube and graphene) in the Cu–Ti–C system10.1016/j.ceramint.2018.08.316 ↗
50. The combined effect of porosity and reactivity of the carbon preforms on the properties of SiC produced by reactive infiltration with liquid Si10.1016/j.carbon.2009.04.002 ↗
51. Interfacial microstructures and mechanical integrity of synthetic diamond brazed by a low-temperature Cu–Sn–Cr filler alloy10.1016/j.diamond.2019.107440 ↗
52. Microstructure and dry sliding wear behavior of Cu–Sn alloy reinforced with multiwalled carbon nanotubes10.1016/S1003-6326(16)64269-3 ↗
53. Microstructure, residual stresses and shear strength of diamond–steel–joints brazed with a Cu–Sn–based active filler alloy10.1016/j.ijrmhm.2011.06.006 ↗
54. Enhanced mechanical and current-carrying wear performances of copper/carbon-matrix composites via interfacial reaction of chromium10.1007/s10853-022-08067-x ↗
55. Enhanced wetting and properties of carbon/carbon–Cu composites with Cr3C2 coatings by Cr–solution immersion method10.1016/j.jmst.2017.01.028 ↗
56. The anomalous dispersion of the disorder-induced and the second-order Raman bands in carbon nanotubes10.1590/S0103-97332000000200026 ↗
57. Characterization of diamond films by Raman spectroscopy10.1557/JMR.1989.0385 ↗
58. Origin of dispersive effects of the Raman D band in carbon materials10.1103/PhysRevB.59.R6585 ↗
59. Interpretation of Raman spectra of disordered and amorphous carbon10.1103/PhysRevB.61.14095 ↗
60. Study of carbon nanotubes in Cu–Cr metal matrix composites10.1007/s11665-012-0198-z ↗
61. Wetting of TiC by molten Al at 1123–1323 K, acta
62. Effects of temperature on reaction path, spreading and wetting mechanism of Cu–20Sn–2Cr/graphite10.1016/j.ceramint.2023.09.021 ↗
63. Chapter 1 – characterization of carbon nanomaterials by Raman spectroscopy
64. Chapter 18 – Raman spectroscopy as a characterization tool for carbon materials
65. Structural evolution in glassy carbon investigated based on the temperature dependence of Young's modulus10.3390/ma16134794 ↗
66. Characterization of carbon nanotubes by Raman spectroscopy
67. Initial damage in graphite under ion irradiation studied by real-time Raman measurement10.1016/0022-3115(92)90785-J ↗
68. Reactive wetting in the liquid-silicon/solid-carbon system10.1111/j.1151-2916.1996.tb08519.x ↗
69. First-principles study of structural, elastic, and electronic properties of chromium carbides10.1063/1.2838345 ↗
70. Investigation of chromium carbide/alumina nano-composite prepared via MOCVD in fluidized bed and densification process10.1016/j.mseb.2005.09.006 ↗
71. Nucleation and growth of Cr7C3 at interface of brazed dia mond with Ni–Cr alloy under protective atmosphere
72. Diamond nanoparticles to carbon onions transformation: X–ray diffraction studies10.1016/S0008-6223(01)00311-6 ↗
73. Scherrer · 1912 · 387
74. Eustathopoulos · 1999
75. Dynamics of wetting in reactive metal/ceramic systems
76. Interface characterisation and wettability properties of carbon particle reinforced copper alloy10.1039/b003836i ↗
77. Epitaxial growth of chromium carbide nanostructures on multiwalled carbon nanotubes (MWCNTs) in MWCNT–copper composites10.1016/j.actamat.2012.10.022 ↗
78. Improvement of interface and mechanical properties in carbon nanotube reinforced Cu–Cr matrix composites10.1016/j.matdes.2012.09.027 ↗
79. Wetting under chemical equilibrium and nonequilibrium conditions10.1021/j100605a009 ↗
80. Croissance et structure des couches minces
81. Wettability and interface reaction of Sn-Cr powder alloy on poly-crystalline diamond (PCD)
82. Resistance of solid surfaces to wetting by water10.1021/ie50320a024 ↗
83. Knowledge about polymer surfaces from contact angle measurements10.1016/0001-8686(90)80012-O ↗
84. Weast · 1990
85. Diffusion in copper and copper alloys. Part III. Diffusion in systems involving elements of the groups IA, IIA, IIIB, IVB, VB, VIB, and VIIB10.1063/1.555516 ↗
86. Modelling kinetics of diffusion controlled reactive wetting: the role of reaction behind the triple line10.4028/www.scientific.net/SSP.72.91 ↗
87. Chemical reaction-limited spreading: the triple line velocity versus contact angle relation10.1016/S1359-6454(02)00309-9 ↗
88. Interfacial Si–O coordination for inhibiting the graphite phase enables superior SiC/Nb heterostructure joining by AuNi10.1016/j.compositesb.2024.111557 ↗
89. Wetting of molten cerium on typical carbon materials (graphite, CVD-diamond and NWCNT) and molten Cu–Ce alloys on graphite at 950 °C10.1016/j.jre.2020.02.021 ↗